Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "FE" wg kryterium: Temat


Tytuł:
FePt3 nanosuspension synthesized from different precursors – a morphological comparison by SAXS, DLS and TEM
Autorzy:
Sarmphim, P.
Soontaranon, S.
Sirisathitkul, C.
Harding, P.
Kijamnajsuk, S.
Chayasombat, B.
Pinitsoontorn, S.
Chingunpitak, J.
Powiązania:
https://bibliotekanauki.pl/articles/201918.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
magnetic nanosuspension
Fe(acac)3
Fe(hfac)3
DLS
TEM
SAXS
Fe (acac) 3
Fe (hfac) 3
Opis:
Annealed iron-platinum (FePt) is ferromagnetic in a nanoscale regime which is necessary for energy and data storage, whereas the as-synthesized form of FePt-based nanoparticles exhibits superparamagnetism useful for biomedical applications. In this study, as-synthesized nanosuspensions from the reaction of Pt(acac)2 with Fe(acac)3 and Fe(hfac)3 are compared. X-ray diffraction (XRD) peaks for both samples are assigned to the FePt3 phase. As shown by transmission electron microscopy (TEM) and small angle X-ray scattering (SAXS), nanoparticles synthesized by using Fe(acac)3 have a smaller average diameter, but larger polydispersity index and particle agglomerations. On the other hand, the nanoparticles synthesized by using Fe(hfac)3 can self-assemble into a longer range of patterned monolayer. Dynamic light scattering (DLS), measuring the size of cluster of nanoparticles as well as oleic acid and oleylamine at their surface, confirms that larger agglomerations in the sample were synthesized by using Fe(acac)3. In addition to the size distribution, magnetic properties were influenced by the composition of these nanoparticles.
Źródło:
Bulletin of the Polish Academy of Sciences. Technical Sciences; 2017, 65, 1; 79-84
0239-7528
Pojawia się w:
Bulletin of the Polish Academy of Sciences. Technical Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 1: Fe-B-Cr
Opis termodynamiczny trójskładnikowych układów Fe-B-X. Część 1: Fe-B-Cr
Autorzy:
Miettinen, J.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/353802.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-Cr system
diagramy fazowe
modelowanie termodynamiczne
układy na bazie Fe
termodynamiczne układy Fe-B-X
układ Fe-B-Cr
Opis:
A thermodynamic description of the Fe-B-Cr system is developed in the context of a new Fe-B-X (X = Cr, Ni, Mn, Si, Ti, V, C) database. The thermodynamic parameters of the binary sub-systems, Fe-B, Fe-Cr and B-Cr, are taken from earlier assessments slightly modifying the Fe-B and B-Cr descriptions, and those of the ternary system are optimized in this study using experimental thermodynamic and phase equilibrium data from the literature. The solution phases are described using substitutional solution model. The borides are treated as stoichiometric or semi-stoichiometric phases and described with two-sublattice models.
Przedstawiono termodynamiczny opis trójskładnikowego układu Fe-B-Cr w kontekście bazy danych dla układów Fe-B-X (X = Cr, Ni, Mn, Si, Ti, V, C). Parametry termodynamiczne dwuskładnikowych stopów Fe-Mn, Fe-B i Mn-B zostały są zaczerpnięte z wcześniejszych opracowań, przy tym opisy Fe-B i B-Cr zostały nieznacznie zmodyfikowane. Parametry dla układu Fe-Mn-B zostały zoptymalizowane w tej pracy w oparciu o eksperymentalne równowagi fazowe i dane termodynamiczne zaczerpnięte z literatury. Roztwory stałe opisano przy użyciu modelu roztworu substytucyjnego, a borki traktowane są jako fazy stechiometryczne lub półstechiometryczne opisane przy użyciu modelu dwu podsieci.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 2; 601-607
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 8: Fe-B-Mo, with Extension to Quaternary Fe-B-Cr-Mo System
Autorzy:
Miettinen, Jyrki
Visuri, Ville-Valtteri
Fabritius, Timo
Powiązania:
https://bibliotekanauki.pl/articles/2049544.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modeling
thermodynamic database
Fe-based systems
Fe-B-X systems
Fe-B-Mo system
Fe-B-Cr-Mo system
Opis:
Thermodynamic optimizations of the ternary Fe-B-Mo system and its binary sub-system B-Mo are presented. The Fe-B-Mo description is then extended to the quaternary Fe-B-Cr-Mo system by assessing the ternary B-Cr-Mo system. The thermodynamic descriptions of the other binaries (Fe-B, Fe-Cr, Fe-Mo, B-Cr, and Cr-Mo) and the other ternaries (Fe-B-Cr and Fe-Cr-Mo) are taken from earlier studies. In this study, the adjustable parameters of the B-Mo, Fe-B-Mo, and B-Cr-Mo systems were optimized using the experimental thermodynamic and the phase equilibrium data from the literature. The solution phases of the system (liquid, bcc and fcc) are described with the substitutional solution model, and most borides are treated as stoichiometric phases or semistoichiometric phases, using a simple two-sublattice model for the latter. The system’s intermetallic phases, Chi, Mu, R, and Sigma (not dissolving boron) as well as boride M3B2, based on a formulation of (Cr,Fe)(Cr,Fe,Mo)2(B)2, are described with a three-sublattice model. Reasonable agreement is obtained between the calculated and measured phase equilibria in all four systems: B-Mo; Fe-B-Mo; B-Cr-Mo; and Fe-B-Cr-Mo.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 1; 281-295
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The influence of heat treatment on point defect concentration in Fe-Al and Fe-Al-Cr systems
Autorzy:
Kansy, J.
Hanc, A.
Giebel, D.
Powiązania:
https://bibliotekanauki.pl/articles/146336.pdf
Data publikacji:
2010
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
positron annihilation
Fe-Al
Fe-Al-Cr
point defects
Opis:
FeAl alloys of nominal Al content 28, 38 and 45 at.% and Fe28Al5Cr with minor alloying elements added to improve their application properties are studied by positron annihilation lifetime analysis. The lifetime spectra of samples FeXAl with X greater-than or equal to 38 (both quenched and cooled with furnace) are described by a single lifetime component related to the saturated positron trapping by quenched-in vacancies of concentration much higher than 100 ppm. A very strong dependence of retained vacancy concentration on the rate of cooling is shown for Fe28Al and Fe28Al5Cr alloys. After quenching, the concentration is of the order of 10.4 whereas in samples slowly cooled it is reduced to 10.5. The chromium addition to Fe28Al5Cr dismisses the vacancies concentration in comparison to the concentration in Fe28Al after the same heat treatment.
Źródło:
Nukleonika; 2010, 55, 1; 21-25
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 3: Fe-B-Mn
Opis termodynamiczny trójskładnikowych układów Fe-B-X. Część 3: Fe-B-Mn
Autorzy:
Miettinen, J.
Lilova, K.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/353752.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-Mn system
diagramy fazowe
modelowanie termodynamiczne
systemy na bazie Fe
termodynamiczny system Fe-B-X
system Fe-B-Mn
Opis:
A thermodynamic optimization of the ternary Fe-B-Mn system is presented. The thermodynamic parameters of the binary sub-systems, Fe-Mn, Fe-B and B-Mn, are taken from earlier assessments slightly modifying the B-Mn system description. The thermodynamic parameters of the Fe-B-Mn system are optimized in this study using literature experimental thermodynamic and phase equilibrium data. The solution phases of the system are described using the substitutional solution model and the borides are treated as stoichiometric or semi-stoichiometric phases of the (A,B)pCq type described with the two-sublattice models.
Przedstawiono termodynamiczny opis trójskładnikowego układu Fe-B-Mn. Parametry termodynamiczne dwuskładnikowych stopów Fe-Mn, Fe-B i B-Mn zostały zaczerpnięte z wcześniejszych opracowań, przy tym opis układu B-Mn został nieznacznie zmodyfikowany. Parametry termodynamiczne dla układu Fe-B-Mn zostały zoptymalizowane w tej pracy w oparciu o eksperymentalne równowagi fazowe i dane termodynamiczne zaczerpnięte z literatury. Roztwory stałe w układzie Fe-B-Mn opisano przy użyciu modelu roztworu substytucyjnego, a borki traktowane sa jako fazy stechiometryczne lub półstechiometryczne typu (A,B)pCq opisane przy użyciu modelu dwu podsieci.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1481-1485
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description Of Ternary Fe-B-X Systems. Part 2: Fe-B-Ni
Autorzy:
Miettinen, J.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/353480.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-Ni system
diagramy fazowe
modelowanie termodynamiczne
układy na bazie Fe
termodynamiczne układy Fe-B-X
układ Fe-B-Ni
Opis:
Opis termodynamiczny trójskładnikowych układów Fe-B-X. Część 2: Fe-B-Ni
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 2; 609-614
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 4: Fe-B-V
Autorzy:
Miettinen, J.
Visuri, V.-V.
Fabritius, T.
Milcheva, N.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/355188.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-V system
Opis:
Thermodynamic descriptions of the ternary Fe-B-V system and its binary sub-system B-V, are developed using experimental thermodynamic and phase equilibrium data from the literature. The thermodynamic parameters of the other binaries, Fe-V and Fe-B, are taken from earlier assessments slightly modifying the Fe-V description. The work is in the context of a new Fe-B-X (X = Cr, Ni, Mn, V, Si, Ti, C) database. The solution phases are described using substitutional solution model. The borides are treated as stoichiometric or semistoichiometric phases and described with two-sublattice models.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 2; 451-456
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Rare earth elements in Fe-Mn nodules from southern Baltic Sea – a preliminary study
Pierwiastki ziem rzadkich w konkrecjach Fe-Mn z południowego Bałtyku – badania wstępne
Autorzy:
Szamałek, K.
Uścinowicz, S.
Zglinicki, K.
Powiązania:
https://bibliotekanauki.pl/articles/2061649.pdf
Data publikacji:
2018
Wydawca:
Państwowy Instytut Geologiczny – Państwowy Instytut Badawczy
Tematy:
konkrecje Fe-Mn
Bałtyk
REE
Fe-Mn nodules
Baltic Sea
Opis:
Between 1976–1990, the Polish Geological Institute performed geological works in the Polish Maritime Areas. During these works, 260 occurrences of concretions were recorded from 7,500 sampled sites. In 1980, the threshold that separates the Bornholm Basin from the Słupsk Furrow was mapped. Numerous Fe-Mn nodules on the seabed were found in that area. The results of detailed analyses of nodule samples collected from four sites are presented in this paper. Analyzed nodules represent discoidal D, irregular I, and transitional D-I types. The nodules are characterized by varied chemical composition of main oxides (Fe, Mn). The maximum Fe2O3 content is 26.63% and MnO 23.18%. Total average amount of REE + Y in the samples is approximately 165.11 ppm, ΣLREE 145.72 ppm and ΣHREE 19.39 ppm. The LREE content is enriched in comparison to HREE. The majority of nodules consist of Fe-Mn oxy-hydroxide minerals with very low crystallinity (practically amorphous phases). The main confirmed Mn-phases are birnessite and todorokite. Other main components of the nodules are: detrital quartz, albite, microcline, glauconite and muscovite, clinochlore, and clay minerals: illite and chlorite. The rate of growth of Fe-Mn nodules has been estimated using a cobalt chronometer. The nodule growth rate ranges from 0.006 to 0.134 mm/yr –1. Based on the Fe, Mn and (Cu + Co + Ni) contents, the origin of studied nodules is determined as hydrogenetic, while using REE (Cesn/Cesn • vs. Nd) – as diagenetic.
W latach 1976–1990 Państwowy Instytut Geologiczny realizował prace geologiczne na Polskich Obszarach Morskich. Opróbowano 7500 miejsc, a w 260 stwierdzono występowanie konkrecji. W roku 1980 prace kartograficzne prowadzono m.in. na obszarze progu oddzielającego Basen Bornholmski od Rynny Słupskiej, gdzie stwierdzono występowanie licznych konkrecji Fe-Mn. W niniejszym artykule są prezentowane wyniki analiz konkrecji pobranych na 4 stanowiskach. Badania dotyczą konkrecji następujących typów: dyskoidalnych D, nieregularnych I oraz przejściowych D-I. Badane konkrecje charakteryzują się zmiennym składem głównych tlenków (Fe, Mn). Maksymalna zawartość Fe2O3 wynosi 26,63%, a MnO 23,18%. Łączna średnia zawartość REE + Y w badanych próbkach jest na poziomie 165,11 ppm, ΣLREE – 145,72 ppm i ΣHREE – 19,39 ppm. Zauważalne jest wzbogacenie w LREE w porównaniu do HREE. Konkrecje w większości są zbudowane z tlenków i wodorotlenków Fe i Mn o bardzo niskim stopniu krystaliczności (praktycznie fazy mineralne są amorficzne). Głównymi potwierdzonymi fazami manganu są birnessyt i todorokit. Pozostałymi głównymi składnikami konkrecji są: kwarc terygeniczny, albit, mikroklin, glaukonit i muskowit, klinochlor, minerały ilaste: illit, chloryt. Wartość tempa wzrostu w badanych konkrecjach, określona z użyciem chronometru kobaltowego, wynosi od 0,006 do 0,134 mm/yr –1. Na podstawie zawartości Fe, Mn oraz (Cu + Co + Ni) badane konkrecje określono jako hydrogeniczne, podczas gdy używając zależności REE (Cesn/Cesn • vs. Nd) jako diagenetyczne.
Źródło:
Biuletyn Państwowego Instytutu Geologicznego; 2018, 472; 199--212
0867-6143
Pojawia się w:
Biuletyn Państwowego Instytutu Geologicznego
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 9: Fe-B-Cu
Autorzy:
Miettinen, Jyrki
Visuri, Ville-Valtteri
Fabritius, Timo
Powiązania:
https://bibliotekanauki.pl/articles/2049545.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
thermodynamic database
Fe-based systems
Fe-B-X systems
Fe-B-Cu system
Opis:
Thermodynamic descriptions of the ternary Fe-B-Cu system and its binary sub-system B-Cu aredeveloped in the context of a new Fe-B-X (X = Cr, Cu, Mn, Mo, Ni, Si, Ti, V, C) database. The thermodynamic parameters of the other binary sub-systems (Fe-B and Fe-Cu) are taken from earlier assessments. Experimental thermodynamic and phase equilibrium data available in the literature have been used for the optimization of the Fe-B-Cu and B-Cu systems’ thermodynamic parameters. The solution phases are described using a substitutional solution model and the compounds (two borides of the Fe-B system) are treated as stoichiometric phases. A good agreement was obtained between the calculated and the experimental thermodynamic and phase equilibrium data.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 1; 297-304
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 5: Fe-B-Si
Autorzy:
Miettinen, J.
Visuri, V.-V.
Fabritius, T.
Milcheva, N.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/355656.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modeling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-Si system
Opis:
Thermodynamic descriptions of the ternary Fe-B-Si system and its binary sub-system, B-Si, are developed in the context of a new Fe-B-X (X = Cr, Ni, Mn, V, Si, Ti, C) database. The thermodynamic parameters of the other binary sub-systems, Fe-Si and Fe-B, are taken from earlier assessments. Experimental thermodynamic and phase equilibrium data available in the literature has been used for the optimization of the thermodynamic parameters of the Fe-B-Si and B-Si systems. The solution phases are described using substitutional solution model and the compounds (silicides and borides) are treated as stoichiometric phases. The calculated and experimental thermodynamic and phase equilibrium data were found to be in good agreement.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 4; 1239-1248
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 6: Fe-B-Ti
Autorzy:
Miettinen, J.
Visuri, V.-V.
Fabritius, T.
Milcheva, N.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/356115.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modeling
Fe-based systems
Fe-B-X systems thermodynamic database
Fe-B-Ti system
Opis:
Thermodynamic optimizations of the ternary Fe-B-Ti system and its binary sub-system, B-Ti are presented. The thermodynamic descriptions of the other binaries, Fe-Ti and Fe-B, are taken from the earlier studies slightly modifying the Fe-Ti system assessment. The adjustable parameters of the Fe-B-Ti and B-Ti systems are optimized in this study using the experimental thermodynamic and the phase equilibrium data from the literature. The solution phases of the system are described using the substitutional solution model and the compounds (including borides) are treated as stoichiometric phases. The results show a good correlation between the calculated and measured thermodynamic and phase equilibrium data.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 4; 1249-1255
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Silicide spherules from Permian sediments of the Fore-Sudetic Monocline (SW Poland)
Autorzy:
Muszer, A.
Powiązania:
https://bibliotekanauki.pl/articles/110639.pdf
Data publikacji:
2014
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
Permian
Fe-silicide spherules
cosmic dust
ore minerals
Fe-Si alloy
Opis:
The presence of Fe-silicides, extremely rare mineral phases were documented in the Permian Cu-bearing ore formation in the Fore-Sudetic Monocline (Polkowice-Sieroszowice and Rudna mines, SW Poland). It is a first report of their occurrence within rocks of Late Palaeozoic age. The Fe-Si alloys forme spherules of various structure and chemical composition. The silicide spherules were found in the flotation concentrates prepared from the copper ore. Their composition varies from FeSi (fersilicite) to Fe2Si3 or Fe4Si9. A dominant constituent is Fe5Si3 (xifengite) with admixtures of P, Ti, Cr and Mn. Native Si and Ti were detected in the marginal part of spherules. The current knowledge do not permit to determine unequivocally whether the Fe-silicide spherules formed as a result of Permian cosmic dust or constitute terrestrial magmatic material of ultramafic character transported into a sedimentary basin from the adjacent terrain.
Źródło:
Physicochemical Problems of Mineral Processing; 2014, 50, 1; 107-118
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
A Mössbauer and structural study of disordered alloys Fe3-xTixAl (0 < x < 1)
Autorzy:
Brząkalik, K.
Frąckowiak, J.
Powiązania:
https://bibliotekanauki.pl/articles/148880.pdf
Data publikacji:
2003
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
Fe2TiAl Heusler phase
Fe-Ti-Al system
Mössbauer spectroscopy
Opis:
A series of the disordered Fe3-xTixAl (x = 0, 0.2, 0.45, 0.55, 0.65, 0.70, 0.75, 1) alloys obtained by arc-melting were studied. Directly after melting the samples were mechanically crashed and in that form examined by the structural and Mössbauer effect methods. The alloys were strongly disordered, but it was possible to identify, apart from Fe-bcc phase, the origins of forming such phases as Fe2TiAl Heusler phase, Fe3Al with DO3 structure, FeAl and FeTi with B2 structure and non-stechiometric Fe2Ti Laves phase with hexagonal C14 structure. For Ti concentration up to x = 0.45, the disordered Fe-bcc phase dominates. For Ti concentration from x = 0.55 to x = 1, the Fe2TiAl phase coexists with FeAl phase (for x = 0.55, 0.65) and with FeTi phase (x = 0.7 and 0.75). In a sample with the nominal Fe2TiAl composition of Fe2TiAl Heusler phase, a non-stoichiometric Fe2Ti Laves phase with hexagonal C14 structure was observed.
Źródło:
Nukleonika; 2003, 48,suppl.1; 13-16
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ocena trwałości resztkowej rur katalitycznych reformerów amoniaku badaniami NDT
Assessment of residual life of ammonia reformers catalytic pipes by NDT test
Autorzy:
Jasiński, W.
Powiązania:
https://bibliotekanauki.pl/articles/107896.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
reforming
stopy Fe-Cr-Ni
mikrostruktura
Fe-Ni-Cr alloys
microstructure
Opis:
The article presents the results of the stability of the microstructure and properties of catalytic cast pipes in steam reforming conditions. The growing prices of catalytic pipes have resulted in the attempts to prolong of the pipe work above 100,000 h stability. Increasing the time and temperature of operating causes coalescence and coagulation of secondary carbides reducing thus the creep resistance of the alloy. Currently there is no definite and commonly used method to assess the degree of degradation of the microstructure and properties of catalytic pipes. The destructive test methods of catalytic pipes are usually reduced to the assessment of the effects of metallographic creeping process, ie. relative volume and distribution of mikrovoids on the pipe wall section, as well as evaluating the mechanical properties of steel. These methods generally give a clear assessment but require disassembly for testing pipes and replace ment with new ones. The author developed the regression which show a significant dependence of mechanical properties (Rm A5, KCU 2) on the operating parameters of the reformer (PLM, σ) and hardness HB cast IN 519. The equations have been applied to assess the possibility of using non-destructive testing for the assessment of the degree of degradation of the catalyst steel pipe.
W artykule przedstawiono wyniki badań stabilności mikrostruktury i właściwości staliwa rur katalitycznych w warunkach reformingu parowego. Wzrastające ceny rur katalitycznych doprowadziły do analizy możliwości przedłużenia czasu eksploatacji rur powyżej projektowej trwałości 100000 h. Zwiększenie czasu i temperatury eksploatacji powoduje koalescencję i koagulację węglików wtórnych, a tym samym zmniejszenie odporności na pełzanie stopu. Obecnie brak jest jednoznacznej i powszechnie stosowanej metody oceny stopnia degradacji mikrostruktury i właściwości staliwa rur katalitycznych. Niszczące metody badań rur katalitycznych sprowadzają sie zwykle do oceny metalograficznej efektów procesu pełzania, tzn. objętości względnej i rozmieszczenie mikropustek na przekroju ścianek rur, a także ocenę właściwości mechanicznych staliwa. Metody te dają na ogół jednoznaczną ocenę ale wymagają demontażu rur do badań i zastąpienie ich nowymi. Wykorzystując opracowane równania regresji wykazujące istotną statystycznie zależność właściwości mechanicznych (Rm, A5, KCU 2) od parametrów eksploatacyjnych reformera (PLM, σ) i twardości HB staliwa IN 519, wykazano możliwość zastosowania badań nieniszczących do oceny stopnia degradacji staliwa rur katalitycznych.
Źródło:
Badania Nieniszczące i Diagnostyka; 2016, 1-2; 57-61
2451-4462
2543-7755
Pojawia się w:
Badania Nieniszczące i Diagnostyka
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Experimental study of Fe-Ni-Ti-Cr system
Autorzy:
Hoppe, Viktoria
Gibas, Anna
Grzegorczyk, Weronika
Małecki, Marcin
Hasiak, Mariusz
Powiązania:
https://bibliotekanauki.pl/articles/1188070.pdf
Data publikacji:
2019
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
właściwości mechaniczne
stopy z pamięcią kształtu
stop Fe-Ni-Ti
stop Fe-Ni-Ti-Cr
mechanical properties
shape memory alloys
Fe-Ni-Ti alloy
Fe-Ni-Ti-Cr alloy
Opis:
The research comprises a discussion about a formation of intermetallic phase with stoichiometric composition Fe2Ti, called Laves phase, and influence of chromium on the whole structure containing this phase by means of comparison of the two alloys. A base Fe35Ni35Ti30 alloy was used as a reference and then compared with a Fe-Ni-Ti chromium doped - Fe30Ni35Ti30Cr5 alloy. The study of microstructure performed with scanning electron microscope enabled to distinguish different phases. These regions are rich in mixture of Fe-Ni and Ti-Ni elements. The identified phases are Fe2Ti and Ni3Ti which was confirmed by X-ray diffraction and simultaneously it is consistent with energy dispersive spectroscopy results. Differential scanning calorimetry confirmed also multi-phase composition. As a result different hardness was measured for these phases using nanoindentation. The overall hardness was established using the Vickers method.
Źródło:
Interdisciplinary Journal of Engineering Sciences; 2019, 7, 1; 1--14
2300-5874
Pojawia się w:
Interdisciplinary Journal of Engineering Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wysokotemperaturowe własności tribologiczne stopów Fe-Al
High temperature tribological properties of Fe-Al alloys
Autorzy:
Śleboda, T.
Krawczyk, J.
Zimowski, S.
Kot, M.
Powiązania:
https://bibliotekanauki.pl/articles/189298.pdf
Data publikacji:
2012
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
stopy Fe-Al
zużycie
współczynnik tarcia
Fe-Al alloys
wear
friction coefficient
Opis:
W niniejszej pracy poddano dyskusji wysokotemperaturowe własności tribologiczne stopów Fe-Al. Jako materiał wyjściowy do badań zastosowano stop FeAl w formie odlewu oraz otrzymany z proszku stopu. Analizie został poddany wpływ rodzaju stopu na jego własności tribologiczne. Badania tribologiczne wykonano w temperaturze 700C w układzie trzpień-tarcza. Określono wielkość zużycia oraz współczynnik tarcia. Dyskusji poddano różnice w mechanizmach zużycia tribologicznego badanych materiałów.
This research was focused on high temperature tribological properties of Fe-Al alloys. Powder and cast FeAl alloy was used in this study. The influence of the alloy morphology on its tribological properties is discussed. Tribological tests were performed at 700C. Wear and friction coefficients of the investigated materials were analysed. The differences in the mechanisms of the wear of the investigated alloys are also presented.
Źródło:
Tribologia; 2012, 3; 209-215
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Numerical analysis of friction influence on the transverse welding phenomenon in the forward extrusion process
Autorzy:
Piwnik, J.
Mogielnicki, K.
Kuprianowicz, J.
Powiązania:
https://bibliotekanauki.pl/articles/279515.pdf
Data publikacji:
2014
Wydawca:
Polskie Towarzystwo Mechaniki Teoretycznej i Stosowanej
Tematy:
extrusion
welding criteria
FE analysis
Opis:
There is often a need to join billets being extruded in the forward extrusion processes in order to preserve the continuity of manufacturing of products. The primary problem connected with joining while extruding is to ensure the required state of stress, deformation and temperature assuring a good weld quality. The paper contains numerical analyses of the transverse joining processes of billets in the course of forward extruding. The impact of the friction between welded objects on the material flow in vicinity of the joints is analyzed. A numerical method for determination of the weld length at the longitudinal section, by assuming the homogeneity of the strain rate at both sides of the joined elements contact line, is proposed. Three cases of the forward extruding are analyzed. Two friction shear factors equal to m = 0.4 and m = 0.9 at the billets interface are modelled for each case and weld the lengths at the longitudinal sections are presented. In addition, distributions of the flowing material velocities and effective strains in the weld vicinity are added for all tested processes.
Źródło:
Journal of Theoretical and Applied Mechanics; 2014, 52, 2; 547-555
1429-2955
Pojawia się w:
Journal of Theoretical and Applied Mechanics
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparison of Residual Stress State on Sheets Faying Surface after Standard and NACA Riveting-Numerical Approach
Autorzy:
Wronicz, W.
Powiązania:
https://bibliotekanauki.pl/articles/97853.pdf
Data publikacji:
2016
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Lotnictwa
Tematy:
NACA riveting
fatigue
FE
joints
Opis:
One crucial characteristic of the aircraft structure are fatigue properties and rivets are usually critical areas in metal airframes due to fatigue cracks nucleation. According to literature, the NACA riveting method offers a huge increase in fatigue life of riveted lap joints. This paper presents FE simulations of quasi-static riveting on a press for standard countersunk rivets and the NACA riveting in two configurations: with a normal brazier rivet and a brazier rivet with a compensator. The analyzed configurations have been compared based on the stress courses on the sheets faying surfaces after riveting process. Due to a lack of data, the rivet length and the squeezing force value were assumed for NACA riveting based on FE simulations. The results indicated beneficial influence of the NACA riveting in the outer sheet (with a countersunk) and disadvantageous influence in the inner sheet. This effect was stronger in the case of the rivet with a compensator.
Źródło:
Fatigue of Aircraft Structures; 2016, 8; 116-126
2081-7738
2300-7591
Pojawia się w:
Fatigue of Aircraft Structures
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Phase structure of the nanocrystalline Nd2Fe14B/alfa-Fe magnets with different grain
Autorzy:
Wnuk, I.
Wysłocki, J.
Przybył, A.
Powiązania:
https://bibliotekanauki.pl/articles/148342.pdf
Data publikacji:
2007
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
Nd2Fe14B + alfa-Fe nanocrystalline magnets
Mössbauer spectroscopy
magnetic properties
Opis:
The effect of the contents of the magnetically hard and magnetically soft phases on the magnetic properties of Nd2Fe14B + alfa-Fe nanocrystalline magnets, as produced by the method of mechanical alloying, has been established. The phase composition of specimens was determined using X-ray diffractometry and Mössbauer spectroscopy. The Mössbauer examination showed that as the powder milling times increased, the content of the Nd2Fe14B phase increased from 42.8% (after the milling time of 10 h, with a grain size of 44.8 nm) to 66.3% (after the milling time of 48 h, with a grain size of 37.3 nm) and then decreased to 40.3% after 120 h of milling. On the other hand, the content of the magnetically soft phase alfa-Fe initially decreased (from 27.7%), reaching a minimum after the milling time of 48 h (17.4%) and then increasing to 36.9% after 120 h of milling.
Źródło:
Nukleonika; 2007, 52, supl. 1; 85-88
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermodynamic Description of Ternary Fe-B-X Systems. Part 7: Fe-B-C
Autorzy:
Miettinen, J.
Visuri, V.-V.
Fabritius, T.
Vassilev, G.
Powiązania:
https://bibliotekanauki.pl/articles/352609.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
phase diagrams
thermodynamic modelling
thermodynamic database
Fe-B-X systems
Fe-B-C system
Opis:
Thermodynamic description of the Fe-B-C system in its iron-rich corner is developed in the context of a new Fe-B-X (X = Cr, Ni, Mn, Si, Ti, V, C) database. The thermodynamic parameters of the binary sub-systems, Fe-B, Fe-C and B-C, are taken from earlier assessments modifying the B-C description. The parameters of the Fe-B-C system are optimized in this study using experimental thermodynamic and phase equilibrium data from the literature. Liquid, beta-rhombo-B and graphite phases are described using the substitutional solution model, while the ferrite (bcc), the austenite (fcc), the cementite (M3C) and the M23C6 phases are described with the sublattice model and the borides, Fe2B, FeB and B4C, are treated as stoichiometric phases. A good correlation was obtained between the calculated and the experimental thermodynamic and phase equilibrium data. The description is recommended to be used at the composition region of wt% C + wt% B < 15 and at temperatures below 2700°C.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 2; 923-933
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
O możliwości zastosowania azotku boru h-BN jako składnika żelaznego porowatego spieku
The possibility of the application of boron nitride h-BN as a component of iron porous sinter
Autorzy:
Kałdoński, T.
Kłos, K.
Powiązania:
https://bibliotekanauki.pl/articles/190802.pdf
Data publikacji:
2013
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
porowaty spiek Fe
azotek boru h-BN
Fe porous sinter
boron nitride h-BN
Opis:
W pracy przedstawiono wyniki badań żelaznych spieków zawierających różne ilości heksagonalnego azotku boru h-BN. Badania tribologiczne przeprowadzono za pomocą maszyn KEWAT-6 i KEWAT-1 w Zakładzie Tribologii, Inżynierii Powierzchni i Logistyki Płynów Eksploatacyjnych IPMiT WME WAT. Stwierdzono, że zawartość do 3% wagowo azotku boru w żelaznym spieku proszku żelaza Höganas NC.100.24 poprawia skutecznie właściwości tribologiczne spieku, tj. zmniejsza wartość współczynnika tarcia, nie zwiększając zużycia spiekanych próbek mimo nieznacznego spadku ich twardości. Wyniki tych badań były podstawą do wykonania pełnogabarytowych tulei porowatych zawierających azotek boru h-BN w spieku, które następnie poddano badaniom stanowiskowym w ramach projektu badawczego rozwojowego PBR/15-249/2007/WAT-OR00002904 [L. 1], finansowanego przez Ministerstwo Nauki i Szkolnictwa Wyższego w latach 2007–2011.
The results of research on the iron sinters containing various amounts hexagonal boron nitride h-BN are presented in this paper. The tribological research was realised with KEWAT-6 and KEWAT-1 machines at the Department of Tribology, Surface Engineering and Service Fluids Logistics of the Institute of Motor Vehicles and Transportation, FME, MUT. The paper concludes that boron nitride up to 3% by weight in the iron sinter of Höganas NC.100.24 iron powder efficiently increases tribological properties of the sinter, i.e. it lowers the value of the friction factor without increasing the wear of sintered samples. However, their hardness was slightly decreased. These results were the basis for making some full-size porous sleeves, which included boron nitride h-BN in the sinter. The sleeves were then subjected to stand tests within the framework of the development and research project number PBR/15-249/2007/WAT-OR00002904 [L. 1], financed by the Ministry of Science and Higher Education, 2007–2011. Very advantageous results were obtained from these tests, which allowed us to make a patent claim [L. 8].
Źródło:
Tribologia; 2013, 3; 21-35
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ball-milled Fe-Ni and Fe-Mn Matrix Powders For Sintered Diamond Tools
Mielone proszki Fe-Ni oraz Fe-Mn przeznaczone do produkcji narzędziowych materiałów metaliczno diamentowych
Autorzy:
Romanski, A.
Konstanty, J.
Powiązania:
https://bibliotekanauki.pl/articles/356795.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ball milling
PM diamond tools
matrix
Fe-Ni alloy
Fe-Mn
hot pressing
mielone proszki
narzędzia diamentowe
stop Fe-Ni
prasowanie na gorąco
Opis:
The work presents the possibility of substitution of expensive, Co-WC powders, that have been traditionally used in the production of sintered diamond tools, with cheap iron-base counterparts manufactured by ball milling. It has been shown that ball-milled Fe-Ni and Fe-Mn powders can be consolidated to a virtually pore-free condition by hot pressing at 900°C. The as-consolidated materials are characterised by high hardness, bending strength and resistance to 3-body abrasion.
W pracy przedstawiono] wyniki badań nad możliwością zastąpienia proszków Co-WC powszechnie stosowanych do pro- dukcji spiekanych materiałów narzędziowych, tańszymi proszkami na bazie żelaza, otrzymanymi metodą mielenia w młynie kulowym. Stwierdzono, że spieki otrzymane z proszków Fe-Ni oraz Fe-Mn, które prasowano na gorąco w temperaturze 900°C. charakteryzują się małą porowatością, wysoką twardością i wytrzymałością na zginanie oraz dużą odpornością na zużycie ścierne w obecności 3 ciał.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 1; 189-193
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Detonation deposited Fe-Al coatings. Part I Morphology of Ni(Al) and Cr(Ni) transition layers and coatings of Fe-Al type sprayed onto carbon steel substrate
Powłoki Fe-Al osadzane detonacyjnie Część I: warstwy pośrednie Ni(Al) i Cr(Ni) oraz powłoki Fe-Al osadzane detonacyjnie na podłożu ze stali 045
Autorzy:
Pawłowski, A.
Senderowski, C.
Bojar, Z.
Faryna, M.
Powiązania:
https://bibliotekanauki.pl/articles/353418.pdf
Data publikacji:
2010
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
fazy międzymetaliczne Fe-Al
powłoki
natryskiwanie detonacyjne
intermetallics of Fe-Al type
D-gun spraying
Opis:
The microstructure of transition layers of Ni(Al) - pure Ni with Al and NiAl particles as well as Cr(Ni) - pure Cr in the Ni matrix, occurred between the coating of Fe-Al type intermetallic phases and the 045 carbon steel substrate was analysed in the present work. The investigations were aimed at the adherence of transition layers and the outer coating deposited with the detonation-gas spraying. The structure was examined using the methods of scanning (SEM) and transmission electron (TEM) microscopies as well as the analysis of chemical composition in microareas (EDS). Silica grains at the boundary of the substrate and the layer of Ni(Al), aluminium oxide at the boundary and inside the Ni(Al) layers, an Al based AlNiOx phase, columnar crystals at the boundary of the coating of Fe-Al type phases and an adjacent Cr(Ni) layer were observed. The results were discussed in reference to earlier examinations of bending strength considering cracking and delamination of the coating off the substrate. They were then compared with the state of the boundary between the coating and the steel substrate analysed in former works. It seems, that the substrate boundary free from silica inclusions and the prevention of the formation of aluminium oxides at the boundary of transition layers and the substrate should improve the adherence of the whole multi layer and the coating.
W pracy poddano analizie mikrostrukturę warstw pośrednich: Ni(Al) - czystego niklu z cząstkami Al i faz NiAl oraz warstwy Cr(Ni) - chromu w osnowie Ni, występujących pomiędzy powłoką faz międzymetalicznych typu Fe-Al i podłożem ze stali węglowej 045. Badania wykonano z punktu widzenia przyczyn przyczepności warstw pośrednich i powłoki zewnętrznej, naniesionych przez natryskiwanie detonacyjno-gazowe DGS. Analizę struktury przeprowadzono na podstawie badań metodą skaningowej (SEM) i transmisyjnej mikroskopii (TEM) elektronowej oraz analizy składu chemicznego w mikroobszarach (EDS). Stwierdzono wystąpienie ziaren krzemionki na granicy podłoża z warstwą Ni(Al), obecności ziaren tlenku glinu na granicy i wewnątrz warstw Ni(Al) oraz fazy na bazie glinu AlNiOx i kryształów kolumnowych na granicy powłoki faz typu Fe-Al oraz warstwy Cr(Ni) chromu do niej przylegającej. Wyniki badań mikrostruktury dyskutowano w odniesieniu do rezultatów wcześniejszych pomiarów wytrzymałości na zginanie w aspekcie pękania powłoki oraz delaminacji podwarstwy od podłoża. Porównano je także do stanu granicy powłoki z podłożem stalowym dokonanych w poprzednich pracach. Jest prawdopodobne, iż granice podłoża pozbawione wtrąceń krzemionki oraz zapobieżenie tworzeniu tlenków glinu na granicy warstw pośrednich i podłoża powinno poprawić przyczepność całej multiwarstwy i powłoki.
Źródło:
Archives of Metallurgy and Materials; 2010, 55, 4; 1061-1071
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evolution of equilibrium composition of MnO-SiO2 and Al2 O3 -MnO-SiO2 inclusions in liquid Fe and Fe-36%Ni alloy during cooling
Ewolucja równowagowego składu ciekłych wtrąceń MnO-SiO2 oraz Al2 O3 -MnO-SiO2 w stopie Fe-36%Ni oraz w ciekłym Fe w czasie chłodzenia
Autorzy:
Jerzak, W.
Kalicka, Z.
Powiązania:
https://bibliotekanauki.pl/articles/355076.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop Fe-36%Ni
chłodzenie
żelazo
nikiel
Fe-Ni melt
deoxidization
liquid inclusions
cooling
thermodynamics
Opis:
Evolution of chemical composition of inclusions for Fe-36%Ni melt on cooling was simulated on the basis of theoretical analysis. The equilibrium states for deoxidization reactions using manganese, silicon and aluminum were found by using the subregular solution thermodynamic model, including the interaction parameters and the activity coefficients for O, Mn, Si i Al at infinite dilution in iron and nickel. The equilibrium compositions of the inclusions when cooling the melt were computed for Fe-36%Ni for the temperatures from 1873K to 1773K. For comparison, the same analysis was made for pure iron melt. The obtained results indicate different behavior of the inclusions for those melts. For Fe-36%Ni, either MnO-SiO2 inclusions or Al2 O3 -MnO-SiO2 ones always increase substantially in MnO content on cooling. When Al2 O3 content goes up, the effect gets weaker. As to the pure iron melt, the inclusions behave more differently, i.e., the MnO content may go up, go down or stay constant depending on the initial inclusion composition. Despite of the fact that Al2 O3 -MnO-SiO2 inclusions fluctuate significantly as to their compositions for Fe-36%Ni melt, it seems however, that it would be easier for this melt - in comparison to pure iron one - to forecast such a chemical target composition which would allow to achieve the desired composition of the inclusions left within the residual melt after metal cooling from 1873K to 1773 K.
Przeprowadzono teoretyczną symulację zmiany składu wtrąceń w stopie Fe-36%Ni podczas chłodzenia. Stałe równowagi reakcji odtleniania manganem, krzemem i glinem obliczono zakładając model subregularny i wykorzystując parametry oddziaływania oraz współczynniki aktywności O, Mn, Si i Al w nieskończonym rozcieńczeniu w żelazie i niklu. Obliczono równowagowe składy wtrąceń w procesie chłodzenia Fe-36%Ni od 1873K do 1773K. Porównawczo wykonano taką samą analizę dla żelaza. Uzyskane wyniki wskazują, że wtrącenia zachowują sie różnie w obu metalach. W stopie Fe 36%Ni, zarówno wtrącenia MnO-SiO2 jak i Al2 O3 -MnO-SiO2 zawsze wzbogacają sie w znacznym stopniu w MnO gdy temperatura spada. Zwiększenie zawartości Al2 O2 osłabia ten efekt. Wtrącenia w żelazie zachowują sie bardziej różnorodnie - ułamek molowy MnO może zwiększać się, zmniejszać lub pozostawać stały, zależnie od początkowego składu wtrącenia. Mimo, że wtrącenia Al2 O3 -MnO-SiO2 ulegają znacznym zmianom w stopie Fe-36%Ni, to wydaje się, że prognozowanie takiego składu wtrąceń w 1873K aby po ochłodzeniu metalu i wypłynięciu części z nich, pozostałe wtrącenia miały pożądany skład, może być łatwiejsze w Fe-36%Ni niż w żelazie.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 2; 449-455
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Adsorption of hydrated Fe(OH)2+ on the kaolinite surface: A density functional theory study
Autorzy:
Wu, Hongqiang
Miao, Yuqi
Long, Qibang
Yan, Huashan
Li, Yong
Qiu, Sen
Wu, Hao
Zhao, Guanfei
Qiu, Tingsheng
Powiązania:
https://bibliotekanauki.pl/articles/27323639.pdf
Data publikacji:
2023
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
kaolinite
adsorption
Fe
density functional theory
Opis:
The present study employed density functional theory (DFT) to analyze the adsorption configuration and mechanism of Fe(OH)2+ on the kaolinite (001) surface. The findings demonstrated that Fe(OH)2(H2O)4+ is the main type in which hydrated Fe(OH)2+ can be found in aqueous solution. On the surface of kaolinite, Fe(OH)2(H2O)4+ will be adsorbed. There are two forms of adsorption: outer-sphere and inner-sphere coordination (monodentate/bidentate) adsorption. Fe(OH)2(H2O)4+ has a moderate propensity to adsorb on the alumina octahedral sheet of kaolinite when the outer-sphere coordination adsorption takes place. In cases of inner-sphere coordination adsorption, Fe exhibits a tendency to form monodentate adsorption compounds in conjunction with Ou atoms. Additionally, it prefers to create bidentate adsorption compounds through coordination with both Ot and Ou atoms. The adsorption mechanism analysis results show that the ionic property of Fe atom decreases after outer-sphere coordination adsorption. After inner-sphere coordination adsorption, some electrons of Fe atom are transferred to the surface O atom. The presence of electrons between the Fe and O atoms enhances the formation of bonds, hence enhancing the covalent nature of the Fe-O bond. Theoretical FT-IR (Fourier transform infrared spectroscopy) calculations show that the formation of Fe-O chemical bonds. Because of the lower adsorption energy and more chemical bonds, hydrate Fe(OH)2+ is more likely to be bidentate adsorbed on the kaolinite surface.
Źródło:
Physicochemical Problems of Mineral Processing; 2023, 59, 6; art. no. 174415
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Special Structures of Graphite Steels After High-Energy Electron Irradiation
Autorzy:
Alexandrova, N. M.
Powiązania:
https://bibliotekanauki.pl/articles/2011024.pdf
Data publikacji:
1999-08
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
61.80.Fe
61.82.Bg
Opis:
The effect of high-energy electron irradiation on the structure and properties of the graphite steels have been investigated. It has been shown that single- and multicycle irradiation allows the improvement of hardness and ductility (≈ twice). A partial dissolution of the graphite, carbides redistribution, and refinement of the grain size allow the formation of the favorable surface structure after irradiation.
Źródło:
Acta Physica Polonica A; 1999, 96, 2; 259-262
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Use of the Phase Locking Information in the Human Auditory System for Frequencies Above 5 kHz
Autorzy:
Sęk, A.
Bukała, M.
Powiązania:
https://bibliotekanauki.pl/articles/1400102.pdf
Data publikacji:
2013-06
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
43.66.Fe
43.66.Hg
Opis:
Accurate allocation of neural impulses to the same phase (i.e. phase locking) in the auditory system, ceases for frequencies above 5 kHz. However, some recent works suggest that it may have a much higher value. A discrimination of harmonic complex and inharmonic complex sound, formed using sound harmonic complex, in which all components were shifted towards higher frequency by the same number in hertzs, was analyzed. Fundamental frequency was $F_0$=1 kHz and signals were bandpass filtered by a fixed filter center frequency of which was $11F_0$ and bandwidth $5F_0$. Discrimination threshold was $\Delta F=0.089F_0$ for 10 normal-hearing subjects. However, replacing the sinusoidal components with the noise bands brought about a significant increase in thresholds. The largest increase was observed for 700 Hz bandwidth. The replacement of sinusoidal components with noisebands reduces information conveyed by phase locking. The differences in excitation pattern for harmonic complex and inharmonic complex signals, for the average threshold, did not exceed 0.7 dB. Therefore they could not be a useful cue for harmonic complex and inharmonic complex discrimination. A simplified model of phase locking showed that the substitution of sinusoids with bands of noise significantly reduced number of intervals between successive neural spikes corresponding to the virtual pitch of harmonic complex and inharmonic complex sounds. This degradation of discrimination suggests that the main source of information about the pitch of harmonic complex and inharmonic complex, especially for sinusoidal components, was the phase locking.
Źródło:
Acta Physica Polonica A; 2013, 123, 6; 1106-1113
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Ho3+ ions for quantitation of iron (Fe) in 0.1 M HCl solution using microwave plasma-atomic emission spectrometry (MP-AES)
Wpływ jonów Ho3+ na jakościowe oznaczanie żelaza w roztworze 0.1 M HCI metodą atomowej spektroskopii emisyjnej z plazmą mikrofalową (MP-AES)
Autorzy:
Stępień, M.
Bukowska, A.
Powiązania:
https://bibliotekanauki.pl/articles/264243.pdf
Data publikacji:
2018
Wydawca:
Akademia Górniczo-Hutnicza im. Stanisława Staszica w Krakowie. Wydawnictwo AGH
Tematy:
MP-AES
ANOVA
Fe
Ho3+
Opis:
During research work in the Non-Ferrous Metals Department on AGH University of Science and Technology concerning new corrosion inhibitors for iron alloys in magnetic fields, Ho3+ ions were proposed as one of the new inhibitors. One of the methods for determining the rate of the corrosion process is determining the concentration of Fe ions in a solution. Due to the required high precision of determining the concentration of Fe ions in a solution contains Ho3+ ions with a wide range of concentrations, the influence of the matrix effect and interferences of Ho3+ ions must be known. The present work investigates the impact of Ho ions within a range of 0 to 100 mg/L for the quantitation of Fe ions in a 0.1 M HCl solution using the MP-AES method. The obtained results were analyzed using the single-factor ANOVA method. In a range of up to 40 mg/L, Ho3+ ions are not a significant factor to determining the Fe concentration by MP-AES.
W trakcie prac badawczych prowadzonych na Katedrze Fizykochemii i Metalurgii Metali Nieżelaznych na Akademii Górniczo-Hutniczej w Krakowie dotyczących nowych inhibitorów korozji stopów żelaza w polu magnetycznym, jako jeden z nowych inhibitorów zaproponowano jony Ho. Jedną z metod określenia postępów procesu korozji było oznaczenie stężenia jonów Fe w roztworze metodą atomowej spektroskopii emisyjnej w plazmie mikrofalowej (MP-AES). Z uwagi na wymaganą wysoką precyzję określenia niewielkiej zawartości jonów Fe w roztworach o różnej zawartości jonów Ho konieczne stało się zbadanie, czy obecność jonów Ho wpływa istotnie na ocenę ilościową jonów Fe metodą MP-AES. W niniejszej pracy zbadano wpływ stężenia jonów Ho w zakresie stężeń od 0 do 100 mg/l na oznaczenie zawartości Fe w 0,1 M kwasie solnym. Uzyskane wyniki poddano analizie statystycznej z wykorzystaniem metody ANOVA. W zakresie stężeń jonów Ho w analicie do 40 mg/L nie wykazano istotnego wpływu na oznaczenie żelaza na poziomie ufności 95%.
Źródło:
Metallurgy and Foundry Engineering; 2018, 44, 3; 109-117
1230-2325
2300-8377
Pojawia się w:
Metallurgy and Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Load carrying capacity numerical study of I-beam pillar structure with blast protective panel
Autorzy:
Mazurkiewicz, L.
Kolodziejczyk, D.
Damaziak, K.
Malachowski, J.
Klasztorny, M.
Baranowski, P.
Powiązania:
https://bibliotekanauki.pl/articles/202056.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
FE analysis
blast protection
stability study
Opis:
The paper presents numerical analyses aimed at preliminary assessment of the protective panel effectiveness, which task is to protect the elements of building structures against explosion. For the criterion of assessing the effectiveness of the panel the load capacity of the column made of steel I-beam was chosen. Ultimate force was determined by using advanced computational procedure, which consisted of four stages: preload, blast simulation, dynamic response and static analysis of deformed structure. Blast load was simulated using Lagrangian- Eulerian domain coupling. Results indicated that the application of the protective panel significantly reduces the plastic deformation of the structure.
Źródło:
Bulletin of the Polish Academy of Sciences. Technical Sciences; 2013, 61, 2; 451-457
0239-7528
Pojawia się w:
Bulletin of the Polish Academy of Sciences. Technical Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analysis of the Corrosion Rate of FeMn-Si Biodegradable Material
Autorzy:
Roman, Ana-Maria
Chelariu, Romeu
Cimpoesu, Ramona
Stirbu, Ioan
Ionita, Iulian
Cazacu, Marius Mihai
Prisecariu, Bogdan Anton
Cimpoesu, Nicanor
Pietrusiewicz, Paweł
Sodor, Alina
Powiązania:
https://bibliotekanauki.pl/articles/2174554.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
biodegradable
Fe-Mn alloy
degradation rate
Opis:
The Fe-based alloy with manganese led to the appearance of new austenitic alloys, with the antiferromagnetic property pursued, resulting in compatibility with the magnetic field as that of magnetic resonance imaging. The corrosion resistance behavior of the biodegradable Fe-Mn-Si alloy was analyzed in a thermostatic chamber at 37±1°C for 24, 48 and 72 hours by immersing in Ringer solution. Also, the cast and laminated samples were subjected to electro-corrosion tests using a potentiostat equipment. Linear and cyclic potentiometry is presented for characterize the corrosion behavior of the experimental samples in electrolyte. Due to the interaction between the alloy and the liquid medium a change in the solution pH was observed. Structure analysis and chemical composition details of the surfaces were obtained using electron scanning microscopy (SEM) and X-ray energy dispersive spectroscopy (EDS).
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 4; 1243--1250
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Densification and Magnetic Properties of Fe Powder Compacts According to Heat-Treatment Conditions
Autorzy:
Yoo, Hyo-Sang
Kim, Yong-Ho
Kim, Cheol-Woo
Son, Hyeon-Taek
Powiązania:
https://bibliotekanauki.pl/articles/2203721.pdf
Data publikacji:
2023
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Fe powder
heat-treatment
microstructure
density
Opis:
In this study, the effects of heat-treatment conditions of Fe powder compacts on densification, microstructure, strength and magnetic properties were investigated. The prepared Fe powder was compressed in a mold of diameter 20 mm at a pressure of 800 MPa for 30 sec. This Fe powder compact was heat-treated under different atmospheres (air and 90% Ar + 10% H2 and heat-treatment temperatures (300 and 700℃). The Fe powder compacts heat-treated in an Ar+H2 mixed gas atmosphere showed a denser microstructure and higher density than the Fe powder compacts heat-treated in an air atmosphere. Oxygen content in the heat-treatment conditions played a significant role in the improvement of the densification and magnetic properties.
Źródło:
Archives of Metallurgy and Materials; 2023, 68, 1; 47--50
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Selected modeling problems of monopile foundations used in the energy industry
Autorzy:
Labocha, Sławomir
Paluszyński, Jarosław
Powiązania:
https://bibliotekanauki.pl/articles/2174977.pdf
Data publikacji:
2021
Wydawca:
Politechnika Częstochowska
Tematy:
fundament słupa
fundamenty z monopalów
modelowanie FE
foundation of the poles
monopiles foundations
FE modeling
Opis:
The paper presents selected practical aspects of the construction of monopile foundations used in the onshore power sector and analysis the effect of these solutions on the design of such structures. The basis for the evaluation of load capacity of such foundations was briefly discussed and the key factors that determine the ability to transfer loads from the structure to the ground were indicated. The main problem presented in the paper was to assess the impact of the reinforced concrete stay-in-place formwork piles built using the well technology. The considerations were supplemented with a computational example illustrating the thesis presented in the paper. A positive effect of prefabricated formwork rings on the load capacity of the foundation was demonstrated.
Źródło:
Budownictwo o Zoptymalizowanym Potencjale Energetycznym; 2021, 10, 2; 77--87
2299-8535
2544-963X
Pojawia się w:
Budownictwo o Zoptymalizowanym Potencjale Energetycznym
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Morphology of the Alumina Films Formed tn The Anodization Process of Aluminium in the Orthophosphoric Acid Solution. The Co-Fe Alloys Electrodeposition Into Obtained Alumina Pores
Morfologia warstewek tlenku glinu otrzymanych w procesie anodowego utleniania aluminium w roztworze kwasu ortofosforowego. Elektroosadzanie stopów CoFe w porach otrzymanego tlenku
Autorzy:
Gumowska, W.
Dobosz, I.
Wrzoszczyk, B.
Powiązania:
https://bibliotekanauki.pl/articles/352773.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
anodic oxidation of aluminium
nanowires
Co-Fe alloy
anodowe utlenianie aluminium
nanodruty
stopy Co-Fe
Opis:
The optimal parameters of the anodic oxidation of aluminium in orthophosphoric acid solution was determined. In the pores of the obtained Al2O3 membranes with the ordered nanometric structure Co-Fe alloys were electrodeposited. The Al2O3 membranes were obtained in the two-stage anodic oxidation of aluminium in the 0.17 M H3PO4 solution in the temperature 1°C and at the electrolysis voltage 180 V. The influence of the anodizing process parameters on the thickness of oxide films and the diameter of pores and the distance between them in the alumina membranes were determined. The electrodeposition of Co-Fe alloys was carried out from sulphate baths containing sulphates (VI) of copper (II) and cobalt (II) of different composition, in potentiostatic conditions. The optimal electrolysis conditions were determined, where the cathodic deposits of the best quality were obtained. The conditions are: the electrolyte composition: 0.3 M Fe; 0.5 M Co; pH = 3, the potential: -0.760 V (vs. SHE)).
Określono optymalne parametry' anodowego utleniania aluminium w roztworze kwasu ortofosforowego W porach uzyska- nych membran AI2O3, o uporządkowanej strukturze nanometrycznej. osadzano elektrolitycznie stopy Co-Fe. Membrany AI2O3 otrzymywano w procesie dwuetapowego utleniania aluminium w roztworze 0.17 M H3PO4. w temperaturze 1°C, przy napięciu elektrolizy 180 V. Zbadano wpływ parametrów anodowania na grubość warstewek tlenkowych, średnicę porów i odległości między nimi w membranach tlenku glinu. Elektroosadzanie stopów Co-Fe prowadzono z roztworów siarczanowych (VI) zawierających jony miedzi (II) i kobaltu (U) o różnym składzie, w warunkach potencjostatycznych. Określono optymalne warunki elektrolizy, w których otrzymano osady katodowe najlepszej jakości. A mianowicie: skład elektrolitu : 0,3 M Fe: 0,5 M Co: pH = 3, potential: -0.760 V (wzgl. SEW).
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 1; 137-143
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mössbauer study of vacuum annealed Fe100-xGax (10 less - than or equal to x less - than or equal to 35) thin films
Autorzy:
Szumiata, T.
Górka, B.
Brzózka, K.
Gawroński, M.
Gzik-Szumiata, M.
Javed, A.
Morley, N. A.
Gibbs, M. R. J.
Powiązania:
https://bibliotekanauki.pl/articles/147332.pdf
Data publikacji:
2013
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
Fe-Ga
thin films
CEMS
MOKE
Opis:
This work reports results from comparative Mossbauer studies of as-deposited and annealed Fe100.xGax (10 less - than or equal to x less - than or equal to 35) high magnetostrictive thin films of constant thickness (50 plus or minus 2 nm). Films were grown on Si(100) substrates using a co-sputtering and evaporation chamber where Fe has been sputtered and Ga was evaporated. During growth of films, a magnetic field of 65 kA/m has been applied in the plane of the film. Annealed films have been obtained by heating in vacuum for 1 h at 350 centigrade without magnetic field. After annealing, the saturation field of the Fe-Ga films has been significantly reduced. By means of the 57Fe CEMS technique the contributions from several phases have been found: Fe-Ga A2 (bcc), traces of DO3 phase, a gallium-rich disordered phase and iron oxides (both geothite and magnetite). For the sample with x = 26.5 the heat treatment reduces the DO3 phase content whereas for the film with x = 16.4 the opposite tendency has been observed. Mossbauer results were compared with XRD and MOKE findings.
Źródło:
Nukleonika; 2013, 58, 1; 27-30
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Nanocrystallization studies of rapidly quenched Fe85.4-xCoxZr6.8-yNbyB6.8Cu1 (x = 0 or 42.7, y = 0 or 1) alloys
Autorzy:
Olszewski, J.
Zbroszczyk, J.
Ciurzyńska, W.
Fukunaga, H.
Wysłocki, B.
Perduta, K.
Łukiewska, A.
Młyńczyk, A.
Lelątko, J.
Świerczek, J.
Powiązania:
https://bibliotekanauki.pl/articles/148787.pdf
Data publikacji:
2003
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
Mössbauer spectra
nanocrystalline Fe-Co alloys
Opis:
The microstructure of amorphous and nanocrystalline Fe42.7Co42.7Zr6.8-xNbxB6.8Cu1 (x = 0 or 1) alloys was investigated. We have stated that the nanocrystalline samples consist of the crystalline alfa-FeCo grains about 8 nm in diameter embedded in an amorphous matrix which is rich in cobalt. From Mössbauer spectroscopy studies we have found that the crystalline alfa-FeCo phase in the nanocrystalline samples obtained by the conventional annealing is atomically ordered. Moreover, the order degree depends on the annealing time. As for the samples partially crystallized during rapid quenching, the crystalline alfa-FeCo phase is atomically disordered.
Źródło:
Nukleonika; 2003, 48,suppl.1; 49-52
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analysis of a light caterpillar vehicle loaded with blast wave from detonated IED
Autorzy:
Barnat, W.
Niezgoda, T.
Panowicz, R.
Powiązania:
https://bibliotekanauki.pl/articles/247638.pdf
Data publikacji:
2010
Wydawca:
Instytut Techniczny Wojsk Lotniczych
Tematy:
IED
vehicle shell
FE analysis
ground
Opis:
More and more impudent attacks on the military convoys in Afghanistan proved a huge danger of the improvised explosive devices - IED. Huger and more clever charges are a serious problem for vehicles protection. Additionally, hitherto defence standards and STANAG didn't predict such huge charges. Majority investigations were based on a 3 kg anti-tank mine. The article presents the results of numerical calculations for the elements of the combat vehicle supporting structure loaded with an impact generated by explosion of a huge explosive charge under the bottom of the vehicle with consideration of the wave reflected from the ground. Such an approach allows obtaining a good approximation of numerical simulations to real conditions of terroristic attacks. Additionally, the analysis of IED side influence on the vehicle shell was conducted. The explosive charge — IED — was simulated with the use of concentrated energy of properly selected (on the base of literature investigations) density and initial energy. During analyses of side explosive on the vehicle structure, the obstacle in the form of a building increasing the pressure impulse was taken into account. The paper presents the results of a numerical analysis in which Euler and Lagrange domains(describing a vehicle) were coupled. A perfect gas model was used to describe air parameters.. Additionally, the ground was described with a gas model. Every kind of material data were selected on the base of experimental investigations. A bilinear material model with a Cowper and Symonds strain rate model was used to describe a vehicle. Such an approach fully describes the phenomena occurring in the system.
Źródło:
Journal of KONES; 2010, 17, 4; 27-34
1231-4005
2354-0133
Pojawia się w:
Journal of KONES
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Frequency Discrimination for Amplitude Modulated Sinusoidal Signals at High Carrier Frequencies
Autorzy:
Sęk, A.
Kordus, M.
Powiązania:
https://bibliotekanauki.pl/articles/1359956.pdf
Data publikacji:
2014-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
43.66.Fe
43.66.Hg
Opis:
The current study is a continuation of experiments presented by Sęk and Bukała (Acta Physica Polonica A 123, 1106 (2013)). The purpose of the present study was to investigate frequency discrimination of amplitude modulated high frequency carriers. Using 2AFC procedure, the subjects were presented with two observation intervals of which the first interval contained four pulses of the same high frequency signal (called SSSS), while in the second interval (called SHSH) the second and fourth pulses had higher frequencies values (i.e. shifted upwards by Δ f). The carrier frequency (in S pulses) was fixed and equal to 10 kHz. Modulation rates were equal to 100, 200, 337, 500, 600, 733, and 800 Hz. The value of the modulation rate was limited to keep all components of the sinusoidal modulation within one auditory filter (17% of the center frequency) centered at the carrier frequency. Two different types of modulation were used: a simple sinusoidal modulation with the modulation depth m set to 100%, and a logarithmic modulation with the modulation depth m set to 50 dB. Results indicate a strong relationship between frequency discrimination threshold and modulation type. The thresholds are significantly higher for logarithmic modulation in comparison to sinusoidal modulation. Amplitude modulation as well as logarithmic modulation applied to the high frequency carrier cause significant increase in the frequency discrimination threshold. For high frequency sinusoidal signal carriers (i.e. close to 10 kHz), frequency discrimination thresholds do not depend on amplitude modulation rates up to about 800 Hz. In general, the excitation pattern mechanism was a primary cue enabling frequency discrimination of modulated and unmodulated signals to compare with the mechanism based on the temporal fine structure. However, the excitation pattern was not the only mechanism responsible for the frequency discrimination.
Źródło:
Acta Physica Polonica A; 2014, 125, 4A; A-149-A-154
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Current-Voltage Characteristic Features of Diodes Irradiated with 170~MeV Xenon Ions
Autorzy:
Poklonski, N.
Gorbachuk, N.
Nha, Vo
Tarasik, M.
Shpakovski, S.
Filipenia, V.
Skuratov, V.
Wieck, A.
Kołtunowicz, T.
Powiązania:
https://bibliotekanauki.pl/articles/1400481.pdf
Data publikacji:
2013-05
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
72.20.Jv
61.80.Fe
Opis:
Diodes manufactured on the wafers of single-crystalline silicon uniformly doped with phosphorus are studied. The wafer resistivity was 90 Ω cm. Xenon ions were implanted into the diodes from the side of the $p^{+}$-region (implantation energy 170 MeV, fluence Φp from $5 \times 10^7$ to $10^9 cm^{-2}$). It is shown that the formation of a continuous irradiation damaged layer with the thickness of the order of magnitude of the average projective range creates prerequisites for the negative differential resistance in the current-voltage characteristics of the irradiated diodes.
Źródło:
Acta Physica Polonica A; 2013, 123, 5; 926-928
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Defects Introduced by Irradiation with 4-9 MeV Helium Ions on Impedance of Silicon Diodes
Autorzy:
Poklonski, N.
Gorbachuk, N.
Nha, Vo
Shpakovski, S.
Filipenya, V.
Skuratov, V.
Kołtunowicz, T.
Kukharchyk, N.
Becker, H.
Wieck, A.
Powiązania:
https://bibliotekanauki.pl/articles/1402222.pdf
Data publikacji:
2015-11
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
72.20.Jv
61.80.Fe
Opis:
Silicon diodes irradiated with helium ions with energies of 4.1, 6.8 and 8.9 MeV are studied. It is shown that the mechanism determining the behaviour of frequency dependence of complex electric module and correspondingly the behavior of impedance of diodes irradiated with helium ions in the frequency region 3-200 kHz is a recharging of vacancy complexes localized in the space charge region.
Źródło:
Acta Physica Polonica A; 2015, 128, 5; 891-893
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effects of Fluences of Irradiation with 107 MeV Krypton Ions on the Recovery Charge of Silicon $p^{+}n$-Diodes
Autorzy:
Poklonski, N.
Gorbachuk, N.
Tarasik, M.
Shpakovski, S.
Filipenia, V.
Skuratov, V.
Wieck, A.
Kołtunowicz, T.
Powiązania:
https://bibliotekanauki.pl/articles/1503994.pdf
Data publikacji:
2011-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
72.20.Jv
61.80.Fe
Opis:
The diodes manufactured on the wafers of single-crystalline silicon uniformly doped with phosphorus are studied. The wafer resistivity was 90 Ω cm. Krypton ions are implanted to the side of the $p^{+}$-region of diodes (energy 107 MeV, fluence Φp from 5 × $10^7$ to 4 × $10^9 cm^{-2}$). It is shown that recovery charge $Q_{rr}$ is inversely proportional to the square root of the irradiation fluence value Φp. When the fluence increases, the part of the recovery charge Q_{rrA}, due to the high reverse conductance phase, decreases faster than the value $Q_{rr}$.
Źródło:
Acta Physica Polonica A; 2011, 120, 1; 111-114
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structure and Properties of Metals
Autorzy:
Kurzydłowski, K. J.
Powiązania:
https://bibliotekanauki.pl/articles/2010997.pdf
Data publikacji:
1999-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
62.20.-x
62.20.Fe
Opis:
Metals are one of the most widely used types of engineering materials. Some of their properties, e.g. elastic constants, can be directly related to the nature of the metallic bonds between the atoms. On the other hand, macro- and microstructural features of metals, such as point defects, dislocations, grain boundaries, and second phase particles, control their yield, flow, and fracture stress. Images of microstructural elements can be obtained by modern imaging techniques. Modern computer aided methods can be further used to obtain a quantitative description of these microstructures. These methods take advantage of the progress made in recent years in the field of image processing, mathematical morphology and quantitative stereology. Quantitative description of the microstructures are used for modeling processes taking place under the action of applied load at a given temperature and test (service) environment. These model considerations can be illustrated on the example of an austenitic stainless steel, which is an important material for power generating and chemical industry. Reports recently published also show that properties of materials can be significantly modified by the effect of free surface. Examples of such situations include environmental effect on the mechanical properties of materials. Data for an austenitic stainless steel is used to discuss contribution of the free surface to the mechanical properties of metals.
Źródło:
Acta Physica Polonica A; 1999, 96, 1; 69-79
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The adsorption mechanism of Al(III) and Fe(III) ions on bastnaesite surfaces
Autorzy:
Cao, Shiming
Cao, Yijun
Ma, Zilong
Liao, Yinfei
Powiązania:
https://bibliotekanauki.pl/articles/110208.pdf
Data publikacji:
2019
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
Al(III)
Fe(III)
bastnaesite
adsorption
Opis:
The adsorption mechanism of Al(III) and Fe(III) ions on bastnaesite surfaces was investigated by a combination of DFT calculation, XPS analysis, adsorption isotherm study and adsorption kinetic investigations. DFT calculation results indicated that ≡CeOH0 and ≡CO3H0 are primary functional groups on bastnaesite surfaces. XPS analysis reveals that Al(III) and Fe(III) ions adsorbed onto the bastnaesite surfaces through the interaction between aluminium/iron hydroxide species and oxygen atoms of surface ≡CeOH0 groups. No interaction between aluminium/iron hydroxide species and ≡CO3H0 groups was detected. Adsorption isotherm studies demonstrated that the adsorption data of Al(III) and Fe(III) ions is fitted relatively well by Freundlich equations, the adsorption kinetic characteristics fitted to pseudo-second order model. Freundlich constants suggested favorable process for Al(III) and Fe(III) ions adsorption, and each adsorbed metal hydroxide specie complex with at least two oxygen atoms of surface ≡CeOH0 groups.
Źródło:
Physicochemical Problems of Mineral Processing; 2019, 55, 1; 97-107
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
General directions in contact modelling development
Autorzy:
Maciolka, Pawel
Jedrzejewski, Jerzy
Powiązania:
https://bibliotekanauki.pl/articles/99664.pdf
Data publikacji:
2019
Wydawca:
Wrocławska Rada Federacji Stowarzyszeń Naukowo-Technicznych
Tematy:
flat surfaces
contact
asperity
FE model
Opis:
This paper presents a survey of works, selected from the period of the last twenty years, on deformations in the contact between rough surfaces. All the selected works use FEM. They deal with the modelling of individual contact asperities or the use of experiment to verify contact models. First, research directions connected with the modelling of single asperities, whose shape is usually approximated with that of a hemisphere or a half cylinder, are presented. Section 3 discusses research directions concerning models which include the layer under asperities, and models for small contact surfaces (about 1 mm2). Section 4 reviews directions in contact modelling which takes into account neighbouring asperities and laterally loaded asperities. Section 5 discusses directions in the development of models and experiments used or suitable for verifying models. Finally, conclusions concerning accurate contact deformation modelling are presented.
Źródło:
Journal of Machine Engineering; 2019, 19, 4; 91-109
1895-7595
2391-8071
Pojawia się w:
Journal of Machine Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Przyjazne dla środowiska katalizatory redukcji tlenku azotu otrzymane z surowców naturalnych
Environmentally friendly catalysts for reduction of nitrogen oxides derived from the natural raw material-ferrierite
Autorzy:
Ćwikła-Bundyra, W.
Powiązania:
https://bibliotekanauki.pl/articles/1217140.pdf
Data publikacji:
2012
Wydawca:
Stowarzyszenie Inżynierów i Techników Przemysłu Chemicznego. Zakład Wydawniczy CHEMPRESS-SITPChem
Tematy:
Co-ferieryt
Fe-ferieryt
redukcja NO
analiza chromatograficzna
Co-ferrierite
Fe-ferrierite
NO reduction
chromatographic analysis
Opis:
Selektywna katalityczna redukcja NO za pomocą metanu została przeprowadzona dla katalizatorów Co- i Fe-zeolitowych o strukturze ferierytu. Podstawienie jonu kobaltowego pozwoliło zauważyć, że powstałe formy Co w zeolicie kobaltowym mają pozytywny wpływ na przebieg SCR-NO za pomocą metanu, głównie poprzez wzrost poziomu redukcji NO do N2. Aktywność badanych zeolitów w procesie SCR za pomocą CH4 (w odniesieniu do ilości wprowadzonego metalu) można przedstawić następująco: Co-Fer > Fe-Fer dla kontaktów o dużej zawartości wprowadzonego metalu; dla próbek kobaltowych o średniej zawartości wprowadzonego metalu przebieg ten wygląda: Co-Fer > Fe-Fer. Najbardziej aktywne katalizatory charakteryzują się najwyższym ładunkiem metalu w strukturze zeolitu. Głównymi czynnikami wpływającymi na aktywność jonów kobaltowych wydają się być położenie kationu w wewnętrznej strukturze zeolitu, struktura koordynacyjna sieci i właściwości katalityczne jonów Co. Rezultaty przeprowadzonych badań katalitycznych pozwoliły zaobserwować przy zastosowaniu metod steady-state, że redukcja NO zachodzi z dużą szybkością na powierzchni ferierytu w temperaturze powyżej 623 K.
Selective catalytic reduction of NO with methane (CH4-SCR) was investigated over Co- and Fe- zeolites with ferrierite structure. The exchanged Co ions have been shown to exhibit activity in CH4-SCR of NO, while protons or Co species in Co-zeolites contributed to the CH4-SCR activity mostly by the increase of the NO reduction towards N2. The zeolites activity in SCR of NO (described as per metal weight) was determined as follows: Co-Fer > Fe-Fer for the highest Co loadings; for the average content of the Co ion in the zeolite (in terms of Turnovem frequency) it was comparable. The most active catalysts are characterized by the Co-laden large metal structure of the zeolite. The main factors contributing to the individual Co ions activity are suggested to be cation location in the inner zeolite structure, coordination to the framework, and catalytic ability of the Co ions. The results of the catalytic activity investigations using the steady-state methods showed that NO reduction occurs at a reasonable rate on the structure of ferrierite surface at temperatures over 623 K.
Źródło:
Chemik; 2012, 66, 6; 601-610
0009-2886
Pojawia się w:
Chemik
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Instalacja do usuwania siarkowodoru z wód geotermalnych
Installation for removal of hydrogen sulphide from geothermal water
Autorzy:
Banaś, J.
Mazurkiewicz, B.
Solarski, W.
Tadajewski, K.
Powiązania:
https://bibliotekanauki.pl/articles/203605.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Instytut Gospodarki Surowcami Mineralnymi i Energią PAN
Tematy:
woda geotermalna
usuwanie siarkowodoru
aeracja
złoże Fe
geothermal water
removing of hydrogen sulphide
aeration
Fe bed
Opis:
Usuwanie z wód geotermalnych siarkowodoru i innych, niepożądanych składników gazowych jak np. Rn-222 prowadzi się metodami fizycznymi polegającymi na wymianie gazów w układach silnie zdyspergowanych. Znane są techniczne rozwiązania, w których rozpyla się wodę w strumieniu powietrza lub dozuje strumień sprężonego powietrza do oczyszczanej wody. Tworzenie zdyspergowanej fazy wodnej lub gazowej w drugiej fazie ciągłej ma na celu fizyczną separację lotnych związków z oczyszczanej wody i ich przechodzenie do powietrza odlotowego. Według pomysłu autorów sposób usuwania gazów z wody geotermalnej polega na fizycznej separacji fazy gazowej oraz utlenieniu siarkowodoru w układzie trójfazowym: stałe złoże reakcyjne – woda geotermalna – powietrze. Zasadę i efektywność oczyszczania wody zweryfikowano za pomocą instalacji modelowej. Projekt instalacji jest przedmiotem zastrzeżonego wzoru użytkowego (zgłoszenie W.125316 z dnia 08.07.2016).
The removal from geothermal water of hydrogen sulphide and other undesirable gases like Rn-222, may be based on physical methods involving the exchange of gases in highly dispersed systems. Technical solutions are known in which water is sprayed in an air stream or pressurized air is injected into the treated water. The formation of the dispersed gas phase in water or the dispersed liquid phase in the air is intended for the physical separation of volatile compounds from water being treated and to pass into the waste air. According to the authors, the idea of a removal process of gases (hydrogen sulphide and radon) from geothermal water is based on the physical separation of the gas phase and the oxidation of hydrogen sulphide in the three-phase system: solid bed – geothermal water – air. The principle and efficiency of water purification was verified by the laboratory model. The project installation is subject to a proprietary utility model (application W.125316 dated 07/08/2016).
Źródło:
Technika Poszukiwań Geologicznych; 2017, R. 56, nr 1, 1; 39-47
0304-520X
Pojawia się w:
Technika Poszukiwań Geologicznych
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of friction condition on failure location of AA5754 aluminium sheet in Nakajima test
Wpływ warunków tarcia na lokalizację uszkodzenia blachy aluminiowej AA5754 w teście Nakajima
Autorzy:
Slota, J.
Šiser, M.
Powiązania:
https://bibliotekanauki.pl/articles/196160.pdf
Data publikacji:
2018
Wydawca:
Politechnika Rzeszowska im. Ignacego Łukasiewicza. Oficyna Wydawnicza
Tematy:
Nakajima test
friction
strain paths
failure
FE simulation
test Nakajima
tarcie
droga odkształcenia
uszkodzenie
symulacja FE
Opis:
This paper presents the results of numerical and experimental investigations on the influence of friction on failure location in Nakajima formability tests. Finite element (FE) simulations were performed using commercial explicit dynamic FE code. The numerical results obtained from the FE simulation were compared with experimental data from Nakajima tests. A 3D digital image correlation system ARAMIS was used in experiments. The location of failure on the sample was detected depending on friction conditions. The studies confirmed that the crack location near the centre of the specimen as required by the ISO standard could be obtained for low values of the friction coefficient. The numerical simulation combined with the inverse analysis was used to estimate a real value of the friction coefficient in the Nakajima formability test.
W pracy przedstawiono numeryczne i eksperymentalne badania wpływu tarcia na lokalizację uszkodzeń w teście Nakajima. Symulację numeryczną testu przeprowadzono przy użyciu komercyjnego jawnego dynamicznego kodu FE. Wyniki uzyskane z symulacji FE porównano z danymi doświadczalnymi. W badaniach eksperymentalnych wykorzystano system ARAMIS do optycznej korelacji obrazu 3D. Lokalizacja uszkodzenia próbki wykazała zależność od warunków tarcia. Badania potwierdziły, że położenie pęknięcia w pobliżu środka próbki, zgodnie z wymaganiami normy ISO, można uzyskać dla niskich wartości współczynnika tarcia. Do oszacowania rzeczywistej wartości współczynnika tarcia w teście odkształcalności według Nakajima zastosowano symulację numeryczną połączoną z analizą odwrotną.
Źródło:
Zeszyty Naukowe Politechniki Rzeszowskiej. Mechanika; 2018, z. 90 [298], 1; 57-66
0209-2689
2300-5211
Pojawia się w:
Zeszyty Naukowe Politechniki Rzeszowskiej. Mechanika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of filling pressure on formation of total efficiency in the 2SZ-FE engine
Wpływ ciśnienia napełniania na kształtowanie się sprawności ogólnej w silniku 2SZ-FE
Autorzy:
Marek, W.
Sochan, A.
Powiązania:
https://bibliotekanauki.pl/articles/263467.pdf
Data publikacji:
2009
Wydawca:
Sieć Badawcza Łukasiewicz. Przemysłowy Instytut Motoryzacji
Tematy:
napełnianie
silnik 2SZ-FE
sprawność
zmiany ciśnienia
2SZ-FE engine
efficiency
filling
pressure change
Opis:
Investigation results of analysis of filling pressure influence on total engine efficiency at variable phases of the valve timing system setting were presented in this paper. Investigations were performed on a combustion engine of Toyota Prius with Atkinson cycle. Making use of an adequate inlet system and proper choice of timing gear setting in relation to load and rotational speed of the engine 2SZ-FE considerable increments of volumetric efficiency were obtained. Profiting from filling pressure measurements performed by means of an electro optic pressure sensor at constant loads and rotational speeds, and prolonging the charging process increase in general engine efficiency was obtained. Using a phase shifter its direct influence on the working field of the whole engine 2SZ-FE work cycle was shown. A further possibility of filling efficiency increase by changing the inlet system at higher rotational speeds of the engine was indicated.
W pracy przedstawiono wyniki badań analizy wpływu ciśnienia napełniania na sprawność ogólną przy zastosowaniu zmiennych faz rozrządu. Wykorzystując odpowiedni układ dolotowy oraz dobór ustawienia rozrządu w stosunku do obciążenia i prędkości obrotowej silnika 2SZ-FE (Toyota Prius) uzyskano znaczne przyrosty sprawności wolumetrycznej (napełniania). Wykorzystując pomiary ciśnień napełniania optoelektronicznym czujnikiem ciśnienia przy stałych obciążeniach i prędkościach obrotowych, wydłużając procesy ładowania wykazano przyrost sprawności ogólnej. Wykorzystując przesuwnik fazowy wykazano bezpośredni wpływ na pole pracy całego obiegu silnika 2SZ-FE. Wykazano dalszą możliwość wzrostu sprawności napełniania poprzez zmianę układu dolotowego przy wyższych prędkościach obrotowych silnika.
Źródło:
Archiwum Motoryzacji; 2009, 2; 151-163
1234-754X
2084-476X
Pojawia się w:
Archiwum Motoryzacji
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of annealing time and temperature on the Fe3Al intermetallic alloys microstructure modification
Autorzy:
Garbala, K.
Patejuk, A.
Powiązania:
https://bibliotekanauki.pl/articles/380040.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
intermetallic alloy
Fe3Al phase
microstructure modification
stop międzymetaliczny
faza Fe3Al
modyfikacja mikrostruktury
Opis:
There is an industry interesting in intermetallic alloys in recent years. There are widely possibilities to adopt this kind of materials for structural units. More expensive materials can be replaced by them. A property which limits their wider application is the low plasticity at environment and elevated temperatures. In paper the results of the thermal microstructure modification are shown. To this end, the influence of annealing time and temperature on the intermetallic phase Fe3Al grain size was investigated. The impact of these factors on micro-hardness was examined as well. It was found that these operations cause the grain size reduction and the micro-hardness decrease.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 39-42
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wpływ soli Fe3+ na fotokatalityczny rozkład substancji promieniochronnych w wodnej zawiesinie TiO2
Effect of Fe3+ salts on the photocatalytic decomposition of sunscreens in the aqueous suspension of TiO2
Autorzy:
Adamek, E.
Baran, W.
Sobczak, A.
Szczepka, N.
Powiązania:
https://bibliotekanauki.pl/articles/126575.pdf
Data publikacji:
2013
Wydawca:
Towarzystwo Chemii i Inżynierii Ekologicznej
Tematy:
fotokataliza
sole Fe3+
TiO2 P25
substancje promieniochronne
photocatalysis
Fe3+ ions
photodegradation
sunscreens
Opis:
Przedmiotem badań były dwie substancje promieniochronne: benzofenon 4 (BP-4) i kwas fenylenobenzimidazolosulfonowy (PBSA). W pracy zbadano możliwość zwiększenia efektywności procesu fotokatalitycznego utleniania tych związków, prowadzonego w obecności TiO2 P25, po dodaniu soli Fe3+. Roztwory wodne zawierające próbki badanych substancji promieniochronnych naświetlano promieniowaniem UVA (λmax 366 nm) w obecności wyłącznie TiO2 P25 lub soli Fe3+ oraz w mieszaninie TiO2 P25 i soli Fe3+, w każdym przypadku przy pH~3. W próbkach pobieranych podczas naświetlania oznaczano metodą HPLC stężenie nierozłożonych substancji promieniochronnych. W pracy oceniano m.in. dynamikę zmian stężenia tych związków w trakcie procesu fotodegradacji oraz określono jego kinetykę. Stwierdzono, że w warunkach doświadczalnych obie substancje promieniochronne ulegały fotokatalitycznej degradacji, a jony Fe3+ miały wpływ na szybkość tego procesu. Efektywność ich fotodegradacji w mieszaninie TiO2 P25 i soli Fe3+ była większa w porównaniu z analogicznym procesem prowadzonym w obecności samego TiO2 P25. Stwierdzono też, że omawiany proces przebiegał zgodnie z kinetyką reakcji pseudopierwszego rzędu.
The subjects of this study were two sunscreens: 2-hydroxy-4-methoxy benzophenone-5-sulphonic acid (benzophenone 4, BP-4) and 2-phenylbenzimidazole-5-sulfonic acid (PBSA). In this paper the possibility of increasing the photocatalytic oxidation efficiency of these compounds after the addition of Fe3+ salts to TiO2 P25 suspension was studied. Aqueous solutions containing the investigated compounds were irradiated with UVA radiation (λmax 366 nm) in the presence of TiO2 P25 or Fe3 + salt only and in a mixture of TiO2 P25 with Fe3+ salt in all cases at pH ~ 3. In the samples taken during irradiation, the concentrations of undecomposed sunscreens were Wpływ soli Fe3+ na fotokatalityczny rozkład substancji promieniochronnych w wodnej zawiesinie TiO2 279 determined using RP-HPLC method. Additionally, the dynamics of the concentration changes during the photodegradation process and its kinetics were determined. It was found that under experimental conditions, both sunscreens underwent the photocatalytic degradation and Fe3+ ions influenced the rate of this process. Their photodegradation efficiency in the presence of TiO2 P25 with Fe3+ salt was higher than that obtained in the process carried out in the presence of TiO2 P25 alone. Moreover, the process was in accordance with the first-order kinetics.
Źródło:
Proceedings of ECOpole; 2013, 7, 1; 273-279
1898-617X
2084-4557
Pojawia się w:
Proceedings of ECOpole
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Characterization of as-spun and annealed Al-Mn-Fe ribbons
Charakterystyka szybko chłodzonych taśm stopu Al-Mn-Fe w stanie wyjściowym oraz po wygrzewaniu
Autorzy:
Stan, K.
Lityńska-Dobrzyńska, L.
Góral, A.
Wierzbicka-Miernik, A.
Powiązania:
https://bibliotekanauki.pl/articles/354244.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stopy Al-Mn-Fe
mikrostruktura stopu
taśmy stopów
Al-Mn-Fe
quasicrystals
melt-spinning
DSC
TEM
Opis:
Microstructure of conventionally cast and melt spun Al91Mn7Fe2 alloy was examined by X-ray diffraction, SEM and TEM techniques. Three different phases were found in a mould cast ingot: Al6(Mn, Fe), Al4(Mn, Fe) and aluminium solid solution. Rapidly quenched ribbons cast using melt spinning technique with different speed values of rotating wheel: 25, 30 and 36 m/s had average width in a range of 30-50 µ. It was found that ribbons contain quasicrystalline particles with different sizes and shapes including large dendrites in a range of micrometers and smaller spherical particles below 1 µ embedded in an aluminium matrix. Composition of these particles was similar to the Al4(Mn, Fe) phase. Also quasicrystals in the form of eutectic were observed with slightly different composition close to the Al6(Mn, Fe) phase. All observed particles revealed 2, 3 and 5- fold symmetry, typical for icosahedral quasicrystals. Increase in microhardness up to 274 HV for melt spun ribbon comparing to 141 HV for the as-cast ingot was observed due to a change in phase composition and refinement of the phases. Thermal stability of quasicrystalline phase in the ribbon was examined by annealing in different temperatures. Temperatures for thermal treatment were chosen based on DSC curve which contains the exothermic peak in the temperature range 300-500degrees Celsius. Analysis of ribbons annealed for 30 minutes at 400degrees Celsius showed that transformation of quasicrystals to stable crystalline phase starts at quasicrystal/Al-matrix interfaces. After annealing for 4 hours at 500degrees Celsius only the Al6(Mn, Fe) phase and aluminium solid solution were observed in the ribbon microstructure.
Mikrostrukturę stopu Al91Mn7Fe2 odlanego do kokili oraz przygotowanego metoda odlewania na wirujący walec (melt spinning) scharakteryzowano za pomocą dyfrakcji rentgenowskiej oraz transmisyjnej i skaningowej mikroskopii elektronowej. W strukturze wlewka zaobserwowano trzy fazy: Al6(Mn, Fe), Al4 (Mn, Fe) oraz roztwór stały aluminium. Szybko chłodzone taśmy odlano przy trzech różnych prędkościach obracającego się walca: 25, 30 i 36 m/s. Grubość wszystkich otrzymanych taśm wynosiła około 30-50 µm. Mikrostruktura taśm składała sie z cząstek kwazikrystalicznych o zróżnicowanych kształtach i rozmiarach (w tym dużych dendrytów rzędu kilku mikrometrów, oraz mniejszych kulistych cząstek poniżej 1µm). Skład chemiczny tych cząstek był zbliżony do składu fazy Al4(Mn, Fe). Zaobserwowano również kwazikryształy w postaci eutektyki o składzie zbliżonym do składu fazy Al6(Mn, Fe). Uzyskane dyfrakcje elektronowe z obserwowanych cząstek wykazywały symetrie 2, 3 i 5-krotna, typowa dla kwazikryształów ikozaedrycznych. Zmiany składu fazowego oraz rozdrobnienia faz spowodowały wzrost mikrotwardości z 140 HV dla stopu wyjściowego do wartości 270 HV dla taśm. Stabilność termiczna fazy kwazikrystalicznej badano poprzez wygrzewanie taśm w różnych temperaturach, które wybrano w oparciu o krzywa DSC zawierająca pik egzotermiczny w przedziale temperatur 300-500 stopni Celsjusza. Analiza mikrostruktury taśmy wygrzewanej przez 30 min w 400 stopniach Celsjusza wykazała, że przemiana fazy kwazikrystalicznej w stabilna fazę krystaliczna rozpoczyna sie na granicy kwazikryształ/osnowa. Po wygrzewaniu przez 4 godz. w 500 stopniach Celsjusza w strukturze taśmy występowała jedynie faza Al6(Mn, Fe) oraz roztwór stały aluminium.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 3; 651-656
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies