Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "non-alloy steel" wg kryterium: Temat


Wyświetlanie 1-6 z 6
Tytuł:
Influence of heat treatment on corrosion properties of non-alloy steel in acidic environment
Autorzy:
Polasz, Sylwia
Powiązania:
https://bibliotekanauki.pl/articles/243175.pdf
Data publikacji:
2019
Wydawca:
Instytut Techniczny Wojsk Lotniczych
Tematy:
corrosion process
non-alloy steel
corrosion preventive coatings
heat treatment
corrosion allowance
Opis:
The article presents the influence of heat treatment on corrosion properties of non-alloy steel. This steel is used in machine elements. Heat treatment has a major impact on corrosion resistance of steel materials. Laboratory methods for measuring the corrosion rate consist of Electrochemical Impedance Spectroscopy and polarization curves. Instead of these types, there are also industrial methods of velocity corrosion measurements like researches in natural conditions and coupons corrosimetry. These days the most popular techniques of corrosion measurements are electrochemical measurements. In order to conduct impact assessments influent of heat treatment to corrosion properties there is need to proceed few steps like prepare samples, carry out heat treatment, hardness measurements, metallographical examination, prepare samples for corrosion and proceed corrosion researches by potentiodynamic method. An important element during researches is corrosion allowance, which has an impact influent on corrosion properties. This is the most popular and efficient method of corrosion protection. These days for corrosion protection are use paints or zinc coatings, cathode protection or stainless.
Źródło:
Journal of KONES; 2019, 26, 3; 181-188
1231-4005
2354-0133
Pojawia się w:
Journal of KONES
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Investigations of the structure and hardness of dissimilar steel-to-aluminum joints made using laser welding technology
Autorzy:
Misiura, Karolina
Konieczny, Jarosław
Labisz, Krzysztof
Boris, Renata
Powiązania:
https://bibliotekanauki.pl/articles/2098135.pdf
Data publikacji:
2021
Wydawca:
Politechnika Śląska. Wydawnictwo Politechniki Śląskiej
Tematy:
aluminium alloy
non-alloy steel
laser welding
microstructure
structure
stop aluminium
stal niestopowa
spawanie laserowe
mikrostruktura
struktura
Opis:
Since welding technology is currently used to assemble the frame of driver’s seats, it is important to develop laser welding technology for steel and aluminium. For this reason, the purpose of the present work was to examine the structure and selected properties of aluminium-steel joints using the example of an EN AW-6060 aluminium alloy and DC04 low-alloy steel welded in laser technology. Overlapping joints were made, weld type -following the hole laser welding method -laser beam (LB) using a high power disk laser (TRUMPF TruDisk3302), in which the active medium is a yttrium-aluminium crystal (YAG). Metallographic microstructure investigations were carried out using a light microscope from Carl Zeiss - Observer Z1m, and the weld microstructures were investigated using an SEM Supra 35 microscope, also from Carl Zeiss. The chemical composition analysis in micro-areas was carried out using an X-ray energy dispersion spectrometer from EDAX, which was a part of the SEM Supra 35. The hardness of the substrate material and the welded area was measured following the Vickers method using an FM-ARS 9000 micro hardness tester from Tokyo, Japan. It was found that there is a potential for commercial use of laser welding to make a low-carbon steel-aluminium alloy joint. During the formation of the weld in its microstructure, intermetallic compounds of the FexAly type were created, which significantly reduced the mechanical and plastic properties of the joint. The hardness of the weld created wasabout seven times higher than that of DC04 carbon steel. The choice of laser welding parameters (primarily, laser power and beam speed) significantly impacted the weld structure and properties.
Źródło:
Transport Problems; 2021, 16, 1; 73--86
1896-0596
2300-861X
Pojawia się w:
Transport Problems
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The properties of thermal sprayed aluminium coatings on non-alloy structural steel
Autorzy:
Czupryński, A.
Powiązania:
https://bibliotekanauki.pl/articles/366927.pdf
Data publikacji:
2019
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
flame-powder spraying
wire arc spraying
non-alloy structural steel
erosion wear resistance
adhesion strength
impact wear
natryskiwanie płomieniowo-proszkowe
natryskiwanie łukowe
stal niestopowa
stal konstrukcyjna
zużycie erozyjne
zużycie ścierne
wytrzymałość adhezyjna
ścieralność
Opis:
Purpose: of this paper was comparison of the structure, hardness and erosive wear of aluminium coatings produced on non-alloy structural steel S355JR (EN 10025-2) using the powder flame spraying and wire arc spraying methods. Design/methodology/approach: The latest model of flame powder sprayer and wire arc sprayer was used in the experiments. This provided very reliable spraying conditions. The additional material for flame-spraying was of Metco 54NS-1 pure aluminium powder (EN AW 1100 series). In the arc spraying process the Metco Aluminium (EN AW 1100 series) 1.6 mm diameter pure aluminium thermal spray wire was used. In each spraying technology binding alloy, i.e. Ni-Al, was employed as a primer coating. The used spray processes produced dense, abrasion and erosion resistant coatings approximal 1.0 mm thick. Aluminium coatings were characterized in accordance with ASTM G 76-95 erosion resistance tests, ASTM C 633-01 adhesion strength, HV 0.1 hardness tests and metallographic analyses. The scope of research included: preparation material for spraying, selection of properly process parameters for each sprayed technique based on preliminary technological tests, coatings manufacturing, examining the structure and tribological properties of aluminium coatings, comparison of obtained samples. Findings: The obtained results have proven superior properties of arc sprayed aluminium material coatings and have shown to be promising in industrial applications. Research limitations/implications: The presented test results are a preliminary assessment of the properties of thermally sprayed aluminium coatings. Therefore, further research is required regarding the resistance of aluminium coatings to abrasion and corrosion. Practical implications: The study is focused on selecting the best and most economical technique for manufacturing of wear and corrosion resistance aluminium coatings with a thickness of approximately 1 mm. Originality/value: It has been demonstrated that the use of a Ni-Al primer coating improves the adhesion of flame and arc sprayed aluminium coatings to steel surfaces.
Źródło:
Journal of Achievements in Materials and Manufacturing Engineering; 2019, 95, 2; 64-73
1734-8412
Pojawia się w:
Journal of Achievements in Materials and Manufacturing Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Use of Barium and Calcium Alloys in the Ladle Furnace Treatment of Selected Grades of Continuously Cast Steels
Zastosowanie stopów baru i wapnia w obróbce pozapiecowej wybranych gatunków stali odlewanych w sposób ciągły
Autorzy:
Derda, W.
Lawenda, P.
Pardela, P.
Powiązania:
https://bibliotekanauki.pl/articles/353156.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
continuous casting of steel
non-metallic inclusion modification
calcium-barium alloy
steel castability
ciągłe odlewanie stali
modyfikacja wtrąceń niemetalicznych
stop wapń-bar
stal odlewana
Opis:
The subject of the paper are the results of laboratory and industrial investigations into the use of Si - Ca - Ba alloys for modifying non-metallic inclusions. Based on laboratory tests, the morphology and chemical composition of non-metallic inclusions in carbon steel were examined before and after refining with the use of the above-mentioned alloy as a refining addition. In particular tests, variable additions of the alloy were used at a constant refining time and temperature. Comparison of the process of casting of a sequence of seven heats of the same steel grade using the stopper system in the tundish was made under industrial conditions. In these heats, additions of Si - Ca (three heats) and Si - Ca - Ba (four heats) were introduced as a non-metallic inclusion modifier in the form of core wires during the process in the ladle furnace. For the investigated heats, the contents of total oxygen and calcium were assayed in the finished steel. A significant effect of the simultaneous addition of barium and calcium on steel castability, and thus on the process of continuous casting of the investigated heats, was found.
Przedmiotem opracowania są wyniki badań laboratoryjnych oraz przemysłowych, dotyczących zastosowania stopów Si - Ca - Ba do modyfikacji wtrąceń niemetalicznych. Na podstawie badań laboratoryjnych zbadano morfologię i skład chemiczny wtrąceń niemetalicznych w stali węglowej przed i po rafinacji przy zastosowaniu ww. stopu w charakterze dodatku rafinacyjnego. W poszczególnych próbach zastosowano zmienne dodatki stopu przy stałym czasie i temperaturze rafinacji. W warunkach przemysłowych dokonano porównania przebiegu odlewania sekwencji siedmiu wytopów tego samego gatunku stali z zastosowaniem układu zatyczkowego w kadzi pośredniej. W wytopach tych podczas procesu w piecu kadziowym wprowadzono w charakterze modyfikatora wtrąceń niemetalicznych dodatki Si - Ca (trzy wytopy) oraz Si - Ca - Ba (cztery wytopy) w postaci drutów rdzeniowych. Dla badanych wytopów w gotowej stali oznaczono zawartości tlenu całkowitego oraz wapnia. Stwierdzono istotny wpływ jednoczesnego dodatku baru i wapnia na lejność stali, a tym samym na przebieg ciągłego odlewania badanych wytopów.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 1; 281-288
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Some aspects of continuous casting of low carbon microalloyed steels with niobium and titanium
Wybrane aspekty ciągłego odlewania niskowęglowych stali z mikrododatkami niobu i tytanu
Autorzy:
Derda, W.
Wiedermann, J.
Powiązania:
https://bibliotekanauki.pl/articles/354585.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ciągłe odlewanie stali
stal niskostopowa
pęknięcia narożne
fazy niemetaliczne
parametry odlewania
continuous casting of steel
high strength low alloy steel
corner cracks
non-metallic phases
casting parameters
Opis:
An analysis of the causes of transverse corner and surface crack formation during continuous casting of low carbon niobium and titanium-containing steel into square billets is presented in this paper. Using X - ray analysis method, the chemical composition of non- metallic phases inside corner cracks was determined. The temperature ranges of the occurrence of nitrides and carbonitrides of Nb, Ti and Al were established using FactSage 6.2., a commercial computer program. The need for the precise selection of cooling conditions during casting of billets both in the mould and in spray cooling regions was pointed out with the aim of obtaining the optimum surface, and particularly corner temperature of the billet before its entrance to the straightening stand.
W referacie przedstawiono na podstawie badań w warunkach przemysłowych, analizę przyczyn powstawania pęknięć na powierzchni i na narożach wlewków ciągłych o przekroju kwadratowym, odlewanych ze stali niskowęglowych z zawartością niobu i tytanu. Przy użyciu metody mikroanalizy rentgenowskiej dokonano oceny składu chemicznego faz niemetalicznych występujących wewnątrz pęknięć. Z wykorzystaniem programu komputerowego FactSage 6.2 wyznaczono zakresy temperatury występowania azotków i węglikoazotków Nb, Ti, Al. Wskazano na konieczność precyzyjnego doboru warunków chłodzenia odlewanych stali w krystalizatorze oraz w strefie chłodzenia natryskowego celem uzyskania optymalnej temperatury wlewka ciągłego w szczególności na narożach przed operacją jego prostowania w klatce walców ciągnąco - prostujących.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 1; 303-310
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The influence of welding heat input on the quality and properties of high strength low-alloy dissimilar steel butt joints
Wpływ ilości wprowadzonego ciepła na jakość i właściwości dwuimiennych złączy doczołowych ze stali o podwyższonej wytrzymałości
Autorzy:
Tomków, Jacek
Haras, Jacek
Powiązania:
https://bibliotekanauki.pl/articles/115208.pdf
Data publikacji:
2020
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
spawanie MAG
badanie nieniszczące
badanie niszczące
ciepło wejściowe
stal wysokiej wytrzymałości
stal niskostopowa
MAG welding
non-destructive test
destructive test
heat input
high strength steel
low alloy steel
Opis:
The paper presents the results of non-destructive and destructive tests of dissimilar high-strength low-alloy S460ML and S460N steel butt joints. These steels are characterized by similar mechanical properties, but their carbon equivalent CeIIW values are much different. The joints were made using different values of heat input for each welding bead. They were tested by non-destructive methods: visual, penetrant, radiographic and ultrasonic tests. Then, the destructive tests were made: static tensile test, bending test, impact test and Vickers HV10 hardness measurements. The results of prepared examinations showed, that welding with higher heat input has significant impact on the mechanical properties of the dissimilar steel joints - the joint welded with bigger heat input was characterized by better mechanical properties.
W pracy przedstawiono wyniki badań niszczących i nieniszczących dwuimiennych złączy doczołowych wykonanych ze stali o podwyższonej wytrzymałości o zbliżonych właściwościach mechanicznych S460ML i S460N, które znacząco różnią się wartością równoważnika węgla CeIIW. Złącza wykonano z zastosowaniem różnych wartości ilości wprowadzonego ciepła dla poszczególnych ściegów. Zostały one poddane badaniom nieniszczącym: wizualnym, penetracyjnym, radiograficznym oraz ultradźwiękowym. Następnie wykonano statyczną próbę rozciągania, próbę gięcia, badania udarnościowe oraz pomiary twardości metodą Vickersa HV10. Wyniki badań pokazały, że spawanie większą energią liniową ma znaczący wpływ na własności mechaniczne złączy badanych stali - złącze wykonane wyższymi wartościami charakteryzowało się lepszymi własnościami mechanicznymi.
Źródło:
Welding Technology Review; 2020, 92, 2; 15-23
0033-2364
2449-7959
Pojawia się w:
Welding Technology Review
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-6 z 6

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies