Tytuł:
Comparative Studies on Degradation of Varistors Subjected to Operation in Surge Arresters and Surge Arrester Counters
Autorzy:
Papliński, P.
Wańkowicz, J.
Śmietanka, H.
Ranachowski, P.
Ranachowski, Z.
Kudela, S. jr.
Aleksiejuk, M.
Powiązania:
https://bibliotekanauki.pl/articles/351611.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
surge arrester
surge arrester counter
MO varistor
microstructure of ceramics
ceramic material degradation
Opis:
The paper presents results of investigation of microstructure and micro-hardness for material of ZnO varistors applied to 110 kV surge arrester and surge arrester counter. The research combined two pairs of varistors, each consisted of one varistor subjected before to operation, while the other one was brand new unit and constituted a reference. All varistors were made of the same material by the reputable manufacture. The tests revealed a different degree of the material degradation for varistors subjected before to operation. This also refers to different degradation mechanism observed for the material of these varistors, if typical effects of degradation of aged ZnO varistors were considered as a reference. Physical state of spinel in the microstructure had a significant impact on the material degradation, however a considerable loosening of the microstructure associated with bismuth oxide was observed too. It was surprising, since the precipitates of the bismuth oxide phase most often showed very good binding to the ZnO matrix and high resistance to associated electrical, thermal and mechanical effects. The degradation effects in the ZnO matrix proved to be limited only.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 1; 367-374
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Investigation of Microstructure of ZnO Varistors Taken From Surge Arrester Counters
Autorzy:
Papliński, P.
Wańkowicz, J.
Ranachowski, P.
Ranachowski, Z.
Powiązania:
https://bibliotekanauki.pl/articles/355223.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
surge arrester counter
ZnO varistors
microstructure of ceramics
ceramic material degradation
Opis:
The paper presents investigations of microstructure of varistors of damaged surge arrester counters. A similar ZnO varistor, not subjected before to operation, was a point of reference in this research. The results of investigations of the ZnO varistors show an untypical phase composition of their material, which was characterized by unsatisfying homogeneity and cohesion. The degradation processes of varistor material in the subsequent stages were recognized and described. A harmful impact of humidity inside the untight surge arrester counter on its operation and its ZnO varistors was proved. Some conclusions being the result of the operation checking of surge arrester counters were presented too.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 1; 191-196
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Degree of Degradation of ZnO Varistors in Surge Arresters Due to Operation
Autorzy:
Papliński, P.
Wańkowicz, J.
Ranachowski, P.
Ranachowski, Z.
Powiązania:
https://bibliotekanauki.pl/articles/356415.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
surge arrester
MO varistor
microstructure of ceramics
ceramic material degradation
Opis:
The paper presents the test results for the microstructure of ZnO varistors comprising high voltage gapless surge arresters. The tests were performed on varistors produced in different periods and by various manufacturers. The research was inspired by different characteristics of changes in values of current flowing through surge arresters as a function of changes in values of system voltage in a 220 kV substation, and the temperature in a multi-year cycle. Furthermore, the effects of varistor microstructure degradation following a failure of an unsealed surge arrester were investigated. The results provided the grounds for assessment of ZnO varistor microstructure parameters in terms of their durability and resistance to degradation processes.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1267-1273
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ocena stanu technicznego komina murowanego i badania eksperymentalne cegły
Evaluation of the technical condition of the brick masonry chimney and experimental studies of brick
Autorzy:
Barnat-Hunek, D.
Smarzewski, P.
Szafraniec, M.
Powiązania:
https://bibliotekanauki.pl/articles/218282.pdf
Data publikacji:
2015
Wydawca:
Stowarzyszenie Konserwatorów Zabytków
Tematy:
komin murowany z cegły
hydrofobizacja
nasiąkliwość
paroprzepuszczalność
mrozoodporność
mikrostruktura materiału
masonry brick chimney
hydrophobization
absorbability
vapor permeability
frost resistance
microstructure of material
Opis:
W artykule przedstawiono ocenę stanu technicznego komina murowanego z cegły oraz zaproponowano zakres prac remontowych. Badania skuteczności hydrofobizacji komina poprzedziła dokładna diagnostyka obiektu, która polegała na sprawdzeniu m.in. zawartości soli i stopnia zawilgocenia płaszcza komina, ponieważ wysoki stopień zasolenia i duża zawartość wody w porach materiału wyklucza zastosowanie hydrofobizacji. Materiał badawczy stanowiła cegła pobrana z płaszcza przemysłowego komina murowanego. W części eksperymentalnej dokonano obiektywnej oceny preparatów, które mogą być wykorzystane do hydrofobizacji powierzchni komina.
The aim of the research presented in the paper was to evaluate the technical condition of the masonry chimney and to propose scope of modernization process. The studies of effectiveness of hydrophobization were preceded by a thorough diagnosis of the building, which involved checking of the salt content and the degree of moisture of chimney jacket. If the salt content and water content in the pores of the material were too high the hydrophobization could not be used. In presented paper the brick from industrial jacket of chimney was tested. Experimental section contains an objective evaluation of preparations which can be used for the chimney surface hydrophobization.
Źródło:
Wiadomości Konserwatorskie; 2015, 41; 7-19
0860-2395
2544-8870
Pojawia się w:
Wiadomości Konserwatorskie
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies