Usable Properties of AlSi7Mg Alloy after Sodium or Strontium Modification
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, M.
Trytek, M.
Markowska, O.
Powiązania:
https://bibliotekanauki.pl/articles/381773.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloy AlSi7Mg
refining
modification
cooling rate
microstructural parameters
usable properties
stop AlSi7Mg
rafinacja
modyfikacja
szybkość chłodzenia
parametry mikrostruktury
właściwości użytkowe
Opis:
The paper deals with the effect of microstructure diversified by means of variable cooling rate on service properties of AlSi7Mg cast alloy refined traditionally with Dursalit EG 281, grain refining with titanium-boron and modified with sodium and a variant of the same alloy barbotage-refined with argon and simultaneously grain refining with titanium-boron and modified with strontium. For both alloy variants, the castings were subject to T6 thermal treatment (solution heat treatment and artificial aging). It turned out that AlSi7Mg alloy after simultaneous barbotage refining with argon and grain refining with titanium-boron and modified with strontium was characterised with lower values of representative microstructure parameters (SDAS – secondary dendrite arm spacing, λE, lmax) and lower value of the porosity ratio compared to the alloy refined traditionally with Dursalit EG 281 and grain refining with titanium-boron and modified with sodium. The higher values of mechanical properties and fatigue strength parameters were obtained for the alloy simultaneously barbotage-refined with argon and grain refining with titanium-boron and modified with strontium.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 129-132
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermal Coefficients of the GTAW Process
Autorzy:
Orłowicz, A. W.
Trytek, A.
Tupaj, M.
Mróz, M.
Powiązania:
https://bibliotekanauki.pl/articles/383027.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
thermal efficiency
remelting process
flow calorimeter
sprawność cieplna
przetapianie
kalorymetr przepływowy
Opis:
The paper presents a discussion on the issue of thermal efficiency of the process of superficial remelting of castings by means of the gas tungsten arc welding (GTAW) process. Described and characterized are calorimeters used in research studies on efficiency of welding processes and the obtained results. Example results are presented from the measurements aimed at determination of thermal efficiency of the welding process carried out with the use of the flow calorimeter.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 63-68
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of the Return Material Implementation into the Production of Silumin Casts on Technological and Economic Indicators of Production Process
Autorzy:
Gaspar, S.
Majernik, J.
Trytek, A.
Podaril, M.
Benova, Z.
Powiązania:
https://bibliotekanauki.pl/articles/2126917.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
HPDC
product development
quality management
mechanical properties
castings defects
rozwój produktu
zarządzanie jakością
właściwości mechaniczne
wady odlewów
Opis:
The production of high pressure die casts also brings difficulties regarding the processing of the waste material. It is mainly formed by runners, overflows and other foundry supplements used and, in the case of machines using the cold chamber, also the remainder from this chamber. As this material is often returned to the production process, we refer to it as return material. In the production process, it is therefore essential to deal with the proportion issue of return material against primary material that can be added to the melt to maintain the required cast properties. The submitted article monitors the quality properties of the alloy, selected mechanical properties of casts and porosity depending on the proportion of the return material in the melt. At the same time, the material savings are evaluated with regards to the amount of waste and the economic burden of the foundries. To monitor the above-mentioned factors, series of casts were produced from the seven melting process variants with a variable ratio of return to the primary material. The proportion ratio of return material in the primary alloy was adjusted from 100% of the primary alloy to 100% of the return material in the melting process. It has been proven that with the increasing proportion of the return material, the chemical composition of the melt changes, the mechanical properties of the alloy decrease and the porosity of the casts increases. Based on the results of the tests and analyzes, the optimal ratio of return and primary material in the melting process has been determined. Considering the prescribed quality of the alloy and mechanical properties, concerning the economic indicator of the savings, the ratio is set at 70:30 [%] in favor of the primary material.
Źródło:
Archives of Foundry Engineering; 2022, 22, 1; 69--76
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of the Heat Flux Density on Microstructure of Surface Remeltings on C355 Alloy Castings
Autorzy:
Orłowicz, A. W.
Mróz, M.
Tupaj, M.
Trytek, A.
Jacek, M.
Radoń, M.
Powiązania:
https://bibliotekanauki.pl/articles/382629.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
C355 alloy
surface remelting
concentrated heat stream
surface microstructure
stop C355
utwardzanie powierzchniowe
strumień ciepła
mikrostruktura powierzchni
Opis:
The paper presents results of a study on the effect of the flux density of heat carried away for the remelting area to substrate in the course of surface remelting with concentrated heat stream on values of structural parameters λ1D and λ2D of α(Al) phase dendrites in C355 alloy. The remeltings were made with the use of GTAW method, at arc current intensity I = 200 A and concentrated heat stream scanning speed vs = 200, 400, 600, and 800 mm/min. The used protective gas was argon supplied at rate of 20 l/min. It has been found that the increase of the rate of scanning with concentrated heat stream results in a change of the remelting-substrate separation surface shape consisting in reduction of the remelting width and depth. This increases the value of the flux density of heat transmitted from the remelting area to substrate which in turn acts in favor of reduction of structural parameters λ1D and λ2D characterizing α(Al) phase dendrites in C355 alloy.
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 35-38
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of Refining and the Cooling Rate on Microstructure and Mechanical Properties of AlSi7Mg Alloy
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/381386.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
AlSi7Mg alloy
material compactness
microstructure parameter
mechanical properties
stop AlSi7Mg
zwięzłość materiału
właściwości mechaniczne
Opis:
The paper presents results of research on the effect of conventional refining with hexachloroethane and the cooling rate vcool. ranging within the solidification temperature regime from 12.5°C/min to 94.5°C/min on compactness of the material, values of microstructure parameters λ2D, λE, lmaxSi, and mechanical properties Rm, R0,2, A5 of unmodified AlSi7Mg alloy after heat treatment (solution treatment 540°C/6 h/water 20°C and aging 175°C/8 h/air). It has been found that as a result of refining and increased cooling rate, an improvement of material compactness occurred (reduction of the density index by 0.4%) accompanied by a decrease of values of parameters characterizing the microstructure: λ2D by 54.4 μm; λE by 4,6 μm; and lmaxSi by 50 μm. As a result of these changes, the value of Rm increased by about 40 MPa and R0.2 improved by about 36 MPa, while the value of A5 decreased by 1.3%.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 83-86
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of Cooling Rate on Properties of Intermetallic Phase in a Complex Al-Si Alloy
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, M.
Trytek, A.
Markowska, O.
Powiązania:
https://bibliotekanauki.pl/articles/380384.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloy Al-Si
intermetallic phase
cooling rate
silicon crystals
stop Al-Si
faza międzymetaliczna
szybkość chłodzenia
kryształy krzemu
Opis:
The cooling rate is one of the main tools available to the process engineer by means of which it is possible to influence the crystallisation process. Imposing a desired microstructure on a casting as early as in the casting solidification phase widens significantly the scope of technological options at disposal in the process of aluminium-silicon alloy parts design and application. By changing the cooling rate it is possible to influence the course of the crystallisation process and thus also the material properties of individual microstructure components. In the study reported in this paper it has been found that the increase of cooling rate within the range of solidification temperatures of a complex aluminium-silicon alloy resulted in a decrease of values of the instrumented indentation hardness (HIT) and the instrumented indentation elastic modulus (EIT) characterising the intermetallic phase occurring in the form of polygons, rich in aluminium, iron, silicon, manganese, and chromium, containing also copper, nickel, and vanadium. Increased cooling rate resulted in supersaturation of the matrix with alloying elements.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 125-128
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of Carbides Orientation in NC11 Steel on Scratch Susceptibility of Die Inserts Used to Press Stampings for Refractory Shapes
Autorzy:
Orłowicz, A. W.
Mróz, M.
Tupaj, M.
Trytek, A.
Kupiec, B.
Korzeniowski, M.
Sondej, K.
Kozak, L.
Powiązania:
https://bibliotekanauki.pl/articles/947360.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
steel NC11
die insert
scratch
stal NC11
wkładka
zarysowania
Opis:
NC11 steel, in view of the specificity of its manufacturing process, is characterised with band-like orientation of carbides. Depending on the direction of cutting the material for the inserts out of commercially available steel products, carbide bands can be oriented in parallel or perpendicularly to the direction in which aggregate grains move in the process of pressing stampings. It has been found that in case of scratches made in direction perpendicular to carbide bands, depth of the scratches is less than this observed when scratches are made in direction coinciding with prevailing orientation of carbide precipitates.
Źródło:
Archives of Foundry Engineering; 2016, 16, 2; 95-98
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of a Thin-Wall Casting Mould Cavity Filling Conditions on the Casting Surface Quality
Autorzy:
Trytek, A.
Orłowicz, A. W.
Tupaj, M.
Mróz, M.
Markowska, O.
Bąk, G.
Abram, T.
Powiązania:
https://bibliotekanauki.pl/articles/382148.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
thin wall casting
grey cast iron
cold shots
computer simulation
odlew cienkościenny
żeliwo szare
symulacja komputerowa
Opis:
The paper presents results of metallographic examination of faults occurring in the course of founding thin-walled cast-iron castings in furan resin sand molds. A non-conformance of the scab type was Observed on surface of the casting as well as sand buckles and cold shots. Studied the chemical composition by means of a scanning electron microscope in a region of casting defects: microanalysis point and microanalysis surface. Around the observed defects discloses high concentration of oxides of iron, manganese and silicon. A computer simulation of the casting process has been carried out with the objective to establish the cause of occurrence of cold shots on casting surface. The simulation was carried out with the use of NovaFlow & Solid program. We analyzed the flowing metal in the mold cavity. The main reason for the occurrence of casting defects on the surface of the casting was gating system, which caused turbulent flow of metal with a distinctive splash stream of liquid alloy.
Źródło:
Archives of Foundry Engineering; 2016, 16, 4; 222-226
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Surface Hardening of Nodular Cast Iron by GTAW Remelting
Autorzy:
Orłowicz, A. W.
Trytek, A.
Korzeniowski, M.
Kupiec, B.
Powiązania:
https://bibliotekanauki.pl/articles/379624.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
solidification process
mechanical properties
nodular cast iron
GTAW process
surface layer
proces krzepnięcia
właściwości mechaniczne
żeliwo sferoidalne
proces GTAW
warstwa powierzchniowa
Opis:
The study reported in this paper was aimed at establishing the effect of values of parameters characterizing the process of superficial remelting of a nodular iron casting on the quantity of introduced heat, geometry of remeltings as well as parameter λ and hardness of cementite eutectic. The remelting process was carried out using GTAW method, at electric arc length of 3 mm in argon atmosphere, welding current intensities I = 50, 130, 210, and 300 A, and electric arc scanning speeds vs = 200, 400, and 800 mm/min. The measurements included estimation of the quantity of heat introduced to the casting in the electric arc-induced remelting process with the use of flow calorimeter. Widths and depths of remetlings were assessed with the use of metallographic method. As a result of fast solidification, cementite eutectic was obtained in remelted material in which, in the course of cooling down to ambient temperature, austenite was subject to partial transformation into martensite. To characterize the cementite eutectic, value of the structural parameter λ was assessed. Values of the parameter were similar for areas of occurrence of both fibrous and laminated eutectic. Remeltings were examined at half of their depths. Micro-hardness measurements were taken in the same areas. The established quantitative relationships may prove to be useful in practice for the purpose of predicting values of parameter λ and hardness of remeltings in studies aimed at improving resistance of cast-iron castings to abrasive wear.
Źródło:
Archives of Foundry Engineering; 2018, 18, 3; 53-58
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Stress rupture test of MAR-M509 alloy with structure refined by rapid resolidification
Autorzy:
Mróz, M.
Orłowicz, W.
Tupaj, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/380450.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop MAR M509
mikrostruktura
MAR-M509 alloy
rapid resolidification
microstructure
stress rupture test
Opis:
This study presents results of stress rupture test of MAR-M-509 cobalt alloy samples, as-cast and after surface refining with a concentrated stream of heat. Tests were conducted on samples of MAR-M-509 alloy castings, obtained using the lost-wax method. Casting structure refining was performed with the GTAW method in argon atmosphere, using the current I = 200 A and electrical arc scanning velocity vs = 100, 150, 200 and 250 mm/min. The effect of rapid resolidification of the MAR-M-509 alloy on the microstructure was examined and significant improvement in stress rupture test was observed.
Źródło:
Archives of Foundry Engineering; 2012, 12, 4; 117-120
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Shaping the Microstructure of Cast Iron Automobile Cylinder Liners Aimed at Providing High Service Properties
Autorzy:
Orłowicz, A. W.
Mróz, M.
Tupaj, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/381241.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
cast iron
automobile cylinder
service properties
żeliwo
cylinder samochodowy
właściwości użytkowe
Opis:
The paper presents an analysis of factors affecting the wear of cylinder liners. The effect of the graphite precipitation morphology on the cylinder liner wear mechanism is presented. Materials used to cast cylinder liners mounted in a number of engines have been examined for their conformity with requirements set out in applicable Polish industrial standard. A casting for a prototype cylinder liner has been made with a microstructure guaranteeing good service properties of the part.
Źródło:
Archives of Foundry Engineering; 2015, 15, 2; 79-84
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Proces niskotemperaturowej biokatalizy na przykładzie grzybowej biotransformacji [alfa]-pinenu
Low-temperature biocatalysis as an example of microbial biotransformation of alpha-pinene
Autorzy:
Skowroński, J.
Trytek, M.
Fiedurek, J.
Powiązania:
https://bibliotekanauki.pl/articles/256660.pdf
Data publikacji:
2013
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Technologii Eksploatacji - Państwowy Instytut Badawczy
Tematy:
biokataliza
biotransformacja
drobnoustroje psychrotroficzne
biocatalysis
biotransformation
psychrotrophic microorganisms
Opis:
Katalizatory warunkują przebieg oraz odpowiednią wydajność wielu reakcji chemicznych. Przemiany biochemiczne w większości przypadków katalizowane są z udziałem enzymów. Szczególne cechy biokatalizatorów są powszechnie wykorzystywane w przemyśle, a w ostatnich latach drobnoustroje ekstremofilne, adaptowane do skrajnych warunków abiotycznych, wzbudzają duże zainteresowanie licznej grupy badaczy. Wyjątkowe predyspozycje biokatalizatora psychrotroficznego z dobrymi efektami zostały wykorzystane w procesie biotransformacji a-pinenu do werbenolu i werbenonu, będących cennymi związkami smakowo-zapachowymi stosowanymi w branży spożywczej i kosmetycznej. Uzyskane wyniki (sumaryczne stężenie produktów przekraczające 0,5 g/dm3) stanowią obiecującą perspektywę wykorzystania tego typu procesów w większej skali (ponadlaboratoryjnej).
Many chemical reactions and their appropriate performance depend on catalysis. Most biochemical reactions are catalysed by enzymes. Special features of these biocatalysts are commonly employed in industry and current researches are focused on psychrotrophic microorganisms. These unique organisms can be a rich source of useful biocatalysts for biotransformation of a-pinene to verbenol and verbenone - valuable compounds used as flavours and fragrances. Results obtained in this study are promising for further application in the large scale.
Źródło:
Problemy Eksploatacji; 2013, 1; 101-111
1232-9312
Pojawia się w:
Problemy Eksploatacji
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Morphology and Material Properties of Carbides in High (24%) Chromium Cast Iron
Autorzy:
Orłowicz, A. W.
Mróz, M.
Tupaj, M.
Trytek, A.
Jacek, M.
Radoń, M.
Powiązania:
https://bibliotekanauki.pl/articles/947498.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
high chromium cast iron
microstructure
material properties
nanoindentation test
żeliwo wysokochromowe
mikrostruktura
właściwości materiału
próba nanoindentacji
Opis:
The present paper is a presentation of results of a study on morphology, chemical composition, material properties (HVIT, HIT, EIT), and nanoindentation elastic and plastic work for carbide precipitates in chromium cast iron containing 24% Cr. It has been found that the carbides differ in chemical composition, as well as in morphology and values characterizing their material properties. The carbides containing the most chromium which had the shape of thick and long needles were characterized with highest values of the analyzed material properties.
Źródło:
Archives of Foundry Engineering; 2018, 18, 1; 77-80
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Materials Used in the Automotive Industry
Autorzy:
Orłowicz, A. W.
Mróz, M.
Tupaj, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/383174.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
automotive industry
foundry material
casting technique
przemysł motoryzacyjny
materiał odlewniczy
technika odlewnicza
Opis:
Elaborated shapes of many car components are the reason for which the use of casting techniques to fabricate them is a solution wellfounded from the economical point of view. Currently applicable regulatory requirements concerning emissions of exhaust fumes force the carmakers to reduce the overall weight of their products, as this is a basic precondition for reducing fuel consumption. As a result, newly launched car models contain a continuously increasing share of thin-walled castings made of materials which ensure a satisfactory level of service properties. At the same time, developing new technological processes allowing to extend the service life of individual components by means of surface improving becomes more and more important.
Źródło:
Archives of Foundry Engineering; 2015, 15, 2; 75-78
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Materials Properties of Iron-rich Intermetallic Phase in a Multicomponent Aluminium-Silicon Alloy
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/381828.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloys Al-Si
intermetallics phase
Fe-rich
primary crystals
silicon
stopy Al-Si
faza międzymetaliczna
wzbogacanie żelazem
kryształy pierwotne
krzem
Opis:
Available technical literature includes a number of reports on harmful effects connected with elevated content of iron in aluminium-silicon alloys but in case of pressure castings, alloys containing up to 2% Fe can be used. This follows from lesser susceptibility of such alloys to sticking to surfaces of metal moulds. One effect of iron presence in aluminium-silicon alloys is precipitation of iron-rich intermetallic phases. In the study reported in this paper it has been found that in a multicomponent aluminium-silicon alloy, the indentation hardness (HIT) and the elastic indentation modulus (EIT) of intermetallic phases occurring in the form of polyhedrons and/or their conglomerates, rich in aluminium, iron, silicon, manganese, and chromium, containing also copper, nickel, and vanadium, are higher than those measured for silicon crystals. This feature can be used to intentional modelling microstructure of mechanical parts which are expected to show high resistance to abrasive wear.
Źródło:
Archives of Foundry Engineering; 2015, 15, 1 spec.; 111-114
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies