Tytuł:
Comparative Study on Mechanical Performances of Circular and Flat Geometry Welds in Friction Stir Welding of Aluminium Alloy
Autorzy:
Senthil, S. M.
Ragu Nathan, Seerangan
Parameshwaran, Rathinasamy
Bhuvanesh Kumar, M.
Powiązania:
https://bibliotekanauki.pl/articles/2049402.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
FSW
aluminium pipe
aluminium plate
tensile test
hardness test
Opis:
This study is to find the extent of variation in mechanical properties between plate and pipe welds fabricated out of the same FSW process parameters. Common thickness of 3 mm along with similar tool specifications is used to fabricate the weld. Process parameters of tool rotational speed 2000 rpm and weld speed 94 mm/min that was defined as optimal for pipe weld is used as common process parameters. Welds are analyzed for hardness and tensile properties. Yield strength and ultimate tensile strength varied about 8.1% and 11.2% respectively between plate and pipe welds. The hardness of the stir zones varied about 11.6% between plate and pipe welds.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 3; 881-886
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication of a Novel Silver-Based Electrical Contact Composites and Assessment of Its Mechanical and Electrical Properties
Autorzy:
Kumar, Praveen S.
Senthil, S. M.
Parameshwaran, Rathinasamy
Rathanasamy, Rajasekar
Powiązania:
https://bibliotekanauki.pl/articles/2049131.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
silver tin oxide
electrical contact
composites
tungsten oxide
conductivity
Opis:
The electrical contactors play a crucial role in closing the circuit in many power distribution components like overhead lines, underground cables, circuit breakers, transformers, and control systems. The failure in these components mainly occurs due to the break-down of contactors due to the continuous opening and closing action of contacts. Silver (Ag)-based oxide contact materials are widely used in practice, among which silver tin oxide (AgSnO2) is most common. An attempt is made in increasing the performance of AgSnO2, by adding Tungsten Oxide (WO3) in various weight proportions, thus finding the optimal proportion of AgSnO2WO3 to have increased mechanical and electrical performances. All the composite samples are fabricated in-house using powder metallurgy process. The assessment of physical and electrical properties namely, density, hardness, porosity, and electrical conductivity, showed that 90%Ag-8.5%SnO2-1.5%WO3 composite yielded superior results. With help of morphological tests, wear characteristics are also investigated, which showed that 90%Ag-8.5%SnO2-1.5%WO2 composite has a wear coefficient of 0.000227 and a coefficient of friction of 0.174 at an optimized load of 10 N and sliding velocity of 0.5 mm/s.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 4; 1087-1094
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies