Microstructure of Friction Stir Welded Dissimilar Wrought 2017A and Cast AlSi9Mg Aluminum Alloys
Autorzy:
Kopyściański, M.
Dymek, S.
Hamilton, C.
Węglowska, A.
Pietras, A.
Szczepanek, M.
Wojnarowska, M.
Powiązania:
https://bibliotekanauki.pl/articles/1032926.pdf
Data publikacji:
2017-05
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
friction stir welding
aluminum alloys
microstructure
Opis:
Friction stir welding was applied to join dissimilar aluminum alloys: wrought 2017A and cast AlSi9Mg. The produced weldment was free from cracks and any discontinuities. The weld microstructure was composed of alternating bands of the welded alloys; however, the alloy that was placed on the advancing side (AlSi9Mg) dominated the weld center. The grain size within the particular bands was similar in both alloys. The hardness profile reflected the microstructure formed during welding. The weld microstructure as well as the shape of hardness profile across the weld were justified by numerical simulation of material flow during welding.
Źródło:
Acta Physica Polonica A; 2017, 131, 5; 1390-1393
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Development of Empirical Relationships for Prediction of Mechanical and Wear Behavior of Copper Matrix Surface Composite by Friction Stir Processing Technique
Autorzy:
Saravanakumar, S.
Gopalakrishnan, Saravanan
Kalaiselvan, K.
Powiązania:
https://bibliotekanauki.pl/articles/2049739.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir processing
microstructure
microhardness
wear
Opis:
In this investigation, Copper Matrix Surface Composites (CMSCs) were reinforced with various ceramic particles like Aluminum Nitrate (AlN), Titanium diboride (TiB2), and Rice Husk Ash (RHA) are used to increase the metallurgical and mechanical properties by Friction Stir Processing (FSP). The Design of the Experiment (DOE) Taguchi L9 orthogonal array method was used. The process parameters considered were groove width and various types of reinforcement particles. The fabrication of CMSCs was achieved by using optimized process parameters, such as the tool transverse speed of 40 mm/min, rotational tool speed of 1000 rpm, and an axial load of 10 kN with one pass. The influence of FSP process parameters on CMSCs in the stir zone is observed through optical microscope (OM), Field Emission Scanning Electron Microscope (FESEM), and Transmission Electron Microscope (TEM). Mechanical properties such as microhardness and wear rate are studied and compared. It reveals that good interfacial bonding was produced between ceramic particles in CMSCs. TiB2 reinforced with copper matrix surface composites enhance microhardness and had a lesser wear rate.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 2; 617-626
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Optimization of T-6 cycle and Characterization of Si3N4 Reinforced High Strength Aluminum Metal Matrix Composites
Autorzy:
Kumar, Ashish
Rana, Ravindra Singh
Purohit, Rajesh
Namdev, Anurag
Powiązania:
https://bibliotekanauki.pl/articles/28099516.pdf
Data publikacji:
2023
Wydawca:
Polska Akademia Nauk. Czasopisma i Monografie PAN
Tematy:
stir casting
microstructure
mechanical properties
optimization
fractography
Opis:
In this research, AA7068/Si3N4 composites were fabricated through stir casting with the attachment of ultrasonic treatment. The quenching medium and aging duration significantly influenced the hardness of Al alloy samples. Peak hardness was achieved after 12 h of artificial aging at the temperature of 140°C. The addition of nano Si3N4 significantly refined the microstructure of unreinforced AA7068. The dispersion of intermetallic compounds (MgZn2) and grain boundary discontinuation were noticed after the T-6 heat treatment. Ultimate tensile strength, yield strength, and hardness were improved by 70.95%, 76.19%, and 44.33%, respectively, with the addition of 1.5 weight % Si3N4 compared to as-cast alloy due to the combined effect of heat treatment, hall-Petch, Orowan, thermal miss match, load-bearing strengthening mechanisms and uniform dispersion of reinforcement. A reduction in percentage elongation was noticed due to composites’ brittle nature by the effect of ceramic Si3N4 particles’ inclusion. The fracture surfaces reveal ductile failure for alloy and mixed-mode failure in the case of composites.
Źródło:
Archives of Metallurgy and Materials; 2023, 68, 2; 775--783
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Mechanical Properties of Friction Stir Welded Joints between Commercially Pure Copper and Al 6351 Alloy
Autorzy:
Sinha, V. C.
Kundu, S.
Chatterjee, S.
Powiązania:
https://bibliotekanauki.pl/articles/350852.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir welding
tensile strength
microstructure
intermetallics
Opis:
In the present study, the effect of tool rotational speed on microstructure and mechanical properties of friction stir welded joints between commercially pure copper and 6351 Al alloy was carried out in the range of tool rotational speeds of 300-900 rpm in steps of 150 rpm at 30 mm/minutes travel speed. Up to 450 rpm, the interface of the joints is free from intermetallics and Al4 Cu9 intermetallic has been observed at the stir zone. However, Al4 Cu9 intermetallic was observed both at the interface and the stir zone at 600 rpm. At 750 and 900 rpm tool rotational speed, the layers of AlCu, Al2 Cu3 and Al4 Cu9 intermetallics were observed at the interface and only Al4 Cu9 intermetallics has been observed in the stir zone. The maximum ultimate tensile strength of ~207 MPa and yield strength of ~168 MPa along with ~6.2% elongation at fracture of the joint have been obtained when processed at 450 rpm tool rotational speed.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 3; 1819-1825
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication of Aluminum - Cr3C2 Surface Composites through Friction Stir Processing and Analyzing its Microstructural and Mechanical Evolution
Autorzy:
Satheeshkumar, J.
Jayaraman, M.
Priyadharshini, G. S.
Sathya Mukesh, C. S.
Powiązania:
https://bibliotekanauki.pl/articles/352635.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
microstructure
microhardness
friction stir processing
ADC-12
chromium carbide
Opis:
In this paper, aluminium alloy of grade ADC-12 was considered as a base metal and chromium carbide (Cr3C2) particles were reinforced through friction stir process. A detailed analysis of mechanical property and metallurgical characterization studies were performed to evaluate the surface composite. Remarkable changes were observed in the developed composite due to the mechanical force produced by the stir tool with an increase in hardness. The metallurgical investigation infers that the presence of silica in ADC-12 alloys has undergone mechanical fracture and long needle structure changed to reduced size. On the other hand, at higher tool rotational speed, the uniform distribution of hard particles was confirmed through SEM micrographs. Thus the modified surface composite has produced good mechanical property with high metallurgical qualities.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 4; 1527-1532
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
An Analysis of Microstructure and Mechanical Properties on Friction Stir Welded Joint of Dissimilar 304 Stainless Steel and Commercially Pure Aluminium
Autorzy:
Balamagendiravarman, M.
Kundu, S.
Chatterjee, S.
Powiązania:
https://bibliotekanauki.pl/articles/353188.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir welding
dissimilar materials
microstructure
mechanical properties
weld nugget
Opis:
In this study, friction stir welding of dissimilar 304 stainless steel and commercially pure aluminium was performed under the following condition of tool rotational speed 1000 rpm, traverse speed 60 mm/min and tool tilt angle 2 degree. Microstructural characterisation was carried out by optical microscope, scanning electron microscope (SEM). Optical images shows that the microstructural change is very minimum in steel side when compared to aluminium side due to the difference in mechanical and thermal properties. The intermetallic compound Al3Fe was observed at the interfacial region and stir region of the welded joint. The maximum ultimate tensile strength is 78% of commercially pure aluminium base metal. Microhardness profile was measured across the weld interface and the maximum value reaches at the stir zone due to the formation of intermettalics.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 3; 1813-1817
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Experimental investigation and modelling of Friction Stir Processing of cast aluminium alloy AlSi9Mg
Autorzy:
Węglowski, M. S.
Dymek, S.
Hamilton, C. B.
Powiązania:
https://bibliotekanauki.pl/articles/200339.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir processing
aluminum alloys
numerical modelling
neural networks
microstructure
Opis:
Friction Stir Processing (FSP) is a novel solid state processing technique which can be used for microstructural modification of surface layers in metallic materials. This paper analyzes the effects of FSP process parameters on spindle torque acting on the tool and on the tool temperature. It has been shown that an increase in the rotational speed brings about a decrease in the torque and an increase of temperature. For temperature estimation in the stir zone a numerical model was applied, while for predicting a relationship between the spindle torque acting on the tool, rotational and travelling speeds and the down force, the artificial neural networks approach was employed. Light and electron (scanning and transmission) microscopy investigation showed that the FSP process reduces porosity and produces a more uniform distribution of second-phase particles.
Źródło:
Bulletin of the Polish Academy of Sciences. Technical Sciences; 2013, 61, 4; 893-904
0239-7528
Pojawia się w:
Bulletin of the Polish Academy of Sciences. Technical Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Microstructure and Mechanical Properties of Al 3003 Alloy Weld by Stationary Shoulder Friction Stir Welding Process
Autorzy:
Jung, Woo-Chul
Park, Joo-Heon
Yoon, Sang-Min
Kim, Young Kyun
Powiązania:
https://bibliotekanauki.pl/articles/2203728.pdf
Data publikacji:
2023
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stationary shoulder friction stir welding
aluminum 3003 alloy
microstructure
mechanical properties
Opis:
The lap joint welding of Al 3003 alloy by stationary shoulder friction stir welding (SSFSW) was performed under the conditions of tool rotation and welding speed, and it was confirmed that the welding was performed under all conditions. The tunnel defects and pores were formed in the weld zone at the lowest tool rotation and welding speed, and it is increased, the weld surface has been improved. At the same tool rotation speed at the welding speed is increased, the grain size was refined in the stir zone (SZ) and thus the hardness increased by about 14% compared to the base metal. The tensile shear strength is measured to be 10 kN or more under most conditions, and in the 4000 rpm with high heat input, the shear tensile strength was measured relatively lower than other conditions due to excessive heat input of the material.
Źródło:
Archives of Metallurgy and Materials; 2023, 68, 1; 113--118
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effects of Friction Stir Welding Parameters on Microstructure, Fatigue Life and Tensile Properties of Aluminum 2024-T3 Alloy
Autorzy:
Şık, Aydın
Özer, Alpay
Powiązania:
https://bibliotekanauki.pl/articles/27313860.pdf
Data publikacji:
2023
Wydawca:
Polska Akademia Nauk. Czasopisma i Monografie PAN
Tematy:
friction stir welding
microstructure
fatigue life
tensile properties
Al 2024-T3
Opis:
In this study, Al 2024-T3 alloy plates were joined by using friction stir welding. Welding was performed at a rotational speed of 930, 1450, 2280 rpm and a welding feed rate of 180 mm min-1. The welded samples were analyzed at the microstructural level. Moreover, both bending fatigue tests and tensile tests were performed on samples. At the end of the microstructural examination of the samples welded at the rotational speed of 930 rpm and the welding feed rate of 180 mm min-1, the formation of tunnel defects was observed. The highest fatigue life was obtained at 2280 rpm and 180 mm min-1. The lowest fatigue life was obtained at 930 rpm and 180 mm min -1. The highest ultimate tensile stress was obtained at 2280 rpm/180 mm min-1 sample, which shows about a 12% reduction relative to the base material. The lowest ultimate tensile stress was obtained at 930 rpm/180 mm min-1 sample. The ultimate tensile stress value of the 930 rpm/180 mm min-1 sample decreased by approximately 25%.
Źródło:
Archives of Metallurgy and Materials; 2023, 68, 2; 499--505
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructural Characterisation of Friction Stir Processed Cast AlSi9Mg Aluminium Alloy
Autorzy:
Węglowski, M. S.
Powiązania:
https://bibliotekanauki.pl/articles/379980.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
cast aluminium alloy
friction stir processing
FSP
microstructure
stop aluminium
obróbka tarciowa
mikrostruktura
Opis:
Aluminium alloy castings become more popular when a refined microstructure and a uniform distribution of Si particles are easily produced. One of the technologies that can fulfil these requirements is Friction Stir Processing (FSP). Therefore, the formation of various microstructural regions during FSP of AlSi9Mg alloy has been studied. It is presented that each of the regions are characterized by unique microstructures. Prior to FSP, the microstructure of a representative as-cast aluminium alloy was composed of Al dendrites and a nonuniform distribution of Si and Fe. FSP microstructurally modified and significantly refined the as-cast material, effectively eliminating the microstructural segregation and porosity of the base material. The characteristic microstructures are reflected in the hardness distribution. The hardness of the modified area was different from the base material.
Źródło:
Archives of Foundry Engineering; 2014, 14, 3 spec.; 75-78
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
High Cycle Fatigue Performance of Hollow-Extruded 6005A-T6 Aluminum Alloy Characterized by a Layered Microstructure
Autorzy:
Ma, Zhongwei
Ma, Lin
Xu, Bo
Dan, Chuchen
He, Zhaokun
Wang, Yue
Powiązania:
https://bibliotekanauki.pl/articles/354038.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir welding
hollow-extruded 6005A-T6 aluminum alloy
fatigue
fracture
microstructure
Opis:
Sound joint of hollow-extruded 6005A-T6 aluminum alloy was achieved by friction stir welding and its high cycle fatigue performance was mainly investigated. As a result, the joint fatigue limit reaches 128.1 MPa which is 55% of the joint tensile strength. The fatigue fracture mainly occurs at the boundary between the stir zone and thermo-mechanically affected zone due to the large difference in the grain size. This difference is caused by the layered microstructure of the base material. The shell pattern with parallel arcs is the typical morphology in the fracture surface and the distance between arcs is increased with the increase of stress level. The specimen with the fracture located in the stir zone possesses a relatively low fatigue life.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 1; 285-292
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparative Study of 2060-T8 Al-Li Alloy Friction Stir Welded Joints Between Natural Cooling and Water Cooling
Autorzy:
Ma, Lin
Niu, Shiyu
Ji, Shude
Gong, Peng
Powiązania:
https://bibliotekanauki.pl/articles/355846.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
2060-T8 Al-Li alloy
friction stir welding
water cooling
microstructure
mechanical properties
Opis:
2060-T8 Al-Li alloy was friction stir butt welded under natural and water cooling conditions. Microstructures and mechanical properties of the welding joints were mainly compared and discussed. By spraying water on the top surface of stir zone, the grain size was reduced, attributing to the improvement of microhardness. The maximum tensile strength under the water cooling reached 461.1 MPa. The joint fractured at the stir zone due to the thickness reduction and the joint softening. The fracture surface consisted of many dimples with various sizes, indicating the typical ductile fracture. The strategy to apply the low heat input at the welding stage and high cooling rate at the cooling stage during FSW is necessary to obtain a high-quality FSW joint.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 1; 305-312
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of friction stir processing (FSP) on microstructure and hardness of AlMg10/SiC composite
Autorzy:
Iwaszko, J.
Kudła, K.
Powiązania:
https://bibliotekanauki.pl/articles/200735.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir processing
AlMg10/SiC composite
microstructure
kompozyt AlMg10/SiC
mikrostruktura
FSP
Opis:
The AlMg10 aluminum alloy reinforced with SiC particles was subjected to friction stir processing (FSP). The composite was made by mechanical mixing and gravity casting. The mass fraction of SiC particles in the composite was about 10%. Evaluation of the effects of FSP treatment was performed by means of light microscopy, scanning electron microscopy, EDS and hardness measurement. It was found that the inhomogeneous distribution of SiC particles and their agglomeration, which were observable in the cast composite, were completely eliminated after FSP modification. The treatment was also accompanied by homogenisation of the material in the mixing zone as well as fragmentation of both the matrix grain of the composite and SiC particles. In the case of SiC particles, a change in their shape was also observed. In the as-cast composite, particles with dimensions from 30 to 60 μm and a sharp-edged polyhedral shape prevailed, while in the material subjected to friction treatment, particles with dimensions from 20 to 40 μm and a more equiangular shape prevailed. Pores and other material discontinuities occurring frequently in the as-cast composite were completely eliminated after friction modification. The recorded changes in the microstructure of the material were accompanied by an increase in the hardness of the composite by nearly 35%. The conducted investigations have shown that FSP modification of the AlMg10/SiC composite made by the casting method leads to favorable microstructural changes in the surface layer and may be an alternative solution to other methods and technologies used in surface engineering.
Źródło:
Bulletin of the Polish Academy of Sciences. Technical Sciences; 2019, 67, 2; 185-192
0239-7528
Pojawia się w:
Bulletin of the Polish Academy of Sciences. Technical Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Volume Percentage of Reinforcement on the Microstructure and Mechanical Properties of an Al6061-T6/SiC Surface Composite Fabricated Through Friction Stir Processing
Autorzy:
Ansari, Abdul Jabbar
Anas, Mohd
Powiązania:
https://bibliotekanauki.pl/articles/2201914.pdf
Data publikacji:
2023
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
friction stir processing
AMMCs
aluminium metal matrix composite
silicon carbide
microstructure
surface composites
composite material
Opis:
In this research, aluminium metal matrix composites (AMMCs) have been manufactured through friction stir processing (FSP) by reinforcing nano-sized SiC particles in an Al6061-T6 alloy. The consequences of the volume percentage of reinforced SiC particles on mechanical properties and microstructural features were analyzed for the developed AMMCs. Microstructural evaluation of a cross-section of a friction stir processed (FSPed) sample has been conducted through Electron backscatter diffraction (EBSD) Energy dispersive spectroscopy (EDS) and a scanning electron microscope (SEM) technique. Microhardness tests were conducted athwart the cross section of FSPed specimen to obtain microhardness feature. A tensile test of FSPed samples has been conducted on a universal testing machine (UTM). Homogeneous distributions of SiC particles were found in the stir zone without any consolidation of particles. The size of the reinforcement particles was decreased slightly by increasing the volume fraction. It has been found that increasing the volume fraction of SiC particles, enhance the tensile strength and microhardness, but decreases the ductility of the aluminium. The maximum ultimate tensile strength (UTS) and microhardness were obtained as 390 MPa and 150.71 HV, respectively, at 12% volume percentage of reinforcement particles. UTS and microhardness of the FSPed Al/SiC have been improved by 38.29% and 59.48% respectively as compared to Al6061-T6. The brittle nature of the FSPed Al/SiC has increased due to a rise in the volume fraction of nanosized SiC particles, which causes a decrease in ductility.
Źródło:
Advances in Science and Technology. Research Journal; 2023, 17, 2; 247--257
2299-8624
Pojawia się w:
Advances in Science and Technology. Research Journal
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mechanical and microstructural properties of EN AW-6060 aluminum alloy joints produced by friction stir welding
Autorzy:
Küçükrendeci, I.
Powiązania:
https://bibliotekanauki.pl/articles/202032.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
friction stir welding
microstructure
mechanical properties
aluminum alloys
spawanie
tarcie
mikrostruktury
właściwości mechaniczne
stopy aluminium
Opis:
In the study, the mechanical and microstructural properties of friction stir welded EN AW-6060 Aluminum Alloy plates were investigated. The friction stir welding (FSW) was conducted at tool rotational speeds of 900, 1250, and 1500 rpm and at welding speeds of 100, 150 and 180 mm/min. The effect of the tool rotational and welding speeds such properties was studied. The mechanical properties of the joints were evaluated by means of micro-hardness (HV) and tensile tests at room temperature. The tensile properties of the friction stir welded tensile specimens depend significantly on both the tool rotational and welding speeds. The microstructural evolution of the weld zone was analysed by optical observations of the weld zones.
Źródło:
Bulletin of the Polish Academy of Sciences. Technical Sciences; 2015, 63, 2; 475-478
0239-7528
Pojawia się w:
Bulletin of the Polish Academy of Sciences. Technical Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies