Tytuł:
The quality assurance of cast and wrought aero jet engine components made from Ni-base superalloys with using of quantitative metallography methods and alloys lifetime prediction
Autorzy:
Belan, Juraj
Kuchariková, Lenka
Mazur, Magdalena
Tillová, Eva
Hanusová, Patrícia
Powiązania:
https://bibliotekanauki.pl/articles/104037.pdf
Data publikacji:
2019
Wydawca:
Stowarzyszenie Menedżerów Jakości i Produkcji
Tematy:
quality assurance
cast Ni-base superalloys
wrought Ni-base superalloys
turbine blades
turbine disc
quantitative metallography
zapewnienie jakości
superstopy na bazie Ni
łopatki turbin
tarcza turbiny
metalografia ilościowa
Opis:
The Ni-base superalloys are used in the aircraft industry for the production of aero engine most stressed parts, turbine blades or turbine discs. Quality of aero jet engine components has a significant influence on the overall lifetime of a jet engine as itself as well as the whole airplane. From this reason a dendrite arm spacing, grain size, morphology, number and value of γ' - phase are very important structural characteristics for blade or discs lifetime prediction. The methods of quantitative metallography are very often used for evaluation of structural characteristics mentioned above. The high-temperature effect on structural characteristics and application of quantitative methods evaluation are presented in this paper. The two different groups of Ni-base alloys have been used as experimental material: cast alloys ZhS6K and IN713LC, which are used for small turbine blades production and wrought alloys EI 698VD and EI 929, which are used for turbine disc production. Selected alloys have been evaluated in the starting stage and after applied heattreatment at 850°C for 24 hrs. This applied heat-treatment causes structural changes in all alloys groups. In cast alloy dendritic structure is degraded and gamma prime average size has grown what has a negative influence on turbine blade creep rupture life. Wrought alloys show partially grain boundary melting and grain size changed due to recrystallization what causes mechanical properties decreasing - ultimate tensile strength mainly.
Źródło:
Quality Production Improvement - QPI; 2019, 1, 1; 222-229
2657-8603
Pojawia się w:
Quality Production Improvement - QPI
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies