A Study on the Correlation between Wood Moisture and the Damping Behaviour of the Tonewood Spruce
Autorzy:
Göken, J.
Fayed, S.
Schäfer, H.
Enzenauer, J.
Powiązania:
https://bibliotekanauki.pl/articles/1030781.pdf
Data publikacji:
2018-05
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
spruce wood
musical instruments
wood moisture
damping measurement
Opis:
In acoustic musical instruments special attention needs to be paid to those particularly sensitive parts made of tonewood whose function is to respond to vibrations. One of the most important tonewoods is spruce because of its good resonance properties. Spruce is especially used for soundboards, these being the primary source of sound. Piano manufacturers dry their soundboards to approximately 6% wood moisture, at which drying stage they are glued into the instrument. Fluctuations of the moisture content in the wood affect the tone. With changing moisture content, the instrument can go out of tune, even cracks can appear at very low moisture content in the wood. In addition, the tone colour will change. This may result from changes in the hammer felt or from changes in the vibration properties of the soundboard. Strain- and frequency-dependent damping measurements were carried out on spruce wood at different wood moisture contents in order to investigate the effect of the moisture content on the vibration behaviour. Wood which is slowly dried in air for several years is preferably used for high-class pianos. Therefore, damping measurements on new and on more than 130-year old spruce wood samples were performed.
Źródło:
Acta Physica Polonica A; 2018, 133, 5; 1241-1260
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Automatic system for measuring wood moisture using quasi-balanced method of dielectric loss factor measurement
Autorzy:
Barwinek, S.
Cichy, A.
Skórkowski, A.
Powiązania:
https://bibliotekanauki.pl/articles/114387.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
wood moisture
virtual instruments
impedance measurement
quasi – balanced method
dielectric loss factor
Opis:
The paper presents an automatic system for measuring the moisture content of wood on the basis of loss factor tanδ. The instrument is based on a structure of the non-bridge, quasi – balanced circuit implemented in a program way. The virtual measuring system uses the data acquisition board NI USB-6251 from National Instruments and LabVIEW environment. The preliminary results of experimental studies were compared with the results of the LCR meters Hioki 3522, MOTECH MIC-4090 and meter of wood humidity Powerfix HG00384C.
Źródło:
Measurement Automation Monitoring; 2016, 62, 12; 426-428
2450-2855
Pojawia się w:
Measurement Automation Monitoring
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Temperature distribution in beech wood during vacuum drying
Autorzy:
Dobrowolska, Ewa
Klimczak, Andrzej
Powiązania:
https://bibliotekanauki.pl/articles/2166519.pdf
Data publikacji:
2021
Wydawca:
Szkoła Główna Gospodarstwa Wiejskiego w Warszawie. Wydawnictwo Szkoły Głównej Gospodarstwa Wiejskiego w Warszawie
Tematy:
Vacuum drying
wood equivalent moisture
drying phases
beech wood
Opis:
Temperature distribution in beech wood during vacuum drying. The temperature distribution and changes in humidity in beech wood in the form of friezes during drying in a vacuum were analysed. The intensity of the occurring phenomena of desorption and the volumetric flow of moisture through the anatomical structures of the wood, depending on the absolute pressure and the temperature of the process, was determined. It was found that the fastest temperature increase took place in the subsurface layers directly adjacent to the heating plates. The introduction of conditioning between the drying phases made it possible to even out the humidity and temperature distribution in the entire element. On the basis of the analysis of changes taking place between the volumes of the three components of wood, it was found that the volume of moisture in the form of vapor removed in the initial phase of drying is over 20 times greater than the volume of voids in wood structures, and in the following phases it decreases to 0.27. The average volume of vapour removed from 1 m3 of wood at the temperature of 55℃ is 13.9 m3/h, decreasing in the following phases to 9.1 m3/h at the drying temperature of 60℃ and then 3.1 m3/h at the temperature of 65℃. The drying rates for these phases reach the value of 0.15%/h, 0.17%/h and 0.075%/h, respectively. Direct measurements of wood moisture, made during the experimental course of the drying process at an absolute pressure of 150 hPa, follow the equivalent moisture, determined on the basis of the Hailwood-Horrobin model, taking into account the appropriate calculation factors.
Rozkład temperatury w drewnie bukowym podczas suszenia próżniowego. Przeanalizowano rozkład temperatury i zmiany wilgotności w drewnie bukowym w postaci fryzów, podczas suszenia w próżni. Ustalono intensywność zachodzących zjawisk desorpcji oraz objętościowego przepływu wilgoci przez struktury anatomiczne drewna, w zależności od ciśnienia bezwzględnego i temperatury przebiegu procesu. Stwierdzono, że najszybszy wzrost temperatury miał miejsce w warstwach przypowierzchniowych bezpośrednio przylegających do płyt grzejnych. Wprowadzenie kondycjonowania między fazami suszenia pozwoliło na wyrównanie wilgotności oraz rozkładu temperatury w całym elemencie. Na podstawie analizy zmian mających miejsce między objętościami trzech składników drewna stwierdzono, że objętość wilgoci w postaci pary usuwanej w początkowej fazie suszenia jest przeszło 20 razy większa od objętości wolnych przestrzeni w strukturach drewna, a w następnych fazach maleje do 0.27. Średnia objętość usuwanej pary z 1 m3 drewna w temperaturze 55℃ wynosi 13,9 m3/h, ulegając w kolejnych fazach obniżeniu do 9.1 m3/h przy temperaturze suszenia 60℃ a następnie 3.1 m3/h w temperaturze 65℃. Szybkości suszenia dla tych faz osiąga wartość odpowiednio 0.15%/h, 0.17%/h i 0.075%/h. Bezpośrednie pomiary wilgotności drewna dokonane podczas eksperymentalnego przebiegu procesu suszenia przy ciśnieniu bezwzględnym równym 150 hPa, nadążają za wilgotnością równoważną, ustaloną na podstawie modelu Hailwooda-Horrobina z uwzględnieniem odpowiednich współczynników obliczeniowych.
Źródło:
Annals of Warsaw University of Life Sciences - SGGW. Forestry and Wood Technology; 2021, 116; 111--122
1898-5912
Pojawia się w:
Annals of Warsaw University of Life Sciences - SGGW. Forestry and Wood Technology
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Pomiar wilgotności drewna wilgotnościomierzami pojemnościowymi
Wood moisture content measurements using capacitance based moisture meters
Autorzy:
Tannenberg, K.
Tannenberg, G.
Powiązania:
https://bibliotekanauki.pl/articles/151451.pdf
Data publikacji:
2011
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
dokładność pomiaru wilgotności drewna
wilgotnościomierz pojemnościowy
rozkład wilgotności
accuracy of wood moisture content measurements
capacitance based moisture meters
cross-section moisture distribution
Opis:
W artykule omówiono zasadę działania pojemnościowych wilgotnościomierzy do drewna. Przedyskutowano główne źródła niepewności pomiaru. Doświadczalnie określono wpływ rozkładu wilgotności wzdłuż przekroju próbki na niepewność pomiaru. Podano analityczną zależność wielkości tej niepewności dla wilgotnościomierzy pojemnościowych i rezystancyjnych. Potwierdzono lepszą dokładność wilgotnościomierzy rezystancyjnych również w przypadkach niejednorodnego rozkładu wilgotności wzdłuż przekroju próbki.
The paper starts with presentation of the basic principles of operation of capacitance-based wood moisture meters (Sections 1, 2, Figs. 1-5) followed by discussion of the main sources of moisture content measurement errors i.e. wood temperature (Section 5), sample timber thickness (Section 6), wood density (Section 7) and moisture distribution along the sample cross-section (Section 8). Next, there is described an experiment conducted to determine the influence of the cross-section moisture distribution on the measurement error (Sections 9, 10). The moisture distribution was measured using an atmospherically insulated sample of wood and a resistance-based moisture meter with insulated needles inserted into the sample on various depths. Simultaneously the measurements were taken by means of a capacitance-based moisture meter. The tests took 28 days. The results are given in Tables 1 and 2. The moisture distribution along the cross-section on subsequent days is shown in Fig. 8. Analytical dependences describing the measurement error as a function of the maximal difference of moisture content along the cross-section were determined. These dependences are given for capacitance and resistance-based moisture meters (Figs. 9, 10). The research confirmed the higher accuracy of resistance-based moisture meters also in cases of heterogeneous distribution of the moisture content.
Źródło:
Pomiary Automatyka Kontrola; 2011, R. 57, nr 2, 2; 161-164
0032-4140
Pojawia się w:
Pomiary Automatyka Kontrola
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Impact of forest growth conditions on the wood density: the case of Amur Region
Autorzy:
Romanova, Natalia A.
Zbirnov, Alexander B.
Yust, Natalia A.
Fucheng, Xu
Powiązania:
https://bibliotekanauki.pl/articles/2045741.pdf
Data publikacji:
2018
Wydawca:
Instytut Badawczy Leśnictwa
Tematy:
forest growth conditions of the Amur region
Amur region
wood density
Dahurian larch
Scots pine
wood moisture content
Asian white birch
Opis:
The problem of determining the dependence of the chainsaw on the density of wood, substantiation of effective options for the number of chainsaws in the assortment and whiplash method of logging is quite relevant. In the Far East of Russia, in particular, in the Amur region, the forest growth conditions are different from the western ones, and therefore, the properties of the wood differ from the generally accepted ones. The article describes forest growth conditions that influence the properties of the wood in areas of the Amur region. Using the method of density determination, the density of larch, pine and birch were studied for first time in the areas of the region. The dependence of the density on humidity, age, species, season of the year and the area of growth was found out. The results of the research showed that under humidity of 70%, the density of larch was 1088.99 kg/m3, it was 919.8 kg/m3 for pine and it was for birch 915.9 kg/m3.
Źródło:
Folia Forestalia Polonica. Series A . Forestry; 2018, 60, 4; 292-298
0071-6677
Pojawia się w:
Folia Forestalia Polonica. Series A . Forestry
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Hybrydowa metoda pomiaru wilgotności drewna
The combined method of measuring wood moisture
Autorzy:
Ivakh, R.
Dominyuk, T.
Powiązania:
https://bibliotekanauki.pl/articles/267002.pdf
Data publikacji:
2014
Wydawca:
Politechnika Gdańska. Wydział Elektrotechniki i Automatyki
Tematy:
wilgotność drewna
metoda pojemnościowa
metody hybrydowe
funkcje dopasowywania
metoda radiometryczna
wood moisture
capacitive method
combined method
combined function
radiometric method
Opis:
W artykule dokonano analizy wpływu czynników zakłócających (temperatura, gęstość, szczelność, itp.) na wyniki pomiaru wilgotności drewna. W oparciu o dostępne analityczne zależności zawartości wilgoci w drewnie, zaproponowano jednoczesne stosowanie kilku metod dla pomiarów wilgotności drewna. W wypadku prawidłowego wyboru tych metod i racjonalnego dopasowania odpowiadających funkcji – w znacznym stopniu można zmniejszyć negatywny wpływ czynników zakłócających na wynik pomiaru wilgotności.
Established that to achieve high measurement accuracy and eliminate the effect of non-informative parameters (temperature, density, thickness of wood, etc.) during the measurement of wood moisture should be used hybrid methods, which are based on the combined search tool that meets specifications.
Źródło:
Zeszyty Naukowe Wydziału Elektrotechniki i Automatyki Politechniki Gdańskiej; 2014, 38; 29-31
1425-5766
2353-1290
Pojawia się w:
Zeszyty Naukowe Wydziału Elektrotechniki i Automatyki Politechniki Gdańskiej
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Metodyczne zagadnienia monitoringu statusu wody w wybranych materialach biologicznych
Methodical questions of monitoring of water status in selected biological materials
Autorzy:
Malicki, M A
Powiązania:
https://bibliotekanauki.pl/articles/1630378.pdf
Data publikacji:
1999
Wydawca:
Polska Akademia Nauk. Instytut Agrofizyki PAN
Tematy:
agrofizyka
materialy biologiczne
zboza
ziarno
drewno
gleby
woda glebowa
wilgotnosc gleby
wilgotnosc ziarna
wilgotnosc drewna
temperatura
zasolenie gleb
potencjal wodny gleby
pomiary wilgotnosci
natlenienie
monitoring
agrophysics
biological material
cereal
grain
wood
soil
soil water
soil moisture
grain moisture
wood moisture
temperature
soil salinity
soil water potential
moisture measurement
oxygenation
Opis:
Methodical questions of monitoring of water status in soil, cereals grain and wood are discused ( where monitoring is understood as registration of time and spatial variability of selected properties). Amount of viariables which is necessary in order to determine water status depends on the complexion of the considered phenomena and is, so far, the matter of arbitrary choice. In most practical cases the water status is expressed only by moisture of the considered material ( like the building timber). In practical terms, two variables suffice to express water status in cereal grain: moisture and temperature. To describe water status in the soil not less then five variables are needed: amount of water (the soil moisture) soil water potential, salinity, oxygenation and temperature. The only sensors that can be integrated in modern data acquisition system must be read electrically. Therefore electroresistance and electrocapacitance methods were considered. Dielectric sensors were recognized as the proper choice.Soil is a complex material having instable characteristics. For this reason it is the most difficult task to monitor soil water status, particularly to determine the soil moisture. Therefore it has been assumed that measuring methods verified for the soil will be also suitable for other, less complex materials. Thus, monitoring of soil water status was mainly discussed. Special attention was focused to the time domain reflectometry, TDR, as the semi selective method for the soil moisture and salinity determination.
Źródło:
Acta Agrophysica; 1999, 19; 1-108
1234-4125
Pojawia się w:
Acta Agrophysica
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Utrata masy i zmiany gęstości średniowymiarowego surowca sosnowego pozyskanego i magazynowanego w okresie letnim
Weight loss and green density changes of Scots pine pulpwood harvested and stored during the summer
Autorzy:
Tomczak, A.
Wesołowski, P.
Jelonek, T.
Jakubowski, M.
Powiązania:
https://bibliotekanauki.pl/articles/989611.pdf
Data publikacji:
2016
Wydawca:
Polskie Towarzystwo Leśne
Tematy:
lesnictwo
pozyskiwanie drewna
lato
sosna zwyczajna
Pinus sylvestris
drewno sosnowe
drewno sredniowymiarowe
drewno swiezo sciete
magazynowanie
utrata masy drewna
gestosc drewna
scots pine
mass of logs
timber
freshly−cut trees
bark
wood moisture
Opis:
The study objectives included: i) determination of the mass and green density of pulpwood (wood+bark) and ii) comparison of the changes in these parameters during 14−day−long storage period. The experiment was conducted between 15 and 28 July 2014 and the material was taken from the 67 year−old Scots pine stand (Tuchola Forest District, northern Poland). Using the Urich method, 30 model trees were selected. After felling and delimbing, logs of 2.5 m length were cut, with diameter at the small end not less than 7 cm outside the bark. In total, 133 logs were harvested (mean diameter inside the bark at the thicker end – 13.1 cm, in the thinner end – 11.4 cm). After diameter measurements were taken, each log was weighed (total over bark volume equaled 4.69 m³, while total weight – 3955 kg). Mass measurement took place daily between 8 and 10 a.m. In Poland, the raw material is not recommended to be stored too long in summer, due to the possibility of its depreciation. Storage time should be as short as possible and not exceed 2 weeks. The mass of the 1 m³ of wood harvested from freshly−cut trees amounted to 844 kg. After 14 days it decreased to 814 kg (–3.5%). Differences were not statistically significant. Because the moisture content has the highest influence on mass, the rain and thereby an increase in the air humidity significantly reduce drying. Mass of 1 m³ of raw material was reduced to the day of rain by 2.9 kg (–0.35%) per day on average. After the occurrence of rainfall, between 10th and 14th day of storage the mean weight loss was 1.3 kg/m³ (–0.16%). The mean weight loss reached 30 kg/m³ in analyzed period. Generally two weeks storage is too short time to obtain a large weight loss. However, in this case of total mass of haulage vehicles together with their cargo may be a few hundred kilos smaller.
Źródło:
Sylwan; 2016, 160, 08; 619-626
0039-7660
Pojawia się w:
Sylwan
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Investigation of round Scots pine wood WC01 class using X-ray computer tomography
Autorzy:
Zatoń, Patrycja
Kozakiewicz, Paweł
Mańkowski, Piotr
Powiązania:
https://bibliotekanauki.pl/articles/2171746.pdf
Data publikacji:
2022
Wydawca:
Szkoła Główna Gospodarstwa Wiejskiego w Warszawie. Wydawnictwo Szkoły Głównej Gospodarstwa Wiejskiego w Warszawie
Tematy:
X-ray computer tomography
quality of round wood
Scots pine wood
density of wood
annual rings
moisture content of wood
Opis:
Investigation of round Scots pine wood WC01 class using X-ray computer tomography. Scots pine is the most widespread type of wood in Poland with wide industrial use. The typical starting material used for the production of layered floor elements are logs of WC01 class (class according to the Polish Standard PN-D-95008: 1992 and Order no 72 - GM-900-5 / 2013 of General Director of the State Forests in Poland). Using X-ray computed tomography, tests of fresh wood in the bark were carried out, confirming the full suitability of this technique for the precise assessment of wood density as well as its grain and distribution of anatomical defects (knots). The different level of humidity of sapwood and heartwood in fresh wood is visible in tomographic images and translates into a much higher recorded density of the wetter zone of sapwood. Calibration of the tomograph used made it possible to convert the Hounsfield density scale into actual densities expressed in kg/m3.
Badania okrągłego drewna sosnowego klasy WC01 z zastosowaniem rentgenowskiej tomografii komputerowej. Sosna zwyczajna to najbardziej rozpowszechniony gatunek drewna w Polsce o szerokim zastosowaniu przemysłowym. Typowym surowcem wyjściowym stosowanym do produkcji warstwowych elementów podłogowych są kłody klasy WC01. Przy wykorzystaniu rentgenowskiej tomografii komputerowej przeprowadzono badania świeżego drewna w korze, potwierdzając pełną przydatność tej techniki do precyzyjnej oceny gęstości drewna a także jego słoistości i rozmieszczenia wad anatomicznych (sęków). Różny poziom wilgotności drewna bieli i twardzieli w świeżym drewnie jest doskonale widoczny w obrazach tomograficznych i przekłada na zdecydowanie wyższą odnotowaną gęstość wilgotniejszej strefy drewna bielastego. Wzorcowanie zastosowanego tomografu w danym trybie nastaw pozwoliło na przeliczenie skali gęstościowej Hounsfilda na rzeczywiste i jednocześnie praktyczne wartości gęstości wyrażone w kg/m3.
Źródło:
Annals of Warsaw University of Life Sciences - SGGW. Forestry and Wood Technology; 2022, 117; 97--105
1898-5912
Pojawia się w:
Annals of Warsaw University of Life Sciences - SGGW. Forestry and Wood Technology
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Produktywność wierzb krzewiastych pozyskiwanych w jednorocznych cyklach zbioru
Productivity of willow short rotation coppice in one-year cutting cycles
Autorzy:
Szczukowski, S.
Tworkowski, J.
Stolarski, M.
Grzelczyk, M.
Powiązania:
https://bibliotekanauki.pl/articles/46696.pdf
Data publikacji:
2005
Wydawca:
Politechnika Bydgoska im. Jana i Jędrzeja Śniadeckich. Wydawnictwo PB
Tematy:
wierzba krzewiasta
produktywnosc
gestosc sadzenia
cykl uprawowy
zbior w cyklach jednorocznych
plony
sucha masa
pedy jednoroczne
wilgotnosc
biomasa
common osier
productivity
planting density
cultivation cycle
harvest
yield
dry mass
annual shoot
wood moisture
biomass
Opis:
W latach 1996-2003 na Nizinie Kwidzyńskiej na madzie ciężkiej (kompleks zbożowo-pastewny mocny 8, klasa IIIb) prowadzono doświadczenie polowe, którego celem było określenie produktywności sześciu klonów wierzb krzewiastych uprawianych w zagęszczeniu 20-60 tys. roślin·ha-1 i pozyskiwanych w jednorocznych cyklach zbioru. Plon jednorocznych pędów w doświadczeniu zawarty był w przedziale od 12,51 do 21,52 t s.m.·ha-1·rok-1. Najwyższy plon suchej masy drewna dał klon Salix viminalis 082, średnio 19,77 t·ha-1·rok-1. Zwiększanie zagęszczenia roślin z 20 do 40 tys.·ha-1 powodowało istotny wzrost plonów suchej masy drewna. Dalsze zwiększanie zagęszczenia roślin do 60 tys. szt.·ha-1 powodowało już tylko nieznaczną tendencję wzrostu plonu. Wilgotność drewna jednorocznych pędów wierzby krzewiastej w czasie zbioru wyniosła od 50,4 do 53,1%.
The 1996-2003 field trial on Kwidzyń Lowland heavy alluvial soil (complex of agricultural suitability 8 and class 3b, according to the Polish Soil Sciences Society) aimed at defining the productivity of six willow clones planted from 20,000 to 60,000 plants·ha-1 and harvested in annual cutting cycles. The yield of one-year old stems ranged from 12.51 to 21.52 t of dry matter ·ha-1·year-1. The highest yield of dry matter of wood was recorded for Salix viminalis 082, 19.77 t·ha-1·year-1 on average. Increasing planting density from 20,000 to 40,000 plants·ha-1 resulted in a significant increase in dry matter of wood. A further increase in planting density up to 60,000 plants·ha-1 resulted in a slight yield increase trend only. The water content in one-year willow stems over harvest ranged from 50.4 to 53.1%.
Źródło:
Acta Scientiarum Polonorum. Agricultura; 2005, 04, 1
1644-0625
Pojawia się w:
Acta Scientiarum Polonorum. Agricultura
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wpływ wilgotności i gatunku drewna opałowego na przebieg procesu łupania
Effect of humidity and species of firewood on the course of cleaving
Autorzy:
Brzózko, J.
Samoraj, P.
Błuszkowska, U.
Aniszewska, M.
Powiązania:
https://bibliotekanauki.pl/articles/987080.pdf
Data publikacji:
2017
Wydawca:
Polskie Towarzystwo Leśne
Tematy:
drewno opalowe
grab pospolity
Carpinus betulus
drewno grabowe
buk zwyczajny
Fagus sylvatica
drewno bukowe
brzoza brodawkowata
Betula pendula
drewno brzozowe
olsza czarna
Alnus glutinosa
drewno olszowe
jesion wyniosly
Fraxinus excelsior
drewno jesionowe
wilgotnosc drewna
lupanie
luparka SplitMaster 9
wydajnosc pracy
wood splitting
solid biofuels
wood moisture
Opis:
Traditional firewood is still the most popular type of solid fuel. This is mainly because of the availability of raw materials and simple production process, which involves mostly just sawing and cleaving. Cleaving increases the surface of the wood through which water evaporates, which in turn speeds up the drying. Dry wood has a higher calorific value and its combustion releases less harmful carbon monoxide and hydrocarbons. Wood cleaving process can be divided into three phases that lasts from the introduction of the wedge till the appearance of a crack (phase I), from the appearance of the crack till the stop of the slots (phase II) and then until the piece of the wood is completely cleaved (phase III). Although it is a conditional phase and it does not always occur in the case of the firewood species popular in Poland, the last phase takes the longest and has the greatest impact on the cleaving performance. The aim of the study was to determine the effect of wood and its moisture content on the duration of the phase III during the trial cleaving. The tested samples comprised of five popular in Poland species: hornbeam, beech, birch, alder and ash. The cleaving were carried out immediately after cutting and sawing the timber and after 3−month−long period of natural drying. For hornbeam, beech and alder humidity does not affect the hollow wedge in wood at the time of rupture. The duration of phase III was significantly longer than duration of phases I and II for each species independently of humidity. Significant dependence was observed for depression wedge as a function of humidity obtained in phase I and II for silver birch, and in phase III for ash.
Źródło:
Sylwan; 2017, 161, 08; 685-692
0039-7660
Pojawia się w:
Sylwan
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Dielectric determination of moisture of wood using time domain reflectometry
Autorzy:
Malicki, M A
Kotlinski, J.
Powiązania:
https://bibliotekanauki.pl/articles/26096.pdf
Data publikacji:
1998
Wydawca:
Polska Akademia Nauk. Instytut Agrofizyki PAN
Tematy:
moisture
determination
wood industry
wood
time domain reflectometry
drying process
Źródło:
International Agrophysics; 1998, 12, 3
0236-8722
Pojawia się w:
International Agrophysics
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Defining the mathematical dependencies of NOx and CO emission generation after biomass combustion in low-power boiler
Autorzy:
Lukáč, Ladislav
Kizek, Ján
Jablonský, Gustáv
Karakash, Yevgeniy
Powiązania:
https://bibliotekanauki.pl/articles/396368.pdf
Data publikacji:
2019
Wydawca:
Uniwersytet Zielonogórski. Oficyna Wydawnicza
Tematy:
wood chips
biomass combustion
emissions CO
emission NOx
wood chips moisture content
mathematical dependence of emission
low power boiler
zrębki drzewne
spalanie biomasy
emisja CO
emisja NOx
wilgotność zrębków drzewnych
matematyczna zależność emisji
kocioł małej mocy
Opis:
The paper deals with the study of the influence of various factors, which have an impact on emissions such as NOx, CO, which have been verified by measurements. Biomass in the form of wood chips as fuel of different moisture content from 9% to 25% has been tested at various boiler outputs. The presented work also defines the mathematical dependencies of NOx and CO emission generation by using regression analysis from measured data after biomass combustion in low-power boilers. The paper also describes a mathematical model of biomass combustion. The mathematical model was created to verify the measured data and prediction of emission generation in the process of biomass combustion. This model consists of combustion of stoichiometry, calculation of combustion temperatures, obtained regression equations of NOx and CO. At the end of this paper, the obtained results are compared with the calculated models as well as the results of the defined dependencies from the regression analysis.
Źródło:
Civil and Environmental Engineering Reports; 2019, 29, 3; 153-163
2080-5187
2450-8594
Pojawia się w:
Civil and Environmental Engineering Reports
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The assessment of mechanical properties of wood treated with ionic liquids
Ocena właściwości mechanicznych drewna zabezpieczonego cieczami jonowymi
Autorzy:
Fojutowski, A.
Noskowiak, A.
Kot, M.
Kropacz, A.
Stangierska, A.
Powiązania:
https://bibliotekanauki.pl/articles/52255.pdf
Data publikacji:
2010
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Technologii Drewna
Tematy:
wood technology
mechanical property
wood
ionic liquid
Scotch pine
compression strength
bending strength
equilibrium moisture
wood property
Opis:
The impregnation of wood with wood preservatives may have an influence on its physical and mechanical properties. The knowledge about the character of that influence is of great importance for characterisation of functional properties of wood and, as a consequence, determination of its use classes. The ionic liquids (ILs) of imidazolium tetrafluoroborates series, which for instance very well penetrate into Scots pine wood, are active against wood-destroying fungi and generally have a positive, although insignificant, influence on physical and mechanical properties of wood, especially on its resistance to colour change during exposure to light. However, various ILs may differ widely in that respect. Under POIG.01.03.01-30-074/08 project investigations were undertaken to clarify the influence of didecyldimethylammonium nitrite ([DDA][NO2]) and IL with didecyldimethylammonium cation and anion of herbicide character ([DDA][herbicide]) on selected physical and mechanical properties of Scots pine wood (Pinus sylvestris L.). The miniature sapwood samples were subjected to sorption with the ILs by vacuum method. The properties of the treated wood were compared with those of control wood, i.e. untreated wood, using twin specimens. The average retention of ILs in wood was on the level of 3.6kg/m3, 7.4kg/m3, and 18.2kg/m3. The tested ILs had only a very small influence, from -0.5% to +1.6%, on the compression strength of wood along the grain when oven-dry wood was tested. However, at equilibrium moisture content the compression strength along the grain, bending strength, and modulus of elasticity at bending of wood treated with ILs were distinctly lower, i.e. by 10%, 20% and 15% respectively. The equilibrium moisture content of wood treated with ILs was greater by 2-3% than that of control wood, which may be the reason for deterioration of wood mechanical properties. However, this speculation requires further investigations.
Impregnacja drewna środkami ochrony drewna może wpływać na jego fizyczne, mechaniczne i biologiczne właściwości. Wiedza o charakterze tego wpływu ma istotne znaczenie dla ustalenia klas użytkowania drewna. W badaniach drewna sosny (Pinus sylvestris L.) zabezpieczonego cieczą jonową: tetrafluoroboranem 3-heptyoloksymetylo-1-metyloimidazoliowym, stwierdzono pozytywny jej wpływ na właściwości fizycznomechaniczne drewna, m.in. na zwiększenie trwałości barwy. Różne ciecze jonowe mogą mieć różny wpływ na właściwości drewna, chociaż nie można wykluczyć podobieństw wpływu związków o zbliżonej budowie. W ramach projektu badawczego POIG.01.03.01-30-074/08 podjęto badania oddziaływania dwóch cieczy jonowych: azotynu didecylodimetyloamoniowego [DDA][NO2] i cieczy z kationem didecylodimetyloamoniowym i anionem o charakterze herbicydu [DDA][herbicyd], wprowadzonych w roztworach wodno-alkoholowych do drewna metodą próżniowo-ciśnieniową, na jego wytrzymałość. Retencje cieczy jonowych w drewnie zróżnicowano przez zastosowanie trzech różnych ich stężeń w roztworach. Badania wykonano na bielu drewna sosny (Pinus sylvestris L.), jako drewnie modelowym. Podstawowej oceny wpływu cieczy jonowych na wytrzymałość drewna dokonano przez zbadanie wytrzymałości na ściskanie wzdłuż włókien (zgodnie z PN-C-04907:1972) po wysuszeniu nasycanych cieczami jonowymi próbek do stanu zupełnie suchego. Następnie dokonano oznaczeń wytrzymałości na ściskanie wzdłuż włókien metodą według PN-D-04102:1979 oraz wytrzymałości i modułu sprężystości przy zginaniu drewna metodami: według PN-D-04103:1977 i PN-D-04117:1963. Oznaczenia te wykonano stosując drewno o równowagowym stanie wilgotności w klimacie normalnym (wilgotność powietrza 65%/20°C). W rezultacie badań wykonanych na bliźniaczych próbkach drewna stwierdzono, że nasycanie bielu drewna sosny zwyczajnej cieczami jonowymi [DDA][NO2] i [DDA] [herbicyd] w ilości 3,5 do 19,0 kg/m3: – nie wpływa na wytrzymałość na ściskanie wzdłuż włókien badaną zgodnie z normą PN-C-04907:1972 w stanie zupełnie suchego drewna (zmiany w zakresie od –0,5% do +1,6% kwalifikowane są według normy jako brak zmian), – powoduje zwiększenie wilgotności równowagowej drewna w klimacie normalnym (65%/20°C) o 2–3%, – zmniejsza wytrzymałość na zginanie statyczne, wytrzymałość na ściskanie wzdłuż włókien oraz moduł sprężystości drewna w stanie wilgotności równowagowej, dla klimatu normalnego (65%, 20°C), odpowiednio o około: 20%, 10% i 15%. Różnice pomiędzy wartościami średnimi wytrzymałości na zginanie, wytrzymałości na ściskanie i modułu sprężystości przy zginaniu próbek kontrolnych i próbek nasycanych cieczami jonowymi są statystycznie istotne (przy poziomie ufności 95%). Różnice pomiędzy wartościami średnimi wytrzymałości na zginanie, wytrzymałości na ściskanie i modułu sprężystości przy zginaniu próbek nasycanych cieczami jonowymi o różnych stężeniach (różne stopnie retencji) są statystycznie nieistotne (przy poziomie ufności 95%). Dalszych badań wymaga sprawdzenie czy obniżenie wytrzymałości i modułu sprężystości przy wilgotności drewna odpowiadającej wilgotności równowagowej dla klimatu normalnego jest wynikiem wyższej wilgotności równowagowej drewna nasycanego testowanymi cieczami, czy oddziaływania tych cieczy na tkankę drzewną.
Źródło:
Drewno. Prace Naukowe. Doniesienia. Komunikaty; 2010, 53, 184
1644-3985
Pojawia się w:
Drewno. Prace Naukowe. Doniesienia. Komunikaty
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The effect of binder addition on the parameters of compacted poplar wood sawdust
Wplyw dodatku lepiszcza na efektywnosc zageszczania trocin topolowych
Autorzy:
Kulig, R.
Skonecki, S.
Lysiak, G.
Powiązania:
https://bibliotekanauki.pl/articles/791909.pdf
Data publikacji:
2012
Wydawca:
Komisja Motoryzacji i Energetyki Rolnictwa
Tematy:
compaction
poplar wood
sawdust
briquetting
binding agent
calcium lignosulphonate
moisture content
wood processing industry
solid biofuel
Źródło:
Teka Komisji Motoryzacji i Energetyki Rolnictwa; 2012, 12, 1
1641-7739
Pojawia się w:
Teka Komisji Motoryzacji i Energetyki Rolnictwa
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Zmienność współczynnika dyfuzji wilgoci w drewnie świerku norweskiego
Variability of moisture diffusion coefficients for norway spruce wood
Autorzy:
Świrska-Perkowska, J.
Powiązania:
https://bibliotekanauki.pl/articles/362902.pdf
Data publikacji:
2017
Wydawca:
Instytut Fizyki Budowli Katarzyna i Piotr Klemm
Tematy:
wilgoć
dyfuzja
współczynnik
drewno
algorytm minimalizacyjny
moisture
diffusion
coefficient
wood
minimization algorithm
Opis:
W pracy przedstawiono wyniki obliczeń współczynnika dyfuzji wilgoci i współczynnika przejmowania wilgoci dla drewna świerku norweskiego (Picea abies), w przypadku dyfuzji wzdłuż i stycznie do włókien. Wykorzystano przy tym wyniki badań desorpcji wilgoci w próbkach świerku pospolitego przedstawione w pracy S.V. Dvinskikh et al. [1], zrealizowane przy pomocy magnetycznego rezonansu jądrowego. Współczynników dyfuzji wilgoci poszukiwano na drodze minimalizacji funkcji błędu, przy założeniu warunków brzegowych III rodzaju i stałym współczynniku przejmowania wilgoci na brzegu próbki. Każdorazowo analizowano dwa przypadki zmienności współczynnika dyfuzji wraz z wilgotnością materiału, a mianowicie w postaci: stałej oraz funkcji kwadratowej.
This work presents results of calculations of diffusion coefficient and surface emission coefficient for wood of Norway spruce (Picea abies) in the case of diffusion along fibres and tangentially to rings of wood. The results of moisture desorption in the samples of spruce presented in the article by S. V. Dvinskikh et al. [1] and realized by means of nuclear magnetic resonance were employed in the work. The values of moisture diffusion coefficients and mass surface emission coefficient were found using the method of minimizing the fitting function, assuming boundary conditions of the second and third kind with constant surface emission coefficient on the suitable edges of samples. Moreover two cases of variations of the moisture diffusion coefficient together with moisture content of the material were analysed each time: in the form of a constant and quadratic function.
Źródło:
Fizyka Budowli w Teorii i Praktyce; 2017, T. 9, nr 2, 2; 37-42
1734-4891
Pojawia się w:
Fizyka Budowli w Teorii i Praktyce
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wyznaczanie współczynnika dyfuzji wilgoci w drewnie sosny zwyczajnej
Determination of moisture diffusion coefficients for Scots pine wood
Autorzy:
Świrska-Perkowska, J.
Gajda, M.
Powiązania:
https://bibliotekanauki.pl/articles/131606.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Komisja Inżynierii Budowlanej PAN Oddział w Katowicach
Tematy:
dyfuzja wilgoci
drewno
kinetyka sorpcji
minimalizacja funkcji celu
diffusion of moisture
wood
sorption kinetics
Opis:
This paper presents an experimental research on the moisture diffusion coefficient in wood of Scots pine within the scope of hygroscopic moisture. It included measurements of kinetics of moisture adsorption within the range of air relative humidity from 25% to 85%.The experiment was carried out with unidirectional flow of moisture, in each of the material principal orthotropic directions. Values of moisture diffusion coefficients and mass surface emission coefficient were found using the method of minimizing the fitting function, that is by fitting the computational adsorption kinetics curves to the experimental curves. At the same time, four cases of variations of the moisture diffusion coefficient together with moisture content of the material have been analysed each time: in the form of a constant, linear function, quadratic function and exponential function, assuming a constant value of mass surface emission coefficient on the absorbing surface of samples. In addition, for the tangential and radial directions, the case of simultaneous linear variations of moisture diffusion coefficient and mass surface emission coefficient was examined. The performed calculations allowed determining what is the impact of various diffusion mechanisms on the whole process of transferring moisture in the considered cases.
Źródło:
Roczniki Inżynierii Budowlanej; 2015, 15; 17-27
1505-8425
Pojawia się w:
Roczniki Inżynierii Budowlanej
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Naturalne suszenie surowca drzewnego w miejscu pozyskania
Natural drying of wood in the cutting area
Autorzy:
Tomczak, A.
Jelonek, T.
Leszczyński, N.
Korzeniewicz, R.
Powiązania:
https://bibliotekanauki.pl/articles/988961.pdf
Data publikacji:
2017
Wydawca:
Polskie Towarzystwo Leśne
Tematy:
lesnictwo
uzytkowanie lasu
surowce drzewne
drewno swiezo sciete
masa drewna
wilgotnosc drewna
suszenie naturalne
magazynowanie
biomass
energy wood
industrial wood
storage
moisture content
Opis:
Wood obtained from freshly cut trees has a high moisture content and therefore its mass per volume unit is higher than the mass of dry wood. The natural drying is a simple and effective method of weight (moisture content) reduction, making a better use of the vehicle's payload, and thus reducing costs, including environmental costs. The conclusion is based on simulations and analyzes attempting to evaluate different solutions. As evidenced, the drying process of logs depends on numerous factors, which entails attempts at development of an optimal logging method, especially concerning energy wood, allowing for maximum value growth in as little time as possible. The suggestions cover various forms of logging (of whole trees, long timber), arranging (in piles, bundles), storing (in stands, by the roadside near cutting areas), and protection. Combined methods such as storing under canvas for winter only or storing in cutting areas and later in piles at the exit road also work in practice, but require more funds because their cost is determined by the number of stages composing the whole process. In case of wood, development of an optimal and simultaneously universal method used to prepare the lumber for transport and its delivery with consideration of as little environmental impact as possible is complicated. The numerous variables, some of which cannot be controlled or affected, create a considerable scientific problem as well. The authors covered in the presented literature review often stress the role of specific weather conditions accompanying an experiment or its location, the storage method, or lumber dimensions in the drying process. Storage time is perceived as equally important, but it is a derivative more or less determined by the previous variables. Previous studies of drying at the cutting area have been focused mainly on energy wood and less on industrial wood. They analysed the results of long−term storage and did not stress the potential advantages of short−term drying. Furthermore, we do not have sufficient information on species, including forest trees, which have a lower share in the volume of the logged wood. Advanced research can help establish the minimum mass (moisture content) with considerable impact on supply chain effectiveness improvement or evaluated various storing and drying methods. We reviewed reports explaining the impact of various factors on natural drying of wood, models and storage effects, and analyzing potential economic and environmental benefits.
Źródło:
Sylwan; 2017, 161, 11; 898-908
0039-7660
Pojawia się w:
Sylwan
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Węglarstwo leśne. Znaczenie produktów węglarstwa leśnego dla postępu technicznego w świecie
Autorzy:
Surmiński, J.
Powiązania:
https://bibliotekanauki.pl/articles/1022534.pdf
Data publikacji:
2005
Wydawca:
Polskie Towarzystwo Leśne
Tematy:
uboczne uzytkowanie lasu
weglarstwo lesne
znaczenie
smola drzewna
lesnictwo
wegiel drzewny
charcoal
pitch
birch bark tar
wooden black
potash
ceramics
bricks
porcelain
glass
black gun powder
flammable materials
metals melting and their processing (metallurgy)
cold steel
fire arms
artillery
shipbuilding
wood impregnation
wood protection against moisture and rot
soap production
printing paint production
Opis:
The author briefly provides information on charcoal, wood tar, birch tar, wooden black and potash as well as in other products of wood thermolysis. As early as in the latest period of the Stone Age (i.e. Neolithic) charcoal was used for burning bricks and ceramics, smelting metal ores, thermal processing of metals as well as in goldsmithing. Both charcoal and wood tar had particular importance in the development of military technology, especially flammable materials, black gun powder and therefore, in the origin of fire arms and artillery. Wood tar was also used for sealing watercrafts, roofs and building timber preservation. Birch tar was used medicine and veterinary. Wooden black and potash was also produced by forestry charcoaling.
Źródło:
Sylwan; 2005, 149, 08; 49-56
0039-7660
Pojawia się w:
Sylwan
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Badania współczynnika tarcia zewnętrznego ziarna zbóż w funkcji wilgotności
Research on the coefficient of external friction of corn grain in humidity function
Autorzy:
Kram, B. B.
Powiązania:
https://bibliotekanauki.pl/articles/289209.pdf
Data publikacji:
2006
Wydawca:
Polskie Towarzystwo Inżynierii Rolniczej
Tematy:
współczynnik tarcia zewnętrznego
pszenica
żyto
pszenżyto
wilgotność
podłoże stalowe
podłoże drewniane
podłoże gumowe
coefficient of external friction
wheat
rye
triticale
moisture
steel base
wood base
rubber base
Opis:
Współczynniki tarcia zewnętrznego ziaren zbóż (pszenica ozima Almari i Rosa, pszenica jara Omega i Eta, żyto Dańkowskie Złote i Motto, pszenżyto ozime Presto i Malno, pszenżyto jare Jago i Maja) wyznaczono na podstawowych materiałach konstrukcyjnych: stali, drewnie i gumie. Badane ziarno było nawilżane od wilgotności W = 9% do W = 33%. Zmienność współczynników tarcia zewnętrznego w funkcji wilgotności na badanych podłożach opisują proste rosnące. Najniższy współczynnik tarcia wynosił µ= 0,2991 (dla pszenżyta Maja, na podłożu stalowym), a najwyższy µ= 0,9999 (dla pszenicy Rosa na podłożu gumowym).
The coefficient of external friction of cereals grain (winter wheat Almari and Rosa, spring wheat Omega and Eta, rye Dańkowskie Złote and Motto, winter triticale Presto and Malno, winter triticale Presto and Malno, spring triticale Jago and Maja) was determined for three major materials: steel, wood and rubber. The grain was wetted in special containers in order to attain the moisture levels within 10%-32%. The values of external friction coefficient have the from of linear regression and show the relationship between the coefficient of external friction and moisture levels. The smallest coefficient of external friction (µ= 0,2991) was for triticale Maja for steel base, and the highest (µ= 0,9999) was for wheat Rosa for the rubber base.
Źródło:
Inżynieria Rolnicza; 2006, R. 10, nr 3(78), 3(78); 175-182
1429-7264
Pojawia się w:
Inżynieria Rolnicza
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Charakterystyka zrębków oraz peletów (granulatów) z biomasy wierzby i ślazowca jako paliwa
Characteristic of chips and pellets from the coppice willow and Virginia mallow biomass as a fuel
Autorzy:
Stolarski, M.
Szczukowski, S.
Tworkowski, J.
Kwiatkowski, J.
Grzelczyk, M.
Powiązania:
https://bibliotekanauki.pl/articles/238545.pdf
Data publikacji:
2005
Wydawca:
Instytut Technologiczno-Przyrodniczy
Tematy:
wierzba krzewiasta
ślazowiec pensylwański
biomasa
wartość energetyczna
zrębki
pelet
granulat
gęstość nasypowa
wilgotność
wartość opałowa
willow
willow poppice
Virginia mallow
biomass
energy
wood chips
pellets
bulk density
moisture content
combustion value
Opis:
Określono wartość energetyczną plonu wierzby zbieranej w 1-rocznym i 4-letnim cyklu oraz ślazowca pozyskiwanego co roku. Określono właściwości fizykochemiczne zrębków i peletów uzyskanych z sezonowanej biomasy tych roślin oraz porównano je z peletem wytworzonym z drewna dębowego i wymaganiami normy DIN 51731. Wartość energetyczna plonu jednorocznych pędów wierzby i ślazowca była zbliżona, natomiast wierzby zbieranej w 4-letnim cyklu była o około 40% wyższa. Zaproponowany sposób suszenia całych pędów wierzby na podłożu ziemnym na wolnym powietrzu jest skuteczny i możliwy do zastosowania w praktyce. Pelet wytworzony z 4-letnich pędów wierzby spełniał wymagania normy, natomiast w uzyskanym z 1-rocznych pędów wierzby i ślazowca wystąpiło przekroczenie oznaczonej zawartości popiołu i azotu. W wyniku granulacji biomasy wierzby i ślazowca gęstość peletów (granulaów) w stosunku do zrębków została zwiększona odpowiednio prawie 4- i 5-krotnie, a koncentracja energii 4,5- i 6,5-krotnie.
The quantities of energy obtained in biomass of coppice willow harvested in annual and four years' cutting cycles and of Virginia mallow (Sida hermaphrodita R) harvested annually were estimated. Some physico-chemical parameters of the chips and pellets produced from biomass of both plants were determined; next they were compared with pelleted oak wood sawdust and related to the requirements of DIN 51731 German standard. Energy yields from willow harvested in annual cycle and Virginia mallow were similar, whereas the willow biomass harvested every four year showed energetic value higher by 40%. Described natural drying system of willow stems on the ground appeared to be effective and easy to implementation. The pellets produced from four years' old willow stems met the DIN 51731 standard requirements whereas in case of annual harvesting cycle of willow and Virginia mallow the pellets contained too much ash and nitrogen. As a result of processing biomass into pellets, the bulk density of material increased four-and fivefold, while the energy concentration grew 4.5 and 6.5 times for willow and Vigginia mallow, respectively.
Źródło:
Problemy Inżynierii Rolniczej; 2005, R. 13, nr 1, 1; 13-22
1231-0093
Pojawia się w:
Problemy Inżynierii Rolniczej
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-21 z 21

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies