Tytuł:
Bond strength of modern self-adhesive resin cements to human dentin and different CAD/CAM ceramics
Autorzy:
Małysa, Andrzej
Weżgowiec, Joanna
Danel, Dariusz
Boening, Klaus
Walczak, Katarzyna
Więckiewicz, Mieszko
Powiązania:
https://bibliotekanauki.pl/articles/27324142.pdf
Data publikacji:
2020
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
shear bond strength
self-adhesive resin cement
dentin
CAD/CAM ceramic
dental material
adhesion
wytrzymałość wiązania na ścinanie
samoadhezyjny cement na bazie żywicy
zębina
Ceramika CAD/CAM
materiał dentystyczny
przyczepność
Opis:
The aim of the study was to evaluate the shear bond strength of CAD/CAM ceramics to dentin after cementation with conventional or self-adhesive resin cements. Methods: Three self-adhesive, self-etching cements (Panavia SA, RelyX U200, Maxcem Elite), and one conventional cement (Panavia V5), were selected to lute three CAD/CAM ceramics (IPS Empress CAD, IPS e.max CAD, IPS e.max ZirCAD) onto the dentin. The bond strength was evaluated using a shear strength test according to the PN-EN ISO 29022:2013-10. Evaluation of the differences was performed using the Statistica software. Failure modes were analyzed using a light microscope. Results: All the studied cements differed (regardless of the ceramic type) in the bond strength. The highest bond strength was observed in Panavia V5, lower – in RelyX U200 and Panavia SA, and the lowest – in Maxcem. For IPS e.max ZirCAD, it was observed that compared to Panavia V5, the other cements were characterized by a significantly higher bond strength. For the IPS Empress CAD and the IPS e.max CAD, Panavia V5 displayed the highest bond strength. For all the studied self-adhesive cements, the failure of adhesion between the cement and dentin was predominant mode. Conclusions: Significant differences were found in the shear bond strengths of the CAD/CAM ceramics luted to dentin using tested self-adhesive and conventional cements. The bond strength depended on the combination of ceramic and cement. The IPS e.max ZirCAD had the highest bond strength to dentin after cementation with RelyX U200, while the IPS Empress CAD and IPS e.max CAD – with Panavia V5.
Źródło:
Acta of Bioengineering and Biomechanics; 2020, 22, 2; 25--34
1509-409X
2450-6303
Pojawia się w:
Acta of Bioengineering and Biomechanics
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies