Tytuł:
The control of solidification kinetics of the vacuum-cast thin-wall nickel-based superalloys by changing the geometrical characteristics of the ceramic mold
Autorzy:
Cygan, R.
Szeliga, D.
Rokicki, P.
Sieniawski, J.
Suchy, J. S.
Powiązania:
https://bibliotekanauki.pl/articles/381982.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
nickel based superalloy
ceramic mold
thin walled casting
investment casting
nadstop niklu
forma ceramiczna
odlewanie cienkościenne
odlewanie precyzyjne
Opis:
This paper provides an analysis of experimental research and results of investment casting process. Temperature field in a ceramic mold is one of the problems during numerical simulation. Reducing the costs of production in precision casting involves the reduction of scraps, which is one of the fundamental problems of the foundry industry. Reducing these costs is associated with optimization of precision casting technology of aircraft engines critical parts, including control of the solidification front in thin-walled castings of nickel super alloys cast in a vacuum. It is achieved by changing the geometrical characteristics of the ceramic mold. The results of the tests were used to optimize the industrial production of aircraft components in Precision Foundry of WSK Rzeszów. Temperature distribution gained in the conducted tests allowed verification and optimization of computer simulations.
Źródło:
Archives of Foundry Engineering; 2013, 13, 4; 21-28
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mathematical forecasting composition of secondary carbides in the single-crystal superalloys
Autorzy:
Glotka, O.A.
Olshanetskii, V.I.
Powiązania:
https://bibliotekanauki.pl/articles/2175759.pdf
Data publikacji:
2021
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
single-crystal nickel-based superalloy
alloying system
CALPHAD method
structure
composition of secondary carbides
krystaliczny nadstop na bazie niklu
układ stopowy
metoda CALPHAD
struktura
skład węglików wtórnych
Opis:
Purpose: Predicting the specifics of the distribution of alloying elements between secondary carbides, their topology, and morphology, as well as the composition for a single-crystal multicomponent system of the type Ni-11.5Cr-5Co-3.6Al-4.5Ti-7W-0.8Mo-0.06C using the calculated CALPHAD (passive experiment) versus scanning electron microscopy (active experiment). Design/methodology/approach: This work presents the results of studies of the distribution of chemical elements in the composition of carbides, depending on their content in the system. The studies were carried out using an electron microscope with computer analysis of images and chemical composition. Findings: It was found that the influence of alloying elements on the composition of carbides is complex and is described by complex dependencies that correlate well with the obtained experimental results. Research limitations/implications: An essential problem is the prediction of the structure and properties of superalloys without or with a minimum number of experiments. Practical implications: The obtained dependencies can be used both for designing new superalloys and for improving the compositions of industrial alloys. Originality/value: The value of this work is that the obtained dependences of the influence of alloying elements on the dissolution (precipitation) temperatures and the distribution of elements in secondary carbides in the superalloy of the Ni-11.5Cr-5Co-3.6Al-4.5Ti-7W- 0.8Mo-0.06C system. It was found that changes in the course of the curves of temperature dependence on the element content closely correlate with thermodynamic processes occurring in the system, that is, the curves exhibit extrema accompanying the change in the stoichiometry of carbides or the precipitation of new phases.
Źródło:
Archives of Materials Science and Engineering; 2021, 111, 1; 34--41
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies