Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "mikrostruktury nadstopów" wg kryterium: Temat


Wyświetlanie 1-1 z 1
Tytuł:
Employing various metallography methods at high temperature alloy fatigue tests evaluation
Autorzy:
Belan, J.
Kucharikova, L.
Vasko, A.
Chalupova, M.
Svecova, I.
Powiązania:
https://bibliotekanauki.pl/articles/111897.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Menedżerów Jakości i Produkcji
Tematy:
Ni-base casting and wrought alloys
gamma prime
gamma double prime
gamma solid solution
light microscopy
scanning electron microscopy
SEM
skaningowa mikroskopia elektronowa
stopy do obróbki plastycznej
mikrostruktury nadstopów
stop
odlew
Opis:
Microstructures of superalloys have dramatically changed throughout the years, as modern technology of its casting or forging has become more sophisticated. The first superalloys have polyedric microstructure consisting of gamma solid solution, some fraction of gamma prime and of course grain boundaries. As demands on higher performance of aero jet engine increases, the changes in superalloys micro-structure become more significant. A further step in microstructure evolution was directionally solidified alloys with columnar gamma prime particles. The latest microstructures are mostly monocrystalline, oriented in [001] direction of FCC gamma matrix. All microstructure changes bring necessity of proper preparation and evaluation of microstructure. Except for the already mentioned structures have gamma double prime and various carbides form can be seen. These structural parameters have mainly positive influence on important mechanical properties of superalloys. The paper deals with a microstructural evaluation of both groups of alloys – cast and as well as wrought. Micro-structure evaluation helps to describe mechanism at various loading and failure of progressive superalloys. Such an example where micro-structure evaluation is employed is fractography of failure surfaces after fatigue tests, which are examples of metallography evaluation de-scribed in this paper as a secondary objective.
Źródło:
Production Engineering Archives; 2016, 13, 4; 11-15
2353-5156
2353-7779
Pojawia się w:
Production Engineering Archives
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies