- Tytuł:
- Effect of Repeated Austenitisation and Cooling on the Microstructure, Hardness and Tensile Behaviour of 0.16 wt % Carbon Steel
- Autorzy:
-
Subhani, A. R.
Mondal, D. K. - Powiązania:
- https://bibliotekanauki.pl/articles/355808.pdf
- Data publikacji:
- 2018
- Wydawca:
- Polska Akademia Nauk. Czytelnia Czasopism PAN
- Tematy:
-
ferrite grain size
pearlite degeneration
hardness
tensile behaviour - Opis:
- Repeated austenitisation and furnace cooling of homogenised 0.16 wt. % carbon steels result in ferrite grain sizes between 27 μm and 24 μm. Similarly, repeated austenitisation and normal-air cooling produces ferrite grain sizes between 17 μm and 12 μm; while repeated austenitisation and forced-air cooling produces a minimum grain size of 9.5 μm. Furnace cooling decomposes the austenite eutectoidally to lamellar pearlite; while normal-air cooling and forced-air cooling after austenitisation cause degen eration of pearlite regions producing grain boundary network as well as cluster of cementite and other carbides. Forced-air cooled samp les provide the highest YS (364 MPa) and UTS (520 MPa); while furnace cooling provides the lowest (290 MPa and 464 MPa) leaving the normal-air cool performance in between. Hardness values depict the role of individual ferrite and pearlite content and the extent of pearlite degeneration occurring after each cyclic treatment.
- Źródło:
-
Archives of Metallurgy and Materials; 2018, 63, 3; 1141-1152
1733-3490 - Pojawia się w:
- Archives of Metallurgy and Materials
- Dostawca treści:
- Biblioteka Nauki