Experimental Studies on Advanced Sheet Explosive Formulations Based on 2,4,6,8,10,12-Hexanitro-2,4,6,8,10,12-hexaazaisowurtzitane (CL-20) and Hydroxyl Terminated Polybutadiene (HTPB), and Comparison with a RDX-based System
Autorzy:
Jangid, S. K.
Talawar, M. B.
Singh, M. K.
Nath, T.
Sinha, R. K.
Powiązania:
https://bibliotekanauki.pl/articles/358055.pdf
Data publikacji:
2016
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Przemysłu Organicznego
Tematy:
hazardous materials
sheet explosive
explosive reactive armour (ERA)
CL-20
RDX
Opis:
The present investigation reports the use of 2,4,6,8,10,12-hexanitro2,4,6,8,10,12-hexaazaisowurtzitane (CL-20) in sheet explosive formulations. In this study, hydroxyl terminated polybutadiene (HTPB) based sheet explosives were prepared incorporating the powerful explosive CL-20 as a partial replacement for hexahydro-1,3,5-trinitro-1,3,5-triazine(RDX). The effects of incorporating CL-20 on the performance, sensitivity, thermal and mechanical properties of the sheet explosive compositions are reported. Sheet explosive formulation containing 80% of RDX and 20% of HTPB-binder was studied as control sample. HTPBbinder consisted of 12% HTPB, 2.9% dioctyl adipate (DOA) and 5.1% dioctyl phthalate (DOP). HTPB was cured with 4,4’-methylene diphenyl di-isocyanate (MDI) to form urethane linkages. The incorporation of 20% of CL-20 in place of RDX led to a remarkable increase in the velocity of detonation (VOD), of the order of 7680 m/s, and to better mechanical properties in terms of tensile strength (1.14 MPa) compared to the control formulation [RDX /HTPB-binder (80/20)]. The 20% CL-20 incorporated sheet explosive formulation also showed remarkable increases in impact and shock sensitivity. Thermal analysis of the sheet explosive compositions has also been carried out using differential scanning calorimetry (DSC).
Źródło:
Central European Journal of Energetic Materials; 2016, 13, 1; 135-147
1733-7178
Pojawia się w:
Central European Journal of Energetic Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies