Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "electrochemical methods" wg kryterium: Temat


Wyświetlanie 1-7 z 7
Tytuł:
Corrosion Reactivity in the Pre-Clinical Study of 316L and 321 Stainless Steel for Dentistry Applications
Autorzy:
Neaga, V.
Benea, Lidia
Powiązania:
https://bibliotekanauki.pl/articles/2048753.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
corrosion
electrochemical methods
stainless steel
human saliva
Opis:
Now, the use of any medical device based on metals or alloys, especially intended for dentistry applications, is impossible without preclinical evaluation of its anticorrosion properties. Today, the use of stainless steels with AISI standardization, with predilection 316L and 321, are preferred for ergonomic reasons due to their high operational reliability and optimal mechanical properties for functionality over time. In this regard, 316L and 321 stainless steels are tested for comparison in the solution that simulates human saliva with different pH. Stainless steel samples were subjected to corrosion in Fusayama-Meyer and Carter-Brugirard saliva. In-situ electrochemical measurements were applied, such as the open circuit potential (OCP) and electrochemical impedance spectroscopy (EIS). The results show that the corrosion resistance of 316L is superior to 321 in saliva solution at both pH values.
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 1; 371-376
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Study of the Process of Electro Evolution of Copper Ions from Waste Regeneration Solutions
Autorzy:
Trokhymenko, Ganna
Magas, Nataliya
Gomelya, Nikolai
Trus, Inna
Koliehova, Anastasiia
Powiązania:
https://bibliotekanauki.pl/articles/125316.pdf
Data publikacji:
2020
Wydawca:
Polskie Towarzystwo Inżynierii Ekologicznej
Tematy:
heavy metals
electrochemical methods
chemical reagents
wastewater treatment
Opis:
The article presents the results of the study on the process of copper electroevolution from the regeneration solutions in one- and two-chamber electrolyzers at different concentrations of sulfuric acid and the solutions of copper chlorides at different concentrations of hydrochloric acid – in a three-chamber electrolyzer. The conditions of electrochemical recovery of heavy metals from acidic and saline solutions were determined. It was shown that the most effective recovery of heavy metal cations from hydrochloric acid solutions occurs in three-chamber electrolyzers. On the basis of the results obtained, a technological scheme of a local plant for treatment of washing water of galvanic industries was proposed.
Źródło:
Journal of Ecological Engineering; 2020, 21, 2; 29-38
2299-8993
Pojawia się w:
Journal of Ecological Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Contribution of Electrochemistry for a Better Understanding of the Degradation by Tribocorrosion of Metallic Implant Materials
Autorzy:
Benea, Lidia
Powiązania:
https://bibliotekanauki.pl/articles/2106586.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
tribocorrosion
biological fluids
biomaterials
nanocomposite layer
electrochemical methods
Opis:
In this paper there are presented some results obtained by open circuit potential and electrochemical impedance spectroscopy measurements from studies performed on the behavior of tribocorrosion on metallic implant biomaterials as: 304L stainless steel, Co/nano-CeO2 nanocomposite layer and Ti6Al4V untreated and oxidized alloy to form a nanoporous TiO2 film. The open circuit potential technique used in measuring the tribocorrosion process provide information on the active or passive behavior of the investigated metallic biomaterial in the biological fluid, before, during friction and after stopping the friction. Thus it clearly show a better behavior of Co/nano-CeO2 nanocomposite coatings as compared with 304L stainless steel to tribocorrosion degradation in Hank solution; as well the better behavior of nanoporous TiO2 film formed annodically on Ti6Al4V alloy surface as compared with untreated alloy to tribocorrosion degradation in artificial saliva Fusayama Meyer. The slight decrease in polarization resistance value resulted from electrochemical impedance spectroscopy measured during friction in the case of the Co/nano-CeO2 nanocomposite layer (four times smaller), compared to 304L stainless steel, whose polarization resistance decreased more than 1000 times during friction shows the higher sensitivity of stainless steel to degradation by tribocorrosion. The same behavior is observed when comparing the polarization resistance of untreated titanium alloy recorded during friction that is about 200 hundred times smaller, while the specific polarization resistance of the oxidized alloy with the nanoporous film of titanium oxide, decreases very little during friction, highlighting the beneficial effect of modifying the titanium alloy by anodic oxidation to increase its resistance to the degradation process by tribocorrosion.
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 2; 547--554
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Odporność korozyjna stopu biomedycznego M30NW w obecności albuminy i γ-globuliny
Corrosion resistance of M30NW biomedical alloy in the presence of albumin and γ-globulin
Autorzy:
Burnat, B.
Błaszczyk, T.
Leniart, A.
Powiązania:
https://bibliotekanauki.pl/articles/284814.pdf
Data publikacji:
2012
Wydawca:
Akademia Górniczo-Hutnicza im. Stanisława Staszica w Krakowie. Polskie Towarzystwo Biominerałów
Tematy:
biomateriały
białka
korozja
metody elektrochemiczne
biomaterials
proteins
corrosion
electrochemical methods
Opis:
Zbadano wpływ albuminy i γ-globuliny osocza wołowego na odporność korozyjną stopu biomedycznego M30NW. Pomiary korozyjne z wykorzystaniem metod elektrochemicznych przeprowadzono w odtlenionym buforowanym roztworze 0,9% NaCl o pH równym 7,4. Badania te przeprowadzone zostały w dniu 0 (badania przyspieszone korozji) i w ciągu 84 dni (badania korozji długoczasowej). W badaniach przyspieszonych korozji wyznaczono szereg wielkości charakteryzujących właściwości korozyjne badanego stopu M30NW: potencjał korozyjny Ecor, opór polaryzacyjny Rp, szybkość korozji CR, gęstość prądu w obszarze pasywnym i04 oraz potencjały przebicia Eb i repasywacji Erep. Stwierdzono, że dodatek albuminy i γ-globuliny do buforowanego roztworu 0,9% NaCl powoduje niewielkie pogorszenie odporności korozyjnej stopu M30NW w dniu 0. Pogorszenie tej odporności praktycznie nie zależy od rodzaju i stężenia białek. W badaniach korozji długoczasowej wykonywano pomiary potencjału korozyjnego i charakterystyk Stern-Geary'ego. Na podstawie uzyskanych wyników stwierdzono, że odporność korozyjna stopu M30NW wzrasta we wszystkich roztworach, z tym że w obecności albuminy wzrost ten jest słabszy niż w obecności γ-globuliny.
In this study we investigated the influence of bovine serum albumin and γ-globulin on the corrosion resistance of M30NW biomedical alloy. Corrosion measurements using electrochemical methods were carried out in deoxygenated buffered 0.9% NaCl solution at pH of 7.4. Corrosion tests were performed on day 0 (accelerated corrosion test) and within 84 days (long-term corrosion test). In accelerated corrosion tests numerous parameters characterizing the corrosion properties of investigated M30NW alloy were determined: corrosion potential Ecor, polarization resistance Rp, corrosion rate CR, passive current density i0 4, breakdown potential Eb and repassivation potential Erep. It was stated that addition of albumin and γ-globulin to buffered 0.9% NaCl solution causes a slight deterioration of corrosion resistance of M30NW alloy. The effect practically does not depend on the type and concentration of proteins. In long-term corrosion test were performed measurements of corrosion potential and Stern-Geary's characteristics. Based on obtained results it was stated that corrosion resistance of M30NW alloy increases in all solutions, but in the presence of albumin, the growth is weaker than in the presence of γ-globulin.
Źródło:
Engineering of Biomaterials; 2012, 15, 115; 32-37
1429-7248
Pojawia się w:
Engineering of Biomaterials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Corrosion Assessment of Nickel - Base - Dental Alloys in Ringer Biological Solution Studied by Electrochemical Techniques
Autorzy:
Benea, Lidia
Dragus, L.
Mocanu, D.
Powiązania:
https://bibliotekanauki.pl/articles/2106581.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
corrosion
biocompatibility
Dental Alloys
Ringer fluid
dental bridge
electrochemical methods
Opis:
The aim of this paper was to study the corrosion behavior of Nickel - Base - Dental Alloys in Ringer biological fluid. The Nickel base alloys are widely used for medical purposes, especially for prosthetic works in the field of dentistry. The applied electrochemical methods used for corrosion investigations are Open Circuit Potential, Linear Polarization during time of immersion in order to calculate the polarization resistance and corrosion rate. Potentiodynamic Polarization diagrams was performed to appreciate the passive domain. Ni-Cr Ugirex alloy show a better corrosion resistance in Ringer solution which will be reflected in a longer life of the dental structures made with this alloy as compared to the Ni-Cr Ducinox alloy, which will result in dental structures with a shorter lifespan. The electrochemical studies has shown that the alloy have a corrosion behavior similar to a passivating alloy, displaying an extensive passivity area due to formation of an oxide film.
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 2; 529--533
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Właściwości antykorozyjne powłoki TiO2 otrzymywanej metodą zol-żel w zależności od pH środowiska i obecności białka osocza krwi
Anticorrosion properties of TiO2 sol-gel coating in relation to pH of solution and presence of serum protein
Autorzy:
Burnat, B.
Błaszczyk, T.
Leniart, A.
Powiązania:
https://bibliotekanauki.pl/articles/283972.pdf
Data publikacji:
2013
Wydawca:
Akademia Górniczo-Hutnicza im. Stanisława Staszica w Krakowie. Polskie Towarzystwo Biominerałów
Tematy:
biomateriały
TiO2
zol-żel
białko
korozja
metody elektrochemiczne
biomaterials
sol-gel
protein
corrosion
electrochemical methods
Opis:
Zbadano wpływ pH środowiska i obecności białka osocza krwi na właściwości antykorozyjne powłoki ditlenku tytanu TiO2. Powłokę TiO2 o strukturze amorficznej z krystalitami anatazu otrzymywano metodą zol-żel na powierzchni stopu biomedycznego M30NW. Badania korozyjne z wykorzystaniem metod elektrochemicznych przeprowadzono w temperaturze 37°C w roztworze 0.9 % NaCl (sól fizjologiczna) o pH 4.5 oraz 7.4. Wartości pH wybrane do badań pozwoliły przybliżyć 51 warunki naturalnie występujące w środowisku tkankowym (pH=7.4) oraz warunki stanu zapalnego, który może pojawić się w organizmie (pH=4.5). Aby jeszcze lepiej odwzorować środowisko tkankowe, do roztworu soli fizjologicznej dodano albuminę - białko występujące w osoczu krwi w największej ilości. Właściwości antykorozyjne powłoki TiO2 określono w oparciu o wyznaczone wartości potencjału korozyjnego Ecor, oporu polaryzacyjnego Rp, szybkości korozji CR, gęstości prądu w obszarze pasywnym i0.5 oraz potencjałów przebicia Eb i repasywacji Erep. Stwierdzono, że modyfikacja powierzchni stopu M30NW powłoką TiO2 powoduje zwiększenie odporności korozyjnej badanego stopu w roztworach NaCl o pH równym 4.5 i 7.4 - antykorozyjne działanie powłoki TiO2 widoczne jest zarówno w potencjale korozyjnym jak i przy polaryzacji anodowej. Dodatek albuminy ma niejednoznaczny wpływ na antykorozyjne właściwości powłoki TiO2 w potencjale korozyjnym. Natomiast przy polaryzacji anodowej wpływ białka zaznacza się jedynie w roztworze NaCl o pH 4.5 - albumina powoduje istotne zwiększenie potencjału przebicia dla stopu z powłoką TiO2.
In this study we investigated the influence of solution pH and serum protein on the anticorrosion properties of titanium dioxide TiO2 coating. This TiO2 coating with amorphous structure containing crystallites of anatase was obtained by the solgel method on the surface of M30NW biomedical alloy. Corrosion measurements using electrochemical methods were carried out in 0.9 % NaCl (physiological saline) solution at pH of 4.5 and 7.4. The pH values selected for the tests simulate both natural body conditions (pH=7.4) and inflammatory conditions which may occur in the body (pH=4.5). Much better simulation of tissue environment was achieved by adding of albumin – protein found in blood plasma in the greatest amount. Anticorrosion properties of TiO2 coating were determined on the basis of corrosion potential Ecor, polarization resistance Rp, corrosion rate CR, current density in the passive range i0.5 and also breakdown Eb and repasssivation potentials Erep. It was stated that modification of M30NW alloy surface by TiO2 coating cause increase in corrosion resistance of the investigated alloy in NaCl solutions both at pH of 4.5 and 7.4 - anticorrosive effect of TiO2 coating is evident both at corrosion potential and during the anodic polarization. The addition of albumin has an ambiguous effect on the anticorrosion properties of the TiO2 coating at the corrosion potential. Whereas during the anodic polarization the protein effect is visible only in NaCl solution at pH of 4.5 – albumin causes significant increase in the breakdown potential of the alloy coated by TiO2.
Źródło:
Engineering of Biomaterials; 2013, 16, no. 122-123 spec. iss.; 50-55
1429-7248
Pojawia się w:
Engineering of Biomaterials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Elektrochemiczna intensyfikacja procesu mikroskrawania
Electrochemical intensification of microcutting process
Autorzy:
Skoczypiec, S.
Ruszaj, A.
Grabowski, M.
Powiązania:
https://bibliotekanauki.pl/articles/269794.pdf
Data publikacji:
2010
Wydawca:
Wrocławska Rada Federacji Stowarzyszeń Naukowo-Technicznych
Tematy:
mikroobróbka
metody hybrydowe
mikroskrawanie
obróbka elektrochemiczna
micromachining
electrochemical machining
microcutting
hybrid methods
Opis:
W artykule przedstawiono koncepcję elektrochemicznej intensyfikacji procesu mikroskrawania. Wprowadzenie oddziaływań elektrochemicznych w warstwie powierzchniowej przedmiotu obrabianego umożliwia zmniejszenie wytrzymałości oraz twardości usuwanego materiału, co w efekcie powoduje obniżenie sił skrawania i zmniejszenie deformacji narzędzia oraz przedmiotu obrabianego. Prowadzi to do poprawy wskaźników technologicznych obróbki, umożliwiając rozszerzenie operacji mikroobróbki mechanicznej na wykonywanie struktur 3D m.in. operacjami mikrotoczenia, mikrowiercenia czy mikrofrezowania.
In group of methods worked out for machining technological equipment, MEMS parts, functional prototypes and tools for micro-casting and micro-forming special attention is paid for application of microcutting and unconventional processes. The recent development is focused on 3D-shaped surfaces manufacturing. In case of microcutting the main problem during machining is connected with size effect. Significant forces in machining area limit microcutting process application to machine 3D parts made of soft materials and dimensions > 50 žm. One of effective methods to overcome these problems and achieves high performance for micromachining process is combining various physical and chemical processes into one machining process, defined as hybrid machining. One of the possibilities to decrease cutting forces is to decrease the mechanical properties by workpiece surface layer electrochemical passivation before or during cutting process. Between workpiece and additional electrode the electrolyte is supplied. When electrolyte pH and voltage are properly selected on the workpiece surface the thin oxide layer occurs. This layer is fragile and softer than core material, so can be easily removed with relatively smaller cutting forces, what increases tool life, decrease probability of tool damage, and increase accuracy of shaping by decreasing tool and workpiece deformation.
Źródło:
Inżynieria Maszyn; 2010, R. 15, z. 3; 92-101
1426-708X
Pojawia się w:
Inżynieria Maszyn
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-7 z 7

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies