Tytuł:
Determination of physico-mechanical properties of some domestic and foreign walnut (Juglans regia L.) varieties
Autorzy:
Gülsoy, E.
Kuş, E.
Altıkat, S.
Powiązania:
https://bibliotekanauki.pl/articles/12690650.pdf
Data publikacji:
2019
Wydawca:
Uniwersytet Przyrodniczy w Lublinie. Wydawnictwo Uniwersytetu Przyrodniczego w Lublinie
Tematy:
Turkey
plant cultivation
walnut tree
walnut
Juglans regia
Sebin cultivar
Kaman cultivar
Bilecik cultivar
Yalova-3 cultivar
Chandler cultivar
Fernor cultivar
plant cultivar
domestic cultivar
foreign cultivar
fruit trait
physico-mechanical characteristics
physical property
mechanical property
Opis:
In this research, we examined some of the physical (fruit dimensions, geometric mean diameter sphericity and surface area) and mechanical (puncture force, deformation, energy absorption and hardness) properties on the four different domestic (Şebin, Kaman, Bilecik and Yalova-3) and two different foreign (Chandler and Fernor) walnut (Juglans regia) varieties. For this purpose, we applied puncture force on the walnuts at the direction of width orientation (x–x), length orientation (y–y) and suture orientation (z-z). According to obtained results, there are significant differences among the walnut varieties for crustacean walnut weight and walnut weight. The maximum and minimum values of crustacean walnut weight were observed as 18.27 g and 10.98 g for Kaman and Chandler, respectively. In addition to these results, Bilecik has a maximum walnut weight – 8.71 g, while the minimum walnut weight was observed for Yalova-3 – 4.57 g. Furthermore, geometric mean diameter and sphericity values ranged to 31.93–38.57 mm and 82.78–92.54%, respectively. There are statistically significant differences on the puncture force, deformation, energy absorption and hardness according to the load axes. The maximum and minimum puncture force values were determined at the Fernor (572 N) with y–y axes and Chandler (211.9 N) with z–z axes, respectively. Also, the highest hardness and the lowest deformation values were obtained for Kaman (y–y axes) and the highest deformation and the lowest hardness were determined at Bilecik (x–x axes). The energy absorption values changed as follows: 0.455–1.086 J, 0.404–0.985 J and 0.426–1.051 J for x–x, y–y and z–z axes, respectively.
Źródło:
Acta Scientiarum Polonorum. Hortorum Cultus; 2019, 18, 6; 67-74
1644-0692
Pojawia się w:
Acta Scientiarum Polonorum. Hortorum Cultus
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies