Wyszukujesz frazę "Yoon, Y.-O." wg kryterium: Autor


Wyświetlanie 1-3 z 3
Tytuł:
Combined Effect of Zr and Si on Isothermal Oxidation of Ti
Autorzy:
Ha, S.-H.
Kim, B.-H.
Yoon, Y.-O.
Lim, H.-K.
Kim, S. K.
Powiązania:
https://bibliotekanauki.pl/articles/353260.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Ti
Zr
Si
silicide
oxidation
Opis:
In this study, the combined effect of Zr and Si on isothermal oxidation of Ti for 25 and 50h at 820°C, which is the temperature related to exhaust valves operation, was investigated. Si addition into Ti-5mass%Zr alloy led to a distribution of silicide Ti5Si3 phase formed by a eutectic reaction. The Ti sample containing only Zr showed more retarded oxidation rate than Ti-6Al-4V, the most prevalent Ti alloy, at the same condition. However, while a simultaneous addition of Zr and Si resulted in greater increase of oxidation resistance. The oxide layer formed after the addition of Zr and Si comprised TiO2, ZrO2, and SiO2.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1493-1495
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Warm Tensile Deformation Behavior and Constitutive Equation of Supersaturated Solid-Solutionized Al-9Mg Extruded Alloy
Autorzy:
Yang, Seung Y.
Kim, Bong H.
Lee, Da B.
Choi, Kweon H.
Kim, Nam S.
Ha, Seong H.
Yoon, Young O.
Lim, Hyun K.
Kim, Shae
Kim, Young J.
Powiązania:
https://bibliotekanauki.pl/articles/2048882.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminum alloy
Al-9Mg alloy
tensile test
constitutive equation
Opis:
In this paper, as a purpose to apply the supersaturated solid-solutionized Al-9Mg alloy to the structural sheet parts of automotive, tensile tests were conducted under the various conditions and a constitutive equation was derived from the tensile test results. Al-9Mg alloy was produced using a special Mg master alloy containing Al2Ca during the casting process and extruded into the sheet. In order to study the deformation behavior of Al-9Mg alloy in warm temperature forming environments, tensile tests were conducted under the temperature of 373 K-573 K and the strain rate of 0.001/s~0.1/s. in addition, by using the raw data obtained from tensile tests, a constitutive equation of the Al-9Mg alloy was derived for predicting the optimized condition of the hot stamping process. Al-9Mg alloy showed uncommon deformation behavior at the 373 K and 473 K temperature conditions. The calculated curves from the constitutive equation well-matched with the measured curves from the experiments particularly under the low temperature and high strain rate conditions.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 4; 1013-1018
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Mechanical Properties of Hot-deformed AlMg4 Alloys with the Variations of Mn, Fe, and Si Contents
Autorzy:
Lee, Da B.
Kim, Bong H.
Choi, Kweon H.
Yang, Seung Y.
Kim, Nam S.
Ha, Seong H.
Yoon, Young O.
Lim, Hyun K.
Kim, Shae
Hyun, Soong K..
Powiązania:
https://bibliotekanauki.pl/articles/351603.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Mg alloy
intermetallic compounds
homogenization
hot-rolling
microstructure
Opis:
This paper aims to investigate the microstructural evolution and mechanical properties of hot-deformed AlMg4 alloys with Mn, Fe, and Si as the main impurities. For this purpose, solidification behavior and microstructural evolution during hot-rolling and heat-treatment processes are investigated by using theoretical calculations and experimental characterization. The crystallization and morphological transformation of intermetallic Al3 Fe, Al6 Mn, and Mg2 Si phases are revealed and discussed in terms of the variation in chemical composition. Following a homogenization heat-treatment, the effect of heat treatment on the intermetallic compounds is also investigated after hot-rolling. It was revealed that the Mg2 Si phase can be broken into small particles and spherodized more easily than the Al3 Fe intermetallic phase during the hot-rolling process. For the Mn containing alloys, both yield and ultimate tensile strength of the hot-rolled alloys increased from 270 to 296 MPa while elongation decreased from 17 to 13%, which can be attributed to Mn-containing intermetallic as well as dispersoid.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 4; 1255-1259
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies