Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Starshinov, A. V." wg kryterium: Autor


Wyświetlanie 1-1 z 1
Tytuł:
Cast Porous Charges on a Base of Ammonium Nitrate-Urea Eutectic
Autorzy:
Litovka, O. B.
Kozak, G. D.
Chugreeva, E. Y.
Starshinov, A. V.
Powiązania:
https://bibliotekanauki.pl/articles/358034.pdf
Data publikacji:
2008
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Przemysłu Organicznego
Tematy:
eutectic
ammonium nitrate
urea
fusion diagram
detonability
detonation velocity
Opis:
There are great number tasks of explosive technique, requiring the charges with low pressure and detonation velocity. Powerful tool of regulation of these parameters is lowering of charge density. The main goal of this work is elaboration of technology of manufacture and investigation of explosive properties of charges on a base of eutectic ammonium nitrate-urea mixtures (AN/UR) that have melting point T[m] < 100 C. The physicochemical properties of these mixtures were investigated by means of DSC method and fusion diagram of them was plotted. The composition AN/UR 80/20, that has Tm= 80-90 C was chosen for subsequent investigation. The molten composition was mixed with fine aluminum powder, portion of it was placed into paper tube. The level of a liquid was less than length of the tube. Crystallization of melted mixtures was carried out in vacuum chamber, the level of liquid increased at pumping because of expansion of air bubbles introduced with aluminum particles and reached the upper cork of tube. In such a way porous charges were formed. The dependence of charge density vs. population of tubes by melted mixtures was plotted. Calculated heat explosion of mixtures at content of aluminum Al = 10-15% is Qv = 4.5-5.3 MJ/kg, calculated detonation velocity at density ρ = 0.5-1 g/cm3 changes from D = 3.2 to 5.2 km/s. Detonability of charges was investigated experimentally. Failure diameter (df) of detonation was measured, it was df = 22 mm (ρ = 0.6-0.7 g/cm3) for charges without confinement at initiation by means of booster or blasting cap.
Źródło:
Central European Journal of Energetic Materials; 2008, 5, 2; 57-66
1733-7178
Pojawia się w:
Central European Journal of Energetic Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies