The influence of NiZnFe₂O₄ content on magnetic properties of supermalloy type material
Autorzy:
Ďáková, L'.
Füzer, J.
Dobák, S.
Kollár, P.
Fáberová, M.
Strečková, M.
Bureš, R.
Hadraba, H.
Powiązania:
https://bibliotekanauki.pl/articles/1053020.pdf
Data publikacji:
2017-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
07.55.-w
75.60.-d
75.50.Bb
75.50.Gg
Opis:
Soft magnetic composites represent a remarkable kind of materials with wide variety of use. Magnetic properties are dependent on the materials composition and also on the method of preparation. Ni-Fe-Mo alloys (supermalloy) have high complex permeability and low eddy current losses. Soft magnetic NiZnFe₂O₄ ferrites have low coercivity and intermediate saturation magnetization. The Ni_{80}Fe_{14.7}Mo_{4.5}Mn_{0.5}Si_{0.3} (wt%) powder sample was prepared by mechanical alloying of the chemical elements for 24 h. Ni_{0.3}Zn_{0.7}Fe₂O₄ ferrite is commercially available by Sigma Aldrich. Both powders were mixed at selected ratio and uniaxially compacted at 800 MPa. In this paper, we report the experimental observations of the effects of Ni_{0.3}Zn_{0.7}Fe₂O₄ content on the electromagnetic properties of NiFeMoMnSi/Ni_{0.3}Zn_{0.7}Fe₂O₄. The samples contained 5, 10, and 15% of Ni_{0.3}Zn_{0.7}Fe₂O₄ ferrite and were sintered for 30 min at 800°C. An addition of Ni_{0.3}Zn_{0.7}Fe₂O₄ ferrite caused decrease of complex permeability and increase coercivity of the samples. The 5% of Ni_{0.3}Zn_{0.7}Fe₂O₄ sample exhibits the highest value of the real part of complex permeability (48 at 1 kHz). The 10% of Ni_{0.3}Zn_{0.7}Fe₂O₄ sample showed the lowest total magnetic losses.
Źródło:
Acta Physica Polonica A; 2017, 131, 4; 813-815
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Imaging of Magnetic Domains and Domain Walls in Spherical Fe-Si Powder Using Magnetic Force Microscopy
Autorzy:
Strečková, M.
Baťková, M.
Baťko, I.
Hadraba, H.
Bureš, R.
Powiązania:
https://bibliotekanauki.pl/articles/1367241.pdf
Data publikacji:
2014-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
75.50.Bb
75.60.Ch
75.70.Kw
Opis:
The commercial Fe-Si powder, produced by Högänes Corporation, represents promising soft magnetic material for technological applications. The powder consists of spherical particles with diameter up to 150 μm. Internal microstructure of the powder is formed by grains of diameter of about 30 μm. Each separate grain has a random orientation of the easy magnetization axis and is sufficiently large to split into several magnetic domains. A comparative study of the atomic force microscopy (AFM) topography and the corresponding magnetic force microscopy (MFM) images was employed in order to examine the correlation between the grain size, boundaries of grains and characterization of the magnetic domains, which gives us an important knowledge about possible behavior of particles under the influence of the external magnetic field and further utilization of the spherical Fe-Si particles in electrotechnical industry. The grain size and the crystallographic orientation of grains were analyzed by the electron backscattering diffraction (EBSD) technique.
Źródło:
Acta Physica Polonica A; 2014, 126, 1; 92-93
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Imaging of Magnetic Domain Structure in $FeSi/Mn_{0.8}Zn_{0.2}Fe_2O_4$ Composite using Magnetic Force Microscopy
Autorzy:
Streckova, M.
Batko, I.
Batkova, M.
Bures, R.
Faberova, M.
Dzunda, R.
Hadraba, H.
Kubena, I.
Powiązania:
https://bibliotekanauki.pl/articles/1398262.pdf
Data publikacji:
2017-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
72.80.Tm
75.50.Bb
75.60.-d
81.20.-n
81.20.Ev
81.20.Fw
Opis:
Soft magnetic composite was prepared by coating the commercial FeSi powder by $Mn_{0.8}Zn_{0.2}Fe_2O_4$ (MnZn) ferrite, which serves as a potential dielectric phase. MnZn ferrite was prepared by the sol-gel method followed by the auto-self combustion process. The spinel structure of MnZn ferrite was analyzed by X-ray diffraction technique. The composite material was prepared by uniaxial compaction technique and sintered either by conventional or unconventional microwave method. The microwave sintering was applied in order to reduce a grain growth and decrease the overall sintering time. The microstructure of FeSi powder is formed by grains of different diameter. Magnetic force microscopy and scanning electron microscopy were used for an investigation of the correlation between the grain size, grain boundaries and magnetic domains. Magnetic force microscopy visualization of magnetic domains in the prepared soft magnetic composite brings insight into how the magnetically active coating (MnZn ferrite) influences the soft magnetic (FeSi) powder under the influence of the external magnetic field.
Źródło:
Acta Physica Polonica A; 2017, 131, 4; 714-716
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
FeSiBAlNiMo High Entropy Alloy Prepared by Mechanical Alloying
Autorzy:
Bureš, R.
Hadraba, H.
Fáberová, M.
Kollár, P.
Füzer, J.
Roupcová, P.
Strečková, M.
Powiązania:
https://bibliotekanauki.pl/articles/1032753.pdf
Data publikacji:
2017-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.05.-t
75.50.Tt
75.50.Kj
62.20.-x
Opis:
High-entropy alloys have attracted increasing attentions because of their unique compositions, microstructures, and adjustable mechanical and functional properties. In this work, mechanical and magnetic properties of the FeSiBAlNiMo high-entropy alloy were studied in heat-treated conditions. Influence of temperature and time of sintering was investigated. The lowest coercivity H_c=370 A/m was reached at sintering temperature 580°C, during 20 min in Ar/10H₂ atmosphere. Resistivity decreases from R=0.006 Ωcm at 580°C of sintering temperature to R=0.0004 Ωcm at temperature 1100°C. Transverse rupture strength TRS = 340 MPa as well as the Young modulus E=87 GPa were much higher in the case of sintering at 1100°C in comparison to TRS = 5 MPa and E=7.5 GPa at sintering temperature 580°C. Low temperature consolidation made possible to structure recovery and stress relief of amorphous-nanocrystalline structure. Higher temperature above 1100°C induced sintering processes and formation of complex borides.
Źródło:
Acta Physica Polonica A; 2017, 131, 4; 771-773
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies