Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Erdenebold, Urtnasan" wg kryterium: Autor


Wyświetlanie 1-2 z 2
Tytuł:
Chemical and Mineralogical Analysis of Reformed Slag During Iron Recovery from Copper Slag in the Reduction Smelting
Autorzy:
Erdenebold, Urtnasan
Wang, Jei-Pil
Powiązania:
https://bibliotekanauki.pl/articles/2049343.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
copper slag
fayalite
pig iron
reformed slag
Opis:
Copper slag is usually a mixture of iron oxide and silicon dioxide, which exist in the form of fayalite (2FeO·SiO2), and contains ceramic components as the SiO2, Al2O3 and CaO depending on the initial ore quality and the furnace type. Our present study was focused on manufacture of foundry pig iron with Cu content from copper slag using high-temperature reduction smelting and investigate utilization of by-products as a reformed slag, which is giving additional value to the recycling in a replacement of raw material of Portland cement. Changes of the chemical and mineralogical composition of the reformed slag are highly dependent on the CaO concentration in the slag. The chemical and mineralogical properties and microstructural analysis of the reformed slag samples were determined through X-ray Fluorescence spectroscopy, X-Ray diffractometer and Scanning Electron Microscopy connected to the dispersive spectrometer studies.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 3; 809-818
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Manufacture of Low Sulphur Pig Iron from Copper Slag
Autorzy:
Erdenebold, Urtnasan
Sung, Choi Moo
Wang, Jei-Pil
Powiązania:
https://bibliotekanauki.pl/articles/354242.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
copper slag
desulphurization
roasting
sulphur
basicity
Opis:
Copper slag differs by chemical composition and structure, depending on the type of processing. Copper slag typically contains about 1 wt.% copper and 40 wt.% iron depending upon the initial ore quality and type of furnace used. The aim is to produce a typical foundry pig iron with the chemical composition of C > 3.40 wt.%, Si 1.40 to 1.80 wt.%, Mn 0.30 to 0.90 wt.%, P < 0.03 wt.% and S < 0.03 wt.% from copper slag. But foundry pig iron manufactured from copper slag contains a high sulphur content. Therefore, this study examines how to conduct desulphurization. Desulphurization roasting and reduction smelting with desulphurization additives used to remove sulphur from the copper slag. The results showed that desulphurization effect of desulphurization roasting is poor but when combined with reduction smelting with CaO addition is possible to manufacture low sulphur pig iron from copper smelting slag.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 1; 349-355
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies