Tytuł:
Magnetic Properties of Zinc Doped Ferrites
Autorzy:
Abd El-Ati, M. I.
Kafafy, Aziz M.
Tawfik, A.
Powiązania:
https://bibliotekanauki.pl/articles/1887816.pdf
Data publikacji:
1991-06
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
75.50.Gg
75.50.Dd
Opis:
A series of samples of the system Co$\text{}_{1-x}$Zn$\text{}_{x}$Fe$\text{}_{2}$O$\text{}_{4}$ (x = 0.0, 0.3, 0.4, 0.5 and 0.8) have been prepared by the usual ceramic technique. X-ray analysis shows that they are cubic spinel (single phase). The lattice parameter a and the bulk density D are measured for the samples. The substitution experiments replacing Co$\text{}^{2+}$ by Zn$\text{}^{2+}$ furnish new significant fact concerning the magnetic behaviour of ferrites. The magnetic strength of the magnetic ions on the Band A-sites can be varried relative to each other by the substitution of Zn$\text{}^{2+}$. The increase of density of the composition increases the magnetic interaction of the dipole moment at the B-sites.
Źródło:
Acta Physica Polonica A; 1991, 79, 6; 889-894
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
High Performance of Electroacoustic Piezoelectric Ceramic Transducers
Autorzy:
Abd El-Ati, M. I.
Mosaad, M. M.
El-Baradie, B.Y.
Powiązania:
https://bibliotekanauki.pl/articles/1920644.pdf
Data publikacji:
1992-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
43.35.+d
77.60.+v
Opis:
Lead zirconate-titanate containing 1 wt % niobium with different Zr/Ti ratios compositions were studied. A pronounced increase in densification during sintering process occurred near tetragonal-rhombohedral phase. Dielectric constant of polarized and unpolarized samples was studied. The rotation of all 90° domains to their original positions caused the more looseness of Ti$\text{}^{4+}$ and Zr$\text{}^{4+}$ in the octahedral configuration leading to greater polarization in the tetragonal structure, thus leading to, higher dielectric constant. Near the phase change, the minimum resonance frequency caused the minimum values of ultrasonic waves, which were emitted from the edge of the polarized ceramic transducers.
Źródło:
Acta Physica Polonica A; 1992, 81, 4-5; 527-533
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies