Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Abbas, S. F." wg kryterium: Autor


Wyświetlanie 1-2 z 2
Tytuł:
Heterosis for yield and yield components in diallel crosses of Brassica napus L.
Heterozja dla plonu i jego składników w krzyżowaniu diallelicznym rzepaku (Brassica napus L.)
Autorzy:
Farhatullah, F.
Khan, N.A.
Abbas, S.J.
Powiązania:
https://bibliotekanauki.pl/articles/832735.pdf
Data publikacji:
2006
Wydawca:
Instytut Hodowli i Aklimatyzacji Roślin
Tematy:
heterosis
yield
yield component
diallel cross
Brassica napus
hybrid
F1 hybrid
rapeseed
Pakistan
breeding programme
plant breeding
Źródło:
Rośliny Oleiste - Oilseed Crops; 2006, 27, 1
1233-8273
Pojawia się w:
Rośliny Oleiste - Oilseed Crops
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure Development of Spark Plasma Sintered Ti-Nb Alloy by Heat Treatment
Autorzy:
Haq, M. A.
Abbas, S. F.
Eom, N. S. A.
Kim, T. S.
Lee, B.
Park, K.-T.
Kim, B. S.
Powiązania:
https://bibliotekanauki.pl/articles/355593.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
TiNb alloy
Spark plasma sintering
Heat treatment
Microstructure
β-phase titanium
Opis:
The β-phase Titanium (β-Ti) alloys have been under the spotlight in the recent past for their use as biomedical prosthetic materials owing to their excellent properties such as low elastic modulus, high corrosion resistance and tensile strength. Recently, Niobium (Nb) has gained a lot of attention as a β-phase stabilizing element in Ti alloys to replace Vanadium (V) due to its excellent solubility in Ti, low elastic modulus and biocompatibility. In this work, low cost Ti-20Nb binary alloy has been fabricated via powder metallurgy procedures. The blended powder mixtures of Ti and Nb were sintered at 900°C for 20 mins by the Spark Plasma Sintering (SPS) with an applied uniaxial pressure of 40 MPa. The heating rate was fixed at 50°C/min. The sintered alloy was subject to heat treatments at 1200°C in vacuum condition for various time durations. The characterizations of microstructure obtained during this process were done using FE-SEM, EDS and XRD. By increasing heat treatment time, as understood, the volume of residual Nb particles was decreased resulting in accelerated diffusion of Nb into Ti. Micro hardness of the alloy increased from 340 to 355 HV with the increase in β phase content from 30 to 45%. The resultant alloys had relatively high densities and homogenized microstructures of dispersed lamellar β grains in α matrix.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1429-1432
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies