Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "cast iron composite" wg kryterium: Temat


Wyświetlanie 1-10 z 10
Tytuł:
Cast Iron Reinforced with Foaming Ceramic Insert
Autorzy:
Dulska, A.
Studnicki, A.
Cholewa, M.
Szajnar, J.
Powiązania:
https://bibliotekanauki.pl/articles/382732.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ceramics
cast iron composite
ceramics insert
materiał ceramiczny
kompozyt żeliwny
wkład ceramiczny
Opis:
This paper presents matters related to production of ceramic and cast iron composite. The composite was made with the use of a foam structured ceramic insert. The tests included measuring of hardness, impact strength and resistance to abrasive wear of the composite produced. On the basis of obtaining results was stated that the use of foamed ceramic filters provides good conditions of filling a ceramic framework with molten grey or chromium cast iron. The growth of hardness of the ceramic-grey cast iron composite is ca. 60% as compared to the grey cast iron hardness. The growth of hardness of the ceramic-chromium cast iron composite is slight and does not exceed 5 % in comparison to the chromium cast iron. Introduction of the ceramic inserts deteriorates the cast iron impact strength by ca. 20 - 30 %. The use of ceramic inserts increases the resistance to abrasive wear in case of grey cast iron by ca. 13% and in case of the chromium cast iron by ca. 10 %.
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 137-140
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Reinforcing cast iron with composite insert
Autorzy:
Dulska, A.
Studnicki, A.
Szajnar, J.
Powiązania:
https://bibliotekanauki.pl/articles/353919.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
composite
cast iron
ceramic
Opis:
The paper presents a proprietary method of making composite cast iron (eutectic) locally reinforced with ceramics. The research included making casts with a ceramic layer, its percentage of the surface was 30%. The research included abrasive wear resistance according to ASTM G 65-00. As a result of the research it has been found that the infiltration of the molten metal into the ceramic preform mainly affects the correct production of the cast with local reinforcement. The research results also have proven that the application of a lattice ceramic insert placed in the mould is the most appropriate option, due to the even distribution of the particles in the cast and obtaining a sound cast.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 355-357
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Characteristics of the Granular State of Ceramic Particles in the Aspect of Producing Metal-Ceramic Composite Layers in Molds
Autorzy:
Dulska, A.
Kilarski, J.
Studnicki, A.
Szajnar, J.
Powiązania:
https://bibliotekanauki.pl/articles/383180.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ceramics
composite
granular
cast iron
properties
ceramika
kompozyty
warstwy metaliczno-ceramiczne
żeliwo
Opis:
The paper presents selected granular ceramic materials available on the Polish market. Their characteristics have been determined in the aspect on application in the production of iron alloy-ceramic composite. The possibility of obtaining a composite layer by means of bulk grains in molds of plates were considered, which was the foundation for experimental molds to be used in service tests. On the basis of obtaining results was stated that the knowledge of the characteristics of bulk grains enables the calculation of their quantity necessary for the composite production. When using the bulk grains the thickness of the composite layer is restricted by the thermal relations (cooler) and the physical phenomena (buoyancy, metal static pressure). Increasing amount of grains above definite condition causes surface defects in the castings. Each casting, due to its weight, shape and place of composite layer production requires an individual approach, both at the stage of formation and that of calculation of the required quantity of ceramic grains.
Źródło:
Archives of Foundry Engineering; 2018, 18, 3; 5-10
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Reinforcement of existing cast-iron structural elements by means of fiber reinforced composites
Wzmacnianie istniejących, żeliwnych elementów konstrukcyjnych za pomocą włóknokompozytów
Autorzy:
Marcinowski, J.
Różycki, Z.
Powiązania:
https://bibliotekanauki.pl/articles/396712.pdf
Data publikacji:
2016
Wydawca:
Uniwersytet Zielonogórski. Oficyna Wydawnicza
Tematy:
cast iron columns
reinforecement
composite jacket
CFRP
destructive tests
słupy żeliwne
wzmocnienie
powłoka kompozytowa
badania nieniszczące
Opis:
The paper deals with tubular, cast-iron columns which should be reinforced due to the planned new structural function of these elements. According to the requirements of the monument conservator the general appearance of columns should not be altered significantly. Reinforcement with an external, thin coating (sleeve or jacket) made of composite (carbon fibre reinforced polymer - CFRP) was proposed. Details of the proposed technique were presented. The reinforcement effect was verified in destructive test sperformed on two columns without reinforcement and the two other columns reinforced with the chosen technique. Due to the expected very high load capacity of the axially loaded column, the test rig was designed in such a manner that the force could be applied on big eccentricity. For this purpose a special base was prepared (comp. Fig. 1). Destructive tests have confirmed the high effectiveness of the adopted strengthening technique.
Praca dotyczy żeliwnych słupów cylindrycznych, które w związku z planowaną ich nową funkcją konstrukcyjną powinny zostać wzmocnione. Wymagania konserwatorskie nie dopuszczają znaczących zmian wyglądu zewnętrznego wzmacnianych słupów, z tego względu zaproponowano wzmocnienie za pomocą cienkiej powłoki włóknokompozytowej CFRP nakładanej na zewnętrzną powierzchnię słupów. W pracy zaprezentowano szczegóły proponowanej techniki wzmocnienia. Uzyskany efekt wzmocnienia zweryfikowano w badaniach niszczących wykonanych na dwóch słupach oryginalnych i dwóch słupach poddanych wzmocnieniu proponowaną techniką. Z powodu spodziewanej bardzo wysokiej odporności słupów na ściskanie osiowe, stanowisko badawcze zaprojektowano w taki sposób, aby siła mogła być przykładana na dużym mimośrodzie. W tym celu zaprojektowano i wykonano dodatkową głowicę. Badania niszczące potwierdziły wysoką efektywność zastosowanej techniki wzmocnienia.
Źródło:
Civil and Environmental Engineering Reports; 2016, No. 20(1); 37-45
2080-5187
2450-8594
Pojawia się w:
Civil and Environmental Engineering Reports
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Composite Material with Cast Iron Matrix Designed for Brake Systems of Technical Means of Transport
Materiał kompozytowy z osnową z żeliwa przeznaczony na układy hamulcowe środków transportu
Autorzy:
Posmyk, Andrzej
Myalski, Jerzy
Powiązania:
https://bibliotekanauki.pl/articles/2171801.pdf
Data publikacji:
2022
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
means of transport
brake disc
composite
cast iron
SiC foam
środki transportu
tarcza hamulcowa
kompozyt
żeliwo
pianka SiC
Opis:
The paper presents the basics of manufacturing and the tribological properties of the developed cast iron-ceramic composite designed for brake discs or drums. The matrix of the composite consists of GJL-150 grey cast iron used for the production of brake discs. The reinforcing phase is a SiC foam with an activated surface. The use of ceramic foam simplifies the production process because it does not require expensive mixing of the matrix and the reinforcing phase to ensure the homogeneity of the composite. An addition of 10% SiC (λSiC= 100–350 Wm-1K-1) improves the thermal conductivity of cast iron (λCI = 50–60 Wm-1K-1). The presence of foam elements homogenously distributed throughout the whole matrix volume reduces the wear of both the composite and the counter-sample. The results of comparative studies of contacts between the cast iron and the composite brake disc showed almost a threefold lower wear of the pad and disc and about a 10°C lower temperature in the pad near the friction zone under the pressure of 1 MPa and at a sliding velocity of 0.5 m/s. The significantly lower wear of the friction elements of the brake system will contribute to a reduction in environmental pollution by wear debris, which is required by European Union directives.
W artykule opisano podstawy wytwarzania i właściwości tribologiczne opracowanego kompozytu żeliwno-ceramicznego przeznaczonego na tarcze lub bębny hamulcowe. Osnowę kompozytu stanowi stosowane do wytwarzania tarcz hamulcowych żeliwo szare GJL-150, a umocnieniem jest pianka z SiC z aktywowaną powierzchnią. Użycie pianki ceramicznej upraszcza proces wytwarzania, ponieważ nie wymaga kosztownego mieszania osnowy i fazy zbrojącej dla zapewnienia homogeniczności kompozytu. Dodanie 10% pianki SiC (λSiC= 100–350 Wm-1K-1) poprawia przewodność cieplną żeliwa (λCI = 50–60 Wm-1K-1). Obecność równomiernie rozłożonych w całej objętości osnowy elementów pianki zmniejsza zużycie zarówno kompozytu, jak i współpracującego z nim materiału ciernego. Wyniki badań porównawczych skojarzeń z tarczą żeliwną i kompozytową wykazały mniejsze prawie trzykrotnie zużycie klocka i tarczy oraz niższą o 10°C temperaturę w klocku w pobliżu strefy tarcia przy nacisku 1 MPa i prędkości 0,5 m/s. Znacząco zmniejszone zużycie elementów ciernych układu hamulcowego przyczyni się do zmniejszenia zapylenia środowiska produktami zużycia, co jest wymagane w dyrektywach Unii Europejskiej.
Źródło:
Tribologia; 2022, 3; 79--86
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mechanizm zużywania w skojarzeniu żeliwo szare-kompozyt zbrojony cząstkami AL2O3
Wear mechanism in pairing grey cast iron - AL2O3 particles reinforced composite
Autorzy:
Posmyk, A.
Bąkowski, H.
Powiązania:
https://bibliotekanauki.pl/articles/189196.pdf
Data publikacji:
2009
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
zużywanie
żeliwo
kompozyt
MES (metoda elementów skończonych)
modelowanie
tlenek glinu
wear
cast iron
composite material
FEM
modelling
aluminium oxide
Opis:
W pracy przedstawiono mechanizm zużywania skojarzenia żeliwo–kompozyt. Żeliwo jest stosowane na pierścienie tłokowe silników spalinowych, a kompozyt na tuleje cylindrowe silników małej mocy. Osnową kompozytu jest stop EN-AW-6062, a fazą zbrojącą są cząstki tlenku glinu. Do wyjaśnienia mechanizmu zbudowano model skojarzenia, wykorzystując metodę elementów skończonych. W modelu uwzględniono zmianę wytrzymałości na styku materiałów osnowy i cząstek fazy zbrojącej. Symulacja z wykorzystaniem zbudowanego modelu pozwoliła wyznaczyć rozkład naprężeń i odkształceń w żeliwie i kompozycie w pobliżu cząstki zbrojącej. Z otrzymanego rozkładu wynika, że w żeliwie w pobliżu cząstek fazy zbrojącej panują naprężenia przekraczające granicę plastyczności żeliwa, co prowadzi do przyspieszonego zużywania żeliwa na etapie docierania skojarzenia. Siły tarcia generują moment, który obraca cząstki słabo związane z osnową. Cząstki usunięte z osnowy powodują zużywanie przez bruzdowanie zarówno żeliwa, jak i materiału osnowy.
The wear mechanism of cast iron-composite material pairing was presented in this paper. Cast iron has been used for piston rings production and composite material for cylinder liners. The matrix of the composite is 6062 alloy and as the reinforcing chase aluminium oxide particles has been used. For an explanation of the wear mechanism the, Finite Elements Method has been used. Three cases have been analysed: first, without movement (ž = 0) and without the transient layer, second, with movement (ž = 0,2) and without the transient layer, third, with movement (ž = 0,2) and with the transient layer. Simulation with the use of a build model allowed us to achieve the distribution of stresses and strains. From the calculated distribution of stresses, it results that the stresses in cast iron near of reinforcing phase particles are higher then the yield strength of cast iron. This lead to accelerated wear of cast iron during the wear-in phase of the rubbing pair. The friction forces generate moment, which rotates the reinforcing particles with weak adherence to the matrix material. Particles are removed from the matrix cause wear of cast iron and matrix material.
Źródło:
Tribologia; 2009, 2; 183-190
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mechanizm zużywania modelowego skojarzenia pierścień tłokowy-tuleja cylindrowa wykonanego z żeliwa i kompozytu zbrojonego włóknami Al2O3 ułożonymi stycznie do powierzchni tarcia
Wear mechanism of piston cylinder liner pairing made of cast iron-composite material reinforced with Al2O3 fibers placed tangential to wear surface
Autorzy:
Posmyk, A.
Bąkowski, H.
Powiązania:
https://bibliotekanauki.pl/articles/188866.pdf
Data publikacji:
2010
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
zużywanie
żeliwo
kompozyt
MES (metoda elementów skończonych)
modelowanie
tlenek glinu
włókna
wear
cast iron
composite material
FEM
modelling
aluminium oxide
fibres
Opis:
W pracy przedstawiono mechanizm zużywania skojarzenia pierścień tłokowy–tuleja cylindrowa wykonanego z żeliwa i siluminu okołoeutektycznego zbrojonego włóknami z tlenku glinu. Żeliwo szare lub sferoidalne jest stosowane na pierścienie tłokowe silników spalinowych, a kompozyt na osnowie siluminu na tuleje cylindrowe silników spalinowych. Osnową kompozytu jest stop EN-AC-4700, a fazą zbrojącą są włókna tlenku glinu. Zadaniem fazy zbrojącej jest zmniejszenie skłonności do sczepiana adhezyjnego żeliwa z aluminium w osnowie. Podczas współpracy ślizgowej ma miejsce styk powierzchni żeliwa z wystającymi ponad powierzchnię włóknami tlenku glinu. Zawartość tych włókien i ich ułożenie w stosunku do powierzchni tarcia decydują o wartości lokalnych naprężeń i odkształceń, które wywierają istotny wpływ na opory tarcia i mechanizm zużywania skojarzenia. W pracy przedstawiono wyniki obliczeń lokalnych naprężeń i odkształceń wykonanych MES na modelu, w którym włókna są ułożone stycznie do powierzchni tarcia i prostopadle do kierunku ruchu pierścienia.
The wear mechanism of piston ring-cylinder liner pairing produced from cast iron and eutectic silumine reinforced with alumina fibers has been presented in this paper. Grey or spheroid cast iron is used for the production of piston rings and composite material is used for cylinder liners of combustion engines. EN-AC-4700 –alloy is the matrix of composite and alumina fibers are the reinforcing phase. The function of the reinforcing phase is the decrease of the tendency to adhesion tacking between cast iron and the aluminium matrix. During sliding, the contact exists between cast iron and alumina fibers protruding over the matrix surface. The content of fibers and their orientation to the friction surface determine the level of local stresses and stains, which exercise a significant influence on friction forces and the wear of pairing. The calculated results of local stresses and strains made by MES on the model are presented. The fibers in this model are oriented tangentially to the friction surface and perpendicularly to the direction of movement.
Źródło:
Tribologia; 2010, 5; 173-180
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The composition of reaction substrates for TiC carbides synthesis and its influence on the thickness of iron casting composite layer
Autorzy:
Olejnik, E.
Janas, A.
Kolbus, A.
Sikora, G.
Powiązania:
https://bibliotekanauki.pl/articles/380875.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
composite layer
composite in situ
SHS process
solidification process
superficial layer
cast iron
TiC carbides
warstwa kompozytowa
kompozyt in situ
synteza wysokotemperaturowa
proces krzepnięcia
warstwa powierzchniowa
żeliwo
Opis:
The effect of reaction substrates for the TiC carbide synthesis on the composite layer thickness produced in cast iron was examined. It was found that, at a constant weight of the charge amounting to 0.5 kg, changing the weight of the, placed in mould, stoichiometric mixture of titanium carbide (from 0.01 to 0.04 kg) changed the thickness of the composite layer from 1 to 15 mm. Carbides synthesis starts directly in mould induced by the temperature of molten alloy poured into this mould (1700 K). The TiC carbides formed in this reaction are later, i.e. during alloy solidification, acting as a base composite material. The size of TiC carbides obtained in the synthesis is from 1 to 10 μm. They occur in the layers as locally compact and coagulated forms. Microstructure, chemical composition and structure of the obtained materials were tested by scanning electron microscopy (SEM), X-ray microanalysis (EDS), and X-ray diffraction (XRD).
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 165-168
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Korozja trących się elementów układów hamulcowych (tarcze, bębny) pojazdów i możliwości jej minimalizacji
Corrosion of braking systems friction elements (disks, drums) of vehicles and possibilities of its prevention
Autorzy:
Siepracka, B.
Szumniak, J.
Nyc, R.
Powiązania:
https://bibliotekanauki.pl/articles/347738.pdf
Data publikacji:
2010
Wydawca:
Akademia Wojsk Lądowych imienia generała Tadeusza Kościuszki
Tematy:
żeliwo
kompozyt cierny
Sywica fenolowo-formaldehydowa
kompleksy metali
tarcie
korozja
hamulce
cast iron
friction composite
phenol-formaldehyde resin
metal complexes
corrosion
brakes
Opis:
W artykule przedstawiono wyniki obserwacji stopnia skorodowania zachodzącego w parze tribologicznej hamulca (tarczowego i bębnowego) w okresie jego postoju w warunkach agresywnego otoczenia miejskiego (przemysłowego). Wyniki przeprowadzonych badań laboratoryjnych, aktywowania powierzchni elementu metalowego przez tarcie z kompozytami, wykazały zróżnicowaną ich podatność korozyjną, w większości przypadków, większą dla powierzchni po tarciu. Wprowadzenie do kompozytu odpowiednich dodatków w ilości 1¸ 2%, np. niektórych kompleksów metali, zwiększa odporność na korozję powierzchni żeliwa kojarzonej z nim tarciowo. Artykuł zawiera przykładowe wyniki badań odporności na korozję przy tarciu żeliwa po żeliwie i kompozytu modyfikowanego.
This paper presents the results of corrosion damage observations occurring in brake tribological pairs (a disk brake and a drum brake) in the period of their standstill in the condition of aggressive municipal environment (industrial). The results of laboratory investigations performed, and activation of metal element surfaces by friction with composites, demonstrated their different corrosion resistance, in many cases, smaller for surface after friction. An introduction to the composite suitable additives in quantity 1¸2%, for example some metal complexes, increases corrosion resistance of cast iron surface frictional interacting with him. This paper contains some results of corrosion resistance investigations by friction of cast iron with cast iron and composite modified by authors.
Źródło:
Zeszyty Naukowe / Wyższa Szkoła Oficerska Wojsk Lądowych im. gen. T. Kościuszki; 2010, 4; 236-242
1731-8157
Pojawia się w:
Zeszyty Naukowe / Wyższa Szkoła Oficerska Wojsk Lądowych im. gen. T. Kościuszki
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structure and Mechanical Properties of HVOF Sprayed (WC-Co+Co) Composite Coating on Ductile Cast Iron
Mikrostruktura i właściwości mechaniczne powłok kompozytowych (WC-Co+Co) natryskiwanych metodą HVOF na żeliwo sferoidalne
Autorzy:
Ksiazek, Marzanna
Boron, Lukasz
Tchorz, Adam
Grzelka, Ryszard
Powiązania:
https://bibliotekanauki.pl/articles/115178.pdf
Data publikacji:
2019
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
natryskiwanie termiczne
żeliwo sferoidalne
HVOF
powłoka WC-Co
powłoka kompozytowa
odporność na zużycie
thermal spraying
ductile cast iron
WC-Co coating
composite coating
wear resistance
Opis:
An investigation was conducted to determine the role of Co particles in the WC-Co coating produced with the High Velocity Oxygen-Fuel (HVOF) spraying on microstructure, mechanical and wear properties in a system of type: WC-Co coating/ductlile cast iron. The microstructure of the thermal sprayed WC-Co+Co coating was characterized by scanning electron (SEM) and transmission electron (TEM) microscopes as well as the analysis of chemical and phase composition in microareas (EDS, XRD). For analysis of the quality and adhesion of coatings, the scratch-test was applied. It was found that as a result of the HVOF spray of WC-Co powders with the addition of Co particles, the coatings of low porosity, high hardness, a very good adhesion to the substrate, compact structure with partially molten Co particles and finely fragmented WC particles embedded in a cobalt matrix, coming to the size of nanocrystalline sizes were obtained. Moreover, the results were discussed in reference to examination of bending strength considering cracking and delamination in the system of (WC-Co+Co)/ductile cast iron as well as hardness and wear resistance of the coating. It was found that the addition of Co particles was significantly increase resistance to cracking and wear behaviour in the studied system.
W pracy przedstawiono wyniki badań, dotyczące wpływu modyfikacji składu chemicznego powłok WC-Co (poprzez domieszkowanie cząstkami Co), wytworzonych techniką natryskiwania proszkowego naddźwiękowego z dużymi prędkościami (HVOF) na mikrostrukturę, właściwości mechaniczne i użytkowe układu typu: powłoka WC-Co/żeliwo sferoidalne. Mikrostruktura powłok WC-Co+Co była analizowana za pomocą mikroskopu świetlnego, skaningowego i transmisyjnego wraz z przeprowadzeniem badań składu chemicznego i fazowego powłok w mikroobszarach przy wykorzystaniu techniki EOS i XRO. Do analizy jakości i przyczepności powłok zastosowano test zarysowania. Stwierdzono, że w wyniku natryskiwania techniką HVOF proszków WC-Co z dodatkiem cząstek Co, powłoki charakteryzują się niską porowatością wysoką twardością bardzo dobrą przyczepnością do podłoża, zwartą budową z częściowo stopionymi cząstkami Co i silnie rozdrobnionymi cząstkami WC osadzonymi w kobaltowej matrycy, dochodzącymi do wymiarów nanometrycznych. Ponadto w pracy przedstawiono wyniki dotyczące wytrzymałości na zginanie układu WC-Co+Co/żeliwo sferoidalne w zestawieniu z analizą pękania i delaminacji powłoki w obszarze granicy rozdziału, oraz wynikami pomiarów twardości i odporności na zużycie powłoki. Stwierdzono, że dodatek cząstek Co znacznie zwiększa odporność na pękanie i zużycie w badanym układzie.
Źródło:
Welding Technology Review; 2019, 91, 3; 41-50
0033-2364
2449-7959
Pojawia się w:
Welding Technology Review
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-10 z 10

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies