The Effect of Si and Mn on Microstructure and Selected Properties of Cr-Ni Stainless Steels
Autorzy:
Kalandyk, B.
Zapała, R.
Starowicz, M.
Powiązania:
https://bibliotekanauki.pl/articles/380853.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
cast stainless
alloy composition
hardness
electrochemical corrosion
Miller test
odlew ze stali nierdzewnej
skład stopu
twardość
korozja elektrochemiczna
test Millera
Opis:
Cast stainless steel of the Cr-Ni duplex type is used, among others, for the cast parts of pumps and valves handling various chemically aggressive media. Therefore, the main problem discussed in this article is the problem of abrasion wear resistance in a mixture of SiC and water and resistance to electrochemical corrosion in a 3% NaCl- H2O solution of selected cast steel grades, i.e. typical duplex cast steel, high silicon and manganese duplex cast steel, and Cr-Ni austenitic cast steel (type AISI 316L). The study shows that the best abrasion wear resistance comparable to Ni-Hart cast iron was obtained in the cast duplex steel, where Ni was partially replaced with Mn and N. This cast steel was also characterized by the highest hardness and matrix microhardness among all the tested cast steel grades. The best resistance to electrochemical corrosion in 3% NaCl- H2O solution showed the cast duplex steel with high content of Cr, Mo and N. The addition of Ni plays rather insignificant role in the improvement of corrosion resistance of the materials tested.
Źródło:
Archives of Foundry Engineering; 2017, 17, 1; 192-196
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Convergent traffic in the environment of wireless MESH technology
Autorzy:
Paszkiewicz, A.
Bolanowski, M.
Zapała, P.
Powiązania:
https://bibliotekanauki.pl/articles/106287.pdf
Data publikacji:
2013
Wydawca:
Uniwersytet Marii Curie-Skłodowskiej. Wydawnictwo Uniwersytetu Marii Curie-Skłodowskiej
Tematy:
wireless MESH
performance
Voice over IP
Video over IP
load balancing
Opis:
The paper presents a performance study of wireless MESH networks in the context of the convergent transmission. Nowadays, the integration of voice, video and data is becoming the norm. However, the wireless LAN environment, and especially MESH technology is an unfriendly environment due to its characteristics. Therefore, the impact of the size of transmitted frames to delays in the network based on mesh technology was analyzed. The sizes of transmitted frames corresponded to standards for Voice over IP, Video over IP that are commonly used. Additionally, a model of effective load balancing in mesh networks was presented. Then, the reliability and flexibility of these networks will be increased.
Źródło:
Annales Universitatis Mariae Curie-Skłodowska. Sectio AI, Informatica; 2013, 13, 1; 83-95
1732-1360
2083-3628
Pojawia się w:
Annales Universitatis Mariae Curie-Skłodowska. Sectio AI, Informatica
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Mechanical Properties of High-Alloyed 23Cr-5Mn-2Ni-3Mo Cast Steel
Mikrostruktura i właściwości mechaniczne wysokostopowego staliwa 23Cr-5Mn-2Ni-3Mo
Autorzy:
Kalandyk, B.
Zapała, R.
Kasińska, J.
Wróbel, M.
Balicki, M.
Powiązania:
https://bibliotekanauki.pl/articles/356347.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
duplex stainless cast steels
microstructure
solution annealing
mechanical properties
staliwo typu duplex
mikrostruktura
roztwór do wyżarzania
właściwości mechaniczne
Opis:
The article presents the microstructure and mechanical properties of cast duplex stainless steel type 23Cr-5Mn-2Ni-3Mo. It has been shown that the structure of the tested cast steel is composed of ferrite enriched in Cr, Mo and Si, and austenite enriched in Mn and Ni. In the initial state, at the interface, precipitates rich in Cr and Mo were present. A high carbon content (0.08%C) in this cast steel indicates that probably those were complex carbides of the M23C6 type and/or σ phase. Studies have proved that the solution annealing conducted at 1060°C was not sufficient for their full dissolution, while at the solutioning temperature of 1150°C, the structure of the tested material was composed of ferrite and austenite. Partial replacement of Ni by two other austenite-forming elements, which are Mn and N, has ensured obtaining mechanical properties comparable to cast duplex 24Cr-5Ni-3Mo steel of the second generation. Basing on the results of static tensile test, a twice higher yield strength was proved to be obtained, compared to the cast austenitic 18Cr-9Ni and 19Cr-11Ni-2Mo steel commonly used in the foundry industry. In addition to the high yield strength (YS = 547 ÷ 572 MPa), the tested cast steel was characterized by the following mechanical properties: UTS = 731 ÷ 750 MPa, EL = 21 ÷ 29.5%, R.A. = 43 ÷ 52%, hardness 256 ÷ 266 HB. Fractures formed in mechanical tests showed ductile-brittle character.
W artykule przedstawiono mikrostrukturę i właściwości mechaniczne, kwasoodpornego staliwa ferrytyczno - austenitycznego 23Cr-5Mn-2Ni-3Mo typu duplex. Wykazano, że struktura badanego staliwa składa się z ferrytu δ wzbogaconego w C r, Mo i S i oraz austenitu wzbogaconego w Mn i Ni. W stanie wyjściowym na granicy międzyfazowej występują wydzielenia wzbogacone w C r i Mo. Wysoka zawartość C (0.08%) w tym staliwie wskazuje, że prawdopodobnie są to złożone węgliki M23C6 i/lub faza σ. Wykazano, że temperatura przesycania 1060°C nie jest wystarczająca do ich całkowitego rozpuszczenia. Natomiast w temperaturze przesycania 1150°C struktura badanego materiału składa się z ferrytu i austenitu. Częściowe zastąpienie Ni przez dwa inne pierwiastki austenitotwórcze jakimi są Mn i N zapewniło uzyskanie porównywalnych właściwości mechanicznych do staliwa duplex 24Cr-5Ni-3Mo drugiej generacji. Na podstawie przeprowadzonej statycznej próby rozciągania wykazano dwukrotnie wyższą granicę plastyczności w porównaniu do często stosowanego w przemyśle odlewniczym austenitycznego staliwa 18Cr-9Ni i 19Cr-11Ni-2Mo. Poza wysoką granicą plastyczności (Rp0,2 = 547 ÷ 572 MPa), badane staliwo charakteryzowało się następującymi właściwościami mechanicznymi: Rm = 731 ÷ 750 MPa, As = 21 ÷ 29,5%, Z = 43 ÷ 52%, HB = 256 ÷ 266. Przełomy po badaniach wytrzymałościowych wykazywały charakter ciagliwo-kruchy.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 4; 2529-2534
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Silicon Addition on the Microstructure of Cast 24Cr-5Ni-2.5Mo-xSi Duplex Steel
Autorzy:
Kalandyk, B.
Zapała, R.
Witkowska, M.
Kowalska, J.
Powiązania:
https://bibliotekanauki.pl/articles/381193.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stainless steels
microstructure of cast
Thermo-Calc
duplex steel
stale nierdzewne
mikrostruktura odlewu
stal duplex
Opis:
Characteristics of the microstructure of corrosion-resistant cast 24Cr-5Ni-2.5Mo duplex steel after introduction of 0.98, 1.67 and 4.3% Si were described. Based on the test results it has been found that silicon addition introduced to the corrosion-resistant cast two-phase duplex steel significantly reduces austenite content in the alloy matrix. Increasing silicon content in the test alloy to 4.3% has resulted, in addition to the elimination of austenite, also in the precipitation of Si-containing intermetallic phases at the grain boundaries and inside the grains. The precipitates were characterized by varying content of Cr and Mo, indicating the presence in the structure of more than one type of the brittle phase characteristic for this group of materials. The simulation using Thermo-Calc software has confirmed the presence of ferrite in all tested alloys. In the material containing 4.3% Si, the Cr and Si enriched precipitates, such as G phase and Cr3Si were additionally observed to occur.
Źródło:
Archives of Foundry Engineering; 2018, 18, 1; 186-190
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Properties of 17Cr-0.8C Cast Steel
Autorzy:
Kalandyk, B.
Zapała, R.
Pałka, P.
Wróbel, M.
Powiązania:
https://bibliotekanauki.pl/articles/353847.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
martensitic cast steel
M23C6
Fe7C3
Fe3C carbides
heat treatment
microstructure
hardness
Opis:
The results of studies of the microstructure and properties of cast high alloy steels containing 17% Cr and 0.8% C subjected to different variants of heat treatment are presented. For phase identification, the light microscopy and scanning electron microscopy as well as the X-ray diffraction analysis were used. The conducted studies revealed the presence of carbides in the microstructure, mainly of the M23C6 carbide, detected after both quenching and tempering at 200 and 600°C. The use of low and high tempering significantly reduced the test alloy hardness from 657.3 HV30 to 403.7 HV30. At the same time, hardness was observed to have an impact on the values of abrasion in the conducted Miller slurry test. Higher material hardness leads to lower wear expressed by mass loss.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 1; 113-117
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluation of Microstructure and Tribological Properties of GX120Mn13 and GX120MnCr18-2 Cast Steels
Autorzy:
Kalandyk, B.
Zapała, R.
Kasińska, J.
Madej, M.
Powiązania:
https://bibliotekanauki.pl/articles/2079812.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
high manganese cast steel
microstructure
hardness
wear resistance
staliwo wysokomanganowe
mikrostruktura
twardość
odporność na zużycie
Opis:
The results of microstructure examinations and hardness measurements carried out on two selected grades of high-manganese cast steel with an austenitic matrix, i.e. GX120Mn13 and GX120MnCr18-2, are presented. The examinations of the cast steel microstructure have revealed that the matrix of the GX120MnCr18-2 cast steel contains the precipitates of complex carbides enriched in Cr and Mn with two different morphologies. The presence of these precipitates leads to an increase in hardness by approx. 30 HB compared to the GX120Mn13 cast steel. Samples cut out from the tested materials were loaded (10 strokes) with an energy of 53 J, and then a ball-on-disc tribological test was performed. The test was carried out in reciprocating motion under technically dry friction conditions. While analyzing the obtained results of the microstructure, hardness, and abrasion tests, it was found that the presence of the hard carbide precipitates in the plastic matrix of the tested GX120MnCr18-2 cast steel promoted an increase in hardness, but also led to chipping of these particles from the alloy matrix, thus contributing to micro-cutting during friction.
Źródło:
Archives of Foundry Engineering; 2021, 21, 4; 67-76
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Stress test of network devices with maximum traffic load for second and third layer of ISO/OSI model
Graniczne wysycanie ruchem urządzeń sieciowych w warstwie drugiej i trzeciej modelu ISO/OSI
Autorzy:
Bolanowski, M.
Paszkiewicz, A.
Zapala, P.
Żak, R.
Powiązania:
https://bibliotekanauki.pl/articles/152544.pdf
Data publikacji:
2014
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
computer network
stress test
network devices
model ISO/OSI
sieci komputerowe
testy wydajnościowe
urządzenia sieciowe
Opis:
Proper selection of network devices have a crucial impact on the entire process of designing and building a modern communication system. At the moment, performance testing of network devices are often implemented by specialized laboratories or by the network devices vendors. To implement this test, the test traffic need be generated with bandwidth of 100 and more Gb/s. The authors of the article proposed their own test topologies that allows to saturate all switch ports based on the entangled traffic between ports or routing instances. In the introduction, the authors present how this type of tests are currently implemented. In the second Chapter, the components of the test bench are presented. The third Chapter presents the topology used to implement the test in the second layer of ISO/OSI model, and shows the influence of the test traffic on the selected devices elements. In the Chapter four proposes topologies that saturate two tested switches with the traffic based on entangling traffic with use of VRF and OSPF protocols. Such approach, based on open standards allows for self-realization of the tests by the final customer who can check the performance of the protocols or application in the environment of maximum traffic load. Note, that the presented method is used only to generate load on the ports of the device. This could be a good basis to start the appropriate tests of specified services or protocols.
Odpowiedni dobór urządzeń sieciowych ma kluczowy wpływ na cały proces projektowania i budowy współczesnego systemu komunikacyjnego. W chwili obecnej testy wydajnościowe urządzeń sieciowych realizowane są najczęściej przez wyspecjalizowane laboratoria lub przez samych producentów urządzeń sieciowych. Do ich przeprowadzenia wymagane jest wygenerowanie ruchu testowego charakteryzującego się niejednokrotnie przepustowościami na poziomie 100 i więcej Gb/s. Autorzy w artykule zaproponowali własne topologie testowe które pozwalają wysycić wszystkie porty testowanego urządzenia. Bazują one na zapętlaniu ruchu pomiędzy portami lub instancjami rutingu. We wstępie autorzy prezentują jak aktualnie realizowane są tego typu testy urządzeń. W rozdziale drugim zaprezentowane zostały elementy składowe stanowiska badawczego. W rozdziale trzecim zaprezentowana została topologia wykorzystywana do realizacji testów w warstwie drugiej modelu ISO/OSI, oraz pokazano wpływ ruchu testowego na wybrane elementy sprzętowe urządzenia. W rozdziale czwartym zaproponowano topologie wysycania ruchem dwóch urządzeń testowych bazującą na zapętleniu ruchu z wykorzystaniem VRF i protokołu OSPF. Takie podejście, bazujące na otwartych standardach pozwala na samodzielną realizację testów urządzeń przez klienta końcowego, który może sprawdzić działanie interesujących go protokołów w środowisku granicznie wysyconego ruchem urządzenia sieciowego. Należy jednak pamiętać, że przedstawiona metoda służy jedynie do generowania obciążenia na portach urządzenia. Może to być dobra podstawa do zrealizowania właściwych testów określonych usług lub protokołów.
Źródło:
Pomiary Automatyka Kontrola; 2014, R. 60, nr 10, 10; 854-857
0032-4140
Pojawia się w:
Pomiary Automatyka Kontrola
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Impact Strength of Austenitic and Ferritic-Austenitic Cr-Ni Stainless Cast Steel in -40 and +20°C Temperature
Udarność kwasoospornego staliwa Cr-Ni w temperaturze -40 i +20°C
Autorzy:
Kalandyk, B.
Zapała, R.
Boroń, Ł.
Solecka, M.
Powiązania:
https://bibliotekanauki.pl/articles/353749.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stainless cast steel
microstructure
impact strength
fractographic examination
staliwo nierdzewne
mikrostruktura
odporność na uderzenia
udarność
Opis:
Studies described in this paper relate to common grades of cast corrosion resistant Cr-Ni steel with different matrix. The test materials were subjected to heat treatment, which consisted in the solution annealing at 1060°C followed by cooling in water. The conducted investigations, besides the microstructural characteristics of selected cast steel grades, included the evaluation of hardness, toughness (at a temperature of -40 and +20°C) and type of fracture obtained after breaking the specimens on a Charpy impact testing machine. Based on the results of the measured volume fraction of ferrite, it has been found that the content of this phase in cast austenitic steel is 1.9%, while in the two-phase ferritic-austenitic grades it ranges from 50 to 58%. It has been demonstrated that within the scope of conducted studies, the cast steel of an austenitic structure is characterised by higher impact strength than the two-phase ferritic-austenitic (F-A) grade. The changing appearance of the fractures of the specimens reflected the impact strength values obtained in the tested materials. Fractures of the cast austenitic Cr-Ni steel obtained in these studies were of a ductile character, while fractures of the cast ferritic-austenitic grade were mostly of a mixed character with the predominance of brittle phase and well visible cleavage planes.
Zaprezentowane w artykule badania dotyczą popularnych gatunków kwasoodpornego staliwa Cr-Ni o różnej osnowie. Zastosowane do badań materiały poddano obróbce cieplnej (przesycanie w temperaturze 1060°C i chłodzenie w wodzie). Przeprowadzone badania oprócz charakterystyki mikrostruktury wybranych gatunków staliwa obejmowały ocenę twardości, udarności (w temperaturze -40 i +20°C) oraz charakteru przełomów uzyskanych w wyniku złamania próbek na młocie Charpie'go. Na podstawie uzyskanych wyników udziału objętościowego ferrytu stwierdzono, że w staliwie austenitycznym występuje 1.9% tej fazy, natomiast w dwóch staliwach ferrytyczno-austenitycznych (F-A) udział ferrytu mieścił się w przedziale 50÷58%. Wykazano, że staliwo o strukturze austenitycznej charakteryzuje się wyższą udarnością w porównaniu do dwufazowego staliwa ferrytyczno-austenitycznego (F-A). Zmiany jakie zaszły w charakterze przełomów próbek były odzwierciedleniem uzyskanych wyników udarności badanych materiałów. W zakresie przeprowadzonych badań przełomy austenitycznego staliwa Cr-Ni wykazują charakter ciągliwo-kruchy, a przełomy staliwa F-A są przeważnie przełomami o charakterze mieszanym z przewagą przełomu kruchego z widocznymi płaszczyznami łupliwości.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 3; 1103-1106
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
High-temperature oxidation of cast steel in water vapour
Wysokotemperaturowe utlenianie staliwa w parze wodnej
Autorzy:
Zapała, R.
Pach, S.
Górny, M.
Homa, M.
Siewiorek, A.
Powiązania:
https://bibliotekanauki.pl/articles/391690.pdf
Data publikacji:
2015
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Odlewnictwa
Tematy:
cast heat-resistant steel
microstructure
high-temperature corrosion
water vapour
staliwo żaroodporne
mikrostruktura
korozja wysokotemperaturowa
para wodna
Opis:
The article presents the results of studies of the oxidation process conducted at 900°C for 12 hours in an atmosphere of water vapour on cast heat-resistant steel with a diversified structure (ferritic-austenitic, austenitic, and austenitic with carbides). Based on the studies of oxidation kinetics, it was found that samples were oxidized in approximation with the rules of linear law. Depending on the chemical composition and structure of tested alloys, the scale formed on the alloy surface had different properties. In the tested material characterised by a ferritic-austenitic structure, the tendency of the scale to detach from the surface of the metallic substrate was observed. It was probably due to different coefficients of the thermal expansion of austenite and ferrite.
Praca prezentuje wyniki badań utleniania w atmosferze pary wodnej staliwa żaroodpornego o różnej strukturze (ferrytyczno-austenitycznej, austenitycznej i austenitycznej z węglikami) w temperaturze 900°C w ciągu 12 godzin. Na podstawie badań kinetyki utleniania stwierdzono, że badane próbki utleniały się w przybliżeniu zgodnie z prawem liniowym. W zależności od składu chemicznego i struktury badanych stopów obserwowano odmienne właściwości powstałych zgorzelin. W przypadku materiału o strukturze ferrytyczno-austenitycznej stwierdzono odpadanie zgorzeliny od powierzchni rdzenia metalicznego związane prawdopodobnie z różnym współczynnikiem rozszerzalności cieplnej austenitu i ferrytu.
Źródło:
Prace Instytutu Odlewnictwa; 2015, T. 55, nr 3, 3; 61-70
1899-2439
Pojawia się w:
Prace Instytutu Odlewnictwa
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Neuromarkers of anxiety and depression in a patient after neuro-ophthalmic surgery of the meningioma - effect of individually-tailored tDCS and neurofeedback
Autorzy:
Mirski, A.
Pachalska, M.
Moskala, M.
Orski, M.
Orska, M.
Miaskiewicz, M.
Zapala, J.
Kropotov, J.D.
Powiązania:
https://bibliotekanauki.pl/articles/51672.pdf
Data publikacji:
2015
Wydawca:
Instytut Medycyny Wsi
Źródło:
Annals of Agricultural and Environmental Medicine; 2015, 22, 4
1232-1966
Pojawia się w:
Annals of Agricultural and Environmental Medicine
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of various strontium concentrations on its uptake and the content of isoflavonesin soybean sprouts
Autorzy:
Wojciak-Kosior, M.
Dresler, S.
Sowa, I.
Luc, K.
Staniak, M.
Latalski, M.
Zapala-Kielbowicz, K.
Kocjan, R.
Powiązania:
https://bibliotekanauki.pl/articles/2117832.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czasopisma i Monografie PAN
Tematy:
glycine max (l.) Merr.
isoflavones
soy
sprouts
strontium
Opis:
Metal ions can modify plant metabolism and change the level of biologically active components. In the present study, the impact of short-term exposure to strontium on the accumulation of the metal as well as the content of isoflavones in soybean sprouts was investigated. The seeds were germinated in hydroponics with 0, 1, 1.5, 2.5, 5.0, or 10.0 mM of Sr for 72 hours. The content of strontium was assessed using flame atomic absorption spectrometry and the amount of isoflavones was determined with high performance liquid chromatography. dose-dependent accumulation of Sr and a linear correlation between the Sr concentration in the growth medium and the content of the element in the plant samples were observed. The largest changes in the isoflavone content, compared to the control, were noted in soy sprouts germinated in the presence of 5 and 10 mM of strontium. daidzin, genistin, malonyldaidzin, and malonylgenistin were the dominant isoflavones and their content increased by approx. 28, 44, 34, and 47%, respectively, compared to the control. low amounts of aglycones were found; moreover, their content decreased by ca. 19–30%. Our research can be important for obtaining a natural product enhanced with strontium and isoflavones, which contribute to prevention of osteoporosis associated with endog- enous oestrogen deficits
Źródło:
Acta Biologica Cracoviensia. Series Botanica; 2019, 61, 2; 7-12
0001-5296
Pojawia się w:
Acta Biologica Cracoviensia. Series Botanica
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Application of computer modelling for planning maxillofacial surgery
Zastosowanie modelowania komputerowego do planowania zabiegów chirurgii szczękowej
Autorzy:
Kromka-Szydek, M.
Ślebioda, P.
Żakowska, M.
Karbowski, K.
Szyper-Szczurowska, J.
Szczurowski, P.
Zapała, J.
Powiązania:
https://bibliotekanauki.pl/articles/176217.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
CAD
reverse engineering
medicine
inżynieria rekonstrukcyjna
medycyna
Opis:
The article describes application of reverse engineering techniques for modeling the appearance and the planning of correction of mandibular prognathism and FEM numerical analysis process components designed to perform anastomoses condylar fracture.
W artykule przedstawiono zastosowanie technik inżynierii odwrotnej dla modelowania wyglądu i planowania zabiegu korekcji progenii. Przeprowadzono proces analizy numerycznej MES elementów przeznaczonych do wykonania zespoleń wyrostka kłykciowego.
Źródło:
Advances in Manufacturing Science and Technology; 2013, 37, 3; 57-72
0137-4478
Pojawia się w:
Advances in Manufacturing Science and Technology
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-13 z 13

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies