Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "alloy" wg kryterium: Temat


Wyświetlanie 1-5 z 5
Tytuł:
The influence of casting defects on fatigue resistance of elektron 21 magnesium alloy
Autorzy:
Pikos, I.
Kiełbus, A.
Adamiec, J.
Powiązania:
https://bibliotekanauki.pl/articles/383305.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
casting defect
mechanical properties
microstructure
magnesium alloy
Elektron 21 alloy
wada odlewu
właściwości mechaniczne
mikrostruktura
stop magnezu
stop Elektron 21
Opis:
The Mg-RE alloys are attractive, constructional materials, especially for aircraft and automotive industry, thanks to combination of low density, good mechanical properties, also at elevated temperature, and good castability and machinability. Present paper contains results of fatigue resistance test carried out on Elektron 21 magnesium alloy, followed by microstructural and fractographical investigation of material after test. The as-cast material has been heat treated according to two different procedures. The fatigue resistance test has been conducted with 106 cycles of uniaxial, sine wave form stress between 9 MPa and 90 MPa. Fractures of specimens, which ruptured during the test, have been investigated with scanning electron microscope. The microstructure of specimens has been investigated with light microscopy. Detrimental effect of casting defects, as inclusions and porosity, on fatigue resistance has been proved. Also the influence of heat treatment's parameters has been described.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 103-106
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure, castability, microstructural stability and mechanical properties of ZRE1 magnesium alloy
Mikrostruktura, lejność, stabilność mikrostruktury i właściwości mechaniczne stopu magnezu ZRE1
Autorzy:
Rzychoń, T.
Szala, J.
Kiełbus, A.
Powiązania:
https://bibliotekanauki.pl/articles/354630.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stopy magnezu
ZRE1
płynność
mikrostruktura
magnesium alloys
ZRE1 alloy
fluidity
microstructure
Opis:
The influence of pouring temperature on the microstructure, fluidity and mechanical properties of ZRE1 magnesium alloy was investigated in this paper. The pouring temperature influences on the fluidity, mean area of grain plane section and mechanical properties. The dependence between pouring temperature and volume fraction of the (Mg, Zn)12RE intermetallic phase was not observed. The investigations enabled to determine the optimal pouring temperature of ZRE1 alloy. Moreover, the microstructural stability of ZRE1 alloy during long-term annealing at 150°C, 200°C and 400°C was investigated. ZRE1 magnesium alloy possesses a high microstructural stability up to 200°C, whereas at 400°C magnesium oxides and rare earth metals oxides are observed in the microstructure.
W pracy przedstawiono wyniki badań wpływu temperatury odlewania na mikrostrukturę, lejność i właściwości mechaniczne stopu magnezu ZRE1. Stwierdzono, że temperatura odlewania wpływa na lejność, średnie pole powierzchni płaskiego przekroju ziarna i właściwości mechaniczne stopu ZRE1. Nie zaobserwowano zależności pomiędzy temperaturą odlewania a udziałem objętościowym wydzieleń fazy miedzymetalicznej (Mg, Zn)12RE. Przeprowadzone badania umożliwiły określenie najkorzystniejszej temperatury odlewania do form piaskowych dla stopu ZRE1. Przeprowadzono także badania stabilności strukturalnej podczas długotrwałego wygrzewania w temperaturze 150°C, 200°C i 400°C. Stwierdzono, że do temperatury 200°C mikrostruktura jest stabilna, natomiast w temperaturze 400°C stop ZRE1 charakteryzuje się niską stabilnością i skłonnością do tworzenia tlenków magnezu i metali ziem rzadkich.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 1; 245-252
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Microstructure of AlSi9Cu3 Alloy after Different Stages of Liquid Metal Preparation
Autorzy:
Poloczek, Ł.
Dybowski, B.
Łuszczak, M.
Kiełbus, A.
Powiązania:
https://bibliotekanauki.pl/articles/380869.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metallography
alloy Al-Si-Cu
microstructure
scrap
liquid metal treatment
metalografia
stop Al-Si-Cu
złom
obróbka metalu ciekłego
Opis:
Aluminium alloys are one of the most important casting alloys. Among them, the Al-Si alloys comprise perhaps the most important group – about 80% of the aluminium casts are made of them. These materials are characterized by a very good technological properties, good corrosion resistance and tribological properties. Their main disadvantage is, however, presence of the massive, brittle silicon crystals. They significantly affect alloys mechanical properties. Liquid metal treatment is essential for modification of Al-Si eutectic structure. The following work presents results of the research on the microstructure of the AlSi9Cu3 alloy after different stages of liquid metal preparation. Three casting processes have been conducted, chemical composition of the material in each case was in agreement with EN 1706 specification. During each casting process, three specimens were gravity cast: first, made from pure ingots; second, after the scrap addition and third one after the liquid metal treatment. Qualitative and quantitative evaluation of the microstructure was done on each specimen. Specimens cast from pure ingots are characterized by a refined Al-Si eutectic microstructure. After scrap addition, the silicon crystals became morphology of the massive platelets. What is more, intermetallic phases observed within the structure posses different morphologies after different stages of liquid metal preparation. After scrap addition, increased gas porosity was observed. Liquid metal treatment reduced slightly the formation of gas pores.
Źródło:
Archives of Foundry Engineering; 2015, 15, 1 spec.; 89-92
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Age Hardening Parameters on the Microstructure and Properties of the AlSi7Mg Sand Cast Alloy
Wpływ parametrów utwardzania wydzieleniowego na strukturę i właściwości stopu AlSi7Mg
Autorzy:
Poloczek, Ł.
Dybowski, B.
Rodak, K.
Jarosz, R.
Kiełbus, A.
Powiązania:
https://bibliotekanauki.pl/articles/352479.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
AlSi7Mg alloy
sand casting
microstructure
electrical conductivity
hardness
heat treatment
AlSi7Mg
mikrostruktura
przewodność elektryczna
twardość
obróbka cieplna
Opis:
Aluminium alloys are characterized by a low density, acceptable mechanical properties and good technological properties. This unique connection of features made aluminium alloys perfect structural material for the transportation industry. Also, due to their good electrical conductivity they also found application in energy production industry. High mechanical properties and electrical conductivity of the Al-Si alloys with Mg addition may be achieved by heat treatment. However, the highest mechanical properties are achieved in the early stages of age hardening - due to precipitation of coherent phases, while high electrical conductivity may be achieved only by prolonged aging, during precipitation of semi-coherent or fully noncoherent, coarse phases. Carefully heat treated AlSi7Mg alloy may exhibit both fairly high electrical conductivity and slightly increased mechanical properties. The following article present results of the research of influence of heat treatment on the properties and microstructure of sand cast AlSi7Mg alloy. Microstructure observations were performed using light microscopy, scanning electron and scanning-transmission electron microscopy. Hardness and electrical conductivity of the AlSi7Mg alloy were investigated both in as-cast condition and after heat treatment. Maximum hardness of the alloy is achieved after solutioning at 540°C for 8h, followed by 72h of aging at 150°C, while maximal electrical conductivity after solutioning at 540°C for 48h, followed by 96h of aging at 180°C. Increase of the electrical conductivity is attributed to increasing distance between Si crystals and precipitation of semi coherent phases.
Stopy aluminium charakteryzują się małą gęstością, dobrymi właściwościami mechanicznymi, a przy tym bardzo dobrymi właściwościami odlewniczymi. Połączenie tych cech powoduje że stopy te znajdują szerokie zastosowanie w przemyśle motoryzacyjnym. Ich dużą zaletą jest również wysoka przewodność elektryczna oraz cieplna, dzięki której znajdują również zastosowanie w przemyśle energetycznym. Uzyskanie tak wysokich właściwości mechanicznych i przewodności elektrycznej w przypadku stopów Al-Si z dodatkiem Mg może być osiągnięte tylko poprzez przeprowadzenie obróbki cieplenj. Najwyższe właściwości mechaniczne są osiągane w początkowej fazie utwardzania wydzieleniowego (wydzielanie się koherentnych faz), podczas gdy uzyskanie wysokich wartości przewodności może być osiągnięte tylko przez długotrwałe starzenie, podczas wydzielania się pół koherentnych lub niekoherentnych, dużych faz. W przypadku stopu AlSi7Mg, starannie dobrana obróbka cieplna może powodować znaczne podwyższenie przewodności oraz polepszenie właściwości mechanicznych. Ninjiejszy artykuł przedstawia wyniki badań wpływu parametrów obróbki cieplnej na strukturę i właściwości stopu AlSi7Mg, odlanego grawitacyjnie do form piaskowych. Obserwacje mikrostruktury prowadzone były prz użyciu metod mikroskopii świetlnej, elektronowej mikroskopii skaningowej oraz elektronowej mikroskopii transmisyjnej. Twardość i przewodności stopu AlSi7Mg badano zarówno w stanie lanym, jak i po obróbce cieplnej. Maksymalną twardość stopu uzyskano po przesycaniu w 540°C przez 8h oraz starzeniu w temperaturze 150°C przez 72h. Maksymalną przewodność elektryczną uzyskano po przesycaniu w 540° C przez 48h, oraz starzeniem w temperaturze 180°C przez 96h. Wzrost przewodności elektrycznej spowodowany jest zwiększeniem się odległości pomiędzy kryształami Si oraz wydzielaniem się półkoherentnych faz.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 4; 3035-3042
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Mould Components on the Cooling Rate, Microstructure, and Quality of WE43 Magnesium Casting Alloy
Wpływ zastosowanych elementów formy na szybkość chłodzenia, mikrostrukturę i jakość stopu magnezu WE43
Autorzy:
Dybowski, B.
Kiełbus, A.
Jarosz, R.
Powiązania:
https://bibliotekanauki.pl/articles/354835.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
WE43 magnesium alloy
sand casting
microstructure
quantitative evaluation
feeding and cooling method
stop magnezu WE43
odlewy piaskowe
mikrostruktura
ocena ilościowa
metoda chłodzenia i zasilania
Opis:
We investigated the impact of the applied cooling and feeding method on the microstructure and metallurgical quality of castings made from WE43 magnesium alloy. Six identical plates with dimensions of 100x50x20 mm were sand cast for use as samples. Each casting was fed and cooled in a different way. The solid solution grain size was evaluated quantitatively using the Met-Ilo software program, and casting defects were observed using a scanning electron microscope Hitachi S3400N. The finest solid solution grain was observed in the castings with only the coolers applied. Non-metallic inclusions were observed in each plate. The smallest shrinkage porosity was observed in the castings with feeders applied.
Celem badań było zbadanie wpływu zastosowanej metody chłodzenia i zasilana na mikrostrukturę i jakość metalurgiczną odlewów wykonanych ze stopu magnezu WE43. Sześć identycznych płyt o wymiarach 100x50x20 mm, chłodzonych i zasilanych na różne sposoby, odlano do formy piaskowej. Wielkość ziarna roztworu stałego zostały wyznaczone ilościowo w programie Met-Ilo. Obserwacje wad odlewniczych prowadzono na skaningowym mikroskopie elektronowym Hitachi S3400N. Najmniejszym ziarnem roztworu stałego charakteryzowały się odlewy z zastosowanymi tylko ochładzalnikami. W strukturze każdego z odlewów stwierdzono wtrącenia niemetaliczne. Najmniejszą porowatością skurczową charakteryzowały się odlewy z zastosowanymi nadlewami.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1527-1532
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-5 z 5

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies