Microstructure and Mechanical Properties of AA5483 after Combination of ECAP and Hydrostatic Extrusion SPD Processes
Mikrostruktura i właściwości mechaniczne stopu AA5483 po kombinacji procesów ECAP oraz wyciskania hydrostatycznego
Autorzy:
Kulczyk, M.
Skiba, J
Pachla, W.
Powiązania:
https://bibliotekanauki.pl/articles/352170.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
severe plastic deformation
hydrostatic extrusion
nanocrystalline structure
grain refinement
aluminum alloy
duże odkształcenie plastyczne
wyciskanie hydrostatyczne
struktura nanokrystaliczna
rozdrobnienie ziarna
stop aluminium
Opis:
Al-Mg alloys of the 5xxx series are strain hardenable and have moderately high strength, excellent corrosion resistance even in salt water, and very high toughness even at cryogenic temperatures to near absolute zero, which makes them attractive for a variety of applications, e.g. in systems exploited at temperatures as low as -270°C, and marine applications. The present study is concerned with the effect of a combination of 2 processes, which generate serve plastic deformation (SPD), equal channel angular pressing (ECAP) and hydrostatic extrusion (HE), on the microstructure and mechanical properties of an alloy that contain Al and Mg. The alloy was subjected to multi-pass ECAP followed by cumulative HE with a total true strain of 5.9. The microstructure of SPD samples was evaluated by transmission and scanning electron microscopy. The mechanical properties were determined by tensile tests and microhardness measurements. The combination of the two processes gave a uniform nanostructure with an average grain size of 70nm. The grain refinement taking place during the SPD processing resulted in the increase of the mechanical strength by 165% (YS) with respect to that of the material in the as- received state. The experiments have shown that the combination of HE and ECAP permits producing homogeneous nanocrystalline materials of large volumes.
Stopy aluminium serii 5XXX (Al-Mg) umacniane odkształceńiowo charakteryzują się relatywnie wysoką wytrzymałością, bardzo dobrą odpornością korozyjną szczególnie w wodzie morskiej i bardzo wysoką odpornością udarnościową nawet w temperaturach kriogenicznych. Własności te sprawiają, że te stopy są atrakcyjne dla wielu zastosowań gdzie wymagana jest praca w niskich temperaturach, nawet do -270°C oraz praca w środowisku morskim. W przeprowadzonych badaniach określono wpływ kombinacji dwóch procesów generujących duże odkształcenia plastyczne, przeciskania przez kanał kątowy (ECAP) oraz wyciskania hydrostatycznego (HE), na mikrostrukturę i własności mechaniczne stopu 5483. Zastosowano kombinację procesu kumulacyjnego wyciskania hydrostatycznego poprzedzonego procesem ECAP z łącznym odkształceniem rzeczywistym 5.9. Badania mikrostrukturalne zostały przeprowadzone z wykorzystaniem transmisyjnej mikroskopii elektronowej. Własności mechaniczne określono w statycznej próbie rozciągania oraz pomiarach mikrotwardości. Kombinacja obu procesów pozwoliła uzyskać materiał o jednorodnej nanostrukturze o średniej wielkości ziarna 70nm. Rozdrobnienie struktury spowodowało wzrost własności mechanicznych (granicy plastyczności) o około 165% w porównaniu do materiału przed odkształceniem plastycznym. Przeprowadzone eksperymenty wykazały że kombinacja procesów HE oraz ECAP pozwala na wytwarzanie jednorodnych nanomateriałów w dużych objętościach.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 1; 163-166
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Severe Plastic Deformation Induced in Al, Al-Si, Ag and Cu by Hydrostatic Extrusion
Zastosowanie metody wyciskania hydrostatycznego do generowania dużych odkształceń plastycznych w Al, Al-Si, Ag oraz Cu
Autorzy:
Kulczyk, M.
Przybysz, S.
Skiba, J
Pachla, W.
Powiązania:
https://bibliotekanauki.pl/articles/351039.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
hydrostatic extrusion
grain refinement
severe plastic deformation
fine wires
wyciskanie hydrostatyczne
rozdrobnienie ziarna
duże odkształcenia plastyczne
cienkie druty
Opis:
The study was concerned with the effect of severe deformation induced in one pass, by hydrostatic extrusion on the properties of fine aluminum, aluminum-silicon alloy, copper and silver wires. The influence of adiabatic heating which takes place during deformation on the mechanical properties and microstructure of the wires was examined. The quality of the surface of the wires was estimated. It has been demonstrated that fine aluminum and silver wires processed by hydrostatic extrusion have very good mechanical properties and a high-quality surface.
W pracy zbadano wpływ dużych odkształceń, uzyskanych w jednym procesie wyciskania hydrostatycznego na właściwości wytworzonych produktów w postaci cienkich drutów z aluminium, stopu aluminium-krzem, miedzi oraz srebra. Uwzględniono efekty grzania adiabatycznego w trakcie procesu odkształcenia i jego wpływ na własności mechaniczne oraz mikrostrukturę produktów. Ocenie została poddana także jakość powierzchni wytwarzanych drutów. Dla aluminium oraz srebra wykazano, że za pomocą procesu wyciskania hydrostatycznego można wytwarzać druty o wysokich własnościach mechanicznych oraz dobrej jakości powierzchni.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 1; 59-64
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of hydrostatic extrusion with back pressure on mechanical properties of grey and nodular cast irons
Wpływ wyciskania hydrostatycznego z przeciwciśnieniem na własności mechaniczne żeliwa szarego i sferoidalnego
Autorzy:
Pachla, W.
Mazur, A.
Skiba, J.
Kulczyk, M.
Przybysz, S.
Powiązania:
https://bibliotekanauki.pl/articles/352637.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
wyciskanie hydrostatyczne
przeciwciśnienie
odkształcenia plastyczne
grafit
żeliwo
własności mechaniczne
hydrostatic extrusion
back pressure
severe plastic deformation
graphite
cast iron
mechanical properties
Opis:
Cold hydrostatic extrusion with and without back pressure of ferritic-pearlitic grey cast iron EN-GJL 250 and ferritic-pearlitic nodular cast iron EN-GJS 500-7 has been performed. The experiments were performed on a originally designed hydrostatic extrusion press operating up to 2000 MPa with back pressure up to 700 MPa. Cast irons were cold hydrostatically extruded with back pressure in one pass with extrusion ratios up to 1.77 and 2.12 for grey and nodular one, respectively. Nodular cast iron was also successfully extruded without back pressure with extrusion ratio 1.35. Severe plastic deformation has led to axial alignment and elongation of graphite inclusions in extrusion direction together with sound flow of the surrounding metal matrix accommodating the strain without cracking. External high pressure has restrained of cracks generation and propagation during the material flow and healed of already existing defects by internal friction caused by plastic flow. It was visualized by aligned and elongated graphite flakes and nodules and no cracks and porosity observed in surrounded metal matrix. Very high compressive strength of both materials has been measured, above 1000 MPa and ~2400 MPa for grey and nodular cast iron, respectively. These values were accompanied by above 3000 MPa and above 3400 MPa microhardnes HV0.2 and by over 15% and over 50% elongation at maximum strength for those materials, respectively. Cast irons with such properties can be classified as a new iron-base structural materials.
Procesowi wyciskania hydrostatycznego na zimno poddano ferrytyczno-perlityczne zeliwa szare EN-GJL 250 i sferoidalne EN-GJS 500-7. Eksperymenty prowadzono na oryginalnej, własnej konstrukcji prasie do wyciskania hydrostatycznego pracujacej do 2000 MPa z przeciwcisnieniem do 700 MPa. Zeliwa były wyciskane z sukcesem z przeciwcisnieniem w jednej operacji ze stopniem redukcji 1.77 i 2.12 odpowiednio, dla zeliwa szarego i sferoidalnego. Zeliwo sferoidalne było równiez wyciskane bez przeciwcisnienia ze stopniem redukcji 1.35. Duze odkształcenie plastyczne prowadziło do osiowego ułozenia i wydłuzenia wtracen grafitu w kierunku wyciskania przy jednoczesnym płynieciu metalowej osnowy zapewniajacej odkształcenie bez pekniec. Wysokie cisnienie przyłozone na zewnatrz odkształcanego produktu powtrzymywało generowanie i propagacje pekniec podczas płyniecia materiału oraz ‘leczyło’ istniejace juz defekty wewnetrzne poprzez zgrzewanie tarciowe podczas odkształcenia plastycznego. Uwidaczniały to ułozone i wydłuzone w kierunku wyciskania płatki i kulki grafitu oraz brak pekniec i porowatosci obserwowany w otaczajacej je osnowie. Zmierzono bardzo wysoka wytrzymałosc na sciskanie obu materiałów, ponad 1000 MPa i ok. 2400 MPa, odpowiednio dla zeliwa szarego i sferoidalnego. Wartosciom tym towarzyszyła mikrotwardosc HV0.2 powyzej 3000 MPa i powyzej 3400 MPa oraz ponad 15% i ponad 50% wydłuzenie przy maksymalnej wytrzymałosci, odpowiednio dla obu tych materiałów. Zeliwa o takich własnosciach mozna kwalifikowac jako nowe materiały konstrukcyjne na bazie zelaza.
Źródło:
Archives of Metallurgy and Materials; 2011, 56, 4; 945-953
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
High strength silicon bronze (C65500) obtained by hydrostatic extrusion
Wysoko wytrzymały brąz krzemowy (C65500) uzyskany metoda wyciskania hydrostatycznego
Autorzy:
Kulczyk, M.
Skiba, J.
Przybysz, S.
Pachla, W.
Bazarnik, P.
Lewandowska, M.
Powiązania:
https://bibliotekanauki.pl/articles/356421.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop C65500
odporność korozyjna
stopy miedzi
severe plastic deformation
hydrostatic extrusion
grain refinement
copper alloys
Opis:
C65500 is a high strength engineering alloy that has excellent resistance to a wide range of corrosive environments. Combination of corrosion resistance, strength, and formability place it among the most widely used copper alloys. In the present study, a C65500 alloy was subjected to severe plastic deformation by hydrostatic extrusion at room temperature with goal to increase its strength by grain refinement without modification of the chemical composition. Cumulative hydrostatic extrusion was applied with a total true strain of 4.1. The microstructure of SPD samples was evaluated by transmission electron microscopy. The size of grains was quantitatively described. The resulting mechanical properties were determined in tensile tests and via microhardness measurements. The results show that the applied cumulative HE route, leads to a substantial grain size refinement accompanied by high increase in strength. In comparison to commercial alloy after conventional plastic treatment, ultimate tensile strength and yield strength were higher by 45% and 130% respectively.
Stop C65500 jest wysoko wytrzymałym stopem inżynierskim charakteryzującym sie bardzo dobrą odpornością korozyjną w wielu agresywnych środowiskach. Połączenie odporności korozyjnej, wysokiej wytrzymałości i podatności do przeróbki plastycznej sprawia że jest powszechnie stosowanym stopem miedzi. W pracy stop C65500 został poddany dużym odkształceniom plastycznym metodą wyciskania hydrostatycznego na zimno. Celem przeprowadzonej obróbki było podniesienie wytrzymałości na drodze rozdrobnienia mikrostruktury, bez modyfikacji składu chemicznego stopu. Zastosowano kumulacyjny proces wyciskania hydrostatycznego z łącznym odkształceniem rzeczywistym 4.1. Mikrostrukturę odkształconych próbek obserwowano technika transmisyjnej mikroskopii elektronowej (TEM). Określono ilościowo średnie wielkości ziaren. Własności mechaniczne były zmierzone w testach rozciągania oraz za pomocą pomiarów mikrotwardości. Uzyskane wyniki wskazują, że zastosowanie kumulacyjnego wyciskania hydrostatycznego prowadzi do wyraźnego rozdrobnienia wielkości ziarna czemu towarzyszy znaczny wzrost wytrzymałości. W porównaniu ze stopem komercyjnym przerabianym na zimno metodami konwencjonalnymi uzyskano wzrost wytrzymałości na zrywanie oraz granicy plastyczności odpowiednio 45% i 130%.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 3; 859-861
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies