Tytuł:
The Defects of Oxide Layers Formed on 10CrMo9-10 Steel Operated for 200,000 Hours at an Elevated Temperature
Autorzy:
Gwoździk, M.
Powiązania:
https://bibliotekanauki.pl/articles/353504.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
oxide layer
10CrMo9-10 steel
LM
SEM
AFM
XRD
Opis:
The paper contains results of studies into the formation of oxide layers on 10CrMo9-10 (10H2M) steel long-term operated at an elevated temperature (T = 545°C, t = 200,000h). The oxide layer was studied on a surface and a cross-section at the inner and outer surface of the tube wall on the outlet both on the fire and counter-fire side of the tube wall surface. The obtained results of research have shown a higher degree of degradation, both of the steel itself and oxide layers, on the fire side. In addition, it has been shown that on the outside tube wall, apart from iron oxides, there are also deposits composed mainly of Al2SiO5.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 2B; 987-992
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Changes of crystallite sizes in the oxide layer forming during long-term operation of 10CrMo9-10 steel
Autorzy:
Gwoździk, M.
Powiązania:
https://bibliotekanauki.pl/articles/298126.pdf
Data publikacji:
2017
Wydawca:
Uniwersytet Warmińsko-Mazurski w Olsztynie
Tematy:
10CrMo9-10 steel
oxide layer
X-ray diffraction
crystallite sizes
Opis:
The paper contains results of the studies on X-ray diffraction analysis XRD (studying the phase composition, crystallite sizes) of oxide layers on 10CrMo9-10 steel, operated for a long time at an elevated temperature (T = 525°C, t = 200,000 h). The oxide layer was studied on a surface and a cross-section at the outer on the inlet both on the fire and counter-fire side of the tube wall surface. X-ray studies were carried out on the outer surface of a tube, and then the layer surface was polished down and the diffraction measurements were performed again to determine crystallite size in oxide layers. Based on the width and the position of the main coat and substrate reflections, the size of the crystallites was determined using the Scherrer formula.
Źródło:
Technical Sciences / University of Warmia and Mazury in Olsztyn; 2017, 20(3); 289-296
1505-4675
2083-4527
Pojawia się w:
Technical Sciences / University of Warmia and Mazury in Olsztyn
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies