Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "heat-treatment" wg kryterium: Temat


Tytuł:
Empirical formulas for the calculations of the hardness of steels cooled from the austenitizing temperature
Autorzy:
Trzaska, J.
Powiązania:
https://bibliotekanauki.pl/articles/356569.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
CCT diagram
modeling
heat treatment
steel
hardness
Opis:
In this paper, the equations applied for the purpose of the calculations of the hardness of continuously cooled structural steels upon the basis of the temperature of austenitizing. The independent variables of the hardness model were: the mass concentrations of elements, the austenitizing temperature and the cooling rate. The equations were developed with the application of the following methods: multiple regression and logistic regression. In this paper, attention was paid to preparing data for the purpose of calculations, to the methodology of the calculations, and also to the assessment of the quality of developed formulas. The collection of empirical data was prepared upon the basis of more than 500 CCT diagrams.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 3; 1297-1302
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
An Influence of Ageing on the Structure, Corrosion Resistance and Hardness of High Aluminum ZnAl40Cu3 Alloy
Autorzy:
Michalik, R.
Tomaszewska, A.
Powiązania:
https://bibliotekanauki.pl/articles/353675.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Zn-Al-Cu alloys
heat treatment
corrosion resistance
hardness
Opis:
Zn-Al-Cu alloys are used primarily because of their tribological properties as an alternative material for bronze, cast iron and aluminum alloy bearings and as a construction material. Particularly interesting are high aluminum zinc alloys. Monoeutectic zinc and aluminum alloys are characterized by the highest hardness, tensile strength and wear resistance of all of the zinc alloys. A significant problem with the use of the Zn-Al-Cu alloys is their insufficient resistance to electrochemical corrosion. Properties of Zn-Al-Cu alloys can be improved by heat treatment. The purpose of examination was to determine the effect of heat treatment (aging at various temperatures) on the microstructure and corrosion resistance of the ZnAl40Cu3 alloy. The scope of the examination included: structural examinations, determination of hardness using Brinell’s method and corrosion resistance examinations. Ageing at higher temperatures causes a creation of areas where is an eutectoid mixture. The study showed that ageing causes a decrease in hardness of ZnAl40Cu3 alloy. This decrease is even greater, when the temperature of ageing is lower. The studies have shown a significant influence of ageing on the corrosion resistance of the alloy ZnAl40Cu3. Maximum corrosion resistance were characterized by the sample after ageing at higher temperatures.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 1; 289-294
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and service properties of copper alloys
Autorzy:
Polok-Rubiniec, M.
Konieczny, J.
Labisz, A.
Włodarczyk-Fligier, A.
Powiązania:
https://bibliotekanauki.pl/articles/354788.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloyed copper
heat treatment
cold rolling
wear resistance
hardness
Opis:
This elaboration shows the effect of combined heat treatment and cold working on the structure and utility properties of alloyed copper. As the test material, alloyed copper CuTi4 was employed. The samples were subjected to treatment according to the following schema: 1st variant - supersaturation and ageing, 2nd variant - supersaturation, cold rolling and ageing. The paper presents the results of inicrostructure, hardness, and abrasion resistance. The analysis of the wipe profile geometry was realized using a Zeiss LSM 5 Exciter confocal microscope. Cold working of the supersaturated solid solution affects significantly its hardness but the cold plastic deformation causes deterioration of the wear resistance of the finally aged CuTi4 alloy.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 3; 1277-1282
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Annealing Treatment on (Mg17Al12) Phase Characterization and Corrosion Behavior in Different Solutions for AZ91 Alloy
Autorzy:
Abass, Marwa H.
Abdulkareem, Makarim H.
Hussein, Hussien A.
Powiązania:
https://bibliotekanauki.pl/articles/2201907.pdf
Data publikacji:
2023
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
AZ91
alloy
heat treatment
corrosion
microstructure
antibacterial
hardness
Opis:
Heat treatment is the most suitable technique for altering the microstructure and, consequently, it is possible to create the optimal balance of corrosion resistance and mechanical strength in a material by carefully regulating the conditions during the heating process. The present work aims to investigate the effect of heat treatments (annealing) at (300°C) at different times (10, 20, and 30 hr) on the magnesium alloy. How the Mg17Al12 phase influences the corrosion behavior of AZ91D magnesium alloy was quantified in different solution (SBF, Lactic and Ringer). It was able to construct an extensive range of Mg17Al12 phase volume fractions by varying the annealing period. The corrosion potential of many specimens with varied proportions of the Mg17Al12 phase was evaluated. The results of the conducted tests manifested that the material's resistance to corrosion greatly improved with an increase in the volume fraction of Mg17Al12 phase. The effect of heat treatment on the microstructure was analyzed using transmission electron microscopy and X-ray diffraction. The SEM photographs evinced that the amount of β-Mg17Al12 phase decreased significantly, with the distribution occurring at the grain boundaries and with increasing the time of annealing, resulting in a highly saturated α-grain. The XRD validated the all material peaks of phases that are present. The corrosion test behavior of AZ91 alloy in the simulated body fluid (SBF), lactic, and Ringer solutions was investigated through electrochemical measurements, the result was elucidated as measured along the Tafel slope, and the corrosion current density of all heat treated samples was lower than that of the as-cast sample. The measurement of hardness (HV) demonstrated that the hardness decreased to (64.5 HV0.5) during the heat treatment. The result antibacterial efficiency was revealed that AZ91 at 30 hr was best then as cast against the bacteria E.coli.
Źródło:
Advances in Science and Technology. Research Journal; 2023, 17, 2; 330--341
2299-8624
Pojawia się w:
Advances in Science and Technology. Research Journal
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Próba ilościowego opisu wpływu parametrów obróbki cieplnej na twardość stali narzędziowej 102Cr6
Attempt at quantitative description of the influence heat treatment parameters have on hardness of 102Cr6 tool steel
Autorzy:
Poprzeczka, A.
Lisica, A.
Powiązania:
https://bibliotekanauki.pl/articles/252306.pdf
Data publikacji:
2012
Wydawca:
Instytut Naukowo-Wydawniczy TTS
Tematy:
obróbka cieplna
stal
102Cr6
twardość
heat treatment
steel
hardness
Opis:
Parametry obróbki cieplnej stali narzędziowej w istotny sposób wpływają na jej strukturę, która z kolei kształtuje właściwości mechaniczne i eksploatacyjne, takie jak np.: twardość, udarność i odporność na zużycie ścierne. Pomimo licznych opracowań na ten temat brak jest w literaturze fachowej ścisłych zależności pomiędzy parametrami obróbki cieplnej stali narzędziowej a jej odpowiednimi właściwościami. W niniejszej pracy przedstawiono próbę zbadania ilościowego wpływu parametrów obróbki cieplnej na twardość stali 102Cr6 stosowanej na narzędzia do pracy na zimno. Do badań i opracowania wyników zastosowano pełnoczynnikową macierz planowania doświadczeń 23 i program komputerowy Statistica.
Heat treatment parameters of the tool steel significantly affect its structure which in turn shapes such mechanical and operating properties as: hardness, impact strength and wear resistance. In spite of numerous studies in this subject, specialist literature does refer to close dependencies between heat treatment parameters of tool steel and its adequate properties. This paper presents an attempt at quantitative analysis of the influence heat treatment parameters have on the hardness of 102Cr6 steel used on cold work tools. The analysis and result handling were performed with the use of the 23 full-factor experiment design matrix and Statistica software.
Źródło:
TTS Technika Transportu Szynowego; 2012, 9; 437-443, CD
1232-3829
2543-5728
Pojawia się w:
TTS Technika Transportu Szynowego
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Use of the Precipitation Hardening to Improve the Properties of Combustion Engine Pistons Made of Eutectic Silumins
Autorzy:
Trepczyńska-Łent, Małgorzata
Műller, K.
Powiązania:
https://bibliotekanauki.pl/articles/2079815.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
silumins
precipitation hardening
heat treatment
hardness
siluminy
utwardzanie
obróbka cieplna
twardość
Opis:
The study presents methods to be used for improving the performance parameters of car engine pistons made of EN AC-AlSi12CuNiMg alloy according to the PN-EN 1706: 2011. Pistons of slow sucking and turbocharged engines were researched. A solution heat and ageing treatments were applied according to four variants. Temperatures of the solution heat treatment were: 550 ±5°C; 510°C ±5°C; and alternate: 276 ±5°C/510 ±5°C. The solution time ranged from 6 min to 4 h. Temperatures of the ageing heat treatment were 20°C and 250°C, while the ageing time ranged from 1,5 to 3h. Natural ageing was performed in 5 days. Measurements of hardness HRB and the piston diameters were performed. An improvement in the performance parameters of combustion engines was observed. Three solution heat treatment and ageing variants, allowed to obtain the pistons with hardness equal/higher than pistons of the turbocharged engines. The test results confirmed the possibility of providing a piston with properties exceeding the high load parameters specified by the manufacturer. Further studies will make it possible to improve the effects of the proposed solutions.
Źródło:
Archives of Foundry Engineering; 2021, 21, 4; 77-81
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The influence of laser re-melting on micro-structure and hardness of gas-nitrided steel
Wpływ parametrów laserowej obróbki cieplnej na mikrostrukturę i mikrotwardość azotowanej gazowo stali
Autorzy:
Panfil, D.
Wach, P.
Kulka, M.
Michalski, J.
Powiązania:
https://bibliotekanauki.pl/articles/94166.pdf
Data publikacji:
2016
Wydawca:
Politechnika Poznańska. Wydawnictwo Politechniki Poznańskiej
Tematy:
gas nitriding
laser heat treatment
microstructure
hardness
azotowanie gazowe
laserowa obróbka cieplna
mikrostruktura
twardość
Opis:
In this paper, modification of nitrided layer by laser re-melting was presented. The nitriding process has many advantageous properties. Controlled gas nitriding was carried out on 42CrMo4 steel. As a consequence of this process, ɛ+ɣ’ compound zone and diffusion zone were produced at the surface. Next, the nitrided layer was laser re-melted using TRUMPF TLF 2600 Turbo CO2 laser. Laser tracks were arranged as single tracks with the use of various laser beam powers (P), ranging from 0.39 to 1.04 kW. The effects of laser beam power on the microstructure, dimensions of laser tracks and hardness profiles were analyzed. Laser treatment caused the decomposition of continuous compound zone at the surface and an increase in hardness of previously nitrided layer because of the appearance of martensite in re-melted and heat-affected zones.
Źródło:
Archives of Mechanical Technology and Materials; 2016, 36; 18-22
2450-9469
Pojawia się w:
Archives of Mechanical Technology and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Experimental investigations of surface wear by dry sliding and induced damage of medium carbon steel
Autorzy:
Elhadi, Abdelmalek
Amroune, Salah
Zaoui, Moussa
Mohamad, Barhm
Bouchoucha, Ali
Powiązania:
https://bibliotekanauki.pl/articles/1840896.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Polskie Towarzystwo Diagnostyki Technicznej PAN
Tematy:
hardness
friction
microstructure of steel
heat treatment
wear
twardość
tarcie
mikrostruktura stali
obróbka cieplna
zużycie
Opis:
This study concerns the wear behaviour of metal couples used in industry, particularly in mechanical sliding systems (numerically controlled machine tools). In general, the nature of the materials of the parts of these systems which are in contact and move relatively, are medium carbon steels, thanks to their good mechanical and tribological properties. The present work aims to study, the dry sliding wear of the contact surface of the pin (machine slide) against the contact surface of a disc (machine groove) and the damage induced on the worn track. The pin is AISI 1038 and AISI 1045 steel, the disc is AISI 1055 steel. The tribological tests were carried out on a pin-disc tribometer, in an atmospheric environment. The wear of the pins being evaluated by weighing and studied according to the hardness of the pin with the variation of the normal load applied. The discussion of the results is based on SEM observations and EDS analyzes of worn surfaces and interfacial phenomena produced by dynamic contact. The results obtained indicated the influence of the applied load and the hardness on the wear of the pin and therefore on the tribological behaviour of the worn surfaces.
Źródło:
Diagnostyka; 2021, 22, 2; 3-10
1641-6414
2449-5220
Pojawia się w:
Diagnostyka
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wpływ obróbki cieplnej i odkształcenia plastycznego, powierzchniowego stali 18HGT i 33H3MF na właściwości warstwy wierzchniej azotowanej
The influence of heat treatment and surface plastic s tra in of 18HGT and 33H3MF steelon the properties ofthe nitrided top layer
Autorzy:
Berkowski, L.
Powiązania:
https://bibliotekanauki.pl/articles/212000.pdf
Data publikacji:
2015
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Obróbki Plastycznej
Tematy:
obróbka cieplna stali
nagniatanie
azotowanie jonowe
twardość
struktura
heat treatment of steel
burnishing
ion nitriding
hardness
structure
Opis:
W artykule przedstawiono wyniki badań dwóch stali konstrukcyjnych (18HGT i 33H3MF) o różnej strukturze; pierwsza to stal tradycyjna stosowana do nawęglania, druga – do azotowania. Próbki nagniatano w przyrządzie do statycznego nagniatania powierzchni walcowej, zamontowanym na tokarce. Elementami nagniatającymi były krążki o średnicy 17,5 mm i długości 150 mm, z nacięciami. Badano wpływ powierzchniowego odkształcenia plastycznego na skutki azotowania jonowego w temperaturze 400oC na strukturę i właściwości warstwy wierzchniej wyżej wymienionej stali. Zmiany strukturalne warstw analizowano pod mikroskopem świetlnym oraz metodą pomiaru twardości z pomocą twardościomierza firmy ZWICK 3212, stosując penetrator Knoopa i obciążenie 0,981 N. Zmiany powierzchniowe oceniano z pomocą profilometru firmy Telysufr-Hobson, porównując (przed i po nagniataniu) parametr chropowatości Ra. Badania wykazały, że oprócz zmian strukturalnych stali obróbka cieplna i nagniatanie powodują istotne zmiany chropowatości powierzchni (parametru Ra). Stale 18HGT i 33H3MF po zabiegach obróbki cieplnej, nagniatania i azotowania jonowego wykazują różne struktury i właściwości. Jedynie w próbce ze stali 18HGT, wyżarzonej, stwierdzono wpływ odkształcenia plastycznego warstwy wierzchniej; wzrost twardości po azotowaniu jonowym. Badane stale 18HGT (tradycyjna do nawęglania) i stal 33H3MF (do azotowania) wykazują wyraźnie różniące się struktury i reagują inaczej na zabiegi obróbki cieplnej, nagniatania i azotowania jonowego. W przypadku stali 18HGT, o pasmowej strukturze, wyżarzonej, nagniatanie spowodowało rozdrobnienie ziaren przy powierzchni i wspomniany już wzrost twardości, a próbki hartowane i ulepszane cieplnie – brak wpływu umocnienia. Stal 33H3MF – po nagniataniu – nie wykazywała zmian strukturalnych i zmian rozkładów twardości po różnych obróbkach.
The paper presents the results of examination of two constructional steels (18HGT and 33H3MF) with different structures; the former is a constructional steel used for carburizing, the latter is used for nitriding. The samples have been burnished in a device for static burnishing of a cylindrical surface, fixed on a lathe. The burnishing elements were disks of 17.5 mm diameter and 150 mm length, with incisions. The investigation concerned the influence of surface plastic strain on the effects of ion nitriding at the temperature of 400oC on the structure and properties of the top layer of the above mentioned steels. The structural changes of the layers have been analysed by means of and optical microscope and by the method of hardness measurement with the application of a ZWICK 3212 hardness tester, using a Knoop penetrator and a load of 0.981 N. Sur-faced changes have been assessed by means of a Telysufr-Hobson profile measurement gauge comparing the parameter of roughness, Ra, before and after burnishing. The investigation has shown that, in addition to structural changes, heat treatment and burnishing result in significant changes of roughness (Ra parameter). The 18HGT and 33H3MF steels show different structures and properties after the operations of heat treatment, burnishing and ion nitriding. Only in an annealed sample of the 18HGT steel, the influence of the top layer plastic strain has been found: increase of hardness after ion nitriding. The examined steels (18HGT, traditional carburizing steel and 33H3MF, for nitriding) show clearly different structures and different responses to the operations of heat treatment, burnishing and ion nitriding. In the case of the 18HGT steel with band structure, annealed, burnishing has resulted in break-up of grains near the surface and the already mentioned increase of hardness; in the case of hardened and toughened samples – no influence of consolidation. The 33H3MF steel has not shown structural changes after burnishing or hardness distribution changes after various treatments.
Źródło:
Obróbka Plastyczna Metali; 2015, 26, 2; 105-114
0867-2628
Pojawia się w:
Obróbka Plastyczna Metali
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Kształtowanie mikrostruktury i odporności na pękanie stopu Ti-6Al-7Nb do zastosowań biomedycznych
The formation of microstructure of and fracture toughness of Ti-6Al-7Nb alloy for biomedical applications
Autorzy:
Dąbrowski, R.
Pacyna, J.
Kochańczyk, J.
Powiązania:
https://bibliotekanauki.pl/articles/261593.pdf
Data publikacji:
2016
Wydawca:
Politechnika Wrocławska. Wydział Podstawowych Problemów Techniki. Katedra Inżynierii Biomedycznej
Tematy:
mikrostruktura
obróbka cieplna
twardość
odporność na pękanie
stopy tytanu
microstructure
heat treatment
hardness
fracture toughness
titanium alloy
Opis:
W artykule dokonano oceny odporności na pękanie dwufazowego stopu tytanu w gatunku Ti-6Al-7Nb w warunkach statycznych i dynamicznych. Własność tę oceniono w próbie statycznego trójpunktowego zginania oraz w dynamicznej próbie udarności sposobem Charpy’ego. Odporność na pękanie stopu kształtowano poprzez zmianę mikrostruktury uzyskanej wskutek zastosowania różnych zabiegów obróbki cieplnej. Jako miary odporności na pękanie wyznaczono tzw. współczynnik intensywności naprężeń (KIc) oraz pracę złamania (KV) stopu w stanie przesyconym, tj. po oziębianiu w wodzie z zakresu dwufazowego oraz po starzeniu w wybranym zakresie temperatur. Badania odporności na pękanie w warunkach statycznych stopu (KIc) uzupełniono dokumentacją fraktograficzną przełomów próbek. Przełomy analizowano przy użyciu skaningowego mikroskopu elektronowego NovaNanoSEM 450. Badania mikrostruktury stopu po obróbce cieplnej wykonano przy użyciu mikroskopu świetlnego Axiovert 200 MAT firmy Zeiss.
Assessment of the fracture toughness of the Ti-6Al-7Nb grade two-phase titanium alloy, under static and dynamic conditions, is performed in the hereby paper. This property was estimated in the static three-point bend test and in the dynamic Charpy impact test. The alloy fracture toughness was shaped by the microstructure changes obtained due to the application of various operations of the heat treatment. As the measures of the fracture toughness the so-called stress intensity factor (KIc) and impact energy (KV) of the alloy in the supersaturating state, i.e. after water-cooling from two-phase range and after ageing at the selected temperature range, were determined. Fracture toughness tests of alloys, under static conditions (KIc), were supplemented by the fractographic documentation of sample fractures. These fractures were analysed by means of the scanning electron microscopy: NovaNanoSEM 450. Investigations of the alloy microstructure, after the heat treatment, were performed by using the light microscope, Axiovert 200 MAT of the Zeiss Company.
Źródło:
Acta Bio-Optica et Informatica Medica. Inżynieria Biomedyczna; 2016, 22, 3; 130-137
1234-5563
Pojawia się w:
Acta Bio-Optica et Informatica Medica. Inżynieria Biomedyczna
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication and microstructure of layers containing intermetallic phases on magnesium
Autorzy:
Mola, R.
Powiązania:
https://bibliotekanauki.pl/articles/381749.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
heat treatment
magnesium
Al-enriched surface layer
intermetallic phases
hardness
obróbka cieplna
warstwa wierzchnia
faza międzymetaliczna
twardość
magnez
Opis:
Al- and Al/Zn-enriched layers containing intermetallic phases were deposited on the Mg substrate by heating the Mg specimens in contact with the powdered materials in a vacuum furnace. The Al-enriched surface layers were produced using Al powder, whereas the Al/Zn-enriched layers were obtained from an 80 wt.% Al + 20 wt.% Zn powder mixture. The microstructure and composition of the layers were analyzed by optical microscopy, scanning electron microscopy and X-ray diffraction. The results showed that the Al-enriched layer comprised an Mg17Al12 intermetallic phase and a solid solution of Al in Mg. The layer obtained from the Al+Zn powder mixture was composed of Mg-Al-Zn intermetalic phases and a solid solution of Al and Zn in Mg. Adding 20% of Zn into the Al powder resulted in the formation of a considerably thicker layer. Moreover, the hardness of the surface layers was much higher than that of the Mg substrate.
Źródło:
Archives of Foundry Engineering; 2013, 13, 1; 99-102
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Properties of 17Cr-0.8C Cast Steel
Autorzy:
Kalandyk, B.
Zapała, R.
Pałka, P.
Wróbel, M.
Powiązania:
https://bibliotekanauki.pl/articles/353847.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
martensitic cast steel
M23C6
Fe7C3
Fe3C carbides
heat treatment
microstructure
hardness
Opis:
The results of studies of the microstructure and properties of cast high alloy steels containing 17% Cr and 0.8% C subjected to different variants of heat treatment are presented. For phase identification, the light microscopy and scanning electron microscopy as well as the X-ray diffraction analysis were used. The conducted studies revealed the presence of carbides in the microstructure, mainly of the M23C6 carbide, detected after both quenching and tempering at 200 and 600°C. The use of low and high tempering significantly reduced the test alloy hardness from 657.3 HV30 to 403.7 HV30. At the same time, hardness was observed to have an impact on the values of abrasion in the conducted Miller slurry test. Higher material hardness leads to lower wear expressed by mass loss.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 1; 113-117
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Tempering temperature effects on hardness and impact toughness of 56NiCrMo7 steel
Wpływ temperatury odpuszczania na twardość i udarność stali 56NiCrMo7
Autorzy:
Dąbrowski, R.
Dziurka, R.
Powiązania:
https://bibliotekanauki.pl/articles/354136.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stal narzędziowa
obróbka cieplna
mikrostruktura
twardość
udarność
heat treatment
hot work tool steel
microstructure
hardness
impact toughness
fractographic examination
Opis:
The assessment of the effect of tempering temperature on hardness and impact toughness of a 56NiCrMo7 grade hot work tool steel was presented in the paper. It has been found that the investigated steel, after quenching in oil from 800°C, softens quite slowly upon tempering within the range between 100 and 675°C, which was confirmed not only by hardness measurements but also by observed changes occurring in its microstructure, whereas the impact energy (KV) absorbed by the test specimen increases with temperature, achieving >66J after tempering at 675°C. The changes observed in the character of the fracture surfaces allows of interpretation of the impact test results for the whole range of tempering temperatures.
W artykule przedstawiono wyniki badań na temat wpływu temperatury odpuszczania na twardość i udarność stali narzędziowej do pracy na gorąco w gatunku 56NiCrMo7. Badania wykonano dla wybranej temperatury austenityzowania równej 800°C. Wykazano, że badana stal zahartowana w oleju od tej temperatury a następnie odpuszczona w zakresie 100-675°C mięknie dość wolno, co potwierdziły nie tylko wyniki pomiarów twardości ale również obserwacje zmian zachodzących w jej mikrostrukturze. Praca złamania (KV) próbki udarnościowej rośnie ze wzrostem temperatury odpuszczania, przekraczając 66 J po odpuszczaniu w 675°C. Potwierdzeniem uzyskanych wyników badan udarności są zmiany zaobserwowane w charakterze przełomów próbek w całym zakresie temperatur odpuszczania.
Źródło:
Archives of Metallurgy and Materials; 2011, 56, 1; 5-11
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Age Hardening Parameters on the Microstructure and Properties of the AlSi7Mg Sand Cast Alloy
Wpływ parametrów utwardzania wydzieleniowego na strukturę i właściwości stopu AlSi7Mg
Autorzy:
Poloczek, Ł.
Dybowski, B.
Rodak, K.
Jarosz, R.
Kiełbus, A.
Powiązania:
https://bibliotekanauki.pl/articles/352479.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
AlSi7Mg alloy
sand casting
microstructure
electrical conductivity
hardness
heat treatment
AlSi7Mg
mikrostruktura
przewodność elektryczna
twardość
obróbka cieplna
Opis:
Aluminium alloys are characterized by a low density, acceptable mechanical properties and good technological properties. This unique connection of features made aluminium alloys perfect structural material for the transportation industry. Also, due to their good electrical conductivity they also found application in energy production industry. High mechanical properties and electrical conductivity of the Al-Si alloys with Mg addition may be achieved by heat treatment. However, the highest mechanical properties are achieved in the early stages of age hardening - due to precipitation of coherent phases, while high electrical conductivity may be achieved only by prolonged aging, during precipitation of semi-coherent or fully noncoherent, coarse phases. Carefully heat treated AlSi7Mg alloy may exhibit both fairly high electrical conductivity and slightly increased mechanical properties. The following article present results of the research of influence of heat treatment on the properties and microstructure of sand cast AlSi7Mg alloy. Microstructure observations were performed using light microscopy, scanning electron and scanning-transmission electron microscopy. Hardness and electrical conductivity of the AlSi7Mg alloy were investigated both in as-cast condition and after heat treatment. Maximum hardness of the alloy is achieved after solutioning at 540°C for 8h, followed by 72h of aging at 150°C, while maximal electrical conductivity after solutioning at 540°C for 48h, followed by 96h of aging at 180°C. Increase of the electrical conductivity is attributed to increasing distance between Si crystals and precipitation of semi coherent phases.
Stopy aluminium charakteryzują się małą gęstością, dobrymi właściwościami mechanicznymi, a przy tym bardzo dobrymi właściwościami odlewniczymi. Połączenie tych cech powoduje że stopy te znajdują szerokie zastosowanie w przemyśle motoryzacyjnym. Ich dużą zaletą jest również wysoka przewodność elektryczna oraz cieplna, dzięki której znajdują również zastosowanie w przemyśle energetycznym. Uzyskanie tak wysokich właściwości mechanicznych i przewodności elektrycznej w przypadku stopów Al-Si z dodatkiem Mg może być osiągnięte tylko poprzez przeprowadzenie obróbki cieplenj. Najwyższe właściwości mechaniczne są osiągane w początkowej fazie utwardzania wydzieleniowego (wydzielanie się koherentnych faz), podczas gdy uzyskanie wysokich wartości przewodności może być osiągnięte tylko przez długotrwałe starzenie, podczas wydzielania się pół koherentnych lub niekoherentnych, dużych faz. W przypadku stopu AlSi7Mg, starannie dobrana obróbka cieplna może powodować znaczne podwyższenie przewodności oraz polepszenie właściwości mechanicznych. Ninjiejszy artykuł przedstawia wyniki badań wpływu parametrów obróbki cieplnej na strukturę i właściwości stopu AlSi7Mg, odlanego grawitacyjnie do form piaskowych. Obserwacje mikrostruktury prowadzone były prz użyciu metod mikroskopii świetlnej, elektronowej mikroskopii skaningowej oraz elektronowej mikroskopii transmisyjnej. Twardość i przewodności stopu AlSi7Mg badano zarówno w stanie lanym, jak i po obróbce cieplnej. Maksymalną twardość stopu uzyskano po przesycaniu w 540°C przez 8h oraz starzeniu w temperaturze 150°C przez 72h. Maksymalną przewodność elektryczną uzyskano po przesycaniu w 540° C przez 48h, oraz starzeniem w temperaturze 180°C przez 96h. Wzrost przewodności elektrycznej spowodowany jest zwiększeniem się odległości pomiędzy kryształami Si oraz wydzielaniem się półkoherentnych faz.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 4; 3035-3042
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Phase Analysis of Explosive Welded Ti-Cr/Ni Steel in As-Received State and after Heat Treatment Using Synchrotron
Analiza fazowa połączenia Ti-Cr/Stali Ni wytworzonego metodą zgrzewania wybuchowego w stanie wyjściowym oraz po obróbce termicznej z wykorzystaniem promieniowania synchrotonowego
Autorzy:
Ostroushko, D.
Mazancová, E.
Saksl, K.
Milković, O.
Powiązania:
https://bibliotekanauki.pl/articles/351787.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Ti-Cr/Ni
explosive bonding
interface area
heat treatment
hardness
phase analysis
łączenie wybuchowe
strefa połączenia
obróbka cieplna
twardość
analiza fazowa
Opis:
Surface coatings protection is one of the most important processes ensuring efficient and economic use of basic materials, mostly of lower-quality. At interface of clad and basic material intermetallic phases are formed, representing quite different matrix with dissimilar properties unlike the welded materials. One type of surface coating is explosive bonding which belongs to group of pressure welding. The work is focused on interface shape line, inhomogeneities in vicinity of the wave joint both in basic material and in vicinity of weld line of the Ti and Cr/Ni stainless steel (SS) matrix. Investigated weld was both in as-received state and after heat treatment carried out at 600°C/90 minutes/air. Presented phases have been identified using X-ray diffraction performed by synchrotron. The Tiα, Fe-fcc, Fe-bcc and intermetallic phases Fe2Ti were detected at interface area.
Jednym z najważniejszych procesów zapewniających skuteczne i ekonomiczne uwarunkowane stosowanie materiałów konstrukcyjnych jest pokrywanie powierzchni warstwą ochronną. W strefie połączenia następuje formowanie się faz międzymetalicznych charakteryzujących się całkowicie odmiennymi od materiałów łączonych własnościami. Jednym ze sposobów pokrycia powierzchni materiałów jest zgrzewanie wybuchowe, które należy do metod ciśnieniowych. Praca została zogniskowana na charakterystyce kształtu linii połaczenia, niejednorodnościach w okolicy rozchodzenia się fali wybuchu obydwu materiałów, jak i w okolicach linii samego połączenia Ti oraz Cr/Ni stali niskowęglowej (SS). Badania fazy przetopionej w obydwu materiałach prowadzono po przeprowadzeniu obróbki termicznej, która przeprowadzono w temperaturze 600°C przez 90 minut, bez atmosfery ochronnej. Pojawiające się fazy zostały przebadane z wykorzystaniem dyfrakcji promieni rentgenowskich w synchrotronie. Ujawniono fazy Tiα, Fe-fcc, Fe-bcc oraz fazę międzymetaliczną Fe2Ti w obszarze połączenia.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1611-1614
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies