Tytuł:
Extraction and separation of zinc, lead, silver, and bismuth from bismuth slag
Autorzy:
Xing, Peng
Ma, Baozhong
Wang, Chengyan
Chen, Yongqiang
Powiązania:
https://bibliotekanauki.pl/articles/109744.pdf
Data publikacji:
2019
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
bismuth
zinc
lead
silver
extraction
separation
Opis:
The present paper deals with the extraction and separation of zinc, lead, silver, and bismuth from a refractory bismuth refining slag via a hydrometallurgical route. The process consists of a preliminary leaching of zinc with water, followed by the selective leaching of lead and silver with a calcium chloride solution, leading to the crystallization of lead chloride and the cementation of silver. The diagrams of the total concentrations of [Pb]/[Ag] versus [Cl-] and temperature in the Pb/Ag-Cl-H2O system were drawn, respectively, to determine the optimum concentration of leaching agent and leaching temperature. The potential-pH diagram of the Pb/Ag/Bi-H2O system indicates that the preferential leaching of lead and silver could be achieved. Finally, 98.8% of lead and 90.4% of silver were selectively removed by further leaching the water leaching residue with 400 g/dm3 of CaCl2 solution at pH 4.5 and 80 °C, while only 3.7% of bismuth was leached in this stage. Fifty-nine percent of lead in the leach liquor was separated out as PbCl2 by natural cooling. Ninety-five percent of silver in mother liquor was recovered by cementation with a lead sheet. The depleted CaCl2 solution can be sent to the leaching step again to close the loop.
Źródło:
Physicochemical Problems of Mineral Processing; 2019, 55, 1; 173-183
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Recovery of nickel and iron from low–grade laterite ore and red mud using co–reduction roasting: Industrial-scale test
Autorzy:
Guo, Xiaoshuang
Xu, Chengyan
Wang, Yingshuo
Li, Xiaohui
Sun, Tichang
Powiązania:
https://bibliotekanauki.pl/articles/1447175.pdf
Data publikacji:
2021
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
co-reduction
low-grade laterite ore
red mud
rotary kiln
powdered ferronicke
Opis:
In this study, the effects of red mud (RM) dosage during the co-reduction roasting of lowgrade laterite ore and RM were investigated. The expanded test was conducted under the following optimized conditions: RM-1 dosage of 15 wt%, anthracite dosage of 13 wt%, a roasting temperature of 1300oC, and roasting time of 3 h. Ferronickel powder was obtained with a nickel grade of 1.95 wt%, iron grade of 83.25 wt%, and nickel and total iron recoveries of 94.71 wt% and 95.98 wt%, respectively. The addition of RM improved the recovery of nickel and total iron in ferronickel powder. The reason was because of the increased intensity of the diffraction peaks of kamacite and iron, and the ferronickel particles grown due to the liquid phase were easier to achieve at a lower melting point. The industrialscale test results showed that ferronickel powder was obtained with average nickel and total iron grades of 1.76 wt% and 86.46 wt%, respectively, which indicated the successful industrial-scale test of co–reduction roasting. Thermodynamic analysis theoretically illustrated the feasibility of the co–reduction of low-grade laterite ore and RM. Increased roasting temperature promoted the reduction of iron oxide and nickel oxide.
Źródło:
Physicochemical Problems of Mineral Processing; 2021, 57, 3; 61-72
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect and mechanism of depressant CK102 on flotation separation of fluorite and dolomite
Autorzy:
Li, Zhengyao
Wang, Xuewen
Xu, Chengyan
Sun, Tichang
Liu, Weiran
Wei, Jinzhi
Powiązania:
https://bibliotekanauki.pl/articles/2146904.pdf
Data publikacji:
2022
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
fluorite
dolomite
flotation
depressant CK102
adsorption
Opis:
For a low grade dolomite type fluorite ore in the Hebei province, it was observed that the depressant CK102, a mixture of sulfuric acid, sodium silicate and aluminum sulfate, can effectively inhibit the gangue mineral dolomite in the flotation of fluorite. However, the inhibition mechanism of the depressant is still unclear. In this paper, the flotation separation performance and underlying mechanism of CK102 inhibiting dolomite were investigated through mineral flotation tests, adsorption measurements, infrared spectroscopy, and X-ray photoelectron spectroscopy (XPS). The flotation results showed that the inhibition effect of CK102 on dolomite flotation was much more remarkable than that of fluorite flotation under optimum conditions. Adsorption measurements revealed that there was competitive adsorption between the depressant and collector and that the adsorption of the depressant CK102 prevented the collector modified sodium oleate from adsorbing onto the surface of minerals. The FT-IR and XPS results showed that the co-oxygen cross-linked component of the depressant CK102 chemisorbed on the surface of dolomite; the CaSiO3 precipitation was generated from the reaction of CK102 with Ca2+ groups on the surface of the dolomite; Al2MgO8Si2 precipitation was also generated from Mg2+ reacting with the sodium silicate and aluminum sulfate of CK102. The above adsorptions and reactions enhanced the hydrophilicity of the dolomite surface and the dolomite was effectively depressed.
Źródło:
Physicochemical Problems of Mineral Processing; 2022, 58, 3; art. no. 145796
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies