Wyszukujesz frazę "Gorka, J." wg kryterium: Wszystkie pola


Tytuł:
Assessment of the Corrosion Resistance, Properties and the Structure of TIG Braze Welded Galvanised Steel Sheets
Autorzy:
Górka, J.
Powiązania:
https://bibliotekanauki.pl/articles/351057.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
braze welding
TIG
galvanised steel
corrosion resistance
galvanostatic tests
Opis:
The article discusses tests concerning the assessment of the corrosion resistance, properties and the structure of TIG braze welded galvanised steel sheets. Test butt joints were made of 0.9 mm thick galvanised car body steel sheets DC04 (in accordancewith EN 10130), using a robotic welding station and a CuSi3Mn1 braze (in accordance with PN-EN 13347:2003) wire having a diameter of 1.0 mm. The research-related tests aimed to optimise braze welding parameters and the width of the brazing gap. The test joints were subjected to visual tests, macro and microscopic metallographic tests, hardness measurements as well as tensile and bend tests. The corrosion resistance of the joints was identified using the galvanostatic method. The tests revealed that it is possible to obtain high quality joints made of galvanised car body steel sheets using the TIG braze welding process, the CuSi3Mn1 braze and a brazing gap, the width of which should be restricted within the range of 0.4 mm to 0.7 mm. In addition, the joints made using the aforesaid parameters are characterised by high mechanical properties. The minimum recommended heat input during process, indispensable for the obtainment of the appropriate spreadability of the weld deposit should be restricted within the range of 50 kJ/mm to 70 kJ/mm. At the same time, the aforesaid heat input ensures the minimum evaporation of zinc. Joints made using the TIG braze welding method are characterised by high resistance to electrochemical corrosion. The galvanostatic tests did not reveal any traces of corrosion in the joint area.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 1; 47-54
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Weldability of Thermomechanically Treated Steels Having a High Yield Point
Spawalność stali obrabianej termomechanicznie o wysokiej granicy plastyczności
Autorzy:
Górka, J.
Powiązania:
https://bibliotekanauki.pl/articles/353588.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
weldability
TMCP steel
HAZ
spawalność
stal TMCP
Opis:
The article concerns the issue of weldability of S700MC steel, treated thermo-mechanically, with high yield point. The weakest area of welded joints of this steel is a high - temperature coarse heat affected zone (HAZ) in which due to the nucleation effect of the dissolved phases, strengthening the matrix and their subsequent uncontrolled separation precipitation in the form of finely disperse and rapid decrease impact strength is observed. Performed arc welding tests here have shown that in order to ensure high quality of welded joints, it is necessary to limit the welding linear heat input. During the welding process of S700MC steel, it is not recommended to use pre heating before the welding process and heat treatment after welding, and the number of repairs should be kept to a minimum, because it leads to a reduction of strength and plastic properties in the HAZ area, as a result of aging processes, dissolution of strengthening phases in the matrix and their subsequent uncontrolled precipitation during cooling.
W pracy przedstawiono problematykę spawalności stali obrabianej termomechanicznie S700MC o wysokiej granicy plastyczności. Najsłabsze miejsce złącza spawanego tej stali stanowi wysokotemperaturowy, gruboziarnisty obszar strefy wpływu ciepła (SWC), w którym na skutek zarodkowania rozpuszczonych faz umacniających w osnowie i ich ponownego, niekontrolowanego wydzielenia w postaci drobnodyspersyjnej, następuje gwałtowny spadek udarności. Przeprowadzone próby spawania łukowego wykazały, że w celu zapewnienia wysokiej jakości złączy spawanych należy ograniczyć energię liniową spawania. Podczas spawania stali S700MC nie zaleca się stosowania podgrzewania wstępnego przed spawaniem oraz obróbki cieplnej po spawaniu, a liczbę napraw należy ograniczyć do minimum, gdyż prowadzi to do obniżenia własności wytrzymałościowych i plastycznych w obszarze SWC, na skutek procesów o charakterze starzeniowym, rozpuszczania faz umacniających w osnowie i ich ponownego, niekontrolowanego wydzielania w czasie chłodzenia.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 1; 469-475
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ocena stabilności procesu oczyszczania ścieków za pomocą kart kontrolnych
Rating of stability of wastewater treatment process by using control cards
Autorzy:
Gorka, J.
Powiązania:
https://bibliotekanauki.pl/articles/5391.pdf
Data publikacji:
2015
Wydawca:
Wydawnictwo Uniwersytetu Ekonomicznego we Wrocławiu
Tematy:
oczyszczanie sciekow
oczyszczalnie sciekow
stabilnosc
karty kontrolne
osady czynne
karty kontrolne CUSUM
wskazniki zanieczyszczen
procesy technologiczne
Opis:
Celem pracy jest ocena stabilności procesu oczyszczania ścieków na przykładzie miejscowości Przeginia Duchowna z województwa małopolskiego. Oczyszczalnia ścieków w tej miejscowości bazuje na biologicznej technologii oczyszczania metodą osadu czynnego. Wyniki do analizy uzyskano z laboratorium Societe Generale de Surveillance (SGS) EKO-PROJEKT w Pszczynie. Badano następujące wskaźniki zanieczyszczeń: BZT5, ChZT i zawiesinę ogólną. Ocenę stabilności procesu dokonano na podstawie kart kontrolnych położenia (x-średnich) i kart kontrolnych sum skumulowanych (CUSUM). Analiza wykazała niestabilne funkcjonowanie oczyszczalni w redukcji danych wskaźników zanieczyszczeń. Ocena efektywności pracy oczyszczalni ścieków metodami statystycznymi z wykorzystaniem kart kontrolnych pozwala na dokładniejsze zbadanie procesów technologicznych oczyszczalni. Dzięki kartom kontrolnym można w łatwy sposób wykryć wszelkiego rodzaju nieprawidłowości oraz szybko je usunąć.
The aim of the study is to assess the stability of the wastewater treatment process on the example of the Przeginia Duchowna village. A sewage treatment plant in this locality is based on biological treatment technology using activated sludge. The results of the analysis were obtained from SGS ECO-DESIGN laboratory in Pszczyna. The following pollutant indicators were studied: BOD5, COD and suspended solids. The evaluation process stability was based on control cards x and control cards CUSUM. The analysis showed an unstable operation of treatment in reducing data indicators of pollution. The assessment of the efficiency of wastewater treatment plants by statistical methods using control cards allows for a closer examination of wastewater treatment processes. Owing to using control cards it is easy to detect all kinds of irregularities and quickly remove them.
Źródło:
Nauki Inżynierskie i Technologie; 2015, 3(18)
2449-9773
2080-5985
Pojawia się w:
Nauki Inżynierskie i Technologie
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structure and Properties of Hybrid Laser Arc Welded T-Joints (Laser Beam - MAG) in Thermo-Mechanical Control Processed Steel S700MC of 10 mm thickness
Autorzy:
Górka, J.
Powiązania:
https://bibliotekanauki.pl/articles/352132.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
HLAW hybrid welding
T-joints
S700MC steel
quality of welded joints
Opis:
In this article examinations of hybrid welding technology (laser beam + MAG) of T-joints from thermomechanically worked high strength steel S700MC 10 mm thick were presented. Joints welded from one side and both sides were made. Carried examinations enabled to classify joints in quality level B according to ISO 12932 (Welding. Laser-arc hybrid welding of steels, nickel and n ickel alloys. Quality levels for imperfections). In case of one sided welding with partial penetration with beam power of 8.5 kW 8 mm of penetration was achieved without noticeable distortion of web. Double sided joints were characterized with correct geometry. Joint metal is bainitic-ferritic in structure and its hardness rises about 40 HV1 in comparison to base metal hardness (280 HV1). In HAZ a slight softening of material in comparison to base metal is present.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1125-1131
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Welding thermal cycle-triggered precipitation processes in steel S700MC subjected to the thermo-mechanical control processing
Autorzy:
Górka, J.
Powiązania:
https://bibliotekanauki.pl/articles/355934.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
hardening phases
precipitation processes
TMCP steel
weld
HAZ
Opis:
This study presents tests concerned with welding thermal process-induced precipitation processes taking place in 10 mm thick steel S700MC subjected to the Thermo-Mechanical Control Process (TMCP) with accelerated cooling. The thermomechanical processing of steel S700MC leads to its refinement, structural defects and solutioning with hardening constituents. Tests of thin foils performed using a transmission electron microscope revealed that the hardening of steel S700MC was primarily caused by dispersive (Ti,Nb)(C,N) precipitates (being between several and less than twenty nanometers in size). In arc welding, depending on a welding method and linear energy, an increase in the base material in the weld is accompanied by the increased concentration of hardening microagents in the weld. The longer the time when the base material remains in the liquid state, the greater the amount of microagents dissolved in the matrix. During cooling, such microagents can precipitate again or remain in the solution. An increase in welding linear energy is accompanied by an increase in the content of hardening phases dissolved in the matrix and, during cooling, by their another uncontrolled precipitation in the form of numerous fine-dispersive (Ti,Nb)(C,N) precipitates of several nm in size, leading to a dislocation density increase triggered by type 2 internal stresses.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 321-326
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Współczesne zagospodarowywanie ogrodów wiejskich w Naprawie koło Jordanowa
Contemporary arrangement of rural gardens in Naprawa village near Jordanów
Autorzy:
Kapczyńska, A.
Malinowska, Z.
Górka, J.
Powiązania:
https://bibliotekanauki.pl/articles/1186469.pdf
Data publikacji:
2005
Wydawca:
Uniwersytet Przyrodniczy we Wrocławiu
Tematy:
ogród wiejski
zagospodarowywanie
rural garden
arrangement
Opis:
Investigations on an arrangement of ten rural gardens in Naprawa village near Jordanów were based on inquiry method and local inspection of the gardens with an inventory of ornamental plants used for the arrangement. All gardens were established after construction of new houses. All, with the exception of one, were managed by women of 20 to 55 years old. Half of the garden owners work in different professions, the rest work at their home farms. The owners pay particular particular attention to the esthetical appearance of their gardens. Only two of the gardens were unattractive. Expansion and arrangement of new borders were observed in ten gardens. However in one garden, the expansion of lawn was at the cost of ornamental plants. Non of the gardens visited were arranged in the rural gardening tradition, except in two cases which were partially traditional. Analysis of the plants used for planting in the gardens indicate low use of annual plants in spite of biennials and no hardy perennials. Borders were planted most often with perennials using mainly native species which flower in spring time. Apart from typical, traditionally recommended species for planting in rural gardens, several new ones were introduced, which are not often used in these kinds of arrangements, with disregard for many traditional, very valuable ornamental plants.
Źródło:
Architektura Krajobrazu; 2005, 3-4; 91-95
1641-5159
Pojawia się w:
Architektura Krajobrazu
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Properties and Structure of Nanocrystalline Layers Obtained by Manual Metal Arc Welding (MMA)
Autorzy:
Górka, J.
Czupryński, A.
Adamiak, M.
Powiązania:
https://bibliotekanauki.pl/articles/351150.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
nanocrystalline layer
crystallite size
manual metal arc welding
deposit weld
Opis:
The present paper is the result of the investigations of the properties and structure of nanocrystalline layers deposited from iron-based nanoalloy on steel S355N substrate by manual metal arc welding method (MMA). In the process of welding a 100 A current intensity was used with desiccation preheating at 80°C while maintaining the interpass temperature at range of 200°C. The resultant deposit welds were subjected to macro and microscopic metallographic examination, X-ray phase analyses and crystallite size was analyzed by X-ray diffractometry (XRD), additionally EDX chemical composition analysis of precipitates during scanning electron microscopy was performed. Working properties of the obtained nanocrystalline deposit welds were evaluated based on hardness and metal-to-mineral abrasive wear. The results of the deposit welds working properties measurements were compared with the properties of wear resistant steel HARDOX 400 type used as the reference material.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 3; 1479-1484
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Napawanie laserowe warstw kompozytowych na osnowie stopu Inconel 625
Laser cladding of Inconel 625-based composite coatings
Autorzy:
Janicki, D.
Górka, J.
Kotarska, A.
Powiązania:
https://bibliotekanauki.pl/articles/115093.pdf
Data publikacji:
2018
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
napawanie laserowe
powłoka kompozytowa
Inconel 625
laser cladding
composite coating
Opis:
Artykuł prezentuje wyniki badań procesu napawania laserem diodowym warstw wierzchnich kompozytowych na osnowie stopu niklu Inconel 625 wzmacnianych cząstkami WC oraz Cr3C2. Określono wpływ energii linowej napawania oraz morfologii cząstek fazy umacniającej (FU) na stopień jej rozpuszczenia w osnowie warstwy. Ponadto, określono wpływ morfologii cząstek FU na odporność erozyjną warstw.
Inconel 625-based composite coatings reinforced by WC and Cr3C2 particles have been produced via a diode laser cladding process. The effect of heat input level and morphology of the reinforcing particles on the degree of their dissolution has been established. Additionally, the influence of the morphology of the reinforcing particles on the erosive wear behaviour of the coatings was studied.
Źródło:
Welding Technology Review; 2018, 90, 9; 6-12
0033-2364
2449-7959
Pojawia się w:
Welding Technology Review
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fizykochemiczne właściwości mezoporowatych węgli z nanocząstkami zawierającymi żelazo i nikiel otrzymanych metodą miękkiego odwzorowania
Physicochemical properties of soft-templated mesoporous carbons with iron- and nickel-containing nanoparticles
Autorzy:
Górka, J.
Jaroniec, M.
Choma, J.
Powiązania:
https://bibliotekanauki.pl/articles/237768.pdf
Data publikacji:
2011
Wydawca:
Polskie Zrzeszenie Inżynierów i Techników Sanitarnych
Tematy:
mezoporowate węgle
synteza metodą miękkiego odwzorowania
kopolimer trójblokowy
nanocząstki węgliku żelaza
nanocząstki niklu
adsorpcja
mesoporous carbons
soft-templating synthesis
block copolymer
iron carbide nanoparticles
adsorption
Opis:
Z powodzeniem zsyntezowano mezoporowate kompozyty węglowe zawierające żelazo i nikiel metodą miękkiego odwzorowania w środowisku kwasowym, wykorzystując floroglucynę i formaldehyd jako prekursory węglowe, trójblokowy kopolimer politlenek etylenu-politlenek propylenu-politlenek etylenu jako miękką matrycę oraz chlorek żelaza(III) i sześciowodny azotan(V) niklu(II) jako prekursory nanocząstek. Zsyntezowane kompozyty karbonizowano w trzech temperaturach: 700 oC, 850 oC i 1000 C. Analizy XRD i TGA wykazały obecność nanocząstek zawierających żelazo i nikiel (poniżej 2% wag.) w postaci Fe3C, Ni i NiH w matrycy węglowej. Adsorpcja azotu, dyfrakcja promieniowania rentgenowskiego (XRD) i spektroskopia Ramana wykazały dobre adsorpcyjne i strukturalne właściwości badanych kompozytów, obejmujące dużą powierzchnię właściwą i dużą całko-witą objętość porów z przeważającym udziałem mezoporów o wymiarach ok. 10 nm. Takie właściwości strukturalne oraz fakt, że otrzymane kompozyty są trwałe termicznie do temperatury 460÷480 C powodują, że materiały te są bardzo atrakcyjne do zastosowań w procesach adsorpcji i katalizy w inżynierii środowiska.
Mesoporous carbon composites containing iron or nickel were successfully synthesized by the soft-templating method under acidic conditions using phloroglucinol and formaldehyde as carbon precursors, the poly(ethylene oxide)-poly(propylene oxide)-poly(ethylene oxide) triblock copolymer as a soft template, and iron(III) chloride or nickel(II) nitrate hexahydrate as nanoparticles precursors. The as-synthesized composites were carbonized at three different temperatures: 700 oC, 850 oC and 1000 oC. XRD and thermogravimetric analysis revealed the presence of Fe- and Ni-containing nanoparticles (below 2 wt.%) in the form of Fe3C, Ni and NiH in the resulting mesoporous carbons. Nitrogen adsorption, X-ray diffraction and Raman spectroscopy proved good adsorption and structural properties of the composites studied, which include high surface area and large total pore volume, with main contribution arising from mesopores with diameters of about 10 nm. The latter and the fact that the resulting composites are stable up to 460-480 oC make them attractive materials for adsorption, catalysis, environmental and energy-related applications.
Źródło:
Ochrona Środowiska; 2011, 33, 2; 3-9
1230-6169
Pojawia się w:
Ochrona Środowiska
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Testing of flame sprayed Al2O3 matrix coatings containing TiO2
Autorzy:
Czupryński, A.
Górka, J.
Adamiak, M.
Tomiczek, B.
Powiązania:
https://bibliotekanauki.pl/articles/356108.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
flame spray process
coating
ceramic powder
abrasive wear resistance
erosion wear resistance
adhesion strength
Opis:
The paper presents the results of the properties of flame sprayed ceramic coatings using oxide ceramic materials coating of a powdered aluininiuni oxide (Al2O3) matrix with 3% titanium oxide (TiO2) applied to unalloyed S235JR grade structural steel. A primer consisting of a metallic Ni-Al-Mo based powder has been applied to plates with dimensions of 5X200X300 mm and front surfaces of ø40x50 mm cylinders. Flame spraying of primer coating was made using a RotoTec 80 torch, and an external coating was made with a CastoDyn DS 8000 torch. Evaluation of the coating properties was conducted using metallographic testing, phase composition research, measurement of microhardness, substrate coating adhesion (acc. to EN 582:1996 standard), erosion wear resistance (acc. to ASTM G76-95 standard), and abrasive wear resistance (acc. to ASTM G65 standard) and thermal impact. The testing performed has demonstrated that flame spraying with 97% Al2O3 powder containing 3% TiO2 performed in a range of parameters allows for obtaining high-quality ceramic coatings with thickness up to ca. 500 μni on a steel base. Spray coating possesses a structure consisting mainly of aluminium oxide and a small amount of NiAl10O16 and NiAl32O49 phases. The bonding primer coat sprayed with the Ni-Al-Mo powder to the steel substrate and external coating sprayed with the 97%Al2O3 powder with 3% TiO2 addition demonstrates mechanical bonding characteristics. The coating is characterized by a high adhesion to the base amounting to 6.5 MPa. Average hardness of the external coating is ca. 780 HV. The obtained coatings are characterized by high erosion and abrasive wear resistance and the resistance to effects of cyclic thermal shock.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 3; 1363-1370
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies