Tytuł:
Review on Oxide Formation and Aluminum Recovery Mechanism during Secondary Smelting
Autorzy:
Osoba, L.O.
Owolabi, O.B.
Talabi, S.I.
Adeosun, S.O.
Powiązania:
https://bibliotekanauki.pl/articles/106915.pdf
Data publikacji:
2018
Wydawca:
Akademia Górniczo-Hutnicza im. Stanisława Staszica w Krakowie. Wydawnictwo AGH
Tematy:
Al dross
Al recovery
hydrometallurgy
oxidation
oxide film
Opis:
The remelting, refining, and casting process of aluminum alloys often generate aluminum dross containing primarily oxides and nitrides of aluminum and entrapped metallic aluminum at the surface of the molten metal as a result of reactions within the furnace atmosphere at elevated temperatures. The handling of dross is an expensive but necessary activity during aluminum smelting. Furthermore, the amorphous Al2O3 oxide film formed on the pure molten aluminum surface due to the liquid metal randomly distributed atoms is impermeable to the diffusion of aluminum metal and oxygen. In amorphous materials, there is a low mobility of the charge carriers and an absence of preferred diffusion paths. This film can transform to crystalline Al2O3 by nucleation and grows with time and opportunity. This review discusses the mechanism of oxide formation and the aluminum metal recovery processes.
Źródło:
Journal of Casting & Materials Engineering; 2018, 2, 2; 45-51
2543-9901
Pojawia się w:
Journal of Casting & Materials Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Badania plastometryczne i mikrostrukturalne stopów Fe-28Al-Cr i Fe-38Al
Plastometric and microstructure tests of alloys Fe-28Al-Cr and Fe-38Al
Autorzy:
Bednarczyk, Iwona
Powiązania:
https://bibliotekanauki.pl/articles/211594.pdf
Data publikacji:
2019
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Obróbki Plastycznej
Tematy:
stopy z układu Fe-Al
mikrostruktura
próba osiowosymetrycznego ściskania
procesy odbudowy struktury
Fe-Al intermetallic phase-based alloys
microstructure
axial-symmetric compression test
structure recovery processes
Opis:
Stopy na bazie uporządkowanych faz międzymetalicznych, tzw. intermetaliki, należą do grupy materiałów metalicznych o właściwościach pośrednich pomiędzy metalami a ceramiką. Szczególne zainteresowanie ze względu na korzystne właściwości znalazły stopy na osnowie faz międzymetalicznych Fe3Al i FeAl z układu Fe-Al. W artykule przedstawiono wpływ parametrów odkształcenia plastycznego na zmiany mikrostruktury stopów z układu Fe-Al. Odkształcenie realizowano w próbie osiowosymetrycznego ściskania na symulatorze Gleeble 3800, przy temperaturze w zakresie od 600 do 1200oC, z prędkością odkształcenia 0,1, 1,0 i 10,0 s-1. Na podstawie zależności naprężenia uplastyczniającego od odkształcenia wyznaczono maksymalne wartości naprężenia uplastyczniającego oraz odkształcenia odpowiadającemu temu naprężeniu w zależności od temperatury i prędkości odkształcenia. W celu obliczenia wartości parametru Zenera-Hollomona Z, czyli skorygowanej ze względu na temperaturę prędkości odkształcenia obliczono energię aktywacji Q procesu odkształcenia plastycznego. Przeprowadzono analizę mikrostruktury z użyciem mikroskopii świetlnej i elektronowej stopów Fe-28Al-5Cr i Fe-38Al w stanie odlewanym i po wyżarzaniu ujednorodniającym oraz po osiowosymetrycznym ściskaniu. Z analizy mikrostruktury wynika, że występują odmienne procesy odbudowy struktury dla stopów Fe-28Al-5Cr oraz Fe- 38Al. Dla stopu Fe-28Al-5Cr dominującym procesem odbudowy struktury jest zdrowienie dynamiczne, a dla stopu o wyższej zawartości aluminium Fe-38Al dominuje rekrystalizacja dynamiczna. Otrzymane wyniki badań plastyczności, analizy ilościowej i jakościowej substruktury oraz opis zjawisk zachodzących w trakcie odkształcenia na gorąco istotnie wpłyną na uzupełnienie dotychczasowej wiedzy o stopach na osnowie faz międzymetalicznych z układu Fe-Al.
Alloys based on systematic intermetallic phases belong to a group of metallic materials which share the characteristics of metals and ceramics. On account of the highly advantageous properties, the Fe-Al intermetallic phase-based alloys, i.e. Fe3Al and FeAl, are considered particularly interesting. This article provides a discussion on the effect of plastic strain parameters on changes to the microstructure of the Fe-Al system alloys. The plastic strain was achieved in a test of axial-symmetric compression using the Gleeble 3800 simulator at temperatures ranging from 600oC to 1200oC with the strain rate of 0.1; 1.0 and 10.0 s-1. Based on the dependences between flow stress and strain thus established, it was possible to determine the maximum flow stress as well as the value of strain corresponding to this stress for different temperatures and strain rates. In order to calculate the Zener-Hollomon parameter Z which is deformation speed corrected due to temperature there was activation energy Q of the plastic deformation process calculated. The microstructure of the Fe-28Al-5Cr and the Fe-38Al alloy was analysed after casting and homogenising, and following the test of axial-symmetric compression using light and electron microscopy techniques. With reference to results of the microstructure analysis, it was evidenced that the Fe-28Al-5Cr and the Fe-38Al alloy displayed disparate processes of structure recovery. The predominant structure recovery process for the Fe-28Al- 5Cr alloy is known as dynamic recovery, while for the Fe-38Al alloy with a higher aluminium content, dynamic recrystallisation was proved to be dominant. The results produced by the plasticity tests, an analysis of the substructure as well as a description of the phenomena that took place during hot strain will exert significant influence on expanding the current state of knowledge about the Fe-Al intermetallic phase-based alloys.
Źródło:
Obróbka Plastyczna Metali; 2019, 30, 2; 121-134
0867-2628
Pojawia się w:
Obróbka Plastyczna Metali
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Study on Recovery of Valuable Metals in Spent Lithium-Ion Batteries by Al2O3-SiO2-CaO-Fe2O3 Slag System
Autorzy:
Moon, Tae Boong
Han, Chulwoong
Hyun, Soong-Keun
Park, Sung Cheol
Son, Seong Ho
Lee, Man Seung
Kim, Yong Hwan
Powiązania:
https://bibliotekanauki.pl/articles/2049176.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
spent lithium-ion battery
smelting
Al2O3-SiO2-CaO-Fe2O3
recovery
slag
Opis:
This study investigated the recovery behavior of valuable metals (Co, Ni, Cu and Mn) in spent lithium ion-batteries based on Al2O3-SiO2-CaO-Fe2O3 slag system via DC submerged arc smelting process. The valuable metals were recovered by 93.9% at the 1250°C for 30 min on the 20 Al2O3-40SiO2-20Cao-20Fe2O3 (mass%) slag system. From the analysis of the slag by Fourier-transform infrared spectroscopy, it was considered that Fe2O2 and Al2O3 acted as basic oxides to depolymerize SiO4 and AlO4 under the addition of critical 20 mass% Fe2O3 in 20 Al2O3-40SiO2-Cao-Fe2O3 (Cao + Fe2O3 = 40 mass%). in addition, it was observed that the addition of Fe2O3 ranging between 20 and 30 mass% lowers the melting point of the slag system.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 4; 983-986
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies