Tytuł:
Curing Properties of Furotec 132 Resin- Bonded Foundry Sand
Autorzy:
Mashingaidze, M. M.
Powiązania:
https://bibliotekanauki.pl/articles/382717.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Furotec 132 resin
Furocure CH
curing properties
foundry sand
acid catalyst
curing temperature
żywica Furotec 132
właściwości utwardzające
piasek odlewniczy
katalizator kwasowy
temperatura utwardzania
Opis:
The study evaluated the curing properties of natural silica sand moulded with 1% by weight Furotec 132 resin binder catalysed by Furocure CH Fast acid and Furocure CH Slow acid. Physical properties of this sand included an AFS number of 47.35, 4.40 % clay, 0 % magnetic components, 0.13 % moisture, and 64.5 % of the size distribution spread over three consecutive sieves (150 – 600 μm). The sand was washed repeatedly to remove all the clay and oven dried. 2 kg washed sand samples were mulled with pre-determined weights of either catalyst to give 30 %, 50 % and 70 % by weight of 20 g Furotec 132 resin which was added last. Furotec 132 resin + Furocure CH Slow acid catalyst system gives longer bench lives and strip times but the maximum compressive strength in excess of 5000 N/cm2 is attained after more than 8.5 hours curing time irrespective of the weight % of catalyst added relative to the resin. On that basis, exceeding 30 weight % Furocure CH Slow acid catalyst when sand moulding with Furotec 132 resin has neither technical nor economic justification. In comparison, the Furotec 132 resin + Furocure CH Fast acid catalyst system was only capable of producing mould specimens with maximum compressive strength above 5000 N/cm2 at 30 weight % catalyst addition rate. At 50 and 70 weight % catalyst addition rates, the mulled sand rapidly turned dark green then bluish with a significant spike in temperature to about 40 oC, far exceeding the optimum curing temperature of Furotec 132. This high temperature accelerates the curing rate but with a very low degree of resin curing which explains the low compressive strength. In fact the sand grains fail to bond and have a dry, crumbly texture implying dehydration. Thus, not more than 30 weight % Furocure CH Fast acid catalyst should be used in sand moulding.
Źródło:
Archives of Foundry Engineering; 2019, 4; 117-123
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies