Tytuł:
Simultaneous transmission and scattering Mössbauer measurements of powder samples
Autorzy:
Fornal, P.
Stanek, J.
Powiązania:
https://bibliotekanauki.pl/articles/148213.pdf
Data publikacji:
2007
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
methodology of Mössbauer spectroscopy
CEMS
micro-powders
Opis:
A vertical experimental set-up for simultaneous recording transmission and scattering Mössbauer spectra is described. Application of the apparatus for the study of model powder mixture of two components with different grain sizes shows differences in the relative intensity ratio of these fractions in absorption and conversion electron Mössbauer spectroscopy (CEMS) spectra. This effect, explained as a result of the size selectivity of CEMS technique, is parameterized by the grain radius ratio of components. The possible application for investigation of isolated surface nano- and microobjects is discussed.
Źródło:
Nukleonika; 2007, 52, supl. 1; 13-16
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructural Characteristics of Ti-Al-Dy Alloy Produced by High Energy Ball Milling
Autorzy:
Kim, Yuri
Rhee, Hoseong
Chang, Si Young
Powiązania:
https://bibliotekanauki.pl/articles/2049319.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
high energy ball milling
Ti-Al-Dy powders
SPS
microstructure
micro-hardness
Opis:
In this study, the alloying of Ti, Al and Dy powders by high energy ball milling, and the spark plasma sintering (SPS) characteristics of as milled powders have been investigated based on the observation of microstructure. Pure Ti, 6wt% Al and 4wt% Dy powders were mixed and milled with zirconia balls at 600 ~ 1000 rpm for 3h in an Ar gas. The initial sizes of Ti, Al and Dy powders were approximately 20, 40, and 200 μm, respectively. With increasing the milling speed from 600 to 1000 rpm, the size of mixing powders reduced from 120 to 15 μm. On the other hand, from XRD results of powders milled at higher speeds than 700rpm, the peaks of Ti3Al and AlDy phases were identified, indicating the successful alloying. Therefore, the powders milled at 800 rpm have been employed for the SPS under the applied pressure of 50 MPa at 1373K for 15 min. In the SPSed sample, the Al3Dy and two ternary Ti-Al-Dy phases were newly detected, while the peak of AlDy phase disappeared. The SPSed Ti-6Al-4Dy alloy revealed high relative density and micro-hardness of approximately 99% and 950Hv, respectively.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 3; 789-783
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies