Tytuł:
Solid-liquid interface morphology of white carbide eutectic during directional solidification
Autorzy:
Trepczyńska-Łent, M.
Powiązania:
https://bibliotekanauki.pl/articles/354873.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
solid-liquid interface
directional solidification
front solidification
white carbide eutectic
Opis:
In this paper the analysis of solid-liquid interface morphology in white carbide eutectic was made. In a vacuum Bridgman-type furnace, under an argon atmosphere, directionally solidified sample of Fe - C alloy was produced. The pulling rate was v = 125 μm/s (450 mm/h) and constant temperature gradient G = 33.5 K/mm. The microstructure of the sample was frozen. The microstructure of the sample was examined on the longitudinal section using an light microscope and scanning electron microscope.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 365-368
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Leading Phase in the Directionally Solidifying Fe – 4.25%C Eutectic Alloy
Autorzy:
Trepczyńska-Łent, M.
Powiązania:
https://bibliotekanauki.pl/articles/380702.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
directional solidification
eutectic alloy Fe-C
solidification front
leading phase
krzepnięcie kierunkowe
stop eutektyczny
front krzepnięcia
Opis:
In order to determine the leading phase of the Fe - 4.25% C eutectic alloy, the method of directional crystallization, which allows to study the character of the solid / liquid growth front, was used. Examined eutectic was directionally solidified with a constant temperature gradient of G = 33,5 K/mm and growth rate of v = 125 μm/s (450 mm/h). The Bridgman technique was used for the solidification process. The sample was grown by pulling it downwards up to 30 mm in length. The alloy quenched by rapid pulling down into the Ga-In-Sn liquid metal. The sample was examined on the longitudinal section using a light microscope and scanning electron microscope. The shape of the solid/liquid interface and particularly the leading phase protrusion were revealed. The formation of the concave – convex interface has been identified in the quasi-regular eutectic growth arrested by quenching. The cementite phase was determined to be a leading phase. The total protrusion d is marked in the adequate figure.
Źródło:
Archives of Foundry Engineering; 2019, 4; 113-116
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies