Tytuł:
Dentinogenesis imperfecta : hardness and Young’s modulus of teeth
Autorzy:
Wieczorek, A.
Loster, J.
Ryniewicz, W.
Ryniewicz, A. M.
Powiązania:
https://bibliotekanauki.pl/articles/306749.pdf
Data publikacji:
2013
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
nanoindentation
enamel
dentinogenesis imperfecta
nanoindentacja
szkliwo nazębne
Opis:
Dentinogenesis imperfecta type II (DI-II) is the most common dental genetic disease with reported incidence 1 in 8000. Elasticity and hardness of the enamel of teeth are important values which are connected with their resistance to attrition. It is hypothesized that values of physical properties for healthy teeth and teeth with DI-II are different. The aim of the study was to investigate some physical properties of teeth extracted from patients with DI-II in comparison with normal teeth. The material of the study was six teeth: three lower molars, with clinical signs of DI-II, which were extracted due to complications of pulp inflammation and three other lower molars which were extracted for orthodontic reasons – well formed, without any signs of pathology. The surfaces of DI-II and normal teeth were tested on the CSM Instruments Scratch Tester machine (producer CSEM Switzerland) by Oliver & Pharr method. The indenter used was Vicker’s VG-73 diamond indenter. Additionally, the Scanning Electron Microscopy (SEM) analysis of the surface of the teeth with DI-II was made. Vickers hardness of the teeth with dental pathology (DI-II) was seven times smaller, and Young’s modulus six times smaller than those of healthy teeth. The parameters of hardness and elasticity of enamel of teeth with clinical diagnosis of DI-II were very much smaller than in normal teeth and because of that can be responsible for attrition.
Źródło:
Acta of Bioengineering and Biomechanics; 2013, 15, 3; 65-69
1509-409X
2450-6303
Pojawia się w:
Acta of Bioengineering and Biomechanics
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Study of the impact of incremental technology on mechanical and tribological properties of biomaterials
Badanie wpływu technologii przyrostowej na właściwości mechaniczne biomateriałów
Autorzy:
Bojko, Ł.
Ryniewicz, W.
Ryniewicz, A.
Kot, M.
Powiązania:
https://bibliotekanauki.pl/articles/190583.pdf
Data publikacji:
2017
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
biomateriały
technologia
nanoindentacja
SEM
tarcie
zużycie
ocena biomechaniczna
biomaterials
technology
nanoindentation
friction
wear
biomechanical estimation
Opis:
The latest method for creating denture replenishment in CAD / CAM systems is Direct Metal Laser Sintering (DMLS) technology. With the use of DMLS, prosthodontics, implant prosthetics, and facial-cranialjaw surgery adapted to individual patient conditions can be realized. The aim is to evaluate the strength, microstructure, and tribological properties of Ti6Al4V and CoCrMo alloys obtained from DMLS technology in the aspect of therapeutic constructions. The conducted tests show that, in the DMLS technology, as compared to milling technology preceded by casting and forging or pressed powder and sintering, for the same percentage composition of elements, the micromechanical properties, microstructural and tribological change. This procedure, from which constructions for various dental applications are obtained, is the new technology preferred for making permanent restorations faced with ceramics, producing intravascular implants, and implants of the temporomandibular joint. It can be an alternative to conventional cast-based methods and CAD / CAM based milling.
Najnowszą metodą tworzenia uzupełnień stomatologicznych w systemie CAD/CAM jest technologia Direct Metal Laser Sintering (DMLS). Z wykorzystaniem DMLS można realizować wykonanie konstrukcji protetyki, implantoprotetyki oraz chirurgii twarzowo-czaszkowo-szczękowej dostosowanej do indywidualnych warunków pacjenta. Celem jest ocena parametrów wytrzymałościowych, mikrostruktury i właściwości tribologicznych stopów Ti6Al4V oraz CoCrMo uzyskanych w technologii DMLS w aspekcie zastosowania na konstrukcje terapeutyczne. Przeprowadzone badania wskazują, że w technologii DMLS, w porównaniu z technologią frezowania poprzedzoną procesami odlewania i kucia lub prasowania proszku i spiekania, dla tego samego składu procentowego pierwiastków, zmieniają się właściwości mikromechaniczne, mikrostrukturalne i tribologiczne. Procedura ta, w wyniku której uzyskuje się konstrukcje dla różnych aplikacji stomatologicznych – jest nową technologią preferowaną do wykonawstwa uzupełnień stałych licowanych ceramiką, do wytwarzania wszczepów śródkostnych oraz implantów stawu skroniowo-żuchwowego. Może ona stanowić alternatywę dla klasycznych metod opartych na odlewnictwie oraz metod CAD/CAM opartych na frezowaniu.
Źródło:
Tribologia; 2017, 273, 3; 29-38
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies