Tytuł:
Ionic conductivity of the CeO2-Gd2O3-SrO system
Przewodnictwo jonowe w układzie CeO2-Gd2O3-SrO
Autorzy:
Dudek, M.
Mosiałek, M.
Mordarski, G.
Socha, R.
Rapacz-Kmita, A.
Powiązania:
https://bibliotekanauki.pl/articles/352955.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
elektrolity stałe tlenku ceru
roztwór stały
stałotlenkowe ogniwo paliwowe
solid oxide electrolytes
ceria-based solid solutions
co-doping
solid oxide fuel cell
Opis:
The Pechini method was used to synthesize nanopowders of CeO2-based solid solutions with the formula Ce0.8-xGd0.2SrxO2- for 0
Jednofazowe proszki roztworów stałych Ce0:8-xGd0:2SrxO2- dla 0
Źródło:
Archives of Metallurgy and Materials; 2011, 56, 4; 1249-1255
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Degradation of nanoclay-filled polylactide composites
Autorzy:
Rapacz-Kmita, A.
Stodolak-Zych, E.
Dudek, M.
Szaraniec, B.
Rozycka, A.
Mosialek, M.
Mandecka-Kamien, L.
Powiązania:
https://bibliotekanauki.pl/articles/110832.pdf
Data publikacji:
2013
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
nanocomposite materials
food packaging
polymer
smectite clay
Opis:
Nanoclay-filled polylactide (PLA 3051D) composite materials were tested in this study and their capacity for degradation was investigated. Activated and lyophilized smectite clay was used. The filler, its morphology, and grain size distribution were characterized by the use of transmission electron microscopy, scanning electron microscopy, and the dynamic light scattering technique. Samples of pure polylactide and polylactide filled with 3% wt., 5% wt., and 10% wt. of nanoclay in subsequent series were obtained by injection molding. The optimum amount of the filler in the nanocomposites was evalu-ated based on an assessment of mechanical properties as well as capacity to degrade. The 3% wt. mass fraction of nanofiller in the polylactide matrix was found to be the most effective in enhancement of both tensile strength (RM) and Young’s Modulus (E). It was also reported that polylactide nanocomposites filled with 3% wt. of smectite clay were characterized by the highest decrease in molecular mass of the matrix polymer after degradation tests (6 weeks incubation in water at 80°C). The observed decrease in degradation time and the overall changes distinguished in the nanocomposite structure suggest the poten-tial for application of the material in the packaging industry.
Źródło:
Physicochemical Problems of Mineral Processing; 2013, 49, 1; 91-99
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies