Scaling Behaviour of Si-alloyed Steel Slabs under Reheating Conditions
Autorzy:
Mikl, Gregor
Höfler, Thomas
Gierl-Mayer, Christian
Danninger, Herbert
Linder, Bernhard
Angeli, Gerhard
Powiązania:
https://bibliotekanauki.pl/articles/2056032.pdf
Data publikacji:
2021
Wydawca:
Akademia Górniczo-Hutnicza im. Stanisława Staszica w Krakowie. Wydawnictwo AGH
Tematy:
steel
hot rolling
oxidation
scale
alloy
Si oxides
Fe2SiO4
stal
walcowanie na gorąco
utlenianie
zgorzelina
stop
tlenki Si
Opis:
Reheating of steel slabs for further processing such as hot rolling usually takes place in gas-fired pusher furnaces. Temperatures well above 1000°C, combined with an atmosphere containing H2O, CO2, and O2, lead to substantial oxidation of most steel grades. Newly developed advanced steels often contain significant amounts of Si. This element plays a dominant role in the scaling behaviour near the steel-scale-interface, since fayalite (Fe2SiO4) forms a eutectic with wuestite (Fe1–xO) that melts as low as 1177°C. To better understand the high temperature oxidation behaviour, lab-scale trials were performed with different steel grades containing up to 3 wt.% Si. Possible interactions of Si with other alloying elements present in the samples such as Cr, Mn and Al were also of interest. The atmosphere contained 20% H2O, 7% CO2, and 3% O2, resembling reheating conditions in pusher furnaces, and temperatures ranged from 1100 to 1240°C. For metallographic investigation, the oxidised samples were cold mounted under vacuum using taper section angles. After preparation, the sections were examined through light microscopy, SEM/EDS, XRD, and TEM. The local distribution of the alloying elements could be mapped efficiently, and phase identification was successful in most parts. Under the applied experimental conditions, the elements of interest were present in their oxidic form either as pure or as mixed oxides. Higher Si-contents led to an increased build-up of eutectic melting phase at the steel-scale-interface at temperatures above 1177°C, which in turn further accelerated the oxidation.
Źródło:
Journal of Casting & Materials Engineering; 2021, 5, 4; 71--74
2543-9901
Pojawia się w:
Journal of Casting & Materials Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies