Tytuł:
Wear Mechanisms Analysis of Dies Used in the Process of Hot Forging a Valve Made of High Nickel Steel
Autorzy:
Hawryluk, M.
Gronostajski, Z.
Kaszuba, M.
Krawczyk, J.
Widomski, P.
Ziemba, J.
Zwierzchowski, M.
Janik, M.
Powiązania:
https://bibliotekanauki.pl/articles/351102.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
tool wear
tools durability
destructive mechanisms
valve engine
high nickel steel
Opis:
The study presents a durability analysis of dies used in the first operation of producing a valve-type forging from high nickel steel assigned to be applied in motor truck engines. The analyzed process of producing exhaust valves is realized in the forward extrusion technology and next through forging in closed dies. It is difficult to master, mainly due to the increased adhesion of the charge material (high nickel steel) to the tool’s substrate. The mean durability of tools made of tool steel W360, subjected to thermal treatment and nitriding, equals about 1000 forgings. In order to perform a thorough analysis, complex investigations were carried out, which included: a macroscopic analysis combined with laser scanning, numerical modelling by FEM, microstructural tests on a scanning electron microscopy and light microscopy (metallographic), as well as hardness tests. The preliminary results showed the presence of traces of abrasive wear, fatigue cracks as well as traces of adhesive wear and plastic deformation on the surface of the dies. Also, the effect of the forging material being stuck to the tool surface was observed, caused by the excessive friction in the forging’s contact with the tool and the presence of intermetallic phases in the nickel-chromium steel. The obtained results demonstrated numerous tool cracks, excessive friction, especially in the area of sectional reduction, as well as sticking of the forging material, which, with insufficient control of the tribological conditions, may be the cause of premature wear of the dies.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 4; 1963-1974
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies