Bending strength and fracture investigations of Cu based composite materials strengthened with \delta-alumina fibres
Autorzy:
Kaczmar, J. W.
Granat, K.
Naplocha, K.
Kurzawa, A.
Grodzka, E.
Samociuk, B.
Powiązania:
https://bibliotekanauki.pl/articles/383012.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metal matrix composite
copper
alumina fibre
squeeze casting
bending strength
kompozyt metalowy
miedź
włókno aluminiowe
prasowanie stopu
wytrzymałość na zginanie
Opis:
Bending strength, thermal and electric conductivity and microstructure examinations of Cu based composite materials reinforced with Saffil alumina fibres are presented. Materials were produced by squeeze casting method applying the designed device and specially elaborated production parameters. Applying infiltration pressure of 90MPa and suitable temperature parameters provided manufacturing of copper based composite materials strengthened with Saffil alumina fibres characterized by the low rest porosity and good fibre-matrix interface. Three point bending tests at temperatures of 25, 100 and 300ºC were performed on specimens reinforced with 10, 15 and 20% of Saffil fibres. Introduced reinforcement effected on the relatively high bending strengths at elevated temperatures. In relation to unreinforced Cu casting strength of composite material Cu – 15vol.% Saffil fibres increase by about 25%, whereas at the highest applied test temperature of 300ºC the improvement was almost 100%. Fibres by strengthening of the copper matrix and by transferring loads from the matrix reduce its plastic deformation and hinder the micro-crack developed during bending tests. Decreasing of thermal and electrical conductivity of Cu after incorporating fibres in the matrix are relatively small and these properties can be acceptable for electric and thermal applications.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 59-63
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Production and wear properties of copper based MMC strengthened with δ-alumina fibres
Wytwarzanie oraz własności tribologiczne materiałów kompozytowych na osnowie miedzi umocnionej włóknami tlenku aluminium
Autorzy:
Granat, K.
Pietrzak, K.
Grodzka, E.
Naplocha, K.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/382379.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metal matrix composite
copper alloy
alumina fibre
squeeze casting
wear resistance
kompozyty o osnowie metalowej
włókna tlenku glinu
infiltracja ciśnieniowa
zużycie ścierne
Opis:
The investigation was carried out on the production by pressure infiltration (squeeze casting) of metal matrix composite materials based on pure Cu-ETP copper containing δ-alumina SAFFIL fibres The microstructure of composite specimens and morphology was examined using SEM and optical microscopy. Physical properties: Brinell hardness HBW and density were characterized. Preforms with 10, 15 and 20 vol. % of fibres were preheated and infiltrated applying the infiltration pressure of 100 MPa. The strengthening of matrix with SAFFIL fibres resulted in significant increase of hardness. Metallographic examinations showed, that SAFFIL fibres are not destroyed in course of the infiltration process and are uniformly distributed in copper matrix. SEM observations confirm the poor wettability of fibres by liquid Cu-ETP. The wear of manufactured MMCs during dry sliding against cast iron applying a pin-on-disc tester were recorded after 1, 3.5 and 8.5 km of friction distance. Increasing content of SAFFIL fibres in the copper matrix results in the significant decreasing of wear.
Przeprowadzono obserwacje mikroskopowe, badania twardości tribologicznej materiałów kompozytowych na osnowie miedzi M1E umocnionej włóknami δ-Al2O3 SAFFIL. Porowate kształtki z włókien ceramicznych nasycano miedzią metodą infiltracji ciśnieniowej (squeeze casting) pod ciśnieniem 100 MPa. Przeprowadzone badania z wykorzystaniem mikroskopu skaningowego oraz optycznego wykazały równomierne rozmieszczenie włókien, jednakże z licznymi defektami i słabą zwilżalnością umocnienia przez ciekłą miedź. Zbadano twardość Brinella HBW oraz gęstość materiałów kompozytowych zawierających 10, 15 i 20 obj. % włókien Al2O3. Stosując urządzenie do badania zużycia typu „pin-on-disc” przeprowadzono badania odporności na zużycie ścierne w warunkach tarcia suchego i stwierdzono, że wraz ze wzrostem zawartości włókien zwiększa się twardość i odporność na zużycie ścierne. W stosunku do nieumocnionej osnowy odporność materiałów kompozytowych zawierających 20% włókien zwiększa się około 10-krotnie. W mniejszym stopniu ulega zmianie współczynnik tarcia, który przy tarciu w parze z materiałami kompozytowymi jest o około 10-20% mniejszy niż przy ścieraniu z nieumocnioną miedzią.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 71-74
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies