Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Erkmen, Z." wg kryterium: Autor


Wyświetlanie 1-2 z 2
Tytuł:
The Effect of Mechanical Alloying on the Microhardness and Fracture Toughness of $BaTiO_3$
Autorzy:
Ertuğ, B.
Çetiner, B.
Sadullahoğlu, G.
Gökçe, H.
Erkmen, Z.
Öveçoğlu, M.
Powiązania:
https://bibliotekanauki.pl/articles/1399670.pdf
Data publikacji:
2013-02
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.07.Bc
62.25.-g
81.20.Ev
62.20.mm
Opis:
In this work, the effects of mechanical alloying on the mechanical properties of $BaTiO_3$ were investigated. In order to examine the milling conditions and sintering parameters on the solid state formation of $BaTiO_3$, X-ray diffraction technique was used. After mechanical alloying process, nanosized powder mixtures were produced. Sintering temperatures were 600, 700, 800, 900, 1000, and 1200C and sintering duration was 1 h. Besides X-ray diffraction examinations, mechanical properties of the $BaTiO_3$ samples were determined by Vickers microhardness test.
Źródło:
Acta Physica Polonica A; 2013, 123, 2; 188-190
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Investigation of Indentation Fracture Toughness (KIC) and Weibull Parameters of 0.25Li2O.2SiO2-0.75BaO.2SiO2 Glass-Ceramic
Autorzy:
Ertuğ, B.
Çetiner, B. R.
Gökçe, H.
Erkmen, Z. E.
Öveçoğlu, M. L.
Powiązania:
https://bibliotekanauki.pl/articles/351907.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lithium barium silicate glass-ceramic
indentation fracture toughness
hardness
statistical analysis
weibull modulus
Opis:
In the present study, mechanical properties of 0.25Li2O.2SiO2-0.75BaO.2SiO2 glass-ceramic were investigated. The trans-formations‘ temperatures were determined by DTA instrument. The optimum nucleation temperature was found to be 540°C. This suggested the crystallization temperatures as 675, 720 and 800°C. After carrying out crystallization heat treatments, Vickers indentation test was applied. In order to determine the indentation fracture toughness (KIC), crack half-length ‚c‘ of the samples was measured. To calculate KIC, Young’s modulus, E and the measured hardness, Hv were used. Using KIC and probability of fracture ‚P‘, ln ln[1/(1 − P)] – ln KIC graph was drawn based on the Weibull distribution equation. Consequently, Weibull modulus, ‚m‘ and scale parameter, ‚K0‘ were determined and compared with each other.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 4; 1963-1968
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies