Tytuł:
Effect of Fe-Mn Solid Solution Precursor Addition on Modified AA 7075
Autorzy:
Kim, Min Sang
Kim, Dae Young
Kim, Young Do
Choi, Hyun Joo
Kim, Se Hoon
Powiązania:
https://bibliotekanauki.pl/articles/2049310.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Zn-Mg alloy
solid solution precursor
mechanical properties
Opis:
This study suggests a new way to modify the size and morphology of Al-Fe phases in modified AA 7075 by using an Fe-Mn solid solution powder as the precursor. When Fe and Mn are added in the form of a solid solution, the diffusion of Fe and Mn toward the Al is delayed, thus altering the chemical composition and morphology of the precipitates. The fine, spherical precipitates are found to provide a good balance between strength and ductility compared to the case where Fe and Mn are separately added.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 3; 783-787
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication of Aluminum Matrix Composite Reinforced with Al0.5CoCrCuFeNi High-Entropy Alloy Particles
Autorzy:
Kim, Min Sang
Son, Han Sol
Joo, Gyeong Seok
Kim, Young Do
Choi, Hyun Joo
Kim, Se Hoon
Powiązania:
https://bibliotekanauki.pl/articles/2174583.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminum matrix composite
high entropy alloys
reinforcement
powder-in-tube
stir casting
Opis:
The aluminum composite with dispersed high entropy alloy were developed by stir casting involving the powder-in-tube method. First, Al0.5CoCrCuFeNi high entropy alloy (HEA) powder was made by mechanical alloying, and the powder was extruded in a tube-type aluminum container to form HEA precursor. The extruded HEA precursor was then dispersed in the aluminum matrix via stir casting. As a result, Fe-Cr-Ni based high-entropy phases was uniformly formed in the aluminum matrix, revealing ~158, 166, 235% enhancement of tensile strength by incorporating 1, 3, and 5 wt% HEA particles, respectively.
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 4; 1543--1546
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies