Structural and magnetic properties of the as - cast Nd10Fe83Zr1B6 ribbons, studied by X-ray diffraction and Mössbauer spectroscopy
Autorzy:
Ceglarek, A.
Płusa, D.
Pawlik, P.
Gębara, P.
Powiązania:
https://bibliotekanauki.pl/articles/147920.pdf
Data publikacji:
2013
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
hard magnetic magnets
melt-spinning technique
Mössbauer spectroscopy
nanocomposites
Opis:
The Nd10Fe83Zr1B6 alloy ribbons, prepared by melt-spinning technique, have been investigated by X-ray diffraction (XRD) and Mossbauer spectroscopy. Magnetic properties were studied by Faraday balance and vibrating sample magnetometry (VSM). The ribbon samples were produced at various surface velocities of the copper wheel from 10 m/s to 20 m/s. The XRD and Mossbauer spectra analysis have shown that the ribbons consist of the soft magnetic alfa-Fe, hard magnetic Nd2Fe14B and disordered phases. The results showed that a uniform Nd2Fe14B/alfa-Fe nanocomposite structure with fine alfa-Fe grains can be obtained at an optimum velocity of the cooper roll of 20 m/s. The samples produced in these conditions had the best magnetic properties (mi0HC= 0.84 T, mi0MR = 1.05 T, mi0MS = 1.36 T, (BH)max = 160 kJ/m3) with strong exchange coupling between the hard magnetic Nd2Fe14B and soft magnetic mi-Fe phases. The amorphous phase existing between grains causes an increase in the remanence and remanence ratio.
Źródło:
Nukleonika; 2013, 58, 1; 105-108
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of heat treatment on magnetic properties of nanocrystalline Nd9Fe84Zr1B6 ribbons received by rapid solidification method
Wpływ obróbki termicznej na własności magnetyczne nanokrystalicznych taśm Nd9Fe84Zr1B6 wytwarzanych metodą szybkiego chłodzenia
Autorzy:
Ceglarek, A.
Płusa, D.
Pawlik, P.
Dośpiał, M.
Powiązania:
https://bibliotekanauki.pl/articles/354463.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
nanokompozyty
metoda szybkiego chłodzenia
stopy Nd-Fe-B
twarde materiały magnetyczne
magnesy nanokrystaliczne
nanocomposites
rapid solidification method
Nd-Fe-B alloys
hard magnetic materials
nanocrystalline magnets
Opis:
The effect of the annealing on the phase composition and magnetic properties of nanocomposite melt-spun Nd9Fe84Zr1B6 ribbons has been investigated. From the X-ray diffraction studies confirmed be thermomagnetic curves measurements results that the microstructure of the material investigated is composed of a mixture of magnetically hard Nd2Fe14B and soft α-Fe, Fe3B nanosized grains. The small amount of undesirable Nd2Fe23B3 metastable phase has been found which do not decompose at the highest annealing temperature. The hysteresis loop measurements certify that the ribbon annealed at 863K show the best coupling between the hard and soft magnetic phases and thus the highest coercivity of 0.38T. The grain sizes increase with increasing annealing temperature causing the coercivity to be decrease.
Zbadano wpływ wygrzewania na skład fazowy i właściwości magnetyczne taśm nanokompozytowych Nd9Fe84Zr1B6 otrzymanych metodą szybkiego chłodzenia cieczy na wirującym miedzianym bębnie. Badania mikrostruktury potwierdzają zależności krzywych termomagnetycznych, z których wynika, że stop składa się z ziaren o rozmiarach nanometrycznych faz: magnetycznie miękkich α-Fe, Fe3B oraz magnetycznie twardej Nd2Fe14B. Stwierdzono niewielką ilość niepożądanej metastabilnej fazy, która nie ulega rozkładowi przy najwyższej temperaturze wygrzewania. Pomiary pętli histerezy magnetycznej dla taśmy wygrzanej w temperaturze 863K świadczą o najsilniejszych oddziaływaniach pomiędzy fazami, twardą i miękką. Rozmiar ziaren wzrasta we wzrostem temperatury wygrzewania, powodując spadek koercji. Koercja taśmy wygrzanej w temperaturze 863K ma największą wartość, wynoszącą 0.38T oraz najmniejszy rozmiar ziarna fazy Nd2Fe14B.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 1; 229-232
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies