Tytuł:
Microstructural Evolution of Sinter-Forged Fe-Cr-Mo-C Alloy Depending on Cu Addition
Autorzy:
Oh, Min Chul
Kim, Moontae
Lee, Jisung
Ahn, Byungmin
Powiązania:
https://bibliotekanauki.pl/articles/355446.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Astaloy CrL
Fe-based alloy
pre-alloyed powder
powder forging
microstructure
Opis:
Pre-alloyed Astaloy CrLTM (Fe-1.5 wt% Cr-0.2 wt% Mo), a commercial Fe-based alloy powder for high strength powder metallurgy products, was sintered and hot forged with additions of 0.5 wt% C and 0~2 wt% Cu. To investigate the influence of various Cu contents, the microstructural evolution was characterized using density measurements, scanning electron microscope (SEM) and electron backscatter diffraction (EBSD). Transverse rupture strength (TRS) was measured for each composition and processing stage. The correlation between Cu additions and properties of sinter-forged Fe-Cr-Mo-C alloy was discussed in detail.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 2; 539-542
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructural Evolution of AlCuFeMnTi-0.75Si High Entropy Alloy Processed by Mechanical Alloying and Spark Plasma Sintering
Autorzy:
Kim, Minsu
Sharma, Ashutosh
Chae, Myoung Jin
Lee, Hansung
Ahn, Byungmin
Powiązania:
https://bibliotekanauki.pl/articles/2049226.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
high entropy alloy
powder metallurgy
mechanical alloying
spark plasma sintering
high energy ball milling
Opis:
In this work, we have designed a new high entropy alloy containing lightweight elements, e.g., Al, Fe, Mn, Ti, Cu, Si by high energy ball milling and spark plasma sintering. The composition of Si was kept at 0.75 at% in this study. The results showed that the produced AlCuFeMnTiSi0.75 high entropy alloy was BCC structured. The evolution of BCC1 and BCC2 phases was observed with increasing the milling time up to 60 h. The spark plasma sintering treatment of milled compacts from 650-950°C showed the phase separation of BCC into BCC1 and BCC2. The density and strength of these developed high entropy alloys (95-98%, and 1000 HV) improved with milling time and were maximum at 850°C sintering temperature. The current work demonstrated desirable possibilities of Al-Si based high entropy alloys for substitution of traditional cast components at intermediate temperature applications.
Źródło:
Archives of Metallurgy and Materials; 2021, 66, 3; 703-707
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies