Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "A.N." wg kryterium: Autor


Wyświetlanie 1-12 z 12
Tytuł:
Effect of arc stud welding parameters on the microstructure and mechanical properties of AA6061 and AA5086 aluminium alloys
Autorzy:
Razzaq, M. K. A.
Abood, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/2055760.pdf
Data publikacji:
2021
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
arc stud welding
aluminium alloys
solidification mode
fusion zone
mechanical properties
spawanie łukowe
stopy aluminium
model krzepnięcia
strefa przetopienia
właściwości mechaniczne
Opis:
Purpose: This paper aims to investigate the effect of arc stud welding (ASW) process parameters on the microstructure and mechanical properties of AA6061-T6 and AA5086-H116 joint. Design/methodology/approach: ASW process was done with argon as a shielding gas. Optical microscope (OM), scanning electron microscope (SEM), and X-Ray Diffraction (XRD) were employed to investigate the influence of welding current, welding time, and gas flow-rate on the microstructure of the fusion zone (FZ). Torque strength and Microhardness tests were used to evaluate the mechanical properties of the welded joints. Findings: OM and SEM showed a cellular dendritic structure with equiaxed zone and columnar dendritic are forming at welding zone and weld interface. XRD analysis showed the precipitation of Mg2Si and Al3Mg2 in the similar and dissimilar joints. Similar ASW of AA6061-T6/AA6061-T6 recorded 19 N.m torque strength, while dissimilar welding of AA6061-T6/AA5086-H116 registered 23 N.m. With increasing heat input, grains in Fusion Zone (FZ) and Heat Affected Zone (HAZ) coarsen and the hardness in both zones decreased. The hardness of similar weldments indicated a remarkable softening of FZ, while lower hardness values were registered in HAZ of dissimilar weldments. Softening of both weldments is due to the dissolution of the strengthening precipitates. Hot cracks exist with similar weldments, while no cracks evidence with dissimilar weldments. Research limitations/implications: The main challenge in this work was how to minimize porosity level and how to avoid hot crack in the FZ. Practical implications: The application of ASW with ceramic ferrule has an important role in different production areas such as; automobile industry, aircraft applications, and appliances industry. Originality/value: Study the effect of welding current, welding time, and gas flow-rate of ASW process on microstructure and mechanical properties of AA6061-T6 and AA5086-H116 joint.
Źródło:
Journal of Achievements in Materials and Manufacturing Engineering; 2021, 108, 1; 24--34
1734-8412
Pojawia się w:
Journal of Achievements in Materials and Manufacturing Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Economical reactive powder concrete cast using available materials in North Sinai, Egypt
Autorzy:
Meleka, N. N.
Bashandy, A. A.
Arab, M. A.
Powiązania:
https://bibliotekanauki.pl/articles/231066.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
proszek reaktywny
beton
właściwości mechaniczne
zawartość
cement
pył krzemionkowy
włókno stalowe
reactive powder
concrete
mechanical properties
silica fume
steel fiber
Opis:
In this research reactive powder concrete (RPC) was prepared using sand from North Sinai. The mechanical properties of locally cast RPC were investigated and evaluated by studying the effects of using different cement and silica fume contents and new steel fibers’ aspect ratios as reinforcement for RPC. Specimens’ preparation, curing regimes and testing procedures to evaluate the compressive strength, the modulus of elasticity, the indirect tensile strength and the flexural strength were discussed. A compressive strength of 154.5MPa, indirect tensile strength of 11.98MPa, modulus of elasticity of 45.1GPa and flexural strength of 30.26MPa have been achieved for reinforced RPC contains 800 kg/m3 cement content and silica fume content 30% of cement weight. The test results showed some improvements by increasing cement and silica fume contentsas well as adding steel fibers on the compressive strength, modulus of elasticity and indirect tensile strength.
Źródło:
Archives of Civil Engineering; 2013, 59, 2; 175-195
1230-2945
Pojawia się w:
Archives of Civil Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Synthesis and properties of vinylpyrrolidone/ (trimethoxysilyl)propyl methacrylate gels containing different amounts of crosslinking agent
Synteza i właściwości żelu N-winylopirolidon/metakrylan3-(trimetoksysililo)propylu z różną zawartością czynnika sieciującego
Autorzy:
Mohammed, A. H.
Ahmad, M. B.
Ibrahim, N. A.
Zainuddin, N.
Powiązania:
https://bibliotekanauki.pl/articles/947044.pdf
Data publikacji:
2018
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Chemii Przemysłowej
Tematy:
high conversion copolymers
swelling parameters
mechanical properties
oxygen permeability
crosslinking density
kopolimery o wysokim stopniu konwersji
parametry pęcznienia
właściwości mechaniczne
przepuszczalność tlenu
gęstość sieciowania
Opis:
High conversion copolymers containing 90 wt % of N-vinylpyrrolidone (NVP) and 10 wt % of 3-(trimethoxysilyl)propyl methacrylate (TMSPM) with 0, 1, 2, 3 and 4 wt % (in conversion to mass of NVP/TMSPM) of ethylene glycol dimethacrylate (EGDMA) as crosslinker have been successfully synthesized. Proton nuclear magnetic resonance (1H NMR) and Fourier transform infrared spectroscopy (FT-IR) were employed to characterize the resulting copolymers. The effect of EGDMA amount on the mechanical and thermal properties, swelling parameters, clarity, and oxygen permeability of the prepared xerogels and hydrogels were studied. 3 wt % of EGDMA is required to obtain clear xerogels and hydrogels. The water content (EWC), volume fraction of polymer (φ2) and weight loss during swelling decrease with increasing EGDMA content. Young’s and shear modulus (E and G) increase as EGDMA content increases, the values of E and G are 0.570–3.531 MPa and 0.217–1.359 MPa, respectively. The hydrogels were characterized in terms of modulus crosslinking density (ve and vt) and polymer-solvent interaction parameters (χ). The results are 0.220–0.613 mol/dm3 for ve, 0.105–0.441 mol/dm3 for vt, and 0.595–0.822 for χ. Thermal properties enhance by adding EGDMA whereas the oxygen permeability (P) of hydrogels decreases from 48.6 to 44.3 as water content decrease from 70.3 to 55.1.
Kopolimery zawierające 90 % mas. N-winylopirolidonu (NVP) i 10 % masmetakrylanu 3-(trimetoksysililo)propylu (TMSPM) z udziałem 0, 1, 2, 3 i 4 % mas. (w przeliczeniu na masę NVP/TMSPM) dimetakrylanu glikolu etylenowego (EGDMA) jako środka sieciującego zsyntetyzowano z wysokim stopniem konwersji. Otrzymane kopolimery charakteryzowano metodami protonowego rezonansu jądrowego (H1 NMR) i spektroskopii w podczerwieni (FT-IR). Badano wpływ udziału środka sieciującego na właściwości mechaniczne i termiczne, parametry pęcznienia, klarowność i przepuszczalność tlenu wytworzonych hydro- i kserożeli. Stwierdzono, że dodatek już 3 % mas. EGDMA wystarcza do uzyskania klarownego żelu, a w miarę zwiększania zawartości EGDMA zmniejsza się zawartość wody (EWC), ułamek objętości polimeru (φ2) oraz strata masy w procesie pęcznienia żelu NVP/TMSPM. Wartość modułu zarówno Younga (E), jak i ścinania (G) zwiększa się (E = 0,570–3,531 MPa, G = 0,217–1,359 MPa) wraz ze wzrostem udziału EGDMA w kompozycji. Wytworzone hydrożele charakteryzowano za pomocą modułów gęstości sieciowania (ve = 0,220–0,613 mol/dm3, vt = 0,105–0,441 mol/dm3) i parametru oddziaływania polimer-rozpuszczalnik (χ = 0,595–0,822). Właściwości termiczne otrzymanych hydrożeli zawierających EGDMA poprawiły się wraz ze zmniejszeniem zawartości wody (70,3–55,1), natomiast przepuszczalność tlenu się pogorszyła (P = 48,6–44,3).
Źródło:
Polimery; 2018, 63, 9; 577-585
0032-2725
Pojawia się w:
Polimery
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The effect of heat treatment on mechanical properties of 42CrMo4 steel
Autorzy:
Çalık, A.
Dokuzlar, O.
Uçar, N.
Powiązania:
https://bibliotekanauki.pl/articles/368557.pdf
Data publikacji:
2020
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
42CrMo4 steel
quenching
tempering
martensite structure
mechanical properties
stal 42CrMo4
hartowanie
odpuszczanie
struktura martenzytyczna
właściwości mechaniczne
Opis:
Purpose: In this study, the effect of heat treatment on the microstructure and mechanical properties of 42CrMo4 steel were investigated. Design/methodology/approach: The samples were annealed at 860°C for 120 min. followed by oil quenching and then tempered at temperatures between 480 and 570°C for 120 min. The microstructure of untreated 42CrMo4 steel mainly consists of pearlite and ferrite whereas the microstructure was found to be as a martensitic structure with a quenching process. Findings: The results showed that there is an increase in yield stress, ultimate tensile stress, hardness and impact energy, while elongation decreases at the end of the quenching process. Conversely, yield stress, ultimate tensile stress and hardness decrease slightly with the increasing of tempering temperature, while elongation and impact energy increase. Research limitations/implications: Other types of steels can be heat treated in a wider temperature range and the results can be compared. Practical implications: It is a highly effective method for improving the mechanical properties of heat treatment materials. Originality/value: A relationship between the mechanical properties and the microstructure of materials can be developed. The heat treatment is an effective method for this process.
Źródło:
Journal of Achievements in Materials and Manufacturing Engineering; 2020, 98, 1; 5-10
1734-8412
Pojawia się w:
Journal of Achievements in Materials and Manufacturing Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparative Studies of Microstructure and Fatigue Life of Selected Lead-free Alloys
Autorzy:
Pietrzak, K.
Klasik, A.
Maj, M.
Sobczak, N.
Wojciechowski, A.
Powiązania:
https://bibliotekanauki.pl/articles/379514.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lead free alloys
microstructure
mechanical properties
stopy bezołowiowe
mikrostruktura
właściwości mechaniczne
Opis:
Lead-free alloys containing various amounts of zinc (4.5%, 9%, 13%) and constant copper addition (1%) were discussed. The results of microstructure examinations carried out by light microscopy (qualitative and quantitative) and by SEM were presented. In the light microscopy, a combinatorial method was used for the quantitative evaluation of microstructure. In general, this method is based on the phase quanta theory according to which every microstructure can be treated as an arrangement of phases/structural components in the matrix material. Based on this method, selected geometrical parameters of the alloy microstructure were determined. SEM examinations were based on chemical analyses carried out in microregions by EDS technique. The aim of the analyses was to identify the intermetallic phases/compounds occurring in the examined alloys. In fatigue testing, a modified low cycle fatigue test method (MLCF) was used. Its undeniable advantage is the fact that each time, using one sample only, several mechanical parameters can be estimated. As a result of structure examinations, the effect of alloying elements on the formation of intermetallic phases and compounds identified in the examined lead-free alloys was determined. In turn, the results of mechanical tests showed the effect of intermetallic phases identified in the examined alloys on their fatigue life. Some concepts and advantages of the use of the combinatorial and MLCF methods in materials research were also presented.
Źródło:
Archives of Foundry Engineering; 2017, 17, 3; 111-116
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructural Aspects of Fatigue Parameters of Lead-Free Sn-Zn Solders with Various Zn Content
Autorzy:
Pietrzak, K.
Klasik, A.
Maj, M.
Wojciechowski, A.
Sobczak, N.
Powiązania:
https://bibliotekanauki.pl/articles/379846.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lutowanie bezołowiowe
mikrostruktura
właściwości mechaniczne
lead-free solders
microstructure
mechanical properties
Opis:
The study includes the results of research conducted on selected lead-free binary solder alloys designed for operation at high temperatures. The results of qualitative and quantitative metallographic examinations of SnZn alloys with various Zn content are presented. The quantitative microstructure analysis was carried out using a combinatorial method based on phase quanta theory, according to which any microstructure can be treated as an array of elements disposed in the matrix material. Fatigue tests were also performed using the capabilities of a modified version of the LCF method hereinafter referred to in short as MLCF, which is particularly useful in the estimation of mechanical parameters when there are difficulties in obtaining a large number of samples normally required for the LCF test. The fatigue life of alloys was analyzed in the context of their microstructure. It has been shown that the mechanical properties are improved with the Zn content increasing in the alloy. However, the best properties were obtained in the alloy with a chemical composition close to the eutectic system, when the Zn-rich precipitates showed the most preferred morphological characteristics. At higher content of Zn, a strong structural notch was formed in the alloy as a consequence of the formation in the microstructure of a large amount of the needle-like Zn-rich precipitates deteriorating the mechanical characteristics. Thus, the results obtained during previous own studies, which in the field of mechanical testing were based on static tensile test only, have been confirmed. It is interesting to note that during fatigue testing, both significant strengthening and weakening of the examined material can be expected. The results of fatigue tests performed on SnZn alloys have proved that in this particular case the material was softened.
Źródło:
Archives of Foundry Engineering; 2017, 17, 1; 131-136
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructural Aspects of Fatigue Life of Sn-Zn Lead-free Solders with 1% of Ag Addition
Autorzy:
Pietrzak, K.
Klasik, A.
Maj, M.
Sobczak, N.
Wojciechowski, A.
Powiązania:
https://bibliotekanauki.pl/articles/382245.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lead-free solders
microstructure
mechanical properties
lutowanie bezołowiowe
mikrostruktura
właściwości mechaniczne
Opis:
The article presents the study results of Sn-Zn lead-free solders with the various Zn content. The results concern the hypoeutectic, eutectic and hypereutectic alloys containing respectively 4.5% Zn, 9% Zn and 13.5% Zn. Moreover, these alloys contain the constant Ag (1%) addition. The aim of the study was to determine the microstructural conditionings of their fatigue life. In particular it was focused on answer the question what meaning can be assigned to the Ag addition in the chemical composition of binary Sn-Zn alloys. The research includes a qualitative and quantitative assessments of the alloy microstructures, that have been carried out in the field of light microscopy (LM). In order to determine some geometrical parameters of the microstructure of alloys the combinatorial method based on the phase quanta theory was applied. Moreover, for the identification necessities the chemical analyses in the micro-areas by SEM/EDS technics were also performed. Based on the SEM/EDS results the phases and intermetallic compounds existing in the examined lead-free solders were identified. The mechanical characteristics were determined by means of the modified low cycle test (MLCF). Based on this method and on the results obtained every time from only one sample the dozen of essential mechanical parameters were evaluated. The research results were the basis of analyzes concerning the effects of microstructural geometrical parameters of lead-free alloys studied on their fatigue life at ambient temperature.
Źródło:
Archives of Foundry Engineering; 2018, 18, 1; 87-92
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Mechanical Characteristics of the Ternary SnZnAl Lead-Free Alloy
Autorzy:
Pietrzak, K.
Klasik, A.
Maj, M.
Sobczak, N.
Powiązania:
https://bibliotekanauki.pl/articles/380398.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lead free alloy
microstructure
mechanical properties
scanning electron microscopy
stop bezołowiowy
mikrostruktura
właściwości mechaniczne
mikroskop skaningowy
Opis:
The paper describes the studies of ternary SnZn9Al1.5 lead-free alloy from the viewpoint of its mechanical behavior as well as microstructure examined by the light and scanning electron microscopy. The authors focused their attention specifically on the fatigue parameters determined by the original modified low-cycle fatigue method (MLCF), which in a quick and economically justified way allows determination of a number of mechanical parameters based on the measurement data coming from one test sample only. The effect of the addition of 1.5% Al to the binary eutectic SnZn9 alloy on its microstructure and the obtained level of mechanical parameters was analyzed. The phases and intermetallic compounds occurring in the alloy were identified based on the chemical analysis carried out in micro-areas by the SEM/EDS technique. It was shown that the addition of 1.5% Al to the binary eutectic SnZn9 alloy resulted in a more favorable microstructure and consequently had a positive effect on the mechanical parameters of the alloy. Based on the conducted research, it was recommended to use a combinatorial method based on the phase quanta theory to quickly evaluate the microstructure and the original MLCF method to determine a number of mechanical parameters.
Źródło:
Archives of Foundry Engineering; 2018, 18, 3; 31-36
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mechanical properties of sugar palm yarn/woven glass fiber reinforced unsaturated polyester composites: effect of fiber loadings and alkaline treatment
Wpływ zawartości włókien i obróbki alkalicznej na właściwości mechaniczne kompozytów z nienasyconej żywicy poliestrowej wzmacnianych włóknem szklanym i włóknem palmy cukrowej
Autorzy:
Mohd Nurazzi, N.
Khalina, A.
Sapuan, S. M.
Ilyas, R. A.
Powiązania:
https://bibliotekanauki.pl/articles/947560.pdf
Data publikacji:
2019
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Chemii Przemysłowej
Tematy:
glass fiber
hybrid composites
mechanical properties
sugar palm fiber
yarn fiber
unsaturated polyester resin
włókno szklane
kompozyty hybrydowe
właściwości mechaniczne
włókno palmy cukrowej
włókno przędzy
nienasycona żywica poliestrowa
Opis:
In this paper, hybrid sugar palm yarn and glass fiber reinforced unsaturated polyester composites were investigated in relation to the effects of fiber loadings and alkaline treatment on the composite mechanical properties, such as tensile, flexural, impact and compression strength. The composites were fabricated at a weight ratio of matrix to reinforcement of 70 : 30 and 60 : 40, respectively, while the ratio of sugar palm yarn fiber to glass fiber was selected at 70 : 30, 60 : 40 and 50 : 50, respectively. The results revealed that the mechanical properties of the hybrid composites were increased with an increase of glass fiber loading for both 30 wt % and 40 wt % reinforcement content. The alkaline treatment of the sugar palm fibers have advantageous effect on the hybrid composite performance. The overall results indicated that the developed hybrid composites can be used as an alternative material for glass fiber reinforced polymer composites for various structural applications.
Zbadano wpływ zawartości włókien i ich obróbki alkalicznej na właściwości mechaniczne wzmacnianych włóknem szklanym kompozytów nienasyconej żywicy poliestrowej z włóknami palmy cukrowej. Oceniano wytrzymałość kompozytów na rozciąganie, zginanie, uderzenie i ściskanie. Wytworzone kompozyty zawierały 30 oraz 40% mas. włókien, przy stosunku masowym włókien palmy cukrowej do włókien szklanych 70/30, 60/40 i 50/50. Stwierdzono, że wytrzymałość mechaniczna kompozytów hybrydowych zwiększa się ze wzrostem zawartości włókna szklanego, a obróbka alkaliczna włókien palmy cukrowej wywiera korzystny wpływ na właściwości zawierających ją kompozytów hybrydowych. Uzyskane wyniki wskazują, że opracowane kompozyty hybrydowe mogą być stosowane jako materiał alternatywny dla kompozytów polimerowych wzmacnianych jedynie włóknem szklanym.
Źródło:
Polimery; 2019, 64, 10; 665-675
0032-2725
Pojawia się w:
Polimery
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Fatigue Life of the Binary Lead-free Alloys with High Zn Content
Autorzy:
Pietrzak, K.
Klasik, A.
Maj, M.
Sobczak, N.
Powiązania:
https://bibliotekanauki.pl/articles/382479.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lead free alloy
alloy microstructure
mechanical properties
stop bezołowiowy
mikrostruktura stopu
właściwości mechaniczne
Opis:
The results of studies presented in this article are an example of the research activity of the authors related to lead-free alloys. The studies covered binary SnZn90 and SnZn95 lead-free alloys, including their microstructure and complex mechanical characteristics. The microstructure was examined by both light microscopy (LM) and scanning electron microscopy (SEM). The identification of alloy chemical composition in micro-areas was performed by SEM/EDS method. As regards light microscopy, the assessment was of both qualitative and quantitative character. The determination of the geometrical parameters of microstructure was based on an original combinatorial method using phase quantum theory. Comprehensive characterization of mechanical behavior with a focus on fatigue life of alloys was performed by means of the original modified low cycle fatigue method (MLCF) adapted to the actually available test machine. The article discusses the fatigue life of binary SnZn90 and SnZn95 alloys in terms of their microstructure. Additionally, the benefits resulting from the use of the combinatorial method in microstructure examinations and MLCF test in the quick estimation of several mechanical parameters have been underlined.
Źródło:
Archives of Foundry Engineering; 2018, 18, 4; 65-70
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
New Funnel Shaped Nozzle for Evaluation of the Mechanical Properties of Woven Fabric by the Extraction Method
Nowy typ dysz lejkowych dla oceny mechanicznych właściwości tkanin metodą ekstrakcji
Autorzy:
Dehghan-Manshadi, N
Alamdar-Yazdi, A.
Bidoki, S M
Powiązania:
https://bibliotekanauki.pl/articles/233663.pdf
Data publikacji:
2014
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Biopolimerów i Włókien Chemicznych
Tematy:
extraction method
force–displacement curve
mechanical properties
woven fabrics
metoda ekstrakcji
siła-odkształcenie krzywej
właściwości mechaniczne
tkaniny
Opis:
Current methods of mechanical property evaluation of fabrics such as the KESF and FAST systems employ several testing devices for measuring tensile, shearing and bending characteristics separately. In this research a new facile and efficient extraction method for simultaneous estimation of different mechanical properties using a funnel-shape nozzle is introduced. The tensile, shearing and bending properties of 84 woven fabric samples were measured using standard methods and subsequently circular specimens of these fabrics were extracted through the funnel shaped nozzle. Sixteen different parameters were graphically selected from the force-displacement curves obtained, and the correlation between these parameters with the experimental mechanical properties was calculated. Finally stepwise multiple linear regression analysis was applied to acquire the best equation for predicting the mechanical properties of the fabrics. Our findings revealed that the shear stiffness and tensile strength can be objectively evaluated by measuring the initial slope (S1) and maximum load (Pmax) on the load-displacement curve. The maximum load in the 4th zone (Fmax) of the graph was introduced as an objective measure of the bending rigidity and tensile module in the warp direction. The area of curve (A) can be used for objective evaluation of bending rigidity in the weft and bias directions.
Obecnie stosowane metody oceny mechanicznych właściwości płaskich materiałów tekstylnych takie jak KESF i FAST wykorzystują rożnego rodzaju urządzenia dla pomiaru i niezależnego określenia charakterystyk rozciągania, ścinania i zginania. W pracy przedstawiono nową wydajną metodę równoczesnej oceny kilku mechanicznych właściwości materiałów przy zastosowaniu dyszy o lejkowatym kształcie. Dla przeprowadzenia badań przygotowano 84 próbki tkanin, które sprawdzono standardowymi metodami, a następnie przeciągnięto przez lejkowatą dyszę rejestrując jednocześnie charakterystyki siły w funkcji wydłużenia. Z tych wykresów wyznaczono 16 parametrów, które skorelowano z uzyskanymi poprzednio właściwościami tkanin oraz poddano analizie statystycznej. Wykazano, że sztywność ścinania i wytrzymałość na rozciąganie można obiektywnie określić z początkowego nachylenia charakterystyki siła-wydłużenie. Maksymalna siła w 4-tej strefie wykresu została skojarzona ze sztywnością zginania i modułem rozciągania w kierunku osnowy. Powierzchnia pod krzywą może stanowić obiektywną miarę w sztywności zginania w kierunku wątku i kąta rozciągania 45 stopni.
Źródło:
Fibres & Textiles in Eastern Europe; 2014, 2 (104); 47-52
1230-3666
2300-7354
Pojawia się w:
Fibres & Textiles in Eastern Europe
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of fiber orientation and fiber loading on the mechanical and thermal properties of sugar palm yarn fiber reinforced unsaturated polyester resin composites
Wpływ orientacji włókien palmy cukrowej i ich zawartości na właściwości mechaniczne i termiczne kompozytów na bazie nienasyconej żywicy poliestrowej
Autorzy:
Mohd Nurazzi, N.
Khalina, A.
Chandrasekar, M.
Aisyah, H. A.
Ayu Rafiqah, S.
Ilyas, R. A.
Hanafee, Z. M.
Powiązania:
https://bibliotekanauki.pl/articles/947398.pdf
Data publikacji:
2020
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Chemii Przemysłowej
Tematy:
sugar palm fibers
unsaturated polyester resin
different fiber orientation
fiber loading
mechanical properties
thermal properties
włókno palmy cukrowej
nienasycona żywica poliestrowa
kompozyty
orientacja włókien
udział włókien
właściwości mechaniczne
właściwości termiczne
Opis:
Sugar palm [Arenga pinnata (Wurmb.) Merr] fiber reinforced unsaturated polyester resin composites with 0°, 45°, and 90° fiber different orientations were prepared and tested. The composites were characterized for tensile, flexural, impact and compression properties using ASTM D3039, ASTM D790, ASTM D250, and ASTM D3410 standards, respectively. For the thermal characterization, dynamic mechanical analysis (DMA) was conducted to characterize the on storage modulus (E’), loss modulus (E’’) and damping behavior (tan δ) of the composites. The highest mechanical performance of composites was achieved at 0° of fiber orientation composites followed by 45° and 90° fiber orientations. The fiber loading was insignificant for the 90° fiber orientation as the properties were inconsistent. The theoretical value of modulus from the tensile test was calculated using rules of mixture (ROM) and compared with the experimental values for all composites specimens. This research showed that the optimum properties occurred at 30 wt % fiber loading as reflected by the superior tensile and flexural strengths. The optimum properties of compression, impact, storage modulus and better damping properties were achieved at 40 wt % fiber loading.
Przygotowano kompozyty na bazie nienasyconej żywicy poliestrowej wzmocnionej różną ilością włókien palmy cukrowej [Arenga pinnata (Wurmb.) Merr] o rozmaite jorientacji: 0°, 45° i 90°. Z zastosowaniem norm, odpowiednio, ASTM D3039, ASTM D790, ASTM D250 i ASTM D3410 oznaczono wytrzymałość na rozciąganie i zginanie oraz odporność na uderzenie i ściskanie otrzymanych kompozytów. Właściwości termiczne scharakteryzowano metodą dynamicznej analizy mechanicznej (DMA); wyznaczono moduł zachowawczy (E’), moduł stratności (E”) i tangens kąta stratności (tan δ) kompozytów. Najlepsze właściwości mechaniczne kompozytów uzyskano w wypadku zastosowania włókien o orientacji 0° względem przyłożonej siły, a najgorsze w wypadku ułożenia włókien pod kątem 90°. W odniesieniu do kompozytów wzmocnionych włóknami o orientacji 90° udział włókien miał nieistotny wpływ na oznaczane właściwości, ponieważ wyniki były niespójne. Wartość teoretyczną modułu rozciągania wszystkich próbek kompozytów obliczono z wykorzystaniem reguły mieszania (ROM) i porównano z wartościami uzyskanymi doświadczalnie. Stwierdzono, że doskonałą wytrzymałość na rozciąganie i zginanie wykazywał kompozyt z 30 % mas. udziałem włókien, podczas gdy optymalne: wytrzymałość na ściskanie, udarność, moduł zachowawczy i właściwości tłumiące uzyskano w wypadku udziału 40 % mas. włókien.
Źródło:
Polimery; 2020, 65, 2; 115-124
0032-2725
Pojawia się w:
Polimery
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-12 z 12

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies