Tytuł:
Investigation of Microstructure of ZnO Varistors Taken From Surge Arrester Counters
Autorzy:
Papliński, P.
Wańkowicz, J.
Ranachowski, P.
Ranachowski, Z.
Powiązania:
https://bibliotekanauki.pl/articles/355223.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
surge arrester counter
ZnO varistors
microstructure of ceramics
ceramic material degradation
Opis:
The paper presents investigations of microstructure of varistors of damaged surge arrester counters. A similar ZnO varistor, not subjected before to operation, was a point of reference in this research. The results of investigations of the ZnO varistors show an untypical phase composition of their material, which was characterized by unsatisfying homogeneity and cohesion. The degradation processes of varistor material in the subsequent stages were recognized and described. A harmful impact of humidity inside the untight surge arrester counter on its operation and its ZnO varistors was proved. Some conclusions being the result of the operation checking of surge arrester counters were presented too.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 1; 191-196
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparative Studies on Degradation of Varistors Subjected to Operation in Surge Arresters and Surge Arrester Counters
Autorzy:
Papliński, P.
Wańkowicz, J.
Śmietanka, H.
Ranachowski, P.
Ranachowski, Z.
Kudela, S. jr.
Aleksiejuk, M.
Powiązania:
https://bibliotekanauki.pl/articles/351611.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
surge arrester
surge arrester counter
MO varistor
microstructure of ceramics
ceramic material degradation
Opis:
The paper presents results of investigation of microstructure and micro-hardness for material of ZnO varistors applied to 110 kV surge arrester and surge arrester counter. The research combined two pairs of varistors, each consisted of one varistor subjected before to operation, while the other one was brand new unit and constituted a reference. All varistors were made of the same material by the reputable manufacture. The tests revealed a different degree of the material degradation for varistors subjected before to operation. This also refers to different degradation mechanism observed for the material of these varistors, if typical effects of degradation of aged ZnO varistors were considered as a reference. Physical state of spinel in the microstructure had a significant impact on the material degradation, however a considerable loosening of the microstructure associated with bismuth oxide was observed too. It was surprising, since the precipitates of the bismuth oxide phase most often showed very good binding to the ZnO matrix and high resistance to associated electrical, thermal and mechanical effects. The degradation effects in the ZnO matrix proved to be limited only.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 1; 367-374
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies