Tytuł:
Electrochemical Deposition of Silver on Aluminum Alloys
Autorzy:
Valov, R.
Petkov, V.
Valkanov, S.
Powiązania:
https://bibliotekanauki.pl/articles/946872.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
silver plating
aluminum alloys
diamond nanoparticles
SEM
posrebrzanie
stopy aluminium
nanocząsteczki diamentu
Opis:
Silver coatings have a very high reflection ability. To avoid their darkening from the hydrogen sulphide in the air, a thin layer of heat-resistant colorless lacquer is applied to the coatings. Silver plating is mainly used in jewelery, optics, electronics and electrical engineering. Depending on their application the thickness of the layer may vary from 2 to 24 μm. It can be done in several ways: chemical, electrochemical, contact, etc. The most common way of silver plating is the electrochemical deposition using cyanide and non-cyanide electrolytes. The cyanide electrolytes produce light, fine crystalline, dense and plastic coatings upon silver-plating. Usually silver coatings are applied with copper or nickel intermediate layer. In order to improve the de-oxidation of the aluminum surface new chemical treatment in acid – alkaline solution was applied. Our previous research shows that the presence of diamond nanoparticles in the electrolyte increase the metal deposition. Samples were prepared from electrolyte containing 10 g/l diamond nanoparticles. Their properties were compared to the properties of reference samples. The diamonds were obtained by detonation synthesis. The aim of this study is to obtain electrochemically deposited silver layer with high density, adhesion and electric conductivity on aluminum alloys substrate. The coating was directly plated without intermediate layer. Non-cyanide electrolyte composition and electrochemical parameters were determined in order to produce Ag coatings on Al alloy substrate without intermediate layer. The coating is with good adhesion, density and thickness of 14-23 μm.
Źródło:
Archives of Foundry Engineering; 2020, 20, 2; 101-104
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies