Modelling of microstructure changes during hot deformation using cellular automata
Modelowanie za pomocą automatów komórkowych zmian mikrostruktury podczas odkształcenia na gorąco
Autorzy:
Kuc, D.
Gawąd, J.
Powiązania:
https://bibliotekanauki.pl/articles/351296.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
modelowanie
automaty komórkowe
stal austenityczna
mikrostruktura
modelling
cellular automata
austenitic steel
flow stress
microstructure
Opis:
The paper is focused on an application of the cellular automata (CA) method to description of microstructure changes in continuous deformation condition. The model approach consists of Cellular Automata model of microstructure development and the thermal-mechanical finite element (FE) code. Dynamic recrystallization phenomenon is taken into account in 2D CA model which takes advantage of explicit representation of microstructure, including individual grains and grain boundaries. Flow stress is the main material parameter in mechanical part of FE and is calculated on the basis of average dislocation density obtained from the CA model. The results obtained from the model were validated with the experimental data. In the present study, austenitic steel X3CrNi18-10 was investigated. The examination of microstructure for the initial and final microstructures was carried out, using light microscopy, transmission electron microscopy and EBSD technique. Compression forces were recorded during the tests and flow stresses were determined using the inverse method.
W artykule przedstawiono model, który opisuje zmiany struktury w warunkach ciągłego odkształcenia z wykorzystaniem automatów komórkowych. Opracowane rozwiązanie wykorzystuje połączenie modelu automatów komórkowych (ang. Cellular Automata, CA) zmian mikrostruktury i kodu elementów skończonych rozwiązującego problem termomechaniczny. Do opracowania modelu zmian mikrostruktury wykorzystano dwuwymiarową siatkę automatów komórkowych. Model zmian naprężenia uplastyczniającego bazuje na średniej gęstości dyslokacji wyliczonej poprzez homogenizację gęstości dyslokacji w siatce automatów komórkowych. Opracowany model zweryfikowano w oparciu o wyznaczone krzywe płynięcia dla stali austenitycznej X3CrNi18-10 i badania mikrostruktury z wykorzystaniem mikroskopii świetlnej, transmisyjnej mikroskopii elektronowej oraz techniki EBSD. Naprężenie uplastyczniające zostało wyznaczone w oparciu o metodę obliczeń odwrotnych na podstawie danych uzyskanych z prób osiowosymetrycznego ściskania.
Źródło:
Archives of Metallurgy and Materials; 2011, 56, 2; 523-532
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Obróbka plastyczna stopów magnezu
Plastic forming of magnesium alloys
Autorzy:
Hadasik, E.
Kuc, D.
Powiązania:
https://bibliotekanauki.pl/articles/212078.pdf
Data publikacji:
2013
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Obróbki Plastycznej
Tematy:
stopy magnezu
charakterystyki plastyczności
mikrostruktura
walcowanie
kucie
wyciskanie
magnesium alloys
plasticity characteristics
microstructure
rolling
forging
extrusion
Opis:
W artykule, który ma charakter przeglądowy, wskazano na rosnące zainteresowanie w ostatnich latach stopami magnezu do zastosowań na elementy środków transportu. Podano klasyfikację stopów magnezu do obróbki plastycznej, metody wytwarzania wyrobów drogą walcowania, wyciskania i kucia oraz wskazano trudności przy realizacji procesów kształtowania plastycznego. W badaniach stopów AZ31, AZ61, AZ80 i WE43 przedstawiono relacje pomiędzy strukturą, a parametrami odkształcania. Wskazano na występowanie dwóch mechanizmów odkształcania w zależności od temperatury: poślizgu i bliźniakowania. Podano zależności pomiędzy wielkościami charakteryzującymi plastyczność a parametrem Zenera–Hollomona. Przedstawiono wyniki prowadzonych prac w zakresie procesów obróbki plastycznej stopów magnezu - walcowania, kucia oraz wyciskania oraz przykłady wykonanych wyrobów.
The article that is a review indicates a growing interest in magnesium alloys concerning applications related to the elements of means of transport over the last few years. It specifies a classification of magnesium alloys intended for plastic forming as well as rolling, extrusion and forging production methods, and, additionally, difficulties connected with plastic forming processes. In the tests of the alloys AZ31, AZ61, AZ80 and WE43 there are presented relations between a structure and deformation parameters. The study shows two deformation mechanisms, i.e. slip and twinning that appear depending on the temperature. Furthermore, the paper lists relationships between the values describing plasticity and the Zener-Hollomon parameter. It also presents results of researches performed within the scope of magnesium alloy plastic forming processes - rolling, forging and extrusion, and examples of manufactured products.
Źródło:
Obróbka Plastyczna Metali; 2013, 24, 2; 131-146
0867-2628
Pojawia się w:
Obróbka Plastyczna Metali
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Cumulative Plastic Deformation on Microstructure of the Fe-Al Intermetallic Phase Base Alloy
Wpływ skumulowanego odkształcenia plastycznego na strukturę stopów Fe-Al na osnowie faz międzymetalicznych
Autorzy:
Bednarczyk, I.
Kuc, D.
Niewielski, G.
Powiązania:
https://bibliotekanauki.pl/articles/350991.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
FeAl alloy
Max train simulator
cumulative plastic deformation
microstructure
stop Fe-Al
symulator MaxStrain
skumulowane odkształcenie plastyczne
mikrostruktura
Opis:
This article is part of the research on the microstructural phenomena that take place during hot deformation of intermetallic phase-based alloy. The research aims at design an effective thermo - mechanical processing technology for the investigated intermetallic alloy. The iron aluminides FeAl have been among the most widely studied intermetallics because their low cost, low density, good wear resistance, easy of fabrication and resistance to oxidation and corrosion. There advantages create wide prospects for their industrial applications for components of machines working at a high temperature and in corrosive environment. The problem restricting their application is their low plasticity and their brittle cracking susceptibility, hampers their development as construction materials. Consequently, the research of intermetallic-phase-based alloys focuses on improvement their plasticity by hot working proceses. The study addresses the influence of deformation parameters on the structure of an Fe-38% at. Al alloy with Zr, B Mo and C microadditions, using multi – axis deformation simulator. The influence of deformation parameters on microstructure and substructure was determined. It was revealed that application of cumulative plastic deformation method causes intensive reduction of grain size in FeAl phase base alloy.
Prezentowana praca stanowi element prowadzonych badań nad możliwością kształtowania stopów na osnowie faz międzymetalicznych z układu Fe-Al drogą obróbki cieplno-plastycznej. Związki międzymetaliczne są traktowane jako przyszłościowe materiały do pracy w wysokich temperaturach i agresywnych środowiskach korozyjnych. Zainteresowanie tą grupą materiałową jest spowodowane dobrymi właściwościami użytkowymi: dobrą odpornością na utlenianie i korozję w środowisku wody morskiej, zużycie ścierne. Ponadto niskie koszty materiałowe stwarzają perspektywy do zastosowań jako alternatywę dla stali odpornych na korozję. Ograniczeniem możliwości szerokiego zastosowania intermetalików z układu Fe-Al, jest ich niedostateczna plastyczność, będąca czynnikiem hamującym ich dalszy rozwój jako materiałów konstrukcyjnych. Stąd badania nad możliwością poprawy plastyczności droga obróbki cieplno-plastycznej. W artykule analizowano wpływ parametrów odkształcania na mikrostrukturę stopu Fe-38% at. Al z mikododatkami cyrkonu, molibdenu, boru węgla. Z wykorzystaniem symulatora Maxstrain, który umożliwa kumulację dużych odkształceń w materiale. Przeprowadzono badania mikrostuktury i substruktury wykazały istotny wpływ odkształcania tą metodą na rozdrobnienie ziarn w badanym stopie.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 3; 987-991
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Characteristics of plasticity and microstructure of hot forming magnesium alloys Mg-Al-Zn type
Charakterystyki plastycznosci i mikrostruktura odkształcanych na gorąco stopów magnezu typu Mg-Al-Zn
Autorzy:
Kuc, D.
Hadasik, E.
Schindler, I.
Kawulok., P.
Śliwa, R.
Powiązania:
https://bibliotekanauki.pl/articles/350870.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop magnezu
badania plastyczności
mikrostruktura
energia aktywacji
magnesium alloy
research of plasticity
microstructure
dynamic recrystallization
activation energy
Opis:
The paper presents analysis of plasticity characteristics and microstructure of magnesium alloys for hot plastic treatment with different aluminium content (3÷8%). Tests were conducted for assessment of susceptibility of tested alloys to hot plastic deformation. A tensile test was run in temperature from 250 to 450°C. Based on the results, ultimate tensile strength (UTS) and reduction of area (Z) were determined for samples. Conducted compression tests allowed to specify the flow stress and microstructure changes after deformation. The activation energy in hot forming was determined for investigated alloys. The parameters of the process where flow is significantly influenced by twin formation in microstructure were determined. A varied plasticity of tested alloys was found depending on aluminium content. Test results will be useful in development of forging technology of selected construction elements which serve as light substitutes for currently used materials.
W pracy analizowano charakterystyki plastyczności i mikrostrukturę stopów magnezu przeznaczonych do przeróbki plastycznej na gorąco ze zróżnicowana zawartością aluminium (3-8%). Badania prowadzono dla oceny podatności badanych stopów do kształtowania plastycznego w warunkach przeróbki plastycznej na gorąco. Przeprowadzono próbę rozciągania w temperaturze od 250 do 450 st.C, na podstawie której określono wytrzymałość na rozciąganie i przewężenie badanych próbek. Wykonane próby ściskania pozwoliły na wyznaczenie naprężenia uplastyczniajacego i zmian mikrostruktury po odkształceniu. Dla badanych stopów wyznaczono energię aktywacji odkształcenia plastycznego na gorąco. Określono parametry procesu, dla których na przebieg plastycznego płynięcia wpływa istotnie bliźniakowanie w mikrostrukturze. Wykazano zróżnicowaną plastyczność badanych stopów w zależności od zawartości aluminium. Wyniki badań będą pomocne do opracowania technologii kucia wybranych elementów konstrukcyjnych stanowiących lekkie zamienniki stosowanych obecnie materiałów.
Źródło:
Archives of Metallurgy and Materials; 2013, 58, 1; 151-156
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies