Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Kawiński, M." wg kryterium: Autor


Wyświetlanie 1-2 z 2
Tytuł:
Ductile Cast Iron Microstructure Adjustment by Means of Heat Treatment
Autorzy:
Mróz, M.
Orłowicz, A. W.
Tupaj, M.
Kupiec, B.
Kawiński, M.
Powiązania:
https://bibliotekanauki.pl/articles/947626.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ductile cast iron
heat treatment
microstructure
żeliwo sferoidalne
obróbka cieplna
mikrostruktura
Opis:
The study presented in this paper concerned the possibility to apply a heat treatment process to ductile cast-iron thin-walled castings in order to remove excessive quantities of pearlite and eutectic cementite precipitates and thus meet the customer’s requirements. After determining the rates of heating a casting up to and cooling down from 900°C feasible in the used production heat treatment furnace (vh = 300°C/h and vc = 200°C/h, respectively), dilatometric tests were carried out to evaluate temperatures Tgr, TAc1start, TAc1end, TAr1start, and TAr1end. The newly acquired knowledge was the base on which conditions for a single-step ferritizing heat treatment securing disintegration of pearlite were developed as well as those of a two-step ferritization process guaranteeing complete disintegration of cementite and arriving at the required ferrite and pearlite content. A purely ferritic matrix and hardness of 119 HB was secured by the treatment scheme: 920°C for 2 hours / vc = 60°C/h / 720°C for 4 hours. A matrix containing 20–45% of pearlite and hardness of 180–182 HB was obtained by applying: 920°C for 2 hours or 4 hours / vc = 200°C/h to 650°C / ambient air.
Źródło:
Archives of Foundry Engineering; 2020, 20, 3; 37-40
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ultrasonic Testing of Vermicular Cast Iron Microstructure
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, M.
Kupiec, B.
Pająk, D.
Kawiński, M.
Powiązania:
https://bibliotekanauki.pl/articles/1837866.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
vermicular cast iron
vermiculatization method
microstructure
ultrasonic testing
graphite precipitation surface density
żeliwo wermikularne
wermikulatyzacja
mikrostruktura
badanie ultradźwiękowe
Opis:
The paper presents results of a study on the effect of passage of time on magnesium content in iron alloys and the effect of magnesium content on the number of vermicular graphite precipitations per unit surface area and value of the longitudinal ultrasonic wave velocity for two different vermicularization methods. The study was carried out with the use of inspection bar castings. For specific production conditions, it has been found that in case of application of both the cored wire injection method and the method of pouring liquid metal over magnesium master alloy on ladle bottom, the satisfactory level of magnesium content in the bottom-pour ladle, for which it was still possible to obtain castings with vermicular graphite, was 0.018% Mg. In case of the cored wire injection method, the “time window” available to a pouring station at which castings of vermicular cast iron are expected to be obtained, was about 5 minutes. This corresponds to the longitudinal ultrasonic wave velocity values exceeding 5500 m/s and the number of graphite precipitations per unit surface area above 320 mm-2. In case of the master alloy method, the respective “time window” allowing to obtain castings of vermicular cast iron was only about 3 minutes long. This corresponds to the longitudinal ultrasonic wave velocity value above 5400 m/s and the number of graphite precipitations per unit surface area above 380 mm-2.
Źródło:
Archives of Foundry Engineering; 2020, 20, 4; 36-40
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies