Tytuł:
Comparison of Microstructure and Mechanical Properties of Cast Steel Carried out on Cast-on Samples and Samples Cast Separately
Autorzy:
Kalandyk, B. E.
Zapała, R. E.
Powiązania:
https://bibliotekanauki.pl/articles/1837717.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
cast steel
cast-on samples
heat treatment
mechanical properties
metallography
staliwo
próbki odlewu
obróbka cieplna
właściwości mechaniczne
metalografia
Opis:
The results of microstructure examinations and UTS, YS, El, RA carried out on low-carbon cast steel containing 0.15% C. The tests were carried out on specimens cut out from samples cast on a large-size casting and from samples cast in separate foundry moulds. It has been shown that significant differences in grain size observed in the material of the separately cast samples and cast-on samples occur only in the as-cast. In the as-cast state, in materials from different tests, both pearlite percent content in the structure and mean true interlamellar spacing remain unchanged. On the other hand, these parameters undergo significant changes in the materials after heat treatment. The mechanical properties (after normalization) of the cast-on sample of the tested cast steel were slightly inferior to the values obtained for the sample cast in a separate foundry mould. The microscopic examinations of the fracture micro-relief carried out by SEM showed the presence of numerous, small non-metallic inclusions, composed mainly of oxide-sulphides containing Mn, S, Al, Ca and O, occurring individually and in clusters.
Źródło:
Archives of Foundry Engineering; 2021, 21, 2; 81-88
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Tempering Temperature on the Mechanical Properties of Cast L35HM Steel
Autorzy:
Zapała, R.
Kalandyk, B.
Wawro, P.
Powiązania:
https://bibliotekanauki.pl/articles/380169.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
heat treatment
mechanical properties
cast L35HM steel
tempering
quenching
obróbka cieplna
właściwości mechaniczne
odlewy ze stali
Opis:
A possibility to control the strength, hardness and ductility of the L35HM low-alloy structural cast steel by the applied tempering temperature is discussed in the paper. Tests were carried out on samples taken from the two randomly selected industrial melts. Heat treatment of the cast samples included quenching at 900°C, cooling in an aqueous solution of polymer, and tempering at 600 and 650°C. The obtained results showed that the difference in the tempering temperature equal to 50°C can cause the difference of 121 MPa in the values of UTS and of 153 MPa in the values of 0.2%YS. For both melts tempered at 600 °C, the average values of UTS and 0.2%YS were equal to 995 MPa and 933 MPa, respectively. The values of EL and RA did not show any significant differences. Attention was drawn to large differences in strength and hardness observed between the melts tempered at 600 and 650°C. Despite differences in the mechanical properties of the examined cast steel, the obtained results were superior to those specified by the standard.
Źródło:
Archives of Foundry Engineering; 2017, 17, 2; 151-156
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Vanadium Microaddition on the Strength of Low-Carbon Cast Steel at Elevated Temperatures
Autorzy:
Kalandyk, B. E.
Zapała, R. E.
Pałka, P.
Powiązania:
https://bibliotekanauki.pl/articles/946865.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
low-carbon cast steel
microaddition elements
mechanical properties
temperature
staliwo niskowęglowe
elementy mikrododycji
właściwości mechaniczne
temperatura
Opis:
The effect of vanadium microaddition on the strength of low-carbon cast steel containing 0.19% C used, among others, for castings of slag ladles was discussed. The tested cast steel was melted under laboratory conditions in a 30 kg capacity induction furnace. Mechanical tests were carried out at 700, 800 and 900°C using an Instron 5566 machine equipped with a heating oven of ± 2°C stability. Non-standard 8- fold samples with a measuring length of 26 mm and a diameter of 3 mm were used for the tests. It has been shown that, compared to cast steel without vanadium microaddition, the introduction of vanadium in an amount of 0.12% to unalloyed, low carbon cast steel had a beneficial effect on the microstructure and properties of this steel not only at ambient temperature but also at elevated temperatures when it promoted an increase in UTS and YS. The highest strength values were obtained in the tested cast steel at 700°C with UTS and YS reaching the values of 193 MPa and 187.7 MPa, respectively, against 125 MPa and 82.8 MPa, respectively, obtained without the addition of vanadium. It was also found that with increasing test temperature, the values of UTS and YS were decreasing. The lowest values of UTS and YS obtained at 900°C were 72 MPa and 59.5 MPa, respectively, against 69 MPa and 32.5 MPa, respectively, obtained without the addition of vanadium.
Źródło:
Archives of Foundry Engineering; 2020, 20, 2; 79-83
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Microstructure and Mechanical Properties of High-Alloyed 23Cr-5Mn-2Ni-3Mo Cast Steel
Mikrostruktura i właściwości mechaniczne wysokostopowego staliwa 23Cr-5Mn-2Ni-3Mo
Autorzy:
Kalandyk, B.
Zapała, R.
Kasińska, J.
Wróbel, M.
Balicki, M.
Powiązania:
https://bibliotekanauki.pl/articles/356347.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
duplex stainless cast steels
microstructure
solution annealing
mechanical properties
staliwo typu duplex
mikrostruktura
roztwór do wyżarzania
właściwości mechaniczne
Opis:
The article presents the microstructure and mechanical properties of cast duplex stainless steel type 23Cr-5Mn-2Ni-3Mo. It has been shown that the structure of the tested cast steel is composed of ferrite enriched in Cr, Mo and Si, and austenite enriched in Mn and Ni. In the initial state, at the interface, precipitates rich in Cr and Mo were present. A high carbon content (0.08%C) in this cast steel indicates that probably those were complex carbides of the M23C6 type and/or σ phase. Studies have proved that the solution annealing conducted at 1060°C was not sufficient for their full dissolution, while at the solutioning temperature of 1150°C, the structure of the tested material was composed of ferrite and austenite. Partial replacement of Ni by two other austenite-forming elements, which are Mn and N, has ensured obtaining mechanical properties comparable to cast duplex 24Cr-5Ni-3Mo steel of the second generation. Basing on the results of static tensile test, a twice higher yield strength was proved to be obtained, compared to the cast austenitic 18Cr-9Ni and 19Cr-11Ni-2Mo steel commonly used in the foundry industry. In addition to the high yield strength (YS = 547 ÷ 572 MPa), the tested cast steel was characterized by the following mechanical properties: UTS = 731 ÷ 750 MPa, EL = 21 ÷ 29.5%, R.A. = 43 ÷ 52%, hardness 256 ÷ 266 HB. Fractures formed in mechanical tests showed ductile-brittle character.
W artykule przedstawiono mikrostrukturę i właściwości mechaniczne, kwasoodpornego staliwa ferrytyczno - austenitycznego 23Cr-5Mn-2Ni-3Mo typu duplex. Wykazano, że struktura badanego staliwa składa się z ferrytu δ wzbogaconego w C r, Mo i S i oraz austenitu wzbogaconego w Mn i Ni. W stanie wyjściowym na granicy międzyfazowej występują wydzielenia wzbogacone w C r i Mo. Wysoka zawartość C (0.08%) w tym staliwie wskazuje, że prawdopodobnie są to złożone węgliki M23C6 i/lub faza σ. Wykazano, że temperatura przesycania 1060°C nie jest wystarczająca do ich całkowitego rozpuszczenia. Natomiast w temperaturze przesycania 1150°C struktura badanego materiału składa się z ferrytu i austenitu. Częściowe zastąpienie Ni przez dwa inne pierwiastki austenitotwórcze jakimi są Mn i N zapewniło uzyskanie porównywalnych właściwości mechanicznych do staliwa duplex 24Cr-5Ni-3Mo drugiej generacji. Na podstawie przeprowadzonej statycznej próby rozciągania wykazano dwukrotnie wyższą granicę plastyczności w porównaniu do często stosowanego w przemyśle odlewniczym austenitycznego staliwa 18Cr-9Ni i 19Cr-11Ni-2Mo. Poza wysoką granicą plastyczności (Rp0,2 = 547 ÷ 572 MPa), badane staliwo charakteryzowało się następującymi właściwościami mechanicznymi: Rm = 731 ÷ 750 MPa, As = 21 ÷ 29,5%, Z = 43 ÷ 52%, HB = 256 ÷ 266. Przełomy po badaniach wytrzymałościowych wykazywały charakter ciagliwo-kruchy.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 4; 2529-2534
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies