Tytuł:
Atmospheric pressure leaching of nickel from a low-grade nickel-bearing ore
Autorzy:
Javanshir, S.
Mofrad, Z. H.
Azargoon, A.
Powiązania:
https://bibliotekanauki.pl/articles/110534.pdf
Data publikacji:
2018
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
leaching
kinetics
calcination
laterite ore
nickel recovery
Opis:
This study focused on the extraction of nickel from a low-grade lateritic ore. The characterization of representative samples was done by X-ray diffraction (XRD), X-ray fluorescence (XRF), and microscopic mineralogical studies. Nickel was uniformly distributed in iron (hydr)oxide minerals. The pre-concentration of nickel was attempted by magnetic separation, but was unsuccessful. The effect of the type of lixiviant, acid concentration, S/L ratio, time, and temperature were investigated in the atmospheric leaching process. Based on the experimental data, optimum conditions for the maximum recovery of nickel were determined under the following conditions: 5 M H2SO4, 25% (w/v), 90 ºC, and two hours. Pre-calcination, for increasing nickel extraction by converting goethite to hematite, was carried out on raw ores at different times (30-180 minutes) and temperatures (180-540 ºC). Recovery was found increasing from 69 to 95% under the same conditions. Kinetic studies were conducted by fitting the data with Shrinking Core (SC) models. The study determined, from the estimate of activation energy, that the rate of reaction controlled by chemical reaction.
Źródło:
Physicochemical Problems of Mineral Processing; 2018, 54, 3; 890-900
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Separation of nickel and iron from lateritic ore using a digestion – roasting – leaching – precipitation process
Autorzy:
Basturkcu, H.
Acarkan, N.
Powiązania:
https://bibliotekanauki.pl/articles/109861.pdf
Data publikacji:
2016
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
laterite
digestion
roasting
salt addition
leaching
precipitation
Opis:
This paper investigates extraction of nickel and iron from a lateritic nickel ore from the Caldag region of Manisa in Turkey. The ore sample contains 1.2% Ni, 24.77% Fe and 0.062% Co. The process applied includes digestion with 40 wt-% sulfuric acid at 200 C for 60 min, roasting at 700 C for 15 min, leaching with water for 30 min at 1:5 solid/liquid ratio (by weight) and precipitation of the remaining iron at pH 3 and 60 C. In order to improve nickel and cobalt extractions using the digestion-roasting- leaching-precipitation process (DRLP), Na2SO4 addition in the roasting stage was examined. Under the optimum conditions and in the presence of Na2SO4, 86.2% Ni and 94.2% Co extractions were obtained with almost zero iron content. As a result, 2.07 g dm-3 Ni, 0.12 g dm-3 Co and 0.05 g dm-3 Fe could be achieved in the pregnant leach solution within nearly 2.5 hours.
Źródło:
Physicochemical Problems of Mineral Processing; 2016, 52, 2; 564-574
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies