Comparative study on the effect of using conventional and high pressure grinding rolls crushing on the ball mill grinding kinetics of an iron ore
Autorzy:
Barani, K.
Balochi, H.
Powiązania:
https://bibliotekanauki.pl/articles/109893.pdf
Data publikacji:
2016
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
high pressure grinding rolls
HPGR
grinding
iron ore
Opis:
The effect of using conventional and high pressure grinding rolls (HPGR) crushing on the ball mill grinding of an iron ore was assessed to determine how these different comminution processes affect the ball mill grinding kinetic. For this purpose, the sample was obtained from the Jalalabad Iron Ore Mine and crushed by conventional crusher and HPGR. Then, the crushing products were ground in a laboratory ball mill. Five single-sized fractions of (–4+3.15 mm), (–2+1.7 mm), (–1+0.850 mm), (–0.500+0.420 mm), and (–0.212+0.180 mm) were selected as the ball mill feed. The specific rates of breakage (Si) and cumulative breakage distribution function (Bi,j) values were determined for those size fractions. It was found that for all fraction the Bi,1 values of the HPGR product were higher than those for the crusher product. It means that the particles produced by the dry ball milling of the HPGR product were finer than by the crusher. Also, the results showed that the specific breakage rate of the material crushed by HPGR at coarse fractions (–4+3.15 mm, -2+1.7 mm, and -1+0.850 mm) was higher than the material crushed by conventional crushers. However, at fine fractions (–0.500+0.420 mm and -0.212+0.180 mm), there was a small difference and the specific breakage rates were the same. This issue can be explained by the fact, that for coarse fractions the particles had longer side surfaces and thus were more affected by the lateral pressure. The results of verification test showed that after 60 seconds of grinding the 80% passing size of the HPGR and crusher products (D80) were reduced from 3311 μm to 760 μm and 1267 μm, respectively.
Źródło:
Physicochemical Problems of Mineral Processing; 2016, 52, 2; 920-931
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies